Examination of Intergranular Crack on SC0234
The microstructure of the SC0234 weld was evaluated per DA-SPEC-01067, ''General Purpose Heat Source (GPHS) Plutonium-238 Dioxide Fueled Clad Product Specification'' and it was determined that the weld microstructure conformed to the quality requirements. During the examination of weld cross section, the metallographic analysis revealed the presence of a surface crack. Prior visual examination per RPS-TA55-303 had not revealed the crack, nor did the surface photography performed per RPS-TA55-302. The presence of the crack does not violate any of the product specifications called out on DA-SPEC-01067. Although there is a well-documented history of weld hot crack susceptibility in the early development of the DOP-26 iridium alloy, a surface crack such as this had not been documented during welding at Los Alamos. In the interest of better understanding the cause; the product engineer/program recommended further examination of the crack. This report discusses the examination of the crack found in the weld cross section of simulant clad SC0234. Metallography, Scanning Electron Microscopy (SEM) and Energy Dispersive Spectroscopy techniques (EDS) where used in the analysis of the crack and the surrounding weld microstructure.