Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “tungsten”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 325 records · Page 18

Characterizing Surface Acidic Sites in Mesoporous-Silica-Supported Tungsten Oxide Catalysts Using Solid State NMR and Quantum Chemistry Calculations

The acidic sites in dispersed tungsten oxide supported on SBA-15 mesoporous silica were investigated using a combination of pyridine titration, both fast-, and slow-MAS {sup 15}N NMR, static {sup 2}H NMR, and quantum chemistry calculations. It is found that the bridged acidic -OH groups in surface adsorbed tungsten dimers (i.e., W-OH-W) are the Broensted acid sites. The unusually strong acidity of these Broensted acid sites is confirmed by quantum chemistry calculations. In contrast, terminal W-OH sites are very stable and only weakly acidic as are terminal Si-OH sites. Furthermore, molecular interactions between pyridine molecules and the dimer Broensted and terminal W-OH sites for dispersed tungsten oxide species is strong. This results in restricted molecular motion for the interacting pyridine molecules even at room temperature, i.e., a reorientation mainly about the molecular 2-fold axis. This restricted reorientation makes it possible to estimate the relative ratio of the Broensted (tungsten dimer) to the weakly acidic terminal W-OH sites in the catalyst using the slow-MAS {sup 1}H-{sup 15}N CP PASS method.

15N NMR↗

Tungsten Transport in an Ion Source

We present a study that gives a deeper insight into the failure mechanism of tungsten ion sources used for ion implantation in the semiconductor industry. Our experimental data, corroborated by literature thermodynamics reports, indicates that tungsten migration is the primary cause of failure for processes utilizing fluorine-containing feed gases. It is shown that tungsten is the predominant constituent of most deposits, and that volatile tungsten fluorides are the transport species responsible for metal redistribution in ion sources. It was also demonstrated that AutoClean, a new product of ATMI, can be used for filament growth control.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

In-situ observation of sputtered particles for carbon implanted tungsten during energetic isotope ion implantation

Tungsten is a candidate for plasma facing materials in future fusion reactors. During DT plasma operations, carbon as an impurity will bombard tungsten, leading to the formation of tungsten-carbon (WC) layer and affecting tritium recycling behavior. The effect of carbon implantation for the dynamic recycling of deuterium, which demonstrates tritium recycling, including retention and sputtering, has been investigated using in-situ sputtered particle measurements. The C{sup +} implanted W, WC and HOPG were prepared and dynamic sputtered particles were measured during H{sub 2}{sup +} irradiation. It has been found that the major hydrocarbon species for C{sup +} implanted tungsten is CH{sub 3}, while for WC and HOPG (Highly Oriented Pyrolytic Graphite) it is CH{sub 4}. The chemical state of hydrocarbon is controlled by the H concentration in a W-C mixed layer. The amount of C-H bond and the retention of H trapped by carbon atom should control the chemical form of hydrocarbon sputtered by H{sub 2}{sup +} irradiation and the desorption of CH{sub 3} and CH{sub 2} are due to chemical sputtering, although that for CH is physical sputtering. The activation energy for CH{sub 3} desorption has been estimated to be 0.4 eV, corresponding to the trapping process of hydrogen by carbon through the diffusion in W. It is concluded that the chemical states of hydrocarbon sputtered by H{sub 2}{sup +} irradiation for W is determined by the amount of C-H bond on the W surface. (authors)

36 MATERIALS SCIENCE↗

SPS Fabrication of Tungsten-Rhenium Alloys in Support of NTR Fuels Development

Abstract. Tungsten metal slugs were fabricated via Spark Plasma Sintering (SPS) of powdered metals at temperatures ranging from 1575 K to 1975 K and hold times of 5 minutes to 30 minutes, using powders with an average diameter of 7.8 ?m. Sintered tungsten specimens were found to have relative densities ranging from 83 % to 94 % of the theoretical density for tungsten. Consolidated specimens were also tested for their Vickers Hardness Number (VHN), which was fitted as a function of relative density; the fully consolidated VHN was extrapolated to be 381.45 kg/mm2. Concurrently, tungsten and rhenium powders with average respective diameters of 0.5 ?m and 13.3 ?m were pre-processed either by High-Energy-Ball-Milling (HEBM) or by homogeneous mixing to yield W-25at.%Re mixtures. The powder batches were sintered at temperatures of 1975 K and 2175 K for hold times ranging from 0 minutes to 60 minutes yielding relative densities ranging from 94% to 97%. The combination of HEBM and sintering showed a significant decrease in the inter-metallic phases compared to that of the homogenous mixing and sintering.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Effects of the Chodura sheath on tungsten ionization and emission in tokamak divertors

The decay of the electric potential in the sheath region in tokamak divertors occurs on a scale length on the order of the main ion gyroradius (Chodura sheath) due to magnetic fields lines intersecting the divertor plates at grazing incidence. As a consequence, high-Z impurities like tungsten ionize within the sheath region in attached plasma conditions. The modification of the electron distribution in the sheath region must thus be taken into account to accurately model ionization and emission of impurities within the sheath region. To that end, an analytical expression of the distribution of the vertical ionization path for impurities sputtered from divertor plasma-facing components is derived. This expression is then used to estimate the fraction of neutral impurities ionizing within the sheath and the average vertical ionization path, and to derive an effective SXB (the number of ionizations per emitted photon) coefficient which includes the effects of the variation of the electron distribution in the sheath region. These results are applied to tungsten impurities sputtered from divertor plates. It is shown that the SXB coefficient for neutral tungsten is significantly reduced in high-density attached divertor plasma conditions (n e ≳ 5 × 10 13 cm -3 ) because of the ionization of neutral tungsten well within the sheath region.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Effect of starting microstructure on helium plasma-materials interaction in tungsten

Here, in a magnetic fusion energy (MFE) device, the plasma-facing materials (PFMs) will be subjected to tremendous fluxes of ions, heat, and neutrons. The response of PFMs to the fusion environment is still not well defined. Tungsten metal is the present candidate of choice for PFM applications such as the divertor in ITER. However, tungsten's microstructure will evolve in service, possibly to include recrystallization. How tungsten's response to plasma exposure evolves with changes in microstructure is presently unknown. In this work, we have exposed hot-worked and recrystallized tungsten to an 80 eV helium ion beam at a temperature of 900 °C to fluences of 2 × 10 23 or 20 × 10 23 He/m 2 . This resulted in a faceted surface structure at the lower fluence or short but well-developed nanofuzz structure at the higher fluence. There was little difference in the hot-rolled or recrystallized material's near-surface (≤50 nm) bubbles at either fluence. At higher fluence and deeper depth, the bubble populations of the hot-rolled and recrystallized were different, the recrystallized being larger and deeper. This may explain previous high-fluence results showing pronounced differences in recrystallized material. The deeper penetration in recrystallized material also implies that grain boundaries are traps, rather than high-diffusivity paths.

36 MATERIALS SCIENCE↗

Degradation of electrical resistivity of tungsten following shielded neutron irradiation

A major challenge for heat transfer in nuclear materials is to ensure thermal mobility after high amounts of neutron irradiation. Tungsten is widely selected as a heat transfer material in fusion reactors. In metals, thermal conductivity is dominated by electrons’ ability to transfer energy. Neutron irradiation generates point defects, clusters, and solid transmutation (e.g.rhenium and osmium in tungsten), which inhibit electron motion. The purpose of this work is to quantify the irradiation-induced change in electron mobility and deconvolute transmutation and microstructural effects on observed changes to electron mobility. Single and polycrystalline tungsten were fast neutron irradiated in the High Flux Isotope Reactor at Oak Ridge National Laboratory to doses between 0.2 and 0.7 displacements per atom (dpa) and temperatures from 500 °C to 1000 °C. Grain growth was observed in all samples. Microstructure and transmutation were quantified. The geometric orientation of samples with elongated grains has been shown to affect electrical resistivity. A mathematical model was developed and used to deconvolute solid-solution transmutation, grain, and temperature-dependent lattice effects on resistivity. At ~0.4 dpa at ~590 °C, the combined resistivity degradation due to voids, vacancies, interstitials, and dislocations is estimated to be greater than the contribution from solid solution Re transmutation, which is greater than the contribution from grain boundaries. At doses of ~0.7 dpa at ~750 °C, solid solution Re contributions are greater than all other effects combined. As a result, this work establishes a basis to predict the effects of irradiation temperature and transmutation on thermal properties of tungsten and highlights the importance of irradiation temperature.

36 MATERIALS SCIENCE↗

Tantalum-tungsten oxide thermite composites prepared by sol-gel synthesis and spark plasma sintering

Energetic composite powders consisting of sol-gel derived nanostructured tungsten oxide were produced with various amounts of micrometer-scale tantalum fuel metal. Such energetic composite powders were ignition-tested and the results show that the powders are not sensitive to friction, spark and/or impact ignition. Initial consolidation experiments, using the High-Pressure Spark Plasma Sintering (HPSPS) technique, on the sol-gel derived nanostructured tungsten oxide produced samples with higher relative density than can be achieved with commercially available tungsten oxide. The sol-gel derived nanostructured tungsten oxide with immobilized tantalum fuel metal (Ta-WO{sub 3}) energetic composite was consolidated to a density of 9.17 g cm{sup -3} or 93% relative density. In addition, those samples were consolidated without significant pre-reaction of the constituents, thus retaining their stored chemical energy. (author)

36 MATERIALS SCIENCE↗

Overview of the US-Japan collaborative investigation on hydrogen isotope retention in neutron-irradiated and ion-damaged tungsten

Plasma-facing components (PFCs) will be exposed to 14 MeV neutrons from deuterium-tritium (D-T) fusion reactions, and tungsten, a candidate PFC for the divertor in ITER, is expected to receive a neutron dose of 0.7 displacement per atom (dpa) by the end of operation in ITER. The effect of neutron-irradiation damage has been mainly simulated using high-energy ion bombardment. While this prior database of results is quite valuable for understanding the behavior of hydrogen isotopes in PFCs, it does not encompass the full range of effects that must be considered in a practical fusion environment due to short penetration depth, damage gradient, high damage rate, and high PKA energy spectrum of the ion bombardment. In addition, neutrons change the elemental composition via transmutations, and create a high radiation environment inside PFCs, which influence the behavior of hydrogen isotope in PFCs, suggesting the utilization of fission reactors is necessary for neutron irradiation. Therefore, the effort to correlate among high-energy ions, fission neutrons, and fusion neutrons is crucial for accurately estimating tritium retention under a neutron-irradiation environment. Under the framework of the US-Japan TITAN program, tungsten samples (99.99 at. % purity from A.L.M.T. Co.) were irradiated by neutron in the High Flux Isotope Reactor (HFIR), ORNL, at 50 and 300C to 0.025, 0.3, and 1.2 dpa, and the investigation of deuterium retention in neutron-irradiation was performed in the INL Tritium Plasma Experiment (TPE), the unique high-flux linear plasma facility that can handle tritium, beryllium and activated materials. This paper reports the recent results from the comparison of ion-damaged tungsten via various ion species (2.8 MeV Fe2+, 20 MeV W2+, and 700 keV H-) with that from neutron-irradiated tungsten to identify the similarities and differences among them.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Recent progress in R&D on tungsten alloys for divertor structural and plasma facing materials

Tungsten materials are candidates for plasma facing components for ITER and DEMO because of their superior thermophysical properties. Knowledge and strategies to improve properties of tungsten-based materials are still under development, as they are not a common structural material such as steel. Consequently, several activities have started in Europe, Japan, USA and China. Research is directed towards manufacturing of new materials based on alloying, microstructure stabilizing and composite formation involving improved processing steps. Beside experimental analyses, work also focuses on computational treatment of open questions, supporting the development of better tungsten materials. Assuming the availability of an ideal material that is ready to use, there remain the questions of inherent safety, the joining of tungsten to steel and the influence of radiation damage. These are topics of increasing interest when the material comes to application.

tungsten alloys, divertor structural materials, fu↗

Characterization of defect clusters in ion-irradiated tungsten by X-Ray diffuse scattering

Defect clusters in ion-irradiated tungsten are characterized by X-ray diffuse scattering. Single crystal tungsten samples are irradiated here at 300 K by 0.5–5 MeV copper ions with total doses of 0.2, 0.6, 2, and 5 displacements per atom (DPA). Analysis of the diffuse scattering intensities allows the determination of the concentration of vacancy- and interstitial-type dislocation loops as a function of loop radius for each sample. More vacancies than interstitials are observed in each sample, and the radius of the vacancy loops increases with irradiation dose. For the 0.2DPA sample the average vacancy loop radius is 10.1 ± 3.0 Å with a defect density (counting all atoms in the loops) of ( 10.2 ± 1.5 ) × 10 - 4 per tungsten atom, increasing to an average loop radius of 16.1 ± 3.1 Å at a density of ( 8.5 ± 1.0 ) × 10 - 4 per tungsten atom for the 5DPA sample.

36 MATERIALS SCIENCE↗

Simulations of grain growth in tungsten armor materials under ARC plasma edge operation conditions using an integrated plasma-edge/materials model

An integrated model of grain growth deuterium-exposed tungsten polycrystals, consisting of a two-dimensional vertex dynamics model fitted to atomistic data, has been developed to assess the grain growth kinetics of deuterium-exposed polycrystalline tungsten (W). The model tracks the motion of grain boundaries under the effect of driving forces stemming from grain boundary curvature and differential deuterium concentration accumulation. Here, we apply the model to experimentally synthesized tungsten polycrystals under deuterium-saturated conditions relevant to the ARC concept design. The results indicate rapid grain growth kinetics in the near-surface region adjacent to the plasma, where the temperature reaches 1400 K, whereas the microstructure remains stable deeper in the material with the lower temperature of 1000 K. The combined modeling and analysis further reveal that monolithic tungsten produced via conventional fabrication routes is highly susceptible to grain coarsening at temperatures exceeding 1000 K, largely independent of the magnitude of the applied driving force. Moreover, the accumulation of deuterium near grain boundaries has a pronounced inhibitory effect on grain boundary migration. High-angle grain boundaries ( > 50°) contribute more significantly to the overall grain growth process.

36 MATERIALS SCIENCE↗

Preparation of size-controlled tungsten oxide nanoparticles and evaluation of their adsorption performance

The present study investigated the effects of particle size on the adsorption performance of tungsten oxide nanoparticles. Nanoparticles 18-73 nm in diameter were prepared by evaporation of bulk tungsten oxide particles using a flame spray process. Annealing plasma-made tungsten oxide nanoparticles produced particles with diameters of 7-19 nm. The mechanism of nanoparticle formation for each synthetic route was examined. The low-cost, solid-fed flame process readily produced highly crystalline tungsten oxide nanoparticles with controllable size and a remarkably high adsorption capability. These nanoparticles are comparable to those prepared using the more expensive plasma process.

36 MATERIALS SCIENCE↗

Crystalline mesoporous tungsten oxide nanoplate monoliths synthesized by directed soft template method for highly sensitive NO{sub 2} gas sensor applications

Graphical abstract: Display Omitted Highlights: ► Mesoporous WO{sub 3} nanoplate monoliths were obtained by direct templating synthesis. ► Enable effective accession of the analytic molecules for the sensor applications. ► The WO{sub 3} sensor exhibited a high performance to NO{sub 2} gas at low temperature. -- Abstract: Controllable synthesis of nanostructured metal oxide semiconductors with nanocrystalline size, porous structure, and large specific surface area is one of the key issues for effective gas sensor applications. In this study, crystalline mesoporous tungsten oxide nanoplate-like monoliths with high specific surface areas were obtained through instant direct-templating synthesis for highly sensitive nitrogen dioxide (NO{sub 2}) sensor applications. The copolymer soft template was converted into a solid carbon framework by heat treatment in an inert gas prior to calcinations in air to sustain the mesoporous structure of tungsten oxide. The multidirectional mesoporous structures of tungsten oxide with small crystalline size, large specific surface area, and superior physical characteristics enabled the rapid and effective accession of analytic gas molecules. As a result, the sensor response was enhanced and the response and recovery times were reduced, in which the mesoporous tungsten oxide based gas sensor exhibited a superior response of 21,155% to 5 ppm NO{sub 2}. In addition, the developed sensor exhibited selective detection of low NO{sub 2} concentration in ammonia and ethanol at a low temperature of approximately 150 °C.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Improvement of charge separation in TiO{sub 2} by its modification with different tungsten compounds

Highlights: • Ammonium m-tungstate doped to TiO{sub 2} highly improved charge separation in TiO{sub 2}. • Negative electrokinetic potential of TiO{sub 2} facilitates holes migration to its surface. • Fast migration of holes to TiO{sub 2} surfaces increased yield of OH radicals formation. • Adsorption of dyes on photocatalyst increased its decomposition under visible light. - Abstract: Three different tungsten precursors were used for TiO{sub 2} modification: H{sub 2}WO{sub 4}, WO{sub 2}, and ammonium m-tungstate. It was proved that modification of TiO{sub 2} with tungsten compounds enhanced its photocatalytic activity through the improvement of charge separation. This effect was obtained by coating of TiO{sub 2} particles with tungsten compound, which changed their surficial electrokinetical potential from positive onto negative. The most efficient tungsten compound, which caused enhanced separation of free carriers was ammonium m-tungstate (AMT). Two dyes with different ionic potential were used for the photocatalytic decomposition. It appeared that cationic dye—Methylene Blue was highly adsorbed on the negatively charged surface of TiO{sub 2} modified by AMT and decomposed, however this photocatalyst was quickly deactivated whereas anionic dye—acid red was better adsorbed on the less acidic surface of TiO{sub 2} and was rapidly decomposed with almost the same rate in the five following cycles.

36 MATERIALS SCIENCE↗

ToF-SIMS spectral analysis of pristine and neutron irradiated single crystal tungsten

Time-of-flight secondary ion mass spectrometry (ToF-SIMS) has many promising features in studying materials including high spatial resolution and high mass accuracy of elements, molecules, and isotopes. Its ability to resolve isotopes is especially attractive in studying transmutation products of single crystal tungsten (SCW) post neutron irradiation. Tungsten (W) is a contender of plasma facing materials (PFMs) due to its high thermal and radiological stability. PFMs to be used in the construction of fusion vessels are subject to high temperature and neutron irradiation, resulting in changes to materials including transmutation, which ultimately impact material mechanical and thermal properties. We used IONTOF TOF.SIMS V instrument equipped with a 30 keV Bi 3 + primary ion beam to study pristine SCW and irradiated SCW speciemens. Scanning electron microscope coupled with focused ion beam (SEM-FIB) was used to reduce the dosage of neutron irradiated tungsten and prepare for specimens for SIMS analysis. Static ToF-SIMS spectra were obtained, and transmutation product peak identification was presented in this work. Identified molecules and molecular fragments were compared against isotope theoretical mass to charge ratios of tungsten, rhenium, osmium, and other relevant products. Our results show that ToF-SIMS provides a viable means to study transmutation products of W post neutron irradiation. Such applications are suitable to investigate transmutation effects on materials that are being considered and developed for fusion pilot plants.

36 MATERIALS SCIENCE↗

Femtosecond laser-induced periodic surface structure formation on tungsten

In this paper, we demonstrate the generation of periodic surface structures on a technologically important material, tungsten, at both 400 and 800 nm, despite that the table values of dielectric constants for tungsten at these two wavelengths suggest the absence of surface plasmons, a wave necessary for forming periodic structures on metals. Furthermore, we find that the structure periods formed on tungsten are significantly less than the laser wavelengths. We believe that the dielectric constants of tungsten change significantly due to intense laser pulse heating and surface structuring and roughening at nanometer scales, permitting surface plasmon excitation and periodic structure formation.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

X-ray And EUV Spectroscopy Of Highly Charged Tungsten Ions

The Berlin EBIT has been established by the Max-Planck-Institut fuer Plasmaphysik to generate atomic physics data in support of research in the field of controlled nuclear fusion, by measuring the radiation from highly charged ions in the x-ray, extreme ultraviolet and visible spectral ranges and providing valuable diagnostics for high temperature plasmas. In future fusion devices, for example ITER, currently being constructed at Cadarache, France, the plasma facing components will be armored with high-Z materials, most likely tungsten, due to the favorable properties of this element. At the same time the tremendous radiation cooling of these high-Z materials represents a threat to fusion and obliges one to monitor carefully the radiation. With EBIT a selected ensemble of ions in specific charge states can be produced, stored and excited for spectroscopic investigations. Employing this technique, we have for example resolved the wide structure observed around 5 nm at the ASDEX Upgrade tokamak as originating from E1-transitions into the open 4d shell of tungsten ions in charge states 25+ to 37+ producing a band-like emission pattern. Further, these ions emit well-separated M1 lines in the EUV range around 65 nm suitable for plasma diagnostics. Kr-like to Cr-like tungsten ions (38+ to 50+) show strong soft-x-ray lines in the range 0.5 to 2 and 5 to 15 nm. Lines of even higher charged tungsten ions, up to Ne-like W{sup 64+}, abundant in the core plasma of present and future fusion test devices, have been investigated with high resolution Bragg-crystal spectroscopy at 0.13 nm. Recently, x-ray spectroscopic measurements of the dielectronic recombination LMn resonances of W{sup 60+} to W{sup 67+} ions have been preformed and compare well with atomic structure calculations.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗