Tribological Evaluation of Candidate Gear Materials Operating Under Light Loads in Highly Humid Conditions

A series of pin-on-disk sliding wear tests were undertaken to identify candidate materials for a pair of lightly loaded timing gears operating under highly humid conditions. The target application involves water purification and thus precludes the use of oil, grease and potentially toxic solid lubricants. The baseline sliding pair is austenitic stainless steel operating against a carbon filled polyimide. The test load and sliding speed (4.9N, 2.7ms) were chosen to represent average contact conditions of the meshing gear teeth. In addition to the baseline materials, the hard superelastic NiTiNOL 60 (60NiTi) was slid against itself, against the baseline polyimide, and against 60NiTi onto which a commercially deposited dry film lubricant (DFL) was applied. The alternate materials were evaluated as potential replacements to achieve a longer wear life and improved dimensional stability for the timing gear application. An attempt was also made to provide solid lubrication to self-mated 60NiTi by rubbing the polyimide against the disk wear track outside the primary 60NiTi-60NiTi contact, a method named stick or transfer-film lubrication. The selected test conditions gave repeatable friction and wear data and smooth sliding surfaces for the baseline materials similar to those in the target application. Friction and wear for self-mated stainless steel were high and erratic. Self-mated 60NiTi gave acceptably low friction (0.2) and modest wear but the sliding surfaces were rough and potentially unsuitable for the gear application. Tests in which 60NiTi pins were slid against DFL coated 60NiTi and DFL coated stainless steel gave low friction and long wear life. The use of stick lubrication via a secondary polyimide pin provided effective transfer film lubrication to self-mated 60NiTi tribological specimens. Using this approach, friction levels were equal or lower than the baseline polyimide-stainless combination and wear was higher but within data scatter observed in these preliminary tests. Based upon these results, self-mated 60NiTi gear teeth utilizing solid lubrication, is a reasonable approach for the target application.

tribology↗

Effectiveness of solid lubricant coatings for friction in hard vacuum (10-9 tor)

A study was made of the efficiency of solid lubricating coatings, based on MoS2 with various binders, during friction and under highvacuum conditions. Mass spectrometry was used for an analysis of the composition of the gas evolved from the coatings in the friction process. It is shown that the vacuum level, loading, and sliding velocity influence coating effectiveness. In the friction process the solid lubricant coatings yield characteristic decay products associated with the chemical nature of the binders. The mechanism of coating breakdown during friction is associated with the binder breakdown mechanism.

Verkin, B. I.↗

Measurement of Gear Tooth Dynamic Friction

Measurements of dynamic friction forces at the gear tooth contact were undertaken using strain gages at the root fillets of two successive teeth. Results are presented from two gear sets over a range of speeds and loads. The results demonstrate that the friction coefficient does not appear to be significantly influenced by the sliding reversal at the pitch point, and that the friction coefficient values found are in accord with those in general use. The friction coefficient was found to increase at low sliding speeds. This agrees with the results of disc machine testing.

Rebbechi, Brian↗

Utah FORGE: Slide-Hold-Slide Experiments on Gneiss at Increased Temperature

Included are data from triaxial, single-inclined-fracture friction experiments. The experiments were performed with slide-hold-slide protocol on Utah FORGE gneiss at increased temperature. With a ~10 MPa normal stress, temperatures vary between experiments from room temperature up to 163 Celsius. Hold times vary during experiment from ~10^1 to ~10^5 seconds. Measured are the frictional response upon reactivation after a hold period, active acoustic data (P-wave velocity and amplitude) and passive acoustic data (acoustic emission occurrence and amplitude). There are two types of datafiles: (1) Datafiles containing the friction data, including the temperature and the active acoustic data measured during the experiment (AEXX_Gneiss_Vp_mixref4). The underscore _Vp means that it includes the Vp or P-wave velocity data, with _mixref meaning that we use a mixed reference point for calculating the P-wave velocity. And (2) the datafiles containing the passive acoustics data, a catalog of the acoustic emissions (AE's) measured during the experiment (AEcatalog_AEXX_runX), where AEXX matches the experiment number and runX denotes which part of the experiment the data was collected, matching the times where active acoustic data was collected. AE catalogs are split in two parts when the file size exceeds 1 GB to aid download/opening times.

15 GEOTHERMAL ENERGY↗

Tribological Evaluation of Candidate Gear Materials Operating Under Light Loads in Highly Humid Conditions

A series of pin-on-disk sliding wear tests were undertaken to identify candidate materials for a pair of lightly loaded timing gears operating under highly humid conditions. The target application involves water purification and thus precludes the use of oil, grease and potentially toxic solid lubricants. The baseline sliding pair is austenitic stainless steel operating against a carbon filled polyimide. The test load and sliding speed (4.9 N, 2.7 m/s) were chosen to represent average contact conditions of the meshing gear teeth. In addition to the baseline materials, the hard superelastic NiTiNOL 60 (60NiTi) was slid against itself, against the baseline polyimide, and against 60NiTi onto which a commercially deposited dry film lubricant (DFL) was applied. The alternate materials were evaluated as potential replacements to achieve a longer wear life and improved dimensional stability for the timing gear application. An attempt was also made to provide solid lubrication to self-mated 60NiTi by rubbing the polyimide against the disk wear track outside the primary 60NiTi-60NiTi contact, a method named stick or transfer-film lubrication. The selected test conditions gave repeatable friction and wear data and smooth sliding surfaces for the baseline materials similar to those in the target application. Friction and wear for self-mated stainless steel were high and erratic. Self-mated 60NiTi gave acceptably low friction (approx. 0.2) and modest wear but the sliding surfaces were rough and potentially unsuitable for the gear application. Tests in which 60NiTi pins were slid against DFL coated 60NiTi and DFL coated stainless steel gave low friction and long wear life. The use of stick lubrication via the secondary polyimide pin provided effective transfer film lubrication to self-mated 60NiTi tribological specimens. Using this approach, friction levels were equal or lower than the baseline polyimide-stainless combination and wear was higher but within data scatter observed in these preliminary tests. Based upon these results, self-mated 60NiTi gear teeth utilizing solid lubrication, is a reasonable approach for the target application.

tribology↗

Lubricating and wear mechanisms for a hemisphere sliding on polyimide-bonded graphite fluoride film

Friction, wear life, rider wear, and film wear for a 440 C high-temperature-stainless-steel, hemispherically tipped rider sliding against polyimide-bonded graphite fluoride films were evaluated in a moist-air atmosphere at 25 C. Optical microscope and surface profilometry observations were made at various sliding intervals to determine how film thickness affected the lubricating and failure mechanisms of the films. Two lubrication regimes operated for the same load. In the first, the film supported the load and the lubricating mechanism consisted of the shear (plastic flow) of a thin layer of the lubricant between the metallic rider and the film surface. In the second, the film did not support the load (it was worn away) and the lubricating mechanism consisted of the shear of very thin lubricant films between flat areas generated on the rider and on sandblasted metallic asperities in the film wear track. Lubricant was supplied from the valleys between the asperities or from the sides of the wear track. With thicker films, wear life increased since a greater lubricant supply was available from the sides of the wear track.

Fusaro, R. L.↗

Control of rotordynamic instability in a typical gas turbine's power system

The effect of rotor internal friction on the system's stability was studied when operated above the first critical speed. This internal friction is commonly caused by sliding press fits or sliding splines. Under conditions of high speed and low bearing damping, these systems will occassionally whirl at a frequency less than the shaft's rotational speed. This subsynchronous precession is a self excited phenomenon and stress reversals are created. This phenomenon was observed during engine testing. The reduction of spline friction and/or the inclusion of squeeze film damping have controlled the instability. Case history and the detail design of the squeeze film dampers is discussed.

Veikos, N. M.↗

The XPS depth profiling and tribological characterization of ion-plated gold on various metals

Friction properties were measured with a gold film; the graded interface between gold and nickel substrate; and the nickel substrate. All sliding was conducted against hard silicon carbide pins in two processes. In the adhesive process, friction arises primarily from adhesion between sliding surfaces. In the abrasion process, friction occurs as a result of the hard pin sliding against the film, indenting into it, and plowing a series of grooves. Copper and 440 C stainless steel substrates were also used. Results indicate that the friction related to both adhesion and abrasion is influenced by coating depth. The trends in friction behavior as a function of film depth are, however, just the opposite. The graded interface exhibited the highest adhesion and friction, while the graded interface resulted in the lowest abrasion and friction. The coefficient of friction due to abrasion is inversely related to the hardness. The greater the hardness of the surface, the lower is the abrasion and friction. The microhardness in the graded interface exhibited the highest hardness due to an alloy hardening effect. Almost no graded interface between the vapor-deposited gold film and the substrates was detected.

Miyoshi, K.↗

Rapid interface flaw extension with friction

An idealized two-dimensional example of rapid interface flow extension is described. Initially undisturbed dissimilar isotropic, homogeneous, linearly elastic half-spaces are perfectly bonded along the interface y=0. Quantities associated with the half-space or = to 0 are denoted by the prime superscript or the subscripts 3 or 4 while those in y or = to 0 carry the subscripts 1 or 2. At time t=0 adjacent material points at x=0, y= + or - 0 are forced apart horizontally with a constant relative velocity delta v. This results in a zone of bond failure which extends symmetrically along the interface at a constant rate c. The newly created flaw surfaces are in sliding contact resisted by Coulomb friction. The friction coefficient is gamma.

Brock, L. M.↗

The Influence of Surface Topography on Polymer Friction

Current friction models for polymers are examined to determine their applicability in predicting the effects of roughness on friction. The two component, adhesion deformation model of friction predicts the variation of friction with the change in the sliding direction with respect to the lay direction on anisotropic rough surfaces. The two component model does not predict the change in friction with changes in roughness. A combination of an energy based model and a slip line deformation model may provide a friction model which could better represent measured friction.

Eiss, N. S., Jr.↗

Adhesion and friction behavior of group 4 elements germanium, silicon, tin, and lead

Adhesion and friction studies were conducted with thin films of the group IV elements silicon, germanium, tin, and lead ion plated on the nickel (011) substrate. The mating surface was gold (111). Contacts were made for the elements in the clean state and with oxygen present. Adhesion and friction experiments were conducted at very light loads of 1 to 10 g. Sliding was at a speed of 0.7 mm/min. Friction results indicate that the more covalently bonded elements silicon and germanium exhibit lower adhesion and friction than the more metallic bonded tin and lead. The adhesion of gold to germanium was observed, and recrystallization of the transferred gold occurred. Plastic flow of germanium was seen with sliding. Oxygen reduced, but did not eliminate, the adhesion observed with germanium and silicon.

Buckley, D. H.↗

Tribochemical Conversion of Methane to Graphene and Other Carbon Nanostructures: Implications for Friction and Wear

Tribochemistry involves chemical reactions occurring at sliding contact interfaces in the presence of gaseous and/or liquid media. It often leads to the formation of a solid reaction film (also termed boundary film) which controls friction and wear and hence the efficiency and reliability of moving mechanical systems (such as engines). Here we demonstrate tribochemical conversion of methane to graphene, nano-onion, and disordered carbons on the sliding surfaces of Ni-, Cu-, and CuNi-containing VN coatings at atmospheric pressure and room temperature, providing 2-3 orders of magnitude reduction in wear and similar to 50% reduction in friction compared to those of the uncoated steels. Transmission electron microscopy confirms that graphene forms preferably on metal rich nanoclusters of the composite coatings, while the carbon nano-onions are scattered throughout the carbon tribofilm. Ab initio molecular dynamics simulations elucidate underlying mechanisms involved in the tribochemical conversion of methane to carbon- based nanostructures in support of microscopic observations. These scientific findings may lead to new materials technologies that can use methane as a source for continuous and in situ lubrication. For example, there is an urgent need to curtail the uses of lubricating oils in natural gas compressors and engines as they contaminate the natural gas being compressed or burnt.

36 MATERIALS SCIENCE↗

Rheological effects on friction in elastohydrodynamic lubrication

An analytical and experimental investigation is presented of the friction in a rolling and sliding elastohydrodynamic lubricated contact. The rheological behavior of the lubricant is described in terms of two viscoelastic models. These models represent the separate effects of non-Newtonian behavior and the transient response of the fluid. A unified description of the non-Newtonian shear rate dependence of the viscosity is presented as a new hyperbolic liquid model. The transient response of viscosity, following the rapid pressure rise encountered in the contact, is described by a compressional viscoelastic model of the volume response of a liquid to an applied pressure step. The resulting momentum and energy equations are solved by an iterative numerical technique, and a friction coefficient is calculated. The experimental study was performed, with two synthetic paraffinic lubricants, to verify the friction predictions of the analysis. The values of friction coefficient from theory and experiment are in close agreement.

Trachman, E. G.↗

Influence of alloying elements on friction and wear of copper

The friction and wear characteristics were determined for copper binary alloys containing 10 atomic percent aluminum, silicon, indium, and tin. A ternary alloy containing 10 atomic percent aluminum and 5 atomic percent silicon was also examined. The effectiveness of each of the alloying elements aluminum and silicon were very effective in reducing friction. Silicon, however, also reduced wear appreciably. With lubrication, silicon, indium, and tin were all effective alloying elements in reducing friction and wear from values obtained for copper. Silicon was the most effective single element in reducing friction and wear in dry sliding and with lubrication.

Buckley, D. H.↗

Friction at small displacement.

Low contact resistance between metal surfaces is often observed in spite of interposed lubricant and/or oxide films. To study this effect an apparatus is used with which normal force and tangential microdisplacement are applied between a small lead rider and a gold flat with various surface film conditions. Under nonoxidized and nonlubricated conditions, and with either oxide or stearic acid lubricant film alone, friction is high and contact resistance is low. With oxide and lubricant together, friction is much lower and slide is smooth, but contact resistance remains low and Ohm's law is obeyed. The results are consistent with Greenwood's theory of contact resistance for a cluster of minute metallic contact spots within the load-supporting area. The contact resistance of such a cluster is indistinguishable, for practical purposes, from that given by complete metallic contact.

Campbell, W. E.↗

Ion-Plated Soft Metallic Films Reduce Friction and Wear

Ion plating is ion-assisted or glow-discharge surface-deposition technique. In this process, ions or energetic atoms transfer energy, momentum, and charge to substrate and deposited surface film. Process controlled to modify physical characteristics of surface, subsurface chemical conditions, and surface and subsurface microstructures as well. Ion plating with such soft, thin metallic films as gold, silver, or lead has great potential for producing self-contained lubricating surfaces. Such films reduce friction, wear, and corrosion on sliding or rotating mechanical surfaces used in wide range of environments.

Spalvins, T.↗

Boron nitride: Composition, optical properties and mechanical behavior

A low energy ion beam deposition technique was used to grow boron nitride films on quartz, germanium, silicon, gallium arsenide, and indium phosphate. The film structure was amorphous with evidence of a hexagonal phase. The peak boron concentration was 82 at %. The carbon and oxygen impurities were in the 5 to 8 at % range. Boron-nitrogen and boron-boron bonds were revealed by X-ray photoelectron spectroscopy. The index of refraction varied from 1.65 to 1.67 for films deposited on III-V compound semiconductors. The coefficient of friction for boron nitride in sliding contact with diamond was less than 0.1. The substrate was silicon.

Pouch, John J.↗