Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Ferritic steels”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 343 records · Page 19

Electric Drive Technologies Research: Bottom-Up Soft Magnetic Composites (FY2022 Annual Progress Report)

In order to meet 2025 goals for enhanced peak power (100 kW), specific power (50 kW/L), and reduced cost (3.3 $\$$/kW) in a motor that can operate at ≥ 20,000 rpm, improved soft magnetic materials must be developed. Better performing soft magnetic materials will also enable rare earth free electric motors. In fact, replacement of permanent magnets with soft magnetic materials was highlighted in the Electrical and Electronics Technical Team (EETT) Roadmap as a R&D pathway for meeting 2025 targets. Eddy current losses in conventional soft magnetic materials, such as silicon steel, begin to significantly impact motor efficiency as rotational speed increases. Soft magnetic composites (SMCs), which combine magnetic particles with an insulating matrix to boost electrical resistivity (ρ) and decrease eddy current losses, even at higher operating frequencies (or rotational speeds), are an attractive solution. Today, SMCs are being fabricated with values of ρ ranging between 10 -3 to 10 -1 μohm∙m, which is significantly higher than 3% silicon steel (~0.05 μohm∙m). The isotropic nature of SMCs is ideally suited for motors with 3D flux paths, such as axial flux motors. Additionally, the manufacturing cost of SMCs is low and they are highly amenable to advanced manufacturing and net-shaping into complex geometries, which further reduces manufacturing costs. There is still significant room for advancement in SMCs, and therefore additional improvements in electrical machine performance. For example, despite the inclusion of a non-magnetic insulating material, the electrical resistivities of SMCs are still far below that of soft ferrites (10 – 10 8 μohm∙m).

33 ADVANCED PROPULSION SYSTEMS↗

Structure and elevated temperature properties of carbon-free ferritic alloys strengthened by a Laves phase

A Laves phase, Fe2Ta, was utilized to obtain good elevated temperature properties in a carbon-free iron alloy containing 1 at. pct Ta and 7 at. pct Cr. Room temperature embrittlement resulting from the precipitation of the Laves phase at grain boundaries was overcome by spheroidizing the precipitate. This was accomplished by thermally cycling the alloys through the alpha to gamma transformation. The short-time yield strength of the alloys decreased very slowly with increase in test temperature up to 600 C, but above this temperature, the strength decreased rapidly. Results of constant load creep and stress rupture tests conducted at several temperatures and stresses indicated that the rupture and creep strengths of spheroidized 1 Ta-7 Cr alloy were higher than those of several commercial steels containing chromium and/or molybdenum carbides but lower than those of steels containing substantial amounts of tungsten and vanadium. When molybdenum was added to the base Fe-Ta-Cr alloy, the rupture and creep strengths were considerably increased.

Bhandarkar, M. D.↗

The microstructural evolution, crystallography, and thermal processing of ultrahigh carbon Fe-1.85 pct C melt-spun ribbon

A study is presented to determine if fine microstructures could be achieved using rapid solidification to produce a fine-grained fully austenitic starting structure and then using thermal processing cycles to produce an even finer ferrite-cementite structure. The evolution, mechanisms of grain refinement, and crystallography of the resultant microstructures were examined by TEM. A thermal processing cycle consisted of quenching the ribbon in liquid nitrogen, tempering at 600 C for 10 sec, 'upquenching' to 750 C for 10 sec, and subsequently quenching again in liquid nitrogen. The heat-treatment resulted in martensite grains with sizes of about 1 micron or less in both length and thickness and cementite particles of 0.4 micron or less. It is concluded that these microstructures could be used for producing fine-grained ultrahigh carbon steels of very high strength without the brittleness associated with the formation of coarse carbide particles of the loss of strength due to graphite formation.

Spanos, G.↗

Investigation of the Effect of Chrome and Nickel Concentrations During Two-Piston Splat Quenching of Austenitic Stainless Steels

For solidification rates at or near equilibrium solidification conditions the effects of chrome (Cr) and nickel (Ni) on stainless steel solidification modes and microstructures are well detailed. However, fusion-based additive manufacturing (FBAM) processes that rely on faster, more rapid solidification rates call for a more in-depth understanding of the effects of rapid solidification on the solidification behavior and how these change with variations in alloy composition. Eleven custom stainless steel (SS) alloys with unique compositions based on 316L were made using targeted alloying element additions to generate feedstock with Cr/Ni eq ratios ranging from 0.9 to 2.1. Two-piston splat quenching (SQ) was used to produce rapid solidification conditions similar to those achieved in powder bed fusion processes in a fraction of the time and cost of traditional methods. Employing heat transfer simulations, SEM, TEM, and STEM characterization techniques, the SQ process was found to consistently produce solidification rates estimated to be between ~ 0.4 and 1.6 m/s. Five unique solidification microstructures were identified within the rapidly solidified SQ samples (primary austenite, massively transformed ferrite to austenite, primary austenite and massively transformed ferrite to austenite, primary ferrite, and primary ferrite and massively transformed ferrite to austenite). Both the primary ferrite solidification mode and primary ferrite phase were found to form at lower Cr/Ni eq values than previously predicted. SQ samples with compositions that were within the compositional specifications for 316L SS, an alloy which is commonly used in FBAM processes, demonstrated a wider range of potential solidification modes and microstructures that could form at rapid solidification rates than expected. Finally, by using SQ as a means to simulate rapid solidification conditions similar to those observed in FBAM processes, potential new alloy compositions can be screened faster and more cost effectively than purchasing and running test batches of the metallic powder.

36 MATERIALS SCIENCE↗

Microstructural Evolution of Steel During Magnetic Field-Assisted Processing

Advancing magnetic field-assisted processing, as an energy-efficient method for tailoring steel microstructures, requires a thorough understanding of how the high magnetic field impacts microstructural evolution, particularly its effect on prior austenite grain structures. The current investigation of a near-eutectoid composition, Fe-C alloy, uses electron backscatter diffraction to examine the morphology and orientation of martensite and pearlite microstructures, and to reconstruct the parent austenite microstructures present during equivalent heating under varied magnetic field strengths (0-T, 2-T, 5-T, and 9-T). It was observed that the magnetic field has a negligible effect on martensite lath/block width, slightly decreases prior austenite grain size, and increases the fraction of austenite grains with annealing twins. Additionally, the magnetic field increases the phase fraction of proeutectoid ferrite but has a negligible effect on pearlite block size and the distribution of boundary misorientation angles. No preferred texture was induced by the magnetic field, regardless of the applied field direction, in the proeutectoid ferrite phase or the martensite and prior austenite microstructures. Furthermore, the observed results contradict previous literature, and the differences are discussed.

Magnetic Materials↗

USE OF TWO-PISTON SPLAT QUENCHING TO INVESTIGATE & CHARACTERIZE THE IMPACT OF COMPOSITIONAL VARIATIONS ON RAPID SOLIDIFICATION MICROSTRUCTURES & SUB-MICROSCALE FEATURES IN STAINLESS STEEL ALLOY.

The objective of this dissertation was to use two-piston splat quenching (SQ) to investigate the impact of compositional modifications on the solidification and microstructure of rapidly solidified austenitic stainless steels (SS) and to demonstrate the ability of SQ to quickly and effectively simulate rapid solidification conditions similar to those found in powder bed fusion (PBF) additive techniques. PBF techniques like laser powder bed fusion (LPBF) are being implemented across a breadth of research and industrial applications to create parts with complex geometries and performance capabilities while pushing the current limits of processing conditions and understanding of material systems. In this work, SQ was used to experimentally produce rapid solidification in 20+ unique austenitic SS compositions with systematic variations of the chrome and nickel equivalency ratio (Cr/Nieq) through targeted compositional modifications. From the targeted change of Cr, Ni, and Mo concentrations in rapidly solidified SS alloys, the ferrite solidification mode was found to be the primary solidification mode at significantly lower Cr/Nieq than previously predicted for RS. Also, decreasing concentrations of Fe at a constant Cr/Nieq ratio (i.e., different Fe isopleths), or increased Mo concentrations at a constant Cr/Nieq ratio were found to suppress the ferrite to austenite massive transformation when compared to alloys with lower concentrations at the same Cr/Nieq. Using an established empirical relationship between cell size and cooling rate, the SQ technique was estimated to produce cooling rates between 106 and 108 K/s. Thermal gradients were extracted from 2-D heat transfer simulations of the SQ solidification event and used with these cooling rates to produce solidification rate estimates for SQ which were between 0.4-1.6m/s. The primary solidification mode was observed to be the determining factor in which elements segregated to the cell boundaries during RS, for which Cr and Mo were the main elements to segregate during primary austenite solidification and Ni during primary ferrite solidification. Finally, the solidification rates and conditions produced by SQ experiments resulted in similar microstructures, features, and microsegregation to what was found in LPBF samples of the same feedstock.

Hasenbusch, Zachary↗

Characteristics of Ferromagnetic Flux Focusing Lens in the Development of Surface/Subsurface Flaw Detector

Electromagnetic NDE techniques have in the past steered away from the use of ferromagnetic materials. Although their high permeabilities lead to increased field levels, the properties of ferrous elements in the presence of alternating magnetic fields are difficult to determine. In addition, their use leads to losses which can be minimized through the use of low conductivity ferrites. In fact, the eddy current probes which do incorporate ferromagnetic materials have focused on these losses and the shielding which can be obtained by surrounding a probe with a high permeability, conducting material. Eddy current probes enclosed in conducting and magnetic shields have been used to prevent the generated fields from interacting with materials in the vicinity of the probe, such as when testing near material boundaries. A recent invention has used ferromagnetic shielding to magnetically separate individual concentric eddy current probes in order to eliminate cross-talk between the probes so that simultaneous detection of different types of flaws at different depths can be achieved. In contrast to the previous uses of ferromagnetic materials purely as magnetic shields, an electromagnetic flaw detector recently developed at NASA Langley Research Center takes advantage of the flux focusing properties of a ferromagnetic mild steel in order to produce a simple, effective device for the non-destructive evaluation of conducting materials. The Flux Focusing Eddy Current Probe has been shown to accurately measure material thickness and fatigue damage. The straight forward flaw response of the probe makes the device ideal for rapid inspection of large structures, and has lead to its incorporation in a computer controlled search routine to locate fatigue crack tips and monitor experimental fatigue crack growth experiments.

Wincheski, Buzz↗

Limiting Retained Austenite Decomposition in Quenched and Tempered Steels: Influences of Rapid Tempering and Silicon

Tempering reactions are critical to microstructure and property control in martensitic steels. Here, retained austenite decomposition and cementite precipitation are monitored using Mössbauer spectroscopy in 4340 and 300-M steel under conventional and rapid tempering conditions. Tempering times are compared at a constant tempered hardness by increasing tempering temperatures associated with short time conditions to achieve equivalent matrix softening to that of longer tempering times. Time-temperature combinations that provide equivalent tempered hardness generated microstructures with similar dislocation densities and cementite precipitation fractions; these mechanisms are controlled by self-diffusion. However, systematic differences in retained austenite content were observed at a given degree of softening, where shorter tempering times exhibited higher levels of retained austenite compared to more conventional conditions. At low temperatures, the differences in retained austenite preservation between explored time-temperature conditions are attributed to corresponding differences in carbon diffusion distance (in austenite), the controlling diffusional process of retained austenite decomposition. At higher temperatures, retained austenite decomposition exhibits C-curve kinetic behavior in 4340. Thus, reduced thermodynamic driving force for cementite and ferrite formation at higher temperature is believed to play a role in restricting retained austenite decomposition within some short-time, high temperature tempering regimes. The addition of silicon pushes cementite precipitation and retained austenite decomposition to higher temperatures, although retained austenite decomposition is suppressed to a greater extent than cementite precipitation. Potential is illustrated for coupling rapid tempering with silicon alloying to produce appreciably tempered martensite (~490 HV) with relatively less retained austenite decomposition compared to conventional tempering conditions.

36 MATERIALS SCIENCE↗

A Comparison of Solidification Structures and Submicroscale Cellular Segregation in Rapidly Solidified Stainless Steels Produced via Two-Piston Splat Quenching and Laser Powder Bed Fusion

Fusion-based additive manufacturing techniques leverage rapid solidification (RS) conditions to create parts with complex geometries, unique microscale/nanoscale morphological features, and elemental segregation. Three custom composition stainless steel alloys with varying chromium equivalence to nickel equivalence ratio (Cr eq /Ni eq ) between 1.53 and 1.95 were processed using laser powder bed fusion (LPBF) and/or two-piston splat quenching (SQ) to produce solidification rates estimated between 0.4 and 0.8 m/s. Both scanning electron microscopy (SEM) and transmission electron microscopy (TEM) were utilized to collect high-resolution images, electron backscatter diffraction (EBSD) phase identification, and measure cellular segregation. Similar features were observed in both LPBF and SQ samples including phase and microstructure, nanoscale oxide particles, cell size, and segregation behavior. However, dislocation pileup was observed along the cell boundaries only in the LPBF austenite solidified microstructure. Targeted adjustment of the SQ feedstock Cr and Ni concentrations, within the ASTM A240 specification for 316L resulted in no observable impact on the cell size, oxide particle size, or magnitude of segregation. Also, the amount of Ni segregation in the ferrite solidified microstructures did not significantly differ, regardless of Cr/Ni eq or processing technique. Here, SQ is demonstrated as capable of simulating RS rates and microstructures similar to LPBF for use as an alternative screening tool for new RS alloy compositions.

42 ENGINEERING↗

The Role of Convection and Growth Competition in Phase Selection in Microgravity: Controlled Convection in the Containerless Processing of Steel Alloys

Containerless processing using electromagnetic levitation (EML) is a powerful technique in the investigation of reactive molten metal systems. On ground, the power required to overcome the weight of the sample is sufficient to cause significant heating and induce substantial melt convection. In microgravity, the heating and positioning fields may be decoupled and the field strength may be varied to achieve the desired level of convection within the limits set by the geometry of the levitation coil and the sample size. From high-speed digital images of the double recalescence behavior of Fe-Cr-Ni alloys in ground-based testing and in reduced-gravity aboard the NASA KC-135 parabolic aircraft, we have shown that phase selection can be predicted based on a growth competition model. An important parameter in this model is the delay time between primary nucleation and subsequent nucleation of the stable solid within the liquid/metastable solid array. This delay time is a strong function of composition and a weak function of the undercooling of the melt below the metastable liquidus. From the results obtained during the first Microgravity Sciences Laboratory (MSL-1) mission, we also know that convection may significantly influence the delay time, especially at low undercoolings. Currently, it is unclear what mechanism controls the formation of a heterogeneous site that allows nucleation of the austenitic phase on the pre-existing ferrite skeleton. By examining the behavior of the delay time under different convective conditions, we hypothesize that we can differentiate between several of these mechanisms to gain an understanding of how to control microstructural. evolution. We will anchor these predictions by examining samples quenched at different times following primary recalescence in microgravity. A second important parameter in the growth competition model is the identification of the growth rate of the stable phase into the semi-solid array that formed during primary recalescence. Current dendritic growth theory is inadequate in predicting solidification behavior under these conditions as metallographic analyses show that stable phase growth proceeds along the interface between the metastable solid and residual liquid. Since growth velocity is independent of the initial undercooling relative to the metastable liquidus, we hypothesize that purely thermal effects can be separated from other important growth model parameters by careful selection of the liquid composition in a ternary system.

Matson, D. M.↗

Acid Dissolution Behavior of Ferritic FeCrAl Tubes Candidates for Nuclear Fuel Cladding

The international materials community is engaged in finding safer alternatives to zirconium alloys for the cladding of fuel in light water reactors. One solution is to replace the zirconium cladding using ferritic iron-chromium-aluminum (FeCrAl) alloys, which offer extraordinary resistance to high-temperature reaction with air or steam due to the formation of a protective alumina layer on the external surface. It is important to characterize the behavior of FeCrAl not only during accident conditions but in the entire fuel cycle, which may include reprocessing of the used fuel after it is removed from the power reactors. The reprocessing may involve the dissolution of the fuel rods in mineral acids. Little or nothing is known on the dissolution of FeCrAl alloys in common mineral acids, therefore the objective of this research was to study the dissolution of typical cladding tubing having two compositions of FeCrAl (APMT and C26M) in three acids (H 2 SO 4 , HNO 3 , and HCl) as a function of the temperature using both standard ASTM immersion tests as well as electrochemical tests. The dissolution behavior of the FeCrAl alloys is compared to the dissolution capability of other traditional nuclear materials such as austenitic stainless steels (304SS and 316SS) and austenitic nickel alloys (Alloy 600 and Hastelloy C-276). Results show that both C26M and APMT have a higher dissolution capability in the studied mineral acids, which will be beneficial for reprocessing procedures.

36 MATERIALS SCIENCE↗

316L Stainless Steel Wire Arc Additive Manufacturing and Characterization for Potential SNF Canister Production

In this paper, 316L stainless steel (316L SS) straight walls, curved walls, and vessels were printed by wire arc additive manufacturing (WAAM) using the 316L SS welding wire, to demonstrate the feasibility of spent nuclear fuel (SNF) canisters using this advanced manufacturing technique. Helium leak test with leak tight criteria of 1 × 10-7 ref-cc/s were performed on printed vessels with various wall thickness, and testing pressures were from 0.345 MPa (50 psi) to 1.724 MPa (250 psi). Printed wall microstructures were characterized using optical microscopy (OM) and scanning electron microscopy (SEM). Tensile specimens were machined out from printed walls along the length, height, and thickness directions, respectively, and tested at different temperature conditions, room temperature, 80 °C, 150 °C and 250 °C, respectively. Results showed t hat, all five WAAM-printed canisters with different thickness passed the helium leaktight criteria of radioactive materials containers by the ANSI N14.5; Dispersed micrometer-level size inclusions/voids were observed at printed wall cross sections, dendritic microstructures were found with grain size variation through the welding torch shifting direction, and very small amount of δ-ferrite and σ-phase were also observed in those cross sections; The printed walls were ductile, all tensile specimens broke with large plastic deformation/elongation and without brittle failure, and printed specimens yield strengths and tensile strengths under room temperature and 80 °C conditions are higher than minimum values of 316L SS for pressure vessels and for general applications at room temperature required by the ASTM standard, respectively.

Tang, Wei↗

Weld Strength and Heat Affected Zone Size in Friction Welded NFA and CostE

Friction welding (FW) enables joining of dissimilar metals parts up to the limits of their strength. CostE and NFA are two high-temperature steel alloys used in land-based power generation. These alloys were joined with FW, and the effect of process parameters on post-welded structure and tensile strength was studied. Weld energy primarily determined the heat-affected zone (HAZ) thickness in both alloys. The highest joint efficiencies – up to 96% – resulted from contact strengthening of thin NFA HAZ regions, but too thin of a HAZ resulted in an unreliable joint. Conversely, thick HAZ regions consistently lowered the weld strength. Optimal welding conditions occur with sufficient energy to create a full bond but not so much to notably lower weld strength.

friction welding, rotary friction welding, nanostr↗

Comprehensive insights into competitive oxidation/sulfidation reactions on binary ferritic alloys at high temperatures

Interpreting high-temperature corrosion induced by mixed-gas atmospheres is challenging due to the different contributions of oxidizing gases. In this work, a comprehensive study on the combined oxidation/sulfidation using label molecules is presented. Fe-Cr model alloys with 2 wt% and 9 wt% Cr were isothermally exposed using a volumetric mixture of 0.5%S 16 O 2 /27%H 2 18 O and 0.5%S 16 O 2 /7%H 2 18 O at 650 °C for 5 h and then characterized by secondary ion mass spectroscopy (SIMS). Additionally, the reactions were followed in-situ utilizing energy dispersive X-ray diffraction. The study showed that both S 16 O 2 and H 2 18 O contribute to the oxidation of the alloys but to different extents depending on the Cr-content.

36 MATERIALS SCIENCE↗

Effect of Initial Microstructure on the Toughness of Coarse-Grained Heat-Affected Zone in a Microalloyed Steel

Toughness of the coarse-grained-heat-affected-zone (CGHAZ) strongly depends on the prior austenite grain size. The prior austenite grain size is affected not only by chemical composition, thermal cycle, and dissolution of second-phase particles, but also by the initial microstructure. The effect of base metal microstructure (ferrite/pearlite obtained by air cooling and martensite obtained by water-quenching) on Charpy impact toughness of the CGHAZ has been investigated for different heat inputs for high-heat input welding of a microalloyed steel. A welding thermal cycle with a heat input of 100 kJ/cm and 400 kJ/cm were simulated on the MMS-300 system. Despite a similar microstructure in the CGHAZ of both the base metals, the average Charpy impact energy for the air-cooled base metal was found to be higher than the water-quenched base metal. Through thermo-kinetic simulations, it was found that a higher enrichment of Mn/C at the ferrite/austenite transformation interface of the CGHAZ of water-quenched base metal resulted in stabilizing austenite at a lower A1 temperature, which resulted in a coarser austenite grain size and eventually lowering the toughness of the CGHAZ.

36 MATERIALS SCIENCE↗

Corrosion behavior of ferritic FeCrAl alloys in simulated BWR normal water chemistry

Ferritic iron-chromium-aluminum (FeCrAl) alloys with varying Cr content were subjected to in-situ irradiation-corrosion with energetic protons or electron beams in pure water with various oxygen concentrations. Oxide microstructure and composition were characterized to compare the corrosion under irradiation with the thermal corrosion in the same water conditions. The dominant effect seems to be the production of H 2 O 2 at the surface by the intense proton and electron beams. The corrosion potential of FeCrAl under BWR-NWC condition is somewhat above the Cr 2 O 3 /CrO 4 2- phase boundary, oxidizing the Cr(III) to Cr(VI) in the outer part of the film, but with some Cr(III) remaining in the interior of the oxide. The beam increases the corrosion potential, significantly reducing Cr(III) content throughout the oxide. Finally, the crystallites on the surface, which form by re-precipitation from solution, do not contain Cr because at low potential Cr(III) is not soluble, and at high potential Cr(VI) is quite soluble.

36 MATERIALS SCIENCE↗

Extended continuous cooling transformation diagram for 410 stainless steel encompassing δ → γ and γ → αʹ transformations determined by dilatometry

In this study, we use dilatometry to construct an extended Continuous Cooling Transformation (CCT) diagram for 410 stainless steel, capturing both δ → γ and γ → αʹ transformations specifically for directed energy deposition (DED) additive manufacturing (AM) applications. To ensure that the findings are representative of AM specific microstructures and compositions, dilatometry coupons were extracted from a wire arc DED wall, thereby preserving the inherent microstructural and compositional variability within the material. The on-heating phase transformations, including A c1 , A c3 , and γ → δ, were found to be essentially location independent, despite the typical heterogeneity associated with AM. Conversely, increasing cooling rates were observed to shift the start and finish temperatures of both δ → γ and γ → αʹ transformations to lower values. The resulting extended CCT diagram offers a more complete depiction of phase transformation behavior in the system, enabling accurate microstructure evolution modeling and residual stress predictions specifically for directed energy deposition additive manufacturing applications.

Additive manufacturing↗

Intermediate-Term Thermal Aging Effect Evaluation for Grade 92 and 316L at The LWR Relevant Temperature

Life extension of the existing nuclear reactors imposes accumulated damages, such as higher fluences and longer period of corrosion, to structural materials, which would result in significant challenges to the traditional reactor materials such as type 304 and 316 stainless steels. Advanced alloys with superior radiation resistance will increase safety margins, design flexibility, and economics for not only the life extension of the existing fleet but also new builds with advanced reactor designs. The Electric Power Research Institute (EPRI) teamed up with Department of Energy (DOE) on the Advanced Radiation Resistant Materials (ARRM) program, aiming to develop and test degradation resistant alloys from current commercial alloy specifications by 2021 to a new advanced alloy with superior degradation resistance in light water reactor (LWR)-relevant environments by 2024. Based on a comprehensive microstructure and property screening performed in Phase-1 of the ARRM program, a total of five alloys, together with 316L and X-750 as references, were down-selected for Phase-2 neutron irradiation studies. Because thermal aging could exert a synergistic effect on neutron irradiation due to the low neutron damage rate on the order of 10 –7 displacements per atom per second (dpa/s), Grade 92 (one of the five down-selected alloys) and two heats of 316L were selected in this task to study the effect of aging at 350°C for 12.5–12.7 kh on microstructure and mechanical properties. The aging time is approximately corresponding to 5 dpa neutron irradiation, which can be served as a reference for the 5-dpa-irradiated samples of the alloys to help understand the independent neutron damage influence on microstructure and mechanical properties. Optical microscopy and scanning electron microscopy were used for microstructural characterization. Hardness, tensile, Charpy impact toughness, and fracture toughness in the ductile regime of the aged samples were examined. The aging of Grade 92 led to the formation of many Laves phase in sizes of ~100–200 nm and resulted in some reduction in hardness and yield/ultimate tensile strength with some increases in uniform and total plastic elongations, which may have helped the enhancement of Charpy impact toughness, e.g., ~4 J increase in upper-shelf energy and 20.5°C reduction in ductile-brittle transition temperature compared with the unaged condition. The fracture toughness of the aged Grade 92 showed decent toughness of ~303 MPa√m (K Jq ) with ~87 tearing modulus at 22°C, which reduced to ~241 MPa√m (~20% reduction) with ~75 tearing modulus at 300°C. The two heats of 316L are differentiated by their amounts of δ-ferrite, i.e., ~1 vol% in heat T1103 and ~4 vol% in heat N5B8. The two heats of 316L were subjected to 15% cold work (CW) as this condition is often used in nuclear reactors to help trapping radiation-induced defects and thus postpone the steady state swelling stage. The aging did not result in any noticeable microstructure changes, except for possible segregations at grain boundaries that need to be further investigated. The aging resulted in slight reduction in hardness of 316L-T1103 and slight increase in hardness of 316L-N5B8, which is consistent with their tensile testing results. The 15%CW might have introduced some inhomogeneity, resulting in large standard deviations in hardness, which were reduced after the aging. The aged 316L followed the same trend as the unaged condition for the strength and elongation results from the tensile testing. Minimum elongations appeared within ~300–600°C, above which the elongations seem to increase. Unlike the negligible or minor changes in microstructure, hardness and tensile results of the two heats of 316L, their fracture toughness showed noticeable difference. The aged 316L-T1103 showed good toughness of ~350 MPa√m with ~80 tearing modulus at 22°C, which reduced to ~271 MPa√m (~23% reduction) with ~83 tearing modulus at 300°C. In contrast, the aged 316L-N5B8 showed lower toughness of ~244 MPa√m with ~53 tearing modulus at 22°C, which reduced to ~180 MPa√m (~26% reduction) with ~31 tearing modulus at 300°C. The preliminary results indicate that the presence of high volume of δ-ferrite would noticeable impair fracture toughness although it may not influence hardness and tensile properties.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗