Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “IRON COMPOUND”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 343 records · Page 19

Structural and magnetic properties of Prussian blue analogue molecular magnet Fe{sub 1.5}[Cr(CN){sub 6}]·mH{sub 2}O

Molecular magnets, based on Prussian blue analogues, Fe{sub 1.5}[Cr(CN){sub 6}]·mH{sub 2}O have been synthesized in the bulk as well as nanoparticle forms using a co-precipitation method, and their structural and magnetic properties have been investigated using x-ray diffraction (XRD) Mössbauer spectroscopy and dc magnetization. The XRD study confirms the single phase crystalline and nanoparticle nature of the compounds with a face centered cubic (fcc) structure of space group Fm3m. The values of lattice constant are found to be ~10.18(5) Å and ~9.98(9)Å, for the bulk and nanoparticle samples, respectively. The dc magnetization shows a Curie temperature (T{sub C}) of ~17 K and ~5 K for the bulk and nanopartcile samples, respectively. The Mossouber spectroscopy reveal that the compound shows spin flipping from the high spin (HS) Fe (Cr{sup III}–C≡N–Fe{sup II}) to low spin (LS) Fe{sup II} ions (Cr{sup III}–N≡C–Fe{sup II}). Moreover, the T{sub C} and the HS state of the Fe ions decreases (converts to its LS states) with time as well as in the nanoparticle form compared to bulk.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Sintering dense NiZn ferrite by two-step sintering process

A two-step sintering process has been adopted to produce NiZn ferrite with composition of (NiO){sub 0.35}(ZnO){sub 0.57}(CuO){sub 0.08}(Fe{sub 2}O{sub 3}). The densification, microstructure, and magnetic properties of the ferrite have been investigated and compared with those of ferrites produced by the traditional final-stage sintering process. It was found that the sample produced by a two-step sintering process with a high temperature of 1200 deg. C and a lower temperature of 1100 deg. C attained more than 96% of the theoretical density and had a uniform microstructure with a small average grain size. It also exhibited good performances in terms of permeability and Q-factor. Hence, this would seem to be an effective method for producing dense ferrites with a microstructure composed of small and even grains, which is a very effective strategy for improving the magnetic properties of ferrites.

36 MATERIALS SCIENCE↗

FORMATION OF DUST IN THE EJECTA OF TYPE Ia SUPERNOVAE

We investigate the formation of dust grains in the ejecta of Type Ia supernovae (SNe Ia), adopting the carbon-deflagration W7 model. In the calculations of dust formation, we apply the nucleation and grain growth theory and consider the two extreme cases of the formation of CO and SiO molecules: complete formation and no formation. The results of the calculations show that for the sticking probability of {alpha}{sub j} = 1, C, silicate, Si, and FeS grains can condense at early times of {approx}100-300 days after the explosion, whereas Fe and SiC grains cannot form substantially. Due to the low gas density in SNe Ia with no H-envelope, the average radii of the newly formed grains are generally below 0.01 {mu}m, being much smaller than those in Type II-P SNe. This supports our previous conclusion that the radius of dust formed in the ejecta is smaller in SNe with less massive envelopes. The total dust mass ranges from 3 x 10{sup -4} M{sub sun} to 0.2 M{sub sun} for {alpha}{sub j} = 0.1-1, depending on whether or not CO and SiO molecules are formed. We also estimate the optical depths and thermal emission by the newly formed dust and compare them to the relevant observations of SNe Ia. We find that the formation of C grains in SNe Ia must be suppressed to be consistent with observational constraints. This implies that energetic photons and electrons heavily depress the formation efficiency of C grains or that the outermost C-O layer of SNe Ia is almost fully burned. Finally, we calculate dust destruction in the SN remnants and find that dust grains formed in the ejecta of SNe Ia are almost completely destroyed in the shocked gas before being injected into the interstellar medium. This indicates that SNe Ia are unlikely to be the major sources of interstellar dust.

79 ASTRONOMY AND ASTROPHYSICS↗

One-dimensional NiCuZn ferrite nanostructures: Fabrication, structure, and magnetic properties

Ni{sub 0.5-x}Cu{sub x}Zn{sub 0.5}Fe{sub 2}O{sub 4} (0.0{<=}x{<=}0.5) ferrite nanofibers with diameters of 80-160 nm have been prepared by electrospinning and subsequent heat treatment. Both the average grain size and lattice parameter are found to increase with the addition of copper. Fourier transform infrared spectra indicate that the portion of Fe{sup 3+} ions at the tetrahedral sites move to the octahedral sites as some of the substituted Cu{sup 2+} ions get into the tetrahedral sites. Vibrating sample magnetometer measurements show that the coercivity of these ferrite nanofibers decreases with increasing Cu concentration, whereas the specific saturation magnetization initially increases, reaches a maximum value at x=0.2 and then decreases with the Cu content further increase. Notable differences in magnetic properties at room temperature (298 K) and 77 K for the Ni{sub 0.3}Cu{sub 0.2}Zn{sub 0.5}Fe{sub 2}O{sub 4} nanofibers and corresponding powders are observed and mainly arise from the grain size and morphological variations between these two materials. - Graphical abstract: NiCuZn ferrite nanofibers with diameters of 80-160 nm have been prepared by electrospinning technique and their magnetic behavior is different from that of the corresponding powder sample.

36 MATERIALS SCIENCE↗

XRD line-broadening characteristics of M-oxides (M = Mg, Mg-Al, Y, Fe) nanoparticles produced by coprecipitation method

Simple coprecipitation method has been used to produce nanoparticles of MgO (magnesia), MgO{center_dot}Al{sub 2}O{sub 3}(spinel), Y{sub 2}O{sub 3}(yttria) and Fe{sub 3}O{sub 4}(ferrite). The raw materials were, in respective, magnesium powder, magnesium and aluminium powders, ytrria powder, and natural sand. The coprecipitation included the use of suitable acid and base to dissolve the powders or sand and to produce precipitates, as well as the use of water to wash and purify the precipitates, and drying at relatively low temperatures, namely lower than 100 deg. C, followed by heating at 450 deg. C, 750 deg. C, 600 deg. C and 200 deg. C to produce magnesia, spinel, yttria and ferrite nanopowders, respectively. X-ray diffractometry was used to characterise the purity and nanocrystallinity of the final powders. It was found qualitatively that the powders were of high purity. Further line-broadening analysis using single-line and Rietveld-based softwares was performed to reveal the nanocrystallinity of the powders. Different line breadth values were found for the powders, indicating different crystallite sizes. It was also found that, particularly for spinel and yttria, the diffraction peaks exhibited 'longer' tails, indicating broader crystallite size distribution. The average crystallite size for the powders ranged from 3 to 70 nm. The results could then be used as 'fingerprints' for nanocrystallinity using x-ray diffractometry. The XRD crystallite sizes for yttria and ferrite nanocrystals are in fair agreement with their counterparts from electron microscopy observation.

36 MATERIALS SCIENCE↗

Electrical Characteristics CuFe{sub 2}O{sub 4} Thick Film Ceramics Made with Different Screen Size Utilizing Fe{sub 2}O{sub 3} Nanopowder Derived from Yarosite for NTC Thermistor

Fabrication of CuFe{sub 2}O{sub 4} thick film ceramics utilizing Fe{sub 2}O{sub 3} derived from yarosite using screen printing technique for NTC thermistor has been carried out. Effect of thickness variation due to different size of screen (screen 225; 300 and 375 mesh) has been studied. X-ray diffraction analyses (XRD) was done to know crystal structure and phases formation. SEM analyses was carried out to know microstructure of the films. Electrical properties characterization was done through measurement of electrical resistance at various temperatures (room temperature to 100 deg. C). The XRD data showed that the films crystalize in tetragonal spinel. The SEM images showed that the screen with the smaller of the hole size, made the grain size was bigger. Electrical data showed that the larger the screen different size thickness variation (mesh), the larger the resistance, thermistor constant and sensitivity. From the electrical characteristics data, it was known that the electrical characteristics of the CuFe{sub 2}O{sub 4} thick film ceramics followed the NTC characteristic. The value of B and R{sub RT} of the produced CuFe{sub 2}O{sub 4} ceramics namely B = 3241-3484 K and R{sub RT} = 25.6-87.0 M Ohm, fitted market requirement.

36 MATERIALS SCIENCE↗

Fe Vacancy Order and Domain Distribution in A{sub x}Fe{sub 2−y}Se{sub 2}

The Fe vacancy and its ordering pattern is a unique property of the A{sub x}Fe{sub 2−y}Se{sub 2} (A = K, Rb, Cs) superconductors. Below the structural transition temperature T{sub S} ∼ 550 K, the system phase separates into the I4/mmm phase with no Fe vacancy and the I4/m phase with the √5×√5×1 vacancy order. In this work, an Ising-like Hamiltonian defined on the Fe-sublattice is constructed and employed in a Metropolis Monte Carlo simulation to study the Fe vacancy order and the domain distribution under different thermal treatments. A third phase with randomly distributed Fe vacancies and space group I4/mmm is observed in the simulation. The response of the volume fraction of this simulated phase under thermal treatment shows a direct connection to the change of the superconducting shielding fraction under annealing and quenching processes, indicating a close relation between the vacancy disordered I4/mmm phase and the superconducting phase.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Electronic Structure, Elastic, Magnetic, and Optical Properties of Fe{sub 2}MnZ (Z = Si, Ge, and Sn) Full Heusler Alloys: First-Principle Calculations

Investigations of the electronic structure, elastic, magnetic, and optical properties of Fe{sub 2}MnZ (Z = Si, Ge, and Sn) full Heusler alloys show mechanical stability with cubic symmetry in all three alloys. They are elastically anisotropic and Fe{sub 2}MnSi is ductile whereas Fe{sub 2}MnGe and Fe{sub 2}MnSn are brittle in nature. The value of total magnetic moment is 3 μ{sub B} for Fe{sub 2}MnSi and Fe{sub 2}MnGe at their equilibrium lattice constants and follows the Slater–Pauling curve. Fe{sub 2}MnSn possess the largest magnetic moment among the three with a value of 5.73 μ{sub B} at equilibrium lattice constant. Fe{sub 2}MnSi shows half-metallic nature with 100% spin polarization for a wide range of lattice parameters and is useful for spintronics devices. Good optical properties over wide photon energies point to the possible use of these alloys as radiation shielding materials, optical filters, and photo-electronic devices.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Ferromagnetism and Carrier Transport in n-type Diluted Magnetic Semiconductors Ge{sub 0.96−x}Bi{sub x}Fe{sub 0.04}Te Thin Film

The structural, Hall effect, electronic transport, and magnetic properties of Ge{sub 0.96−x}Bi{sub x}Fe{sub 0.04}Te epitaxial thin film as prepared by pulsed laser deposition technique were reported. X-ray diffraction patterns including linear scans and phi scans confirmed that all films are high quality epitaxy and crystallinity. With the substitution of high valence Bi for Ge element, we found that the previous carriers of hole were changed to electron, which was testified by the negative slopes obtained from the measurements of Hall effect under different temperatures. The electronic transports show a typical semiconductor behavior and can be understood by the small polaron hopping model because the lattice distortions increase the electron-phonon interaction. An obvious ferromagnetic properties occur in the high Bi-doping Ge{sub 0.64}Bi{sub 0.32}Fe{sub 0.04}Te rather than in that with low Bi-doping concentration, indicating that the ferromagnetic establishment is entirely dependent on carrier’s transmissions. The first-principles calculation performed on this system also reveals that the ferromagnetic state exactly exists in the present n-type diluted magnetic semiconductors with Bi co-dopants.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

The Evolution of the Weld Metal Microstructures in Dissimilar Titanium Welds Based on Al and Mo Equivalents

CO{sub 2} laser welding of Ti-15V-3Cr-3Al-3Sn to Ti-4.5Al-3V-2Fe-2Mo was conducted in the study. The notched fracture and microstructures of the weld metal (WM) with various post-weld aging treatments were studied. In the as-welded sample, the WM comprised only β phase, which was relatively soft and ductile. Moreover, the phase constituent of the as-welded WM was related to the Al and Mo equivalents and further compared with other welds. The microstructural morphologies and microhardness of the WMs of dissimilar welds exhibited significant changes after post-weld aging at distinct temperatures. Increasing the Al equivalent ([Al]{sub EQ}) of the WM caused an increased response to age-hardening during post-weld aging treatments. When the aging temperature was increased from 426 to 593 °C, the α precipitates in the WM grew in size, causing a decrease in hardness, but an improvement in toughness.

36 MATERIALS SCIENCE↗

Series of compositions Bi{sub 2}(M'{sub x}M{sub 1-x}){sub 4}O{sub 9} (M', M=Al, Ga, Fe; 0{<=}x{<=}1) with mullite-type crystal structure: Synthesis, characterization and {sup 18}O/{sup 16}O exchange experiment

Series of compositions Bi{sub 2}(M'{sub x}M{sub 1-x}){sub 4}O{sub 9} with x=0.0, 0.1,..., 1.0 and M'/M=Ga/Al, Fe/Al and Fe/Ga were synthesized by dissolving appropriate amounts of corresponding metal nitrate hydrates in glycerine, followed by gelation, calcination and final heating at 800 {sup o}C for 24 h. The new compositions with M'/M=Ga/Al form solid-solution series, which are isotypes to the two other series M'/M=Fe/Al and Fe/Ga. The XRD data analysis yielded in all cases a linear dependence of the lattice parameters related on x. Rietveld structure refinements of the XRD patterns of the new compounds, Bi{sub 2}(Ga{sub x}Al{sub 1-x}){sub 4}O{sub 9} reveal a preferential occupation of Ga in tetrahedral site (4 h). The IR absorption spectra measured between 50 and 4000 cm{sup -1} of all systems show systematic shifts in peak positions related to the degree of substitution. Samples treated in {sup 18}O{sub 2} atmosphere (16 h at 800 {sup o}C, 200 mbar, 95% {sup 18}O{sub 2}) for {sup 18}O/{sup 16}O isotope exchange experiments show a well-separated IR absorption peak related to the M-{sup 18}O{sub c}-M vibration, where O{sub c} denotes the common oxygen of two tetrahedral type MO{sub 4} units. The intensity ratio of M-{sup 18}O{sub c}/M-{sup 16}O{sub c} IR absorption peaks and the average crystal sizes were used to estimate the tracer diffusion coefficients of polycrystalline Bi{sub 2}Al{sub 4}O{sub 9} (D=2x10{sup -22} m{sup 2}s{sup -1}), Bi{sub 2}Fe{sub 4}O{sub 9} (D=5x10{sup -21} m{sup 2}s{sup -1}), Bi{sub 2}(Ga/Al){sub 4}O{sub 9} (D=2x10{sup -21} m{sup 2}s{sup -1}) and Bi{sub 2}Ga{sub 4}O{sub 9} (D=2x10{sup -20} m{sup 2}s{sup -1}). - Graphical abstract: Fig. Perspective view of the mullite-type Bi{sub 2}(M'{sub x}M{sub 1-x}){sub 4}O{sub 9} unit cell (M', M=Al, Ga, Fe). Display Omitted

36 MATERIALS SCIENCE↗

High-temperature synthesis of highly hydrothermal stable mesoporous silica and Fe-SiO{sub 2} using ionic liquid as a template

Mesoporous silicas and Fe-SiO{sub 2} with worm-like structures have been synthesized using a room temperature ionic liquid, 1-hexadecane-3-methylimidazolium bromide, as a template at a high aging temperature (150-190 {sup o}C) with the assistance of NaF. The hydrothermal stability of mesoporous silica was effectively improved by increasing the aging temperature and adding NaF to the synthesis gel. High hydrothermally stable mesoporous silica was obtained after being aged at 190 {sup o}C in the presence of NaF, which endured the hydrothermal treatment in boiling water at least for 10 d or steam treatment at 600 {sup o}C for 6 h. The ultra hydrothermal stability could be attributed to its high degree of polymerization of silicate. Furthermore, highly hydrothermal stable mesoporous Fe-SiO{sub 2} has been synthesized, which still remained its mesostructure after being hydrothermally treated at 100 {sup o}C for 12 d or steam-treated at 600 {sup o}C for 6 h. -- Graphical abstract: Worm-like mesoporous silica and Fe-SiO{sub 2} with high hydrothermal stability have been synthesized using ionic liquid 1-hexadecane-3-methylimidazolium bromide as a template under the assistance of NaF at high temperature. Display Omitted Research highlights: {yields} Increasing aging temperature improved the hydrothermal stability of materials. {yields}Addition of NaF enhanced the polymerization degree of silicates. {yields} Mesoporous SiO{sub 2} and Fe-SiO{sub 2} obtained have remarkable hydrothermal stability.

36 MATERIALS SCIENCE↗

Influences of doping Cr/Fe/Ta on the performance of Ni/CeO{sub 2} catalyst under microwave irradiation in dry reforming of CH{sub 4}

The structure of Ni/CeO{sub 2} catalyst with doping of Cr, Fe and Ta was investigated with XRD, N{sub 2} physisorption, XPS and HRTEM and the catalytic activity of the catalysts under microwave irradiation in dry reforming of methane was tested in a microwave reactor. The results show that the introduction of Cr and Ta to Ni/CeO{sub 2} can enhance the interaction between Ni and the support/promoter and inhibit the enlargement of NiO particles during the synthesis. The CH{sub 4} conversions in dry reforming on the catalysts follow the order: Ni/CeO{sub 2}<2Fe–Ni<2Ta–Ni<2Cr–Ni. The superior performance of 2Ta–Ni and 2Cr–Ni may be attributed to the locally-heated Ni particles caused by the strong microwave absorption of the in-situ grown graphene attached on them under microwave irradiation. - Highlights: • The influences of doping Cr, Fe and Ta on Ni/CeO{sub 2} were investigated. • The catalytic performances before and after doping were investigated. • The in-situ grown graphene can promote the conversion of reactants.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Premartensite transition in Ni{sub 2}FeGa Heusler alloy

Martensitic phase transformation of Ni{sub 2}FeGa Heusler alloy was studied by differential scanning calorimetry. Atomic ordering induced in the austenite structure by quenching from high temperature plays a significant role on martensitic phase transformation. Higher magnetization and larger magneto-crystalline anisotropy of martensite phase than that of austenite phase are noticed. Tweed contrast regions observed in the transmission electron microscopy were correlated to premartensite phenomena. A shift in premartensitic transition temperature prior to martensitic transformation as measured by differential scanning calorimetry is being reported for the first time in this system. - Highlights: • Atomic ordering influences martensitic transformation in Ni{sub 2}FeGa Heusler alloy. • Observation of tweed contrast in TEM was correlated to premartensite phenomena. • For the first time the shift in premartensite peak was observed in DSC.

36 MATERIALS SCIENCE↗

Study of the Al-T-Si (T = Fe, Co, Ni) alloys in the solid, liquid and as-quenched states

Highlights: • Analysis of the formation and evolution of crystalline phases during heat-treatment of as-quenched alloys using in-situ high-temperature XRD. • XRD study and MD simulations of SRO in liquid and amorphous Al-T-Si (T = Fe, Co, Ni) alloys. • Similarity between the CSRO in amorphous Al{sub 65}T{sub 15}Si{sub 20} (T = Fe, Ni) alloys and crystalline Al{sub 9}Fe{sub 2}Si{sub 2} and Al{sub 3}Ni phases. - Abstract: Local atomic structure of liquid and amorphous Al{sub 80 − x}T{sub x}Si{sub 20} (where T = Fe, Co, Ni and x = 10, 15) alloys has been studied by X-ray diffraction (XRD) and molecular dynamics simulations. Chemical short-range order in the liquid and amorphous alloys has been found to be similar to that in the corresponding crystalline counterparts. Formation and evolution of crystalline phases during heat-treatment of the as-quenched ternary alloys up to liquid state were shown using in-situ XRD. Analysis of the morphology of the as-quenched and annealed Al-T-Si ribbons has been performed by transmission electron microscopy.

36 MATERIALS SCIENCE↗

Characterization of the microstructures and the shape memory properties of the Fe-Mn-Si-Cr-Ni-C shape memory alloy after severe plastic deformation by differential speed rolling and subsequent annealing

Highlights: • The Fe-SMA was subjected to severe plastic deformation and then annealed. • Recovery strain increased with increasing grain size. • An optimum grain size existed for the largest recovery stress. • Grain reduction is useful for having a high recovery stress. - Abstract: The Fe-13.51Mn-4.82Si-8.32Cr-3.49Ni-0.15C shape memory alloy was subjected to severe plastic deformation by high-ratio differential speed rolling and subsequent annealing (between 873 and 1373 K) to find the factors that affect recovery stress and recovery strain. As the annealing temperature increased (i. e., as grain size increased), the recovery strain increased. This was attributed to decrease in the density of grain boundaries and the density of twins with increasing grain size. The recovery stress, however, showed a different behavior. It increased with annealing temperature up to 973 K, at which an ultrafine grain size near 1.6 μm was obtained, and then decreased with further increase in the temperature. The difference between the recovery strain and the plastic strain induced by recovery stress under constrained displacement during cooling was proposed to determine the amount of recovery stress. There was an optimum grain size for the largest difference between the recovery strain and the plastic strain. The current study shows that grain-size reduction is not good for having a high recovery strain but it is beneficial for having a high recovery stress in the Fe-Mn-Si shape memory alloys.

36 MATERIALS SCIENCE↗

A new tetragonal phase in CoFeCrGe Heusler alloy

Highlights: • CoFeCrGe ribbons were prepared. The ribbons annealed at 500 °C are composed of three compounds. • The primary compound is the L2{sub 1}-type with a = 0.571 nm and the B2 type with a = 0.286 nm in further disorder case. • The secondary compound has a cubic Cr{sub 3}Ge structure with a = 0.461 nm. • The tertiary compound is a new tetragonal structure with lattice parameters a = 0.76 nm, c = 0.284 nm. • The difference in the magnetic hysteresis loops of the samples annealed at 300 °C and 500 °C has been interpreted. - Abstract: CoFeCrGe ribbons were prepared by melt spinning and then annealed at 300 °C for 4 h and 500 °C for 4 h, respectively. The as-spun ribbons of CoFeCrGe have the B2 type structure with a = 0.287 nm. The CoFeCrGe ribbons annealed at 300 °C are composed mainly of the L2{sub 1} type structure with a = 0.578 nm in partial disorder and the B2 type structure with a = 0.289 nm in further disorder case. The ribbons annealed at 500 °C are composed of three compounds with average compositions of Co{sub 26.0}Fe{sub 26.5}Cr{sub 23.5}Ge{sub 24.0}, Co{sub 3.8}Fe{sub 6.4}Cr{sub 68.5}Ge{sub 21.3} and Co{sub 53.4}Fe{sub 30.4}Cr{sub 8.6}Ge{sub 7.6}, listed in a sequence of volume percentage from major to minor. The primary compound Co{sub 26.0}Fe{sub 26.5}Cr{sub 23.5}Ge{sub 24.0} is the L2{sub 1}-type structure with a = 0.571 nm in partial disorder and the B2 type structure with a = 0.286 nm in further disorder case. The secondary compound Co{sub 3.8}Fe{sub 6.4}Cr{sub 68.5}Ge{sub 21.3} has a cubic Cr{sub 3}Ge structure with a = 0.461 nm. The tertiary compound Co{sub 53.4}Fe{sub 30.4}Cr{sub 8.6}Ge{sub 7.6} is a new tetragonal structure with lattice parameters a = 0.76 nm, c = 0.284 nm, which were determined by using tilt-series electron diffraction technique in this work. The tertiary (Co, Fe)-rich phase is usually embedded in the matrix of the secondary Cr-rich phase, but there is no special orientation between the two phases. The difference in the magnetic hysteresis loops of the samples annealed at 300 °C and 500 °C has been interpreted as the appearance of the new tetragonal crystalline phase. Element doping is the possible way for further developing the single tetragonal phase or increasing the amount of this phase.

36 MATERIALS SCIENCE↗

Effect of cooling rate and Co content on the formation of Fe-rich intermetallics in hypoeutectic Al7Si0.3Mg alloy with 0.5%Fe

Highlights: • Co element is firstly used in Al-0.7Si-0.3Mg alloy with 0.5 wt.% Fe to modify the morphology of Fe-rich intermetallics. • 0.75 wt.% Co addition is sufficient to suppress the undesirable effect of acicular Fe-rich intermetallics. • Co/Fe ratio determine the morphology and crystal structure of intermetallics and the optical ratio is in the range of 1-2. - Abstract: The effects of cooling rate and Co addition (0–1 wt%) on the Fe-rich intermetallics in Al7Si0.3Mg alloy with 0.5%Fe were studied in this study. The evolution of microstructure and crystal structure have been characterized by metallographic and transmission electron microscopy. The results indicated that higher cooling rate and Co addition were beneficial to modify the morphology and decrease the size of Fe-rich intermetallics. At the particular cooling rate of 2 k/s, 0.75 wt% Co was proved to be sufficient to improving the morphology of intermetallics from harmful acicular β-Al5FeSi phase to Chinese script or skeleton α-Al15(Fe,Co)3Si2 phase. Above all, the Co/Fe ratio in intermetallics was found to be an importance parameter in determining the morphology and crystal structure of (Fe,Co)-rich intermetallics. With the ratio increased from 0 to 3, the morphology changed gradually: acicular shape→short rod-like shape→Chinese script/skeleton like shape→rod-like shape. And the crystal structure of (Fe,Co)-rich intermetallics evolved from Monoclinic→Hexagonal→Simple cubic→Body-centered structure correspondingly. The optimal ratio of Co to Fe in intermetallics, which has Chinese script with hexagonal structure, was in the range of 1–2.

36 MATERIALS SCIENCE↗