Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “fatigue”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 325 records · Page 18

Creep and Creep-Fatigue Crack Growth at Structural Discontinuities and Welds

The subsection ASME NH high temperature design procedure does not admit crack-like defects into the structural components. The US NRC identified the lack of treatment of crack growth within NH as a limitation of the code and thus this effort was undertaken. This effort is broken into two parts. Part 1, summarized here, involved examining all high temperature creep-fatigue crack growth codes being used today and from these, the task objective was to choose a methodology that is appropriate for possible implementation within NH. The second part of this task, which has just started, is to develop design rules for possible implementation within NH. This second part is a challenge since all codes require step-by-step analysis procedures to be undertaken in order to assess the crack growth and life of the component. Simple rules for design do not exist in any code at present. The codes examined in this effort included R5, RCC-MR (A16), BS 7910, API 579, and ATK (and some lesser known codes). There are several reasons that the capability for assessing cracks in high temperature nuclear components is desirable. These include: (1) Some components that are part of GEN IV reactors may have geometries that have sharp corners - which are essentially cracks. Design of these components within the traditional ASME NH procedure is quite challenging. It is natural to ensure adequate life design by modeling these features as cracks within a creep-fatigue crack growth procedure. (2) Workmanship flaws in welds sometimes occur and are accepted in some ASME code sections. It can be convenient to consider these as flaws when making a design life assessment. (3) Non-destructive Evaluation (NDE) and inspection methods after fabrication are limited in the size of the crack or flaw that can be detected. It is often convenient to perform a life assessment using a flaw of a size that represents the maximum size that can elude detection. (4) Flaws that are observed using in-service detection methods often need to be addressed as plants age. Shutdown inspection intervals can only be designed using creep and creep-fatigue crack growth techniques. (5) The use of crack growth procedures can aid in examining the seriousness of creep damage in structural components. How cracks grow can be used to assess margins on components and lead to further safe operation. After examining the pros and cons of all these methods, the R5 code was chosen as the most up-to-date and validated high temperature creep and creep fatigue code currently used in the world at present. R5 is considered the leader because the code: (1) has well established and validated rules, (2) has a team of experts continually improving and updating it, (3) has software that can be used by designers, (4) extensive validation in many parts with available data from BE resources as well as input from Imperial college's database, and (5) was specifically developed for use in nuclear plants. R5 was specifically developed for use in gas cooled nuclear reactors which operate in the UK and much of the experience is based on materials and temperatures which are experienced in these reactors. If the next generation advanced reactors to be built in the US used these same materials within the same temperature ranges as these reactors, then R5 may be appropriate for consideration of direct implementation within ASME code NH or Section XI. However, until more verification and validation of these creep/fatigue crack growth rules for the specific materials and temperatures to be used in the GEN IV reactors is complete, ASME should consider delaying this implementation. With this in mind, it is this authors opinion that R5 methods are the best available for code use today. The focus of this work was to examine the literature for creep and creep-fatigue crack growth procedures that are well established in codes in other countries and choose a procedure to consider implementation into ASME NH. It is very important to recognize that all creep and creep fatigue crack growth procedures that are part of high temperature design codes are related and very similar. This effort made no attempt to develop a new creep-fatigue crack growth predictive methodology. Rather examination of current procedures was the only goal. The uncertainties in the R5 crack growth methods and recommendations for more work are summarized here also.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Fatigue Performance of Advanced High-Strength Steels (AHSS) GMAW Joints

The fatigue performance of gas metal arc welding (GMAW) joints of advanced high strength steels (AHSS) are compared and analyzed. The steel studied included a number of different grades of AHSS and baseline mild steels: DP600, DP780, DP980, M130, M220, solution annealed boron steel, fully hardened boron steels, HSLA690 and DR210 (a mild steel). Fatigue testing was conducted under a number of nominal stress ranges to obtain the S/N curves of the weld joints. A two-phase analytical model is developed to predict the fatigue performance of AHSS welds. It was found that there are appreciable differences in the fatigue S/N curves among different AHSS joints made using the same welding practices, suggesting that the local microstructure in the weld toe and root region plays non-negligible role in the fatigue performance of AHSS welds. Changes in weld parameters can influence the joint characteristics which in turn influence fatigue life of the weld joints, particularly of those of higher strength AHSS. The analytical model is capable of reasonably predicting the fatigue performance of welds made with various steel grades in this study.

36 MATERIALS SCIENCE↗

Fatigue-crack initiation and growth in notched 2024-T3 specimens monitored by a video tape system

Fatigue-crack initiation and early stages of growth in notched 2024-T3 aluminum alloy sheet specimens were monitored during constant-amplitude fatigue tests conducted for a range of stress ratios. A video tape system was developed to detect fatigue cracks 0.1 mm in length on the sheet surface and to monitor their growth. Fatigue cracks initiated either at the notch corner or on the notch surface. Most of the first fatigue cracks started as notch-corner cracks, and the crack-initiation period was defined as the number of cycles for which the crack was 0.1 mm in length on the sheet surface. For each of the stress ratios used, the results showed that at the low stress levels, the crack-initiation period constituted at least 90 percent of the fatigue lives. However, for the negative stress ratios at the high stress levels, cracks started as early as at about 40 percent of the fatigue lives.

Sova, J. A.↗

Rolling-element fatigue life of AMS 5749 corrosion resistant, high temperature bearing steel

The rolling element fatigue lives of AMS 5749 and AISI M-50 were compared in tests run in the five ball fatigue tester and the rolling contact fatigue tester. The effects of double vacuum melting and retained austenite on the life of AMS 5749 were determined in five ball fatigue tests. The double vacuum melting process consisted of induction vacuum melting followed by vacuum arc remelting (VIM-VAR). In the five ball tests, VIM-VAR AMS 5749 gave lives at least six times that of VIM-VAR AISI M-50. Similar tests in the rolling contact fatigue tester showed no significant difference in the lives of the two materials. The rolling element fatigue life of VIM-VAR AMS 5749 was at least 14 times that of vacuum induction melted AMS 5749. A trend toward increased rolling element fatigue life with decreased retained austenite is apparent, but the confidence that all experimental differences are significant is not great.

Parker, R. J.↗

A temperature dependent fatigue failure criterion for graphite/epoxy laminates

A fatigue failure criterion applicable to composite materials is developed and applied to predict the fatigue behavior of graphite/epoxy laminates with particular emphasis on the influence of temperature. Tensile stress-strain curves and tension-tension fatigue curves for various unidirectional, angle-ply and symmetrically balanced laminates were developed at test temperatures of 25 C, 74 C, and 114 C. For most laminates a reduction in both static strength and fatigue strength is observed with increasing temperature. This reduction appeared more severe in fatigue loading than in static tensile loading and most severe where the shear stress in the lamina is the dominate failure mode. Through an analytical formulation of shifting functions for the influences of temperature, all fatigue data are shown to be capable of being reduced to a single reference curve at some temperature. Examples are given which demonstrate the capability of the fatigue failure criterion to predict failure of complex symmetrically balanced laminates from relevant parameters obtained from the observed behavior of unidirectional and angle-ply laminates.

Rotem, A.↗

A temperature dependent fatigue failure criterion for graphite/epoxy laminates

A fatigue failure criterion applicable to composite materials is developed and applied to predict the fatigue behavior of graphite/epoxy laminates with particular emphasis on the influence of temperature. Tensile stress-strain curves and tension-tension fatigue curves for various unidirectional, angle-ply and symmetrically balanced laminates were developed at test temperatures of 25 C, 74 C and 114 C. In general for most laminates a reduction in both static strength and fatigue strength is observed with increasing temperature. This reduction appeared more severe in fatigue loading than in static tensile loading and most severe where the shear stress in the lamina is the dominant failure mode. Through an analytical formulation of shifting functions for the influences of temperature, all fatigue data are shown to be capable of being reduced to a single reference curve at some temperature. Additionally, examples are given which demonstrate the capability of the fatigue failure criterion to predict failure of complex symmetrically balanced laminates from relevant parameters obtained from the observed behavior of unidirectional and angle-ply laminates.

Rotem, A.↗

Fatigue behavior of SiC reinforced Ti/6Al-4V/ at 650 C

Axial, low cycle fatigue properties of 25 and 44 fiber vol pct SiC/Ti(6Al-4V) composites, measured at 650 C, were compared with the fatigue properties of unreinforced Ti(6Al-4V) at the same temperature. A prior study of the fatigue behavior of this composite system at room temperature indicated that the SiC fiber reinforcement did not provide the anticipated improvement of fatigue resistance of this alloy. At 650 C, the composite fatigue properties degraded somewhat from those at room temperature. However, these properties degraded more for the unreinforced matrix at 650 C with the result that the composite fatigue strength was two to three times the fatigue strength of the matrix alloy. The reasons for this reversal are discussed in terms of crack initiation at broken fibers and residual matrix stresses.

Bhatt, R. T.↗

Residual strength of five boron/aluminum laminates with crack-like notches after fatigue loading

Boron/aluminum specimens were made with crack-like slits in the center and with various proportions of 0 and + or - 45 deg plies. They were fatigue loaded and then fractured to determine their residual strengths. The fatigue loads were generally in the range of 60 to 80 percent of the static tensile strength of the specimen as determined from a previous study, and the stress ratio was .05. For virtually all of the specimens the fatigue loading was continued for 100,000 cycles. The specimens were radiographed after the fatigue loading to determine the nature of the fatigue damage. A few specimens were sectioned and examined in a scanning electron microscope after being radiographed in order to verify the interpretation of the radiographs and also to get a better insight into the nature of the fatigue damage. The results indicate that the fatiguing does not significantly affect the strength of the specimens tested. The results of the radiography and of the scanning electron microscopy indicate that the 45 deg plies suffer extensive damage in the form of split and broken fibers and matrix cracking in the vicinity of the ends of the split. By contrast, the only significant damage to the 0 deg plies was a single 0 deg matric crack growing from the ends of the slit and between the 0 deg fibers.

Simonds, R. A.↗

Fatigue behavior of continuous fiber silicon-carbide-aluminum composites

Four lay-ups of continuous fiber silicon carbide (SCS2) fiber/aluminum matrix composites were tested to assess fatigue mechanisms including stiffness loss when cycled below their respective fatigue limits. The lay-ups were 0 (sub 8), 0(sub 2)/ + or - 45 (sub 2s), 0/90 (sub 2s),and 0/ + or 45/90 (subs). The data were compared with predictions from the author's previously published shakedown model which predicts fatigue-induced stiffness loss in metal matrix composites. A fifth lay-up, + or - 45 (sub 2s), was tested to compare shakedown and fatigue limits. The particular batch of silicon-carbide fibers tested in this program had a somewhat lower modulus (340 GPa) than expected and displayed poor bonding to the aluminum matrix. Good agreement was obtained between the stiffness loss model and the test data. The fatigue damage below the fatigue limit was primarily in the form of matrix cracking. The fatigue limit corresponded to the laminate shakedown for the + or - 45 (sub 2s) laminate.

Johnson, W. S.↗

Fatigue life extension

Potential fatigue rejuvenation processes were carried out on fatigue-damaged material both with and without observable surface-connected fatigue cracks. The fatigue life of fatigue-damaged MAR-M246(Hf)(DS), a directionally solidified nickel-base superalloy used in turbine airfoils, was extended by reheat treatment. The fatigue life of fatigue-cracked Inconel 718, a wrought nickel-base superalloy used in a wide variety of advanced rocket engine components, was extended by electron-beam welding to close off the surface-connected crack, followed by hot isostatic pressing and reheat treatment.

Matejczyk, D. E.↗

Creep-fatigue behavior of NiCoCrAlY coated PWA 1480 superalloy single crystals

Single crystal specimens of a Ni base superalloy, PWA 1480, with a low pressure plasma sprayed NiCoCrAlY coating were tested in various 0.1 Hz fatigue and creep fatigue cycles both at 1015 and 1050 C. Creep fatigue tests of the cp, pc, and cc types were conducted with various constant total strain ranges employing creep dwells at various constant stresses. Considerable cyclic softening occurred as was evidenced particularly by rapidly increasing creep rates in the creep fatigue tests. The cycle time in the creep fatigue tests typically decreased by more than 80 percent at 0.5 N sub f. Though cyclic life did correlate with delta epsilon sub in a better correlation existed with sub f for both the fatigue and creep fatigue tests, and poor correlations were observed with either sigma sub max or the average cycle time. A model containing both delta sigma and delta sigma (sub in), N sub f = alpha delta sigma (sub in) beta delta sigma gamma, with best fit values of sigma for each cycle type, but the same values of beta and gamam, was found to provide good correlations. Life lines were not greatly different among the cycle types, differing only by a factor of about three. The cp cycle life line was lowest for both test temperatures, however among the other three cycle types there was no consistent ranking. For all test types failure occurred predominately by multiple internal cracking originating at pores. The strong correlation of life with delta sigma may reflect a significant crack growth period in the life of the specimens.

Miner, R. V.↗

Elevated temperature biaxial fatigue

A 3 year experimental program for studying elevated temperature biaxial fatigue of a nickel based alloy Hastelloy-X has been completed. A new high temperature fatigue test facility with unique capabilities has been developed. Effort was directed toward understanding multiaxial fatigue and correlating the experimental data to the existing theories of fatigue failure. The difficult task of predicting fatigue lives for nonproportional loading was used as an ultimate test for various life prediction methods being considered. The primary means of reaching improved understanding were through several critical nonproportional loading experiments. The direction of cracking observed on failed specimens was also recorded and used to guide the development of the theory. Cyclic deformation responses were permanently recorded digitally during each test. It was discovered that the cracking mode switched from primarily cracking on the maximum shear planes at room temperature to cracking on the maximum normal strain planes at 649 C. In contrast to some other metals, loading path in nonproportional loading had little effect on fatigue lives. Strain rate had a small effect on fatigue lives at 649 C. Of the various correlating parameters the modified plastic work and octahedral shear stress were the most successful.

Jordan, E. H.↗

Fatigue behavior of continuous-fiber silicon carbide/aluminum composites

Four lay-ups of continuous fiber silicon carbide (SCS2) fiber/aluminum matrix composites were tested to assess fatigue mechanisms including stiffness loss when cycled below their respective fatigue limits. The lay-ups were 0 (sub 8), 0(sub 2)/ + or - 45 (sub 2s), 0/90 (sub 2s), and 0/ + or - 45/90 (subs). The data were compared with predictions from the author's previously published shakedown model which predicts fatigue-induced stiffness loss in metal matrix composites. A fifth lay-up, + or - 45 (sub 2s), was tested to compare shakedown and fatigue limits. The particular batch of silicon-carbide fibers tested in this program had a somewhat lower modulus (340 GPa) than expected and displayed poor bonding to the aluminum matrix. Good agreement was obtained between the stiffness loss model and the test data. The fatigue damage below the fatigue limit was primarily in the form of matrix cracking. The fatigue limit corresponded to the laminate shakedown for the + or - 45 (sub 2s) laminate.

Johnson, W. S.↗

Residual strength of five boron/aluminum laminates with crack-like notches after fatigue loading

Boron/aluminum specimens were made with crack-like slits in the center and with various proportions of 0 and + or - 45 deg plies. They were fatigue loaded and then fractured to determine their residual strengths. The fatigue loads were generally in the range of 60 to 80 percent of the static tensile strength of the specimen as determined from a previous study, and the stress ratio was .05. For virtually all of the specimens the fatigue loading was continued for 100,000 cycles. The specimens were radiographed after the fatigue loading to determine the nature of the fatigue damage. A few specimens were sectioned and examined in a scanning electron microscope after being radiographed in order to verify the interpretation of the radiographs and also to get a better insight into the nature of the fatigue damage. The results indicate that the fatiguing does not significantly affect the strength of the specimens tested. The results of the radiography and of the scanning electron microscopy indicate that the 45 deg plies suffer extensive damage in the form of split and broken fibers and matrix cracking in the vicinity of the ends of the split. By contrast, the only significant damage to the 0 deg plies was a single 0 deg matric crack growing from the ends of the slit and between the 0 deg fibers.

Simonds, R. A.↗

Extending Fatigue Lives Of Selected Alloys

Rejuvenating treatments demonstrated. Experiments with three alloys show some combinations of heat treatment, hot isostatic pressing, and/or surface treatment extends cycle lives of fatigue-damaged or fatigue-precracked specimens. For each alloy, tests were first done to determine "baseline" high-cycle-fatigue lives and high-cycle-fatigue failure modes over range of test conditions. Controlled fatigue damage introduced into specimens. Damaged specimens subjected to candidate rejuvenating treatments, then tested to failure. Effectiveness of each treatment judged by comparing fatigue data of damaged and treated specimens to "baseline" fatigue and data taken at same test conditions.

Matejczyk, D. E.↗

Fatigue testing and damage development in continuous fiber reinforced metal matrix composites

A general overview of the fatigue behavior of metal matrix composites (MMC) is presented. The first objective is to present experimental procedures and techniques for conducting a meaningful fatigue test to detect and quantify fatigue damage in MMC. These techniques include interpretation of stress-strain responses, acid etching of the matrix, edge replicas of the specimen under load, radiography, and micrographs of the failure surfaces. In addition, the paper will show how stiffness loss in continuous fiber reinforced metal matrix composites can be a useful parameter for detecting fatigue damage initiation and accumulation. Second, numerous examples of how fatigue damage can initiate and grow in various MMC are given. Depending on the relative fatigue behavior of the fiber and matrix, and the interface properties, the failure modes of MMC can be grouped into four categories: (1) matrix dominated, (2) fiber dominated, (3) self-similar damage growth, and (4) fiber/matrix interfacial failures. These four types of damage will be discussed and illustrated by examples with the emphasis on the fatigue of unnotched laminates.

Johnson, W. S.↗

The relationship between observed fatigue damage and life estimation models

Observations of the surface of laboratory specimens subjected to axial and torsional fatigue loadings has resulted in the identification of three damage fatigue phenomena: crack nucleation, shear crack growth, and tensile crack growth. Material, microstructure, state of stress/strain, and loading amplitude all influence which of the three types of fatigue damage occurs during a dominant fatigue life fraction. Fatigue damage maps are employed to summarize the experimental observations. Appropriate bulk stress/strain damage parameters are suggested to model fatigue damage for the dominant fatigue life fraction. Extension of the damage map concept to more complex loadings is presented.

Kurath, Peter↗

Creep-fatigue behavior of NiCoCrAlY coated PWA 1480 superalloy single crystals

Single crystal specimens of a Ni base superalloy, PWA 1480, with a low pressure plasma sprayed NiCoCrAlY coating were tested in various 0.1 Hz fatigue and creep fatigue cycles both at 1015 and 1050 C. Creep fatigue tests of the cp, pc, and cc types were conducted with various constant total strain ranges employing creep dwells at various constant stresses. Considerable cyclic softening occurred as was evidenced particularly by rapidly increasing creep rates in the creep fatigue tests. The cycle time in the creep fatigue tests typically decreased by more than 80 percent at 0.5 N sub f. Though cyclic life did correlate with delta epsilon sub in a better correlation existed with sub f for both the fatigue and creep fatigue tests, and poor correlations were observed with either sigma sub max or the average cycle time. A model containing both delta sigma and delta sigma (sub in), N sub f = alpha delta sigma (sub in) beta delta sigma gamma, with best fit values of sigma for each cycle type, but the same values of beta and gamam, was found to provide good correlations. Life lines were not greatly different among the cycle types, differing only by a factor of about three. The cp cycle life line was lowest for both test temperatures, however among the other three cycle types there was no consistent ranking. For all test types failure occurred predominately by multiple internal cracking originating at pores. The strong correlation of life with delta sigma may reflect a significant crack growth period in the life of the specimens.

Miner, R. V.↗