Fracture Toughness Evaluation for Sandia Mock-up Stainless Steel Canister Weldment Using Spiral Notch Torsion Fracture Toughness Test

Many radioactive materials within the nuclear fuel cycle present a significant hazard. Such materials include spent nuclear fuel, high-level waste, legacy waste and other nuclear materials that have no current outlet than storage. These materials are often held in long-term storage as an interim stage within their lifecycle. Lifecycles can include reuse or disposal. Safety and security of spent nuclear fuel (SNF) interim storage installations are very important, due to a great concentration of fission products, actinides and activation products. Stress corrosion cracking of interim storage containers has been identified as a high priority data gap by the Department of Energy. However, little has been done with regards to the canister weld material properties, including the fracture toughness, and their impact on stress corrosion, until recently from Sandia National Laboratory canister mockup program. Furthermore, because no post-weld heat treatment was required, the associated high tensile residual stress within these canister welds can drive the initiation and growth of stress corrosion cracking (SCC) cracks. Thus, the fracture mechanical property, such as fracture toughness, is an essential information to understand the canister weldment fracture resistance behavior and to support mitigation protocol development to counter SCC. In this work, we carried out fracture toughness evaluation on the received mock-up canister weldments from Sandia, using spiral notch torsion fracture test technology. The details of the weldment fracture toughness evaluation program development at ORNL are presented in this progress report. The objective of this research is to collect fracture toughness data on the mock-up canister weldment from Sandia National Laboratory. Data will be collected under quasi-static fracture loading using the Oak Ridge National Laboratory (ORNL) developed Spiral Notch Torsion Test (SNTT) technology carried out on a biaxial tension/torsion tester. These data will be used to support the ongoing SNF dry storage canister modeling activities and to address regulatory issues associated with canister container integrity and the follow-on SNF system transport reliability. SNTT has been a recent breakthrough in measuring fracture toughness for different materials, including metals, ceramics, concrete and polymers composites. Due to its high geometry constraint and unique loading condition, SNTT can be used to measure the fracture toughness with smaller specimens without concern of size effects. The application of SNTT to brittle materials has been proved to be successful. The micro-cracks induced by original notches in brittle materials could ensure crack growth in SNTT samples. Therefore, no fatigue pre-cracks are needed. The application of SNTT to the ductile material to generate valid toughness data will require a test sample with sufficient crack length to increase the sample fracture tip localized constraint. Fatigue pre-crack growth techniques are employed to introduce sharp crack front into the sample. Previously, only rough calculations were applied to estimate the compliance evolution in the SNTT crack growth process; while accurate quantitative descriptions have never been attempted. This generates an urgent need to understand the crack evolution during the SNTT fracture testing process of ductile materials. The newly developed governing equations for SNTT crack growth estimate are used to control the fatigue crack growth to effectively reaching the target crack length. The detailed SNTT approach and its estimated fracture toughness for the as-received Sandia canister weldment and the associated baseline 304 stainless steel are presented in this report. In the past SNTT technology has also been successfully applied to investigate the fracture behavior of X52 and X80 steels and the X52 welded materials used for hydrogen infrastructures. The current study in supporting Sandia SNF Dry Storage Mock-up Canister Program is the first attempt of applying SNTT to the highly ductile stainless steel and the associated weld materials. The SNTT test results indicate that SNTT method is a reliable test approach with good repeatability in applying to SS304 steel and SS304/308 weld material. The estimate JQ upon fracture for the baseline SS304 steel is at 1618 lb/in. The estimate JQ upon fracture for the SS304/308 weld from HAZ and weld specimens are 720 lb/in and 850 lb/in, respectively.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

CRACK GROWTH RESPONSE OF ALLOY 690 IN SIMULATED PWR PRIMARY WATER

The stress corrosion crack growth response of three extruded alloy 690 CRDM tube heats was investigated in several thermomechanical conditions. Extremely low propagation rates (< 1 x 10{sup -9} mm/s) were observed under constant stress intensity factor (K) loading at 325-350 C in the as-received, thermally treated (TT) materials despite using a variety of transitioning techniques. Post-test observation of the crack-growth surfaces revealed only isolated intergranular (IG) cracking. One-dimensional cold rolling to 17% reduction and testing in the S-L orientation did not promote enhanced stress corrosion rates. However, somewhat higher propagation rates were observed in a 30% cold-rolled alloy 690TT specimen tested in the T-L orientation. Cracking of the cold-rolled material was promoted on grain boundaries oriented parallel to the rolling plane with the % IG increasing with the amount of cold rolling.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

FY23 Update: Surface Sampling Activities for the Canister Deposition Field Demonstration

This report describes the results of a field demonstration of the proposed surface sampling techniques and plan for the multi-year Canister Deposition Field Demonstration (CDFD). The CDFD will evaluate salt deposition rates on three commercial 32PTH2 NUHOMS welded stainless steel storage canisters in Advanced Horizontal Storage Modules. Exposure testing is planned for up to 10 years and will incorporate periodic surface sampling campaigns. The goal of the planned dust sampling and analysis is to determine important environmental parameters that impact the potential occurrence of stress corrosion cracking on spent nuclear fuel (SNF) dry storage canisters. Specifically, measured dust deposition rates and deposited particle sizes will improve parameterization of dust deposition models employed to predict the potential occurrence and timing of stress corrosion cracks on the stainless steel SNF canisters. Previously, a preliminary sampling plan was developed, identifying possible sampling locations on the canister surfaces and sampling intervals; possible sampling methods were also described. Building from previous work, this report documents hand sampling from a spent nuclear fuel canister on a transfer skid mockup designed by Sandia National Laboratories. The sampling took place from a boom lift and salts were collected from mounted sample plates. The results of these efforts are presented in this report and compared to previous laboratory-controlled tests. The information obtained from the CDFD will be critical for ongoing efforts to develop a detailed understanding of the potential for stress corrosion cracking of SNF dry storage canisters.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Experimental Methods for the Performance Test of Environment-Assisted Cracking (EAC) in Nuclear Industry and Examples through NSUF

Environmentally assisted cracking (EAC) is a critical failure mode in nuclear reactor environments, where materials are exposed to high temperatures, radiation, and corrosive media. Specific EAC studies in nuclear environments include stress corrosion cracking in primary water chemistry, irradiation-assisted stress corrosion cracking (IASCC) under neutron exposure, and hydrogen induced cracking (HIC) in reactor pressure vessels. The experimental methodologies of EAC include slow strain rate testing (SSRT), constant load, and cyclic loading techniques, conducted in autoclaves designed to simulate the reactor’s operational environments. This paper highlights several experimental case studies, especially on IASCC, conducted within the Nuclear Science User Facilities (NSUF).

36 - MATERIALS SCIENCE↗

The corrosion performance of die-cast magnesium alloy MRI230D in 3.5% NaCl solution saturated with Mg(OH){sub 2}

The environmental behavior of die-cast magnesium alloy MRI230D designated for high-temperature applications was evaluated in comparison with regular AZ91D alloy. The microstructure examination was carried out using SEM, TEM, and X-ray diffraction analysis; the corrosion performance in 3.5% NaCl solution was evaluated by immersion test, salt spray testing, potentiodynamic polarization analysis, and stress corrosion behavior by Slow Strain Rate Testing (SSRT). Although the general corrosion resistance of MRI230D was slightly improved compared to that of AZ91D alloy its stress corrosion resistance was relatively reduced. The variations in the environmental behavior of the two alloys were mainly due to the differences in their chemical composition and microstructure after die casting. In particular, the differences were related to the reduced Al content in MRI230D and the addition of Ca to this alloy, which consequently affected its relative microstructure and electrochemical characteristics. - Research Highlights: {yields}Corrosion and SCC resistance of a new Mg alloy MRI230D was evaluated vs. regular AZ91D. {yields}MRI230D has a minor advantage in corrosion performance compared with AZ91D. {yields}The SCC resistance of MRI230D by SSRT analysis was relatively reduced. {yields}The reduced SCC resistance of MRI230D was due to the detrimental effect of Ca on ductility.

36 MATERIALS SCIENCE↗

Materials for Consideration in Standardized Canister Design Activities.

This document identifies materials and material mitigation processes that might be used in new designs for standardized canisters for storage, transportation, and disposal of spent nuclear fuel. It also addresses potential corrosion issues with existing dual-purpose canisters (DPCs) that could be addressed in new canister designs. The major potential corrosion risk during storage is stress corrosion cracking of the weld regions on the 304 SS/316 SS canister shell due to deliquescence of chloride salts on the surface. Two approaches are proposed to alleviate this potential risk. First, the existing canister materials (304 and 316 SS) could be used, but the welds mitigated to relieve residual stresses and/or sensitization. Alternatively, more corrosion-resistant steels such as super-austenitic or duplex stainless steels, could be used. Experimental testing is needed to verify that these alternatives would successfully reduce the risk of stress corrosion cracking during fuel storage. For disposal in a geologic repository, the canister will be enclosed in a corrosion-resistant or corrosion-allowance overpack that will provide barrier capability and mechanical strength. The canister shell will no longer have a barrier function and its containment integrity can be ignored. The basket and neutron absorbers within the canister have the important role of limiting the possibility of post-closure criticality. The time period for corrosion is much longer in the post-closure period, and one major unanswered question is whether the basket materials will corrode slowly enough to maintain structural integrity for at least 10,000 years. Whereas there is extensive literature on stainless steels, this evaluation recommends testing of 304 and 316 SS, and more corrosion-resistant steels such as super-austenitic, duplex, and super-duplex stainless steels, at repository-relevant physical and chemical conditions. Both general and localized corrosion testing methods would be used to establish corrosion rates and component lifetimes. Finally, it is unlikely that the aluminum-based neutron absorber materials that are commonly used in existing DPCs would survive for 10,000 years in disposal environments, because the aluminum will act as a sacrificial anode for the steel. We recommend additional testing of borated and Gd-bearing stainless steels, to establish general and localized corrosion resistance in repository-relevant environmental conditions.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

RELATIVE HUMIDITY TESTS IN SUPPORT OF THE 3013 STORAGE AND SURVEILLANCE PROGRAM

Techniques to control the initial relative humidity over oxide/salt mixtures have been developed using cerium oxide as a surrogate for plutonium oxide. Such control is required to validate certain assumptions in the Department of Energy Standard DOE-STD-3013, and to provide essential information to support field surveillance at the storage sites for excess plutonium oxides. Concern over the validity of the assumption that corrosion induced degradation in 3013 containers could be controlled by assuring that the moisture content of any stored oxide/salt mixture was below 0.5 w t% arose when stress corrosion cracks were found in test samples exposed at room temperature to plutonium oxide/salt mixtures having a moisture content only marginally above 0.5 wt %. Additionally, analysis of the stress corrosion cracking observations suggests that the initial relative humidity over the oxide/salt mixture may play a major role in the cracking process. The investigations summarized in this report provide the procedures necessary to control the initial relative humidity to selected values within the range of 16 to 50% by controlling the loading relative humidity (18 to 60%) and the oxide/salt mixture water content (0.05 to 0.45 wt %). The studies also demonstrated that the initial relative humidity may be estimated by calculations using software EQ3/6. Cerium oxide/salt mixtures were used in this study because qualification tests with non-radioactive materials will reduce costs while increasing the breadth of the test programs required to support field surveillances of stored 3013 containers.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

SNF Interim Storage Canister Corrosion and Surface Environment Investigations (FY2020 Status Report)

This progress report describes work performed during FY20 at Sandia National Laboratories (SNL) to assess the localized corrosion performance of container/cask materials used in the interim storage of spent nuclear fuel (SNF). Of particular concern is stress corrosion cracking (SCC), by which a through-wall crack could potentially form in a canister outer wall over time intervals that are shorter than possible dry storage times. Work in FY20 further defined our understanding of the potential chemical and physical environment present on canister surfaces, evaluated the relationship between the environment and the resultant corrosion that occurs, and initiated crack growth rate testing under relevant environmental conditions. In FY20, work to define dry storage canister surface environments included several tasks. First, collection of dust deposition specimens from independent spent fuel storage installation (ISFSI) site locations helped to establish a more complete understanding of the potential chemical environment formed on the canister. Second, the predicted evolution of canister surface relative humidity RH) values was estimated using ISFSI site weather data and the horizontal canister thermal model used by the SNL probabilistic SCC model. These calculations determined that for typical ISFSI weather conditions, seasalt deliquescence to produce MgCl2-rich brines could occur in less than 20 years at the coolest locations on the canister surface, and, even after nearly 300 years, conditions for NaCl deliquescence (75% RH) are not reached. This work illustrates the importance of understanding the stability of MgCl2-rich brines on the heated canister surface, and the potential impact of brine composition on corrosion processes, including pitting and stress corrosion cracking. In an additional study, the description of the canister surface environment was refined in order to define more realistic corrosion testing environments including diurnal cycles, soluble salt chemistries, and inert mineral particles. The potential impacts of these phenomena on canister corrosion are being evaluated experimentally. Finally, work over the past few years to evaluate the stability of magnesium chloride brines continued in FY20. MgCl2 degassing experiments were carried out, confirming that MgCl2 brines slowly degas HCl on heated surfaces, converting to less deliquescent magnesium hydroxychloride phases and potentially leading to brine dryout.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Chromium Grain-boundary Segregation and Effect of Ion Beam Cleaning on Fe-Ni-Cr Alloys

The grain boundaries play important role to control the mechanical strength of ternary alloys. From spacecrafts to naval vessels to nuclear reactors, stress corrosion cracking, brittleness, oxidation mostly originates at the grain boundaries and cause long term structural stability problems in most of the metallic structures [1]. Fe-Ni-Cr based ternary metal alloys have been widely studied for more than fifty years [2, 3]. Despite of vast amount of research, chromium diffusion in stainless steel or other Ni-Fe-Cr based ternary alloys is still an open scientific problem with challenges in structural stability and corrosion resistance [4]. Particularly, austenite Fe-Ni-Cr is looked upon favorably in space and jet engine industry for their improved resistance to stress corrosion cracking [5]. In solid oxide fuel cells (SOFC), Ni-alloys are frequently used as interconnects and seals [6]. In this communication, simultaneous energy dispersive spectroscopy (EDS) and electron backscatter diffraction (EBSD) mapping is utilized to study chemical and structural aspects of chromium segregation in Fe-Ni-Cr alloy. A focused Ga-ion beam is also utilized to study the effect of ion beam cleaning on EBSD image quality (IQ) and inverse pole figure (IPF) maps of Fe-Ni-Cr alloy.

30 DIRECT ENERGY CONVERSION↗

Corrosion Assessment of Candidate Materials for the SHINE Subcritical Assembly Vessel and Components FY15 Report

In the previous report of this series, a literature review was performed to assess the potential for substantial corrosion issues associated with the proposed SHINE process conditions to produce 99 Mo. Following the initial review, substantial laboratory corrosion testing was performed emphasizing immersion and vapor-phase exposure of candidate alloys in a wide variety of solution chemistries and temperatures representative of potential exposure conditions. Stress corrosion cracking was not identified in any of the exposures up to 10 days at 80°C and 10 additional days at 93°C. Mechanical properties and specimen fracture face features resulting from slow-strain rate tests further supported a lack of sensitivity of these alloys to stress corrosion cracking. Fluid velocity was found not to be an important variable (0 to ~3 m/s) in the corrosion of candidate alloys at room temperature and 50°C. Uranium in solution was not found to adversely influence potential erosion-corrosion. Potentially intense radiolysis conditions slightly accelerated the general corrosion of candidate alloys, but no materials were observed to exhibit an annualized rate above 10 μm/y.

36 MATERIALS SCIENCE↗

Development of Friction Stir Processing for Repair of Nuclear Dry Cask Storage System Canisters

The Nuclear Regulatory Commission has identified chloride-induced stress corrosion cracking (CISCC) of austenitic stainless steel dry cask storage systems (DCSS) as an area of great concern. Friction Stir Processing (FSP) was used to repair laboratory-generated stress corrosion cracking (SCC) in representative stainless steel 304 coupons. Results of this study show FSP is a viable method for repair and mitigation CISCC. This paper highlights lessons learned and developed techniques relative to FSP development for crack repair in sensitized thick section stainless steel 304. These include: development of process parameters, welding at low spindle speed, use of weld power and temperature control and optimization of these controls. NDE and destructive analysis are also presented to demonstrate effectiveness of the developed methods for SCC crack repair.

Friction Stir↗

Comparison of selective oxidation in Ni-based alloys exposed to PWR primary water and Rhines Pack environments

A mechanistic understanding of corrosion and oxidation processes is crucial to ensure long-term resistance to stress corrosion cracking of Ni-based structural alloys in PWR primary and secondary systems. Aqueous corrosion of complex Ni-based alloys under PWR water conditions as well as gaseous oxidation of low-solute Ni binary alloys at high temperatures (>800 °C) have been studied extensively. However, a significant knowledge gap exists between response of Ni-based alloys in aqueous and gaseous environmental conditions. Selective oxidation at different temperatures was investigated in a series of gaseous Rhines Pack experiments for a high-purity Ni-5Cr binary alloy and a commercial Ni-18Cr-9Fe Alloy 600. Focused ion beam milling enabled the extraction of site-specific specimens containing high-energy grain boundaries. Analytical transmission electron microscopy was employed to analyze the microstructure and chemical composition of the resulting localized oxidation. The oxidation mechanism in the gaseous Rhines Pack atmosphere at 420 °C included the formation of a protective Cr-oxide cap above grain boundaries in all cases. At higher temperatures (600 and 800 °C), penetrative intergranular and transgranular internal oxidation was observed. Direct comparisons are made to corrosion response for these same materials in simulated PWR primary water at 320-360 °C. These results reveal a temperature dependence for gaseous oxidation and indicate mechanistic differences between aqueous and gaseous degradation in Ni-Cr alloys. These results imply that selective intergranular corrosion in PWR water is governed by processes beyond mere oxidation. Consideration of complex corrosion/dissolution processes at surfaces and in open cracks is essential for the better understanding of stress corrosion cracking mechanisms in PWR primary water.

Rhines Pack, Alloy 600, Ni-base alloys, Internal O↗

ANALYSIS OF EMERGING NDE TECHNIQUES: METHODS FOR EVALUATING AND IMPLEMENTING CONTINUOUS ONLINE MONITORING

One of the goals of the program for the proactive management of materials degradation (PMMD) is to manage proactively the in-service degradation of metallic components in aging NPPs. As some forms of degradation, such as stress corrosion cracking, are characterized by a long initiation time followed by a rapid growth phase, new inspection or monitoring technologies may be required. New nondestructive evaluation (NDE) techniques that may be needed include techniques to find stress corrosion cracking (SCC) precursors, on-line monitoring techniques to detect cracks as they initiate and grow, as well as advances in NDE technologies. This paper reports on the first part of the development of a methodology to determine the effectiveness of these emerging NDE techniques for managing metallic degradation. This methodology will draw from experience derived from evaluating techniques that have "emerged" in the past. The methodology will follow five stages: a definition of inspection parameters, a technical evaluation, laboratory testing, round robin testing, and the design of a performance demonstration program. This methodology will formalize the path taken for previous techniques and set a predictable course for future NDE techniques. This paper then applies the expert review section of the methodology to the acoustic emission technique to evaluate the use of acoustic emission in performing continuous online monitoring of reactor components.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Novel effects of grain size and ion implantation on grain boundary segregation in ion irradiated austenitic steel

Nuclear reactor environments are extreme in nature due to the combination of exposure to corrosive coolant, mechanical stresses, and neutron irradiation damage. This combination of environments can lead to irradiation induced/assisted precipitation, segregation, and embrittlement coupled with enhanced creep and stress corrosion cracking. While nanostructured materials are of interest in a variety of applications due to their unique properties including high mechanical strength, for nuclear applications nanostructured materials have the added benefit of irradiation resistance due to the high volume density of sinks for irradiation-induced defects. In this study, we show unique radiation-induced segregation (RIS) behavior in nanocrystalline 304 stainless steel (SS304). Typical RIS in austenitic steels includes Ni enrichment and Cr depletion within the grain boundaries. In nanostructured SS304 this RIS is reduced. Furthermore, interestingly, some grain boundaries in the nanocrystalline SS304 in this study were found to be enriched in Cr after Fe 2+ ion irradiation at 500 °C up to 50 displacements per atom (dpa). To understand this unique observation, lattice-based atomic kinetic Monte Carlo simulations were performed to investigate the effects of grain size, thermal segregation, as well as injected interstitials (introduced as Fe self-ions). The results indicate that the Cr enrichment at grain boundaries may be caused by combined effects of grain size, self-ion injection and preferential Cr diffusion via the interstitial mechanism. In conclusion, the findings also suggest a possible difference in RIS between ion and neutron irradiations.

36 MATERIALS SCIENCE↗

An examination of the precipitation behavior of proton irradiated dual phase 308L weldment filler materials

Voids, G phase particles, and Ni-Si rich clusters in proton irradiated dual phase 308L groove filler of a SA508–304 L dissimilar metal weldment are analyzed using advanced characterization techniques. These weldments are often used in light water nuclear reactors and are subject to enhanced corrosion and associated stress corrosion cracking (SCC). Radiation damage is known to accelerate SCC. Ni-Si enriched clusters were observed in proton irradiated γ austenite, while G phase M 6 Ni 16 Si 7 (where M transition metal element) precipitates were observed in proton irradiated δ ferrite. Compositional analysis of the G phase precipitates and Ni-Si clusters from STEM-EDS and APT are compared. Unlike G phase particles in proton irradiated δ ferrite, Ni-Si clusters in proton irradiated γ austenite are not rich in Mn. Both STEM-EDS and APT line-scan profiles of the Ni-Si clusters show that the Fe and Cr concentration gradient between matrix γ austenite and the Ni-Si clusters is not as sharp as those between matrix δ ferrite and G phase. Further, HR-STEM imaging indicates that the lattice parameter of the Ni-Si clusters is commensurate with γ austenite and the clusters do not represent the precipitation of a second phase. Finally, our analysis demonstrates the density and volume fraction of G phase particles and the density of voids scales with proton irradiation damage and the energy to recoils.

308L groove filler↗

Thermal Analysis Capability of UNF-ST&DARDS

In the United States, approximately 2,500 casks are loaded with commercial spent nuclear fuel (SNF) that has transitioned from wet storage (spent fuel pools) to dry storage. The number of loaded dry storage casks is increasing by approximately 200 each year. Over time, cask designs have evolved to enhance safety and to accommodate more fuel and higher heat loads. Also, higher burnup fuel is being transitioned into dry storage. The SNF is being stored in dry casks for longer times than specified in the original certification period. Several degradation mechanisms related to fuel assemblies and canisters are affected by temperature. For the cladding, temperature-dependent phenomena include creep and annealing, hydride reorientation and embrittlement, and the ductile-to-brittle transition. Temperature can also influence phenomena that affect the long-term integrity of the storage system, including deliquescence, corrosion, and stress-corrosion cracking. Therefore, accurate determination of the temperatures of various components is needed to evaluate potential safety-related issues during transportation after extended storage and to ensure SNF retrievability. The Used Nuclear Fuel-Storage, Transportation & Disposal Analysis Resource and Data System (UNF ST&DARDS) is being developed for the US Department of Energy Office of Nuclear Energy to streamline analyses for the waste management system [1]. Lastly, the thermal analysis capability within UNF-ST&DARDS and example results are discussed herein.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

High efficiency thermal storage system for solar plants (HELSOLAR). Final report

The project objective was to develop a high temperature Thermal Storage System (TES) based on graphite and able to provide both economical and technical advantages with respect to existing solutions contributing to increase the share of Concentrated Solar Plants (CSP). One of the main disadvantages of most of the renewable energy systems is their dependence to instantaneous irradiation and, thus, lack of predictability. CSP plants with thermal storage have proved to offer a good solution to this problem although still at an elevated price. The identification of alternative concepts able to work more efficiently would help to speed up the convergence of CSP towards grid parity. One way to reduce costs is to work in a range of temperatures higher than those allowed by the actual molten salt systems, currently the benchmark for TES in CSP. This requires the use of alternative energy storage materials such as graphite, as well as the utilization of Heat Transfer Fluids (HTF) other than molten salts or organic oils. The main technical challenges identified are derived from the high temperatures and significant high pressures, which pose risks such as potential graphite and insulation oxidation, creep, fatigue, corrosion and stress-corrosion in the pipes, leakages in the joints, high blower drivers’ electrical power consumption, thermal compatibility or relative deformations of the different materials. At the end, the main challenge of the project, is to identify a technical solution able to overcome all these problems but still at a competitive cost when compared to already existing thermal storage solutions. Special attention is given to all these issues during this project.

14 SOLAR ENERGY↗

Crack Growth Rate and Fracture Toughness Tests on Irradiated Cast Stainless Steels

Cast austenitic stainless steels are used in the cooling system of light water reactors for components with complex shapes, such as pump casings, valve bodies, and coolant piping. In the present study, crack growth rate and fracture toughness JR curve tests were performed on irradiated cast stainless steels in low-corrosion-potential environments (low-dissolved-oxygen high-purity water or simulated pressurized water reactor environment) at 320°C. Both as received and thermally aged materials were included to investigate the combined effect of thermal aging and irradiation embrittlement on the fracture behavior of cast stainless steels. The samples were irradiated to approximately 0.08 dpa at the Halden reactor. Good resistance to corrosion fatigue and stress corrosion cracking was observed for all samples. Thermal aging had little effect on the crack growth behavior at this dose level. Cleavage-like fracture was the dominant cracking morphology during the crack growth rate tests, and the ferrite phase was deformed to a lesser extent compared with the surrounding austenite phase. The fracture toughness results showed a dominant effect of neutron irradiation, and the fracture resistances were decreased considerably for all cast specimens regardless of their thermal aging conditions. The reduction in fracture toughness was more significant in the unaged than thermally aged materials. Nonetheless, the fracture toughness values of thermally aged specimens were about 30% lower than their unaged counterparts, suggesting a combined effect of thermal aging and neutron irradiation in cast stainless steel.

Chen, Y.↗