Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Reduced Defects”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 343 records · Page 19

(3-Aminopropyl)trimethoxysilane Surface Passivation Improves Perovskite Solar Cell Performance by Reducing Surface Recombination Velocity

We demonstrate reduced surface recombination velocity (SRV) and enhanced power-conversion efficiency (PCE) in mixed-cation mixed-halide perovskite solar cells by using (3-aminopropyl)trimethoxysilane (APTMS) as a surface passivator. We show the APTMS serves to passivate defects at the perovskite surface, while also decoupling the perovskite from detrimental interactions at the C 60 interface. We measure a SRV of ~125 ± 14 cm/s, and a concomitant increase of ~100 meV in quasi-Fermi level splitting in passivated devices compared to the controls. We use time-resolved photoluminescence and excitation-correlation photoluminescence spectroscopy to show that APTMS passivation effectively suppresses non-radiative recombination. We show that APTMS improves both the fill factor and open-circuit voltage (V OC ), increasing V OC from 1.03 V for control devices to 1.09 V for APTMS-passivated devices, and leads to a PCE increase from 15.90% to 18.03%. Here, we attribute the enhanced performance to reduced defect density resulting in suppressed nonradiative recombination and lower SRV at the perovskite/transport layer interface.

14 SOLAR ENERGY↗

A Fast-Cycle Charge Noise Measurement for Better Qubits

Defects in materials are an ongoing challenge for quantum bits, so called qubits. Solid state qubits—both spins in semiconductors and superconducting qubits—suffer from losses and noise caused by two-level-system (TLS) defects thought to reside on surfaces and in amorphous materials. Understanding and reducing the number of such defects is an ongoing challenge to the field. Superconducting resonators couple to TLS defects and provide a handle that can be used to better understand TLS. We develop noise measurements of superconducting resonators at very low temperatures (20 mK) compared to the resonant frequency, and low powers, down to single photon occupation.

36 MATERIALS SCIENCE↗

Role of p-GaN layer thickness in the degradation of InGaN-GaN MQW solar cells under 405 nm laser excitation

GaN-based solar cells with InGaN multiple quantum wells (MQWs) are promising devices for application in space environment, concentrator solar systems, wireless power transmission and multi-junction solar cells. It is therefore important to understand their degradation kinetics when submitted to high-temperature and high-intensity stress. We submitted three samples of GaN-InGaN MQW solar cells with p-AlGaN electron-blocking-layer with different thickness of the p-GaN layer to constant power stress at 310 W/cm 2 , 175 °C for several hundred hours. The main degradation modes are a reduction of open-circuit voltage, short-circuit current, external quantum efficiency, power conversion efficiency and electroluminescence. In particular, we observed that a thinner p-GaN layer results in a stronger degradation observed on the cell operating parameters. The analysis of the dark I-V characteristics showed an increase in low-forward bias current and the analysis of electroluminescence showed a decrease in the electroluminescene emitted by the (forward biased) cell, as a consequence of stress. This work highlights that the cause of degradation is possibly related to a diffusion mechanism, which results in an increase of defect density in the active region. Finally, the impurities involved in the diffusion processes possibly originate from the p-side of the devices, therefore a thicker p-GaN layer reduces the amount of defects reaching the active region.

14 SOLAR ENERGY↗

A Role for the Plastidial GPT2 Translocator in the Modulation of Lignin Biosynthesis

ABSTRACT Engineering plants with reduced lignin content can result in pleiotropic growth defects. In stems of Arabidopsis plants with reduced expression of hydroxycinnamoyl CoA: shikimate hydroxycinnamoyl transferase (HCT), the plastidial glucose 6‐phosphate: phosphate co‐transporter GPT2 is highly overexpressed, and this coincides with reduced lignin levels and extensive transcriptional and metabolic reprogramming. To explore the potential relationship between GPT2 expression and lignin accumulation, GPT2 transcript levels were evaluated in a suite ofArabidopsis thalianaandMedicago truncatulalignin‐defective lines. We also examined lignin levels and composition, and transcriptomic and metabolic profiles in GPT2 loss‐of‐function, GPT2 overexpression, and wild‐type Arabidopsis plants. Loss of GPT2 had no effect on lignin, but its overexpression caused a decrease in stem lignin levels due to reduced accumulation of both guaiacyl and syringyl lignins and their associated monolignol pools.HCTtranscript levels were diminished in 35S‐GPT2 lines, indicating a potential transcriptional regulatory connection between lignin biosynthesis and GPT2. Based on our transcriptomic and metabolomic analyses, we suggest that GPT2 operates to balance the flux between the biosynthesis of lignin and light‐protective phenylpropanoid derivatives.

Plant Sciences↗

Fiber optic instrumentation for nuclear fuels and materials irradiations

The ability to predict the safety and reliability of new and advanced nuclear fuels and materials requires high-fidelity measurements during instrumented irradiation experiments. Optical fiber-based sensors are promising candidates for instrumentation in high-temperature (300-1200 C. degrees) irradiation environments, provided that signal attenuation due to radiation damage and/or high-temperature operation is not prohibitively large. To determine the feasibility of using silica optical fibers in instrumented irradiation capsules, a computational model has been developed to predict broadband optical attenuation in fused silica fiber materials as a function of time, temperature, and dose. Defect concentrations are calculated using a set of 11 coupled differential equations that include neutron-induced displacement, radiation-induced bond cleavage at precursor sites, and thermally-assisted molecular diffusion and defect recombination at elevated temperatures. Defect concentrations are coupled with the known optical properties of the various defects in fused silica to predict optical attenuation. The effects of radiation-induced compaction (i.e., formation of the 'metamict' phase) on the optical attenuation are also included. Results show that elevated temperatures significantly reduce attenuation resulting from defect centers (attenuation below ∼750 nm) as well as attenuation resulting from radiation-induced compaction (attenuation above ∼800 nm). The predicted attenuation is acceptable for most fiber optic-based sensor systems with a dynamic range on the order of 20-50 dB for a reasonable length (1-2 meters) of fiber in the high-flux region. Many optical components use a wavelength of 850 nm, which lies in the low-attenuation window. An irradiation campaign has been initiated to provide temperature-dependent optical attenuation data at high dose to validate the predictive model. (author)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microstrain screening towards defect-less layered transition metal oxide cathodes

Microstrain and the associated surface-to-bulk propagation of structural defects are known to be major roadblocks to developing high-energy and long-life batteries. However, the origin and effects of microstrain during the synthesis of battery materials remain largely unknown. Here, in this study, we perform microstrain screening during real-time and realistic synthesis of sodium layered oxide cathodes. Evidence gathered from multiscale in situ synchrotron X-ray diffraction and microscopy characterization collectively reveals that the spatial distribution of transition metals within individual precursor particles strongly governs the nanoscale phase transformation, local charge heterogeneity and accumulation of microstrain during synthesis. This unexpected dominance of transition metals results in a counterintuitive outward propagation of defect nucleation and growth. These insights direct a more rational synthesis route to reduce the microstrain and crystallographic defects within the bulk lattice, leading to significantly improved structural stability. The present work on microstrain screening represents a critical step towards synthesis-by-design of defect-less battery materials.

25 ENERGY STORAGE↗

Advanced method for increasing the efficiency of white light quantum dot LEDs

Covering a light-emitting diode (LED) with quantum dots (QDs) can produce a broad spectrum of white light. However, current techniques for applying QDs to LEDs suffer from a high density of defects and a non-uniform distribution of QDs, which respectively diminish the efficiency and quality of emitted light. Oak Ridge National Laboratory (ORNL) has the unique capability to thermally anneal QD structures at extremely high power densities for very short durations. This process, called pulse thermal processing (PTP), reduces the number of point defects while maintaining the size and shape of the original QD nanostructure. The efficiency of the QD wavelength conversion layer is improved without altering the emission spectrum defined by the size distribution of the quantum dot nanoparticles. As a result, the current research uses a thermal model to predict annealing temperatures during PTP and demonstrates up to a 300% increase in photoluminescence for QDs on passive substrates

42 ENGINEERING↗

Fatigue stress concentration and notch sensitivity in nanocrystalline metals

Recent studies have shown the potential for nanocrystalline metals to possess excellent fatigue resistance compared to their coarse-grained counterparts. Although the mechanical properties of nanocrystalline metals are believed to be particularly susceptible to material defects, a systematic study of the effects of geometric discontinuities on their fatigue performance has not yet been performed. In the present work, nanocrystalline Ni–40 wt%Fe containing both intrinsic and extrinsic defects were tested in tension–tension fatigue. The defects were found to dramatically reduce the fatigue resistance, which was attributed to the relatively high notch sensitivity in the nanocrystalline material. Microstructural analysis within the crack-initiation zones underneath the defects revealed cyclically-induced abnormal grain growth (AGG) as a predominant deformation and crack initiation mechanism during high-cycle fatigue. Furthermore, the onset of AGG and the ensuing fracture is likely accelerated by the stress concentrations, resulting in the reduced fatigue resistance compared to the relatively defect-free counterparts.

36 MATERIALS SCIENCE↗

Optical detection of the defects associated with the magnetic properties observed in GaN:Gd layers grown by reactive molecular beam epitaxy

The effect of annealing on the magnetic and the optoelectronic properties of Gd-doped GaN layers, which are grown by reactive molecular beam epitaxy technique, has been investigated using photoluminescence, photoconductivity, and vibrating sample magnetometry techniques. The study reveals that the multiple types of defects are formed in GaN layers during the Gd incorporation. However, the density of only one defect type, which results in a strong luminescence feature at 3.05 eV in the photoluminescence spectra recorded at low temperatures in GaN:Gd layers, has been found to decrease significantly upon annealing and at the same time, the saturation magnetization is also observed to reduce, suggesting that these defects are responsible for the magnetic properties observed in this system.

36 MATERIALS SCIENCE↗

Oxygen vacancy defect engineering using atomic layer deposited HfAlO{sub x} in multi-layered gate stack

This work evaluates the defects in high quality atomic layer deposited (ALD) HfAlO{sub x} with extremely low Al (<3% Al/(Al + Hf)) incorporation in the Hf based high-k dielectrics. The defect activation energy estimated by the high temperature current voltage measurement shows that the charged oxygen vacancies, V{sup +}/V{sup 2+}, are the primary source of defects in these dielectrics. When Al is added in HfO{sub 2}, the V{sup +} type defects with a defect activation energy of E{sub a} ∼ 0.2 eV modify to V{sup 2+} type to E{sub a} ∼ 0.1 eV with reference to the Si conduction band. When devices were stressed in the gate injection mode for 1000 s, more V{sup +} type defects are generated and E{sub a} reverts back to ∼0.2 eV. Since Al has a less number of valence electrons than do Hf, the change in the co-ordination number due to Al incorporation seems to contribute to the defect level modifications. Additionally, the stress induced leakage current behavior observed at 20 °C and at 125 °C demonstrates that the addition of Al in HfO{sub 2} contributed to suppressed trap generation process. This further supports the defect engineering model as reduced flat-band voltage shifts were observed at 20 °C and at 125 °C.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Laser welding and post weld treatment of modified 9Cr-1MoVNb steel

Laser welding and post weld laser treatment of modified 9Cr-1MoVNb steels (Grade P91) were performed in this preliminary study to investigate the feasibility of using laser welding process as a potential alternative to arc welding methods for solving the Type IV cracking problem in P91 steel welds. The mechanical and metallurgical testing of the pulsed Nd:YAG laser-welded samples shows the following conclusions: (1) both bead-on-plate and circumferential butt welds made by a pulsed Nd:YAG laser show good welds that are free of microcracks and porosity. The narrow heat affected zone has a homogeneous grain structure without conventional soft hardness zone where the Type IV cracking occurs in conventional arc welds. (2) The laser weld tests also show that the same laser welder has the potential to be used as a multi-function tool for weld surface remelting, glazing or post weld tempering to reduce the weld surface defects and to increase the cracking resistance and toughness of the welds. (3) The Vicker hardness of laser welds in the weld and heat affected zone was 420-500 HV with peak hardness in the HAZ compared to 240 HV of base metal. Post weld laser treatment was able to slightly reduce the peak hardness and smooth the hardness profile, but failed to bring the hardness down to below 300 HV due to insufficient time at temperature and too fast cooling rate after the time. Though optimal hardness of weld made by laser is to be determined for best weld strength, methods to achieve the post weld laser treatment temperature, time at the temperature and slow cooling rate need to be developed. (4) Mechanical testing of the laser weld and post weld laser treated samples need to be performed to evaluate the effects of laser post treatments such as surface remelting, glazing, re-hardening, or tempering on the strength of the welds.

36 MATERIALS SCIENCE↗

Precipitation of boron in silicon on high-dose implantation

Precipitation of boron implanted in silicon with a dose of 1 x 10{sup 16} cm{sup -2} is studied in relation to the concentration of substitutional boron C{sub B{sub 0}} introduced before implantation and before subsequent annealing at 900 deg. C. It is shown that C{sub B{sub 0}} = 2.5 x 10{sup 20} cm{sup -3} is the critical concentration, at which the formation of precipitates is independent of the concentration of point defects introduced by implantation (far from or close to the mean projected range R{sub p}) and constitutes the prevailing channel of deactivation of boron. At lower concentrations C{sub B{sub 0}} close to the equilibrium concentration, precipitation is observed only far from R{sub p}, in the regions of reduced concentrations of point defects. At the same time, in the region of R{sub p} with a high concentration of point defects, most boron atoms are drawn into clustering with intrinsic interstitial atoms with the formation of dislocation loops and, thus, become electrically inactive as well.

36 MATERIALS SCIENCE↗

Two disulfide-reducing pathways are required for the maturation of plastid c -type cytochromes in Chlamydomonas reinhardtii

Abstract In plastids, conversion of light energy into ATP relies on cytochrome f, a key electron carrier with a heme covalently attached to a CXXCH motif. Covalent heme attachment requires reduction of the disulfide-bonded CXXCH by CCS5 and CCS4. CCS5 receives electrons from the oxidoreductase CCDA, while CCS4 is a protein of unknown function. In Chlamydomonas reinhardtii, loss of CCS4 or CCS5 yields a partial cytochrome f assembly defect. Here, we report that the ccs4ccs5 double mutant displays a synthetic photosynthetic defect characterized by a complete loss of holocytochrome f assembly. This defect is chemically corrected by reducing agents, confirming the placement of CCS4 and CCS5 in a reducing pathway. CCS4-like proteins occur in the green lineage, and we show that HCF153, a distant ortholog from Arabidopsis thaliana, can substitute for Chlamydomonas CCS4. Dominant suppressor mutations mapping to the CCS4 gene were identified in photosynthetic revertants of the ccs4ccs5 mutants. The suppressor mutations yield changes in the stroma-facing domain of CCS4 that restore holocytochrome f assembly above the residual levels detected in ccs5. Because the CCDA protein accumulation is decreased specifically in the ccs4 mutant, we hypothesize the suppressor mutations enhance the supply of reducing power through CCDA in the absence of CCS5. We discuss the operation of a CCS5-dependent and a CCS5-independent pathway controlling the redox status of the heme-binding cysteines of apocytochrome f.

Genetics & Heredity↗

Combined molecular and spin dynamics simulation of BCC iron with vacancy defects

Utilizing an atomistic computational model, which handles both translational and spin degrees of freedom, combined molecular and spin dynamics simulations have been performed to investigate the effect of vacancy defects on spin wave excitations in ferromagnetic iron. Fourier transforms of space- and time-displaced correlation functions yield the dynamic structure factor, providing characteristic frequencies and lifetimes of the spin wave modes. A comparison of the system with a 5% vacancy concentration with pure lattice data shows a decrease in frequency and a decrease in lifetime for all transverse spin wave excitations observed. In addition, the clearly defined transverse spin wave excitations are distorted with the introduction of vacancy defects, and we observe reduced excitation lifetimes due to increased magnon–magnon scattering. We observe further evidence of increased magnon–magnon scattering, as the peaks in the longitudinal spin wave spectrum become less distinct. Finally, similar impacts are observed in the vibrational subsystem, with a decrease in characteristic phonon frequency and flattening of lattice excitation signals due to vacancy defects.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Characterisation and modelling of defect formation in direct-chill cast AZ80 alloy

Wrought magnesium alloys for demanding structural applications require high quality defect free cast feedstock. The aim of this study was to first identify and characterise typical defects in direct chill cast magnesium–aluminium–zinc (AZ) alloy billet and then use modelling to understand the origins of these defects so they can be prevented. Defects were first located using ultrasonic inspection and were then characterised using X-ray computed tomography (XCT) and serial sectioning, establishing the presence of oxide films and intermetallic particles Al{sub 8}Mn{sub 5} in all defects. A model was developed to predict the flow patterns and growth kinetics of the intermetallic phases during casting, which influence the formation of defects. Simulation of the growth of the intermetallic particles demonstrated that precipitation from the liquid occurs in the mould. The combination of the entrained oxide films and intermetallic particles recirculates in the liquid metal and continues to grow, until large enough to settle, which is predicted to occur at the centre of the mould where the flow is the slowest. Based on these predictions, strategies to reduce the susceptibility to defect formation are suggested. - Highlights: • Casting defects in magnesium direct chill casting have been imaged and characterised in 3-dimensions. • The occurrences of co-located clusters of particles and oxide films have been characterised and explained. • A coupled model has been developed to help interpret the observed trend for defects located towards the centre of billets.

36 MATERIALS SCIENCE↗

Defect-engineered GaN high electron mobility transistors for enhanced radiation tolerance

This study explores the radiation resilience of GaN high-electron-mobility transistors (HEMTs) under various preconditioning treatments—pristine, electro-pulsed, electrically overstressed, and 60 Co gamma-irradiated—with a focus on enhancing survivability in high-radiation environments. Key findings emphasize the gate region’s central role in radiation sensitivity, with increased defect concentrations leading to reduced sensitivity—as determined from reduced single-event transient intensities during pulsed-laser studies—and impacting charge-transport dynamics. Notably, the most sensitive region shifted as a function of bias state, with the drain side of the gate being most sensitive under negative gate bias and the source side under unbiased conditions due to two-dimensional electron gas disruptions. These insights clarify the mechanisms influencing radiation sensitivity in microelectronics and highlight the potential of defect and strain engineering to enhance the radiation hardness of GaN HEMTs across various operational states, providing valuable guidance for applications in space, defense, and other radiation-rich environments.

36 MATERIALS SCIENCE↗

EUV actinic defect inspection and defect printability at the sub-32 nm half pitch

Extreme ultraviolet (EUV) mask blanks with embedded phase defects were inspected with a reticle actinic inspection tool (AIT) and the Lasertec M7360. The Lasertec M7360, operated at SEMA TECH's Mask Blank Development Center (MBDC) in Albany, NY, has a sensitivity to multilayer defects down to 40-45 nm, which is not likely sufficient for mask blank development below the 32 nm half-pitch node. Phase defect printability was simulated to calculate the required defect sensitivity for a next generation blank inspection tool to support reticle development for the sub-32 nm half-pitch technology node. Defect mitigation technology is proposed to take advantage of mask blanks with some defects. This technology will reduce the cost of ownership of EUV mask blanks. This paper will also discuss the kind of infrastructure that will be required for the development and mass production stages.

36 MATERIALS SCIENCE↗