Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Stacking faults”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 325 records · Page 18

Ultrasmall-angle X-ray scattering analysis of photonic crystal structure

The results of an ultrasmall-angle X-ray scattering study of iron(III) oxide inverse opal thin films are presented. The photonic crystals examined are shown to have fcc structure with amount of stacking faults varying among the samples. The method used in this study makes it possible to easily distinguish between samples with predominantly twinned fcc structure and nearly perfect fcc stacking. The difference observed between samples fabricated under identical conditions is attributed to random layer stacking in the self-assembled colloidal crystals used as templates for fabricating the inverse opals. The present method provides a versatile tool for analyzing photonic crystal structure in studies of inverse opals made of various materials, colloidal crystals, and three-dimensional photonic crystals of other types.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Subsolidus phase relations of the SrO-WO 3 -CuO system at 800 °C in air

The subsolidus phase relations of the SrO-WO 3 -CuO system were investigated in air. The samples were equilibrated at 800 °C. Under these conditions, eight binary oxides are stable. The pseudo-ternary section contains two ternary oxide phases: the previously described Sr 2 CuWO 6 phase as well as a new phase with Sr 8 CuW 3 O 18 stoichiometry. The crystal structure of this new compound was solved and refined in the R-3 space group, unit cell parameters a = 5.7202 Å and c = 28.873 Å. Sr 8 CuW 3 O 18 has a distorted perovskite type structure, where some of the Sr atoms are positioned at the B sites, and the composition may be given as: Sr 6 (Sr 2 CuW 3 )O 18 . There are indications of existence of a superstructure or stacking faults related to Cu/Sr ordering.

36 MATERIALS SCIENCE↗

Structural transformation features in titanium crystallite under mechanical loading

The features of defect structure generation and development in titanium crystallites were studied on the basis of molecular dynamics method. Interatomic interaction was described using many-body potentials calculated in the approximation of the embedded atom method. It is shown that local structural changes begin to occur in the crystallite at the achievement of a threshold strain value, which is accompanied by a dramatic decrease of potential energy. The features of the formation of local structural changes, which are precursors of classical stacking faults, were studied.

36 MATERIALS SCIENCE↗

Substructure of Intermetallic Thin-Film Cu{sub 3}Sn

The crystalline structure of intermetallic Cu{sub 3}Sn synthesized by successively condensing thin layers of copper and tin on a substrate at 150°C has been studied. Cu{sub 3}Sn compound exists in a very narrow homogeneity range and has a long-period close-packed ordered D0{sub 19} superstructure. It has been found that the crystal lattice exhibits many slip traces associated with dislocation motion. The dislocation motion is due to the stressed state of the crystal, which can be characterized as uniform extension. Electron micrographs show that slip traces in the Cu{sub 3}Sn crystal are parallel to the ( 1-bar 1-bar 21) and (11 2-bar 1) planes belonging to pyramidal slip system II, which is a main slip system along with pyramidal and basal ones. Slip traces result from the motion of partial dislocations, as indicated by the amount of slip, which is equal to half the interplanar distance. Since the crystal is ordered, slip is accomplished by a pair of superpartial dislocations and a slip trace may be a superstructural or complex stacking fault.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

A Mechanistic Study on the Formation of Silver Nanoplates in the Presence of Silver Seeds and Citric Acid or Citrate Ions

The world on a plate: In addition to their role as a capping agent that selectively binds to the {l_brace}111{r_brace} faces of silver, the carboxylate group can coordinate with Ag+ ions to form complexes and thus substantially reduce the reduction rate of Ag+ ions, leading to the formation of silver seeds with both twin planes and stacking faults.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Quickest ever single-step mechanosynthesis of Cd{sub 0.5}Zn{sub 0.5}S quantum dots: Nanostructure and optical characterizations

Highlights: Black-Right-Pointing-Pointer Cd{sub 0.5}Zn{sub 0.5}S QDs prepared in 30 min by ball-milling elemental Cd, Zn and S powders. Black-Right-Pointing-Pointer Microstructure characterization is made by XRD employing Rietveld method and HRTEM. Black-Right-Pointing-Pointer Stacking faults in QDs are ascertained both from Rietveld analysis and HRTEM images. Black-Right-Pointing-Pointer Presence of both cubic and hexagonal phases is confirmed by XRD and HRTEM. Black-Right-Pointing-Pointer Quantum confinement is ascertained by blue-shift and optical band gap increment. -- Abstract: Multiphase Cd{sub 0.5}Zn{sub 0.5}S quantum dots (QDs) are prepared for the first time in a record minimum time of 30 min by mechanical alloying the stoichiometric mixture of elemental Cd, Zn and S powders at room temperature under Ar. Initially, the hexagonal phase is formed as major one and then gradually transforms to the cubic phase which is formed coherently on the hexagonal lattice with (0 0 2){sub hexagonal}||(1 1 1){sub cubic} mechanism. In the course of milling up to 15 h, the molar ratio of cubic to hexagonal phase becomes {approx}0.7:0.3. Both high resolution transmission electron microscopy (HRTEM) and X-ray microstructure analyses reveal that these QDs are isotropic in nature, their size reduces to {approx}5 nm after 15 h of milling with a very narrow size distribution and they contain a significant amount of stacking and twin faults. These QDs show very distinct quantum confinement effect and their optical band gaps are higher than that of the bulk CdZnS.

36 MATERIALS SCIENCE↗

Atomic faulting induced exceptional cryogenic strain hardening in gradient cell–structured alloy

Coarse-grained materials are widely accepted to display the highest strain hardening and the best tensile ductility. We experimentally report an attractive strain hardening rate throughout the deformation stage at 77 kelvin in a stable single-phase alloy with gradient dislocation cells that even surpasses its coarse-grained counterparts. Contrary to conventional understanding, the exceptional strain hardening arises from a distinctive dynamic structural refinement mechanism facilitated by the emission and motion of massive multiorientational tiny stacking faults (planar defects), which are fundamentally distinct from the traditional linear dislocation–mediated deformation. In conclusion, the dominance of atomic-scale planar deformation faulting in plastic deformation introduces a different approach for strengthening and hardening metallic materials, offering promising properties and potential applications.

Gradient dislocation structure↗

Distribution of electric fields in ZnS:Mn single crystals during electroluminescence

Brightness-voltage characteristics of the ZnS:Mn single crystals and their dependence on the frequency and strength of the electric field are studied. A model of the mechanism of excitation of electroluminescence in these crystals on the basis of excitation of the electroluminescence centers by electrons accelerated in the electric fields of the Schottky-type barriers is suggested. Such barriers are formed by dislocations at the sites of interrupting the stacking faults by them. The experimental and calculated data are in good agreement.

36 MATERIALS SCIENCE↗

Defect-free ZnSe nanowire and nanoneedle nanostructures

We report the growth of ZnSe nanowires and nanoneedles using molecular beam epitaxy (MBE). Different growth regimes were found, depending on growth temperature and the Zn-Se flux ratio. By employing a combined MBE growth of nanowires and nanoneedles without any postprocessing of the sample, we achieved an efficient suppression of stacking fault defects. This is confirmed by transmission electron microscopy and by photoluminescence studies.

36 MATERIALS SCIENCE↗

Mechanical behavior of twinned SiC nanowires under combined tension-torsion and compression-torsion strain

The mechanical behavior of twinned silicon carbide (SiC) nanowires under combined tension-torsion and compression-torsion is investigated using molecular dynamics simulations with an empirical potential. The simulation results show that both the tensile failure stress and buckling stress decrease under combined tension-torsional and combined compression-torsional strain, and they decrease with increasing torsional rate under combined loading. The torsion rate has no effect on the elastic properties of the twinned SiC nanowires. The collapse of the twinned nanowires takes place in a twin stacking fault of the nanowires.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Epitaxial relationship of semipolar s-plane (1101) InN grown on r-plane sapphire

The heteroepitaxy of semipolar s-plane (1101) InN grown directly on r-plane sapphire by plasma-assisted molecular beam epitaxy is studied using transmission electron microscopy techniques. The epitaxial relationship is determined to be (1101){sub InN} Parallel-To (1102){sub Al{sub 2O{sub 3}}}, [1120]{sub InN} Parallel-To [2021]{sub Al{sub 2O{sub 3}}}, [1102]{sub InN}{approx} Parallel-To [0221]{sub Al{sub 2O{sub 3}}}, which ensures a 0.7% misfit along [1120]{sub InN}. Two orientation variants are identified. Proposed geometrical factors contributing to the high density of basal stacking faults, partial dislocations, and sphalerite cubic pockets include the misfit accommodation and reduction, as well as the accommodation of lattice twist.

36 MATERIALS SCIENCE↗

On the Relationship Between Dislocation Creep Strength and Microstructure of a Solid-Solution-Strengthened Ni-Base Superalloy

It is shown that the dislocation creep strength of a solid-solution-strengthened Ni-base superalloy is critically dependent upon the cooling rate from the annealing temperature. This behavior is correlated with the effect of cooling rate on the morphology of M{sub 23}C{sub 6}-type carbide which precipitates at grain boundaries during cooling. Experiment shows that the creep strength is enhanced by rapid cooling which results in discrete carbide particles with irregular shape following a zigzag path along the grain boundaries. However, the creep strength is degraded as the morphology is changed into lamellar type by a discontinuous grain boundary reaction which occurs during slower cooling rates. Due to the transition from the discrete particle into the lamellar morphology, plastic deformation becomes more localized alongside the grain boundaries which accelerates the creep rate leading to premature intergranular failure. On the other hand, it is also shown that the stacking fault energy of the alloy increases with temperature which can allow dislocations to rearrange themselves into subgrain structure with relative ease during steady-state creep.

36 MATERIALS SCIENCE↗

The chromium doping of Ni{sub 3}Fe alloy and restructuring of grain boundary ensemble at the phase transition A1→L1{sub 2}

The grain boundary structure of the Ni{sub 3}(Fe,Cr) alloy is studied in states with a short and long-range order formed at the phase transition A1→L1{sub 2}. It is found that the new boundaries of general and special types are formed during an ordering annealing, wherein the special boundaries share increases. The spectrum of special boundaries is changed due to decreasing of ∑3 boundary share. It leads to weakening of the texture in the alloy with atomic long-range order. The features of change of the special boundaries spectrum at the phase transition A1→L1{sub 2} in the Ni{sub 3}(Fe,Cr) alloy are determined by decreasing of the stacking fault energy and the atomic mean square displacement at the chromium doping.

36 MATERIALS SCIENCE↗

Neutron diffraction study of the formation of ordered antiphase domains in cubic titanium carbide TiC{sub 0.60}

A series of superstructural reflections (described within the sp. gr. Fd3m) are found to be split into three symmetric parts in the neutron powder diffraction pattern of titanium carbide TiC{sub 0.60} annealed at a temperature of 600 Degree-Sign C. No splitting of superstructural reflections is observed in the neutron diffraction pattern of TiC{sub 0.60} annealed at relatively high temperatures (780 Degree-Sign C). This phenomenon can be explained by that fact that the ordering of carbon atoms at relatively high temperatures (780 Degree-Sign C) is accompanied by the formation of randomly oriented rather large antiphase domains (APDs) (450 A). At relatively low temperatures (600 Degree-Sign C), stacking faults arise in the arrangement of partially ordered carbon atoms. In this case, relatively small ordered APDs (290 A) are formed, along with disordered ones.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Measurement of Young's modulus of GaAs nanowires growing obliquely on a substrate

A convenient and fast method for measuring Young's modulus of semiconductor nanowires obliquely standing on the growth substrate is presented. In this method, the nanowire is elastically bent under the force exerted by the probe of an atomic-force microscope, and the load-unload dependences for the bending of the probe cantilever are recorded. Next, these curves are used to find the bending stiffness of the tilted nanowires, after which, taking into account the nanowire dimensions, Young's modulus is obtained. The implementation of this method is demonstrated for tilted GaAs nanowires growing on a GaAs (111) substrate. Young's modulus is determined by applying finite-element analysis to the problem of the stationary elastic bending of a nanowire taking into account the actual nanowire shape and faceting. It proves that a fairly accurate estimate of Young's modulus can be obtained even if the nanowire shape is approximated by a circular cylinder with a single cross-sectional area. The values of Young's modulus obtained for GaAs nanowires of cubic lattice symmetry are 2 to 3 times smaller than its value for bulk GaAs. This difference is attributed to the presence of stacking faults in the central part of the nanowires.

36 MATERIALS SCIENCE↗

Effect of different stages of deformation on the microstructure evolution of Ti-rich NiTi shape memory alloy

The main objective of this work was to investigate the thermomechanical behavior and microstructural changes of a Ti-rich NiTi shape memory alloy (SMA). The microstructural and texture evolution of aged NiTi alloy at different degrees of deformation were elicited by transmission electron microscopy (TEM). An effort was made to correlate results obtained from the tensile test with results from microstructure studies. The undeformed sample reveals a self-accommodated morphology with straight and well defined twin boundaries. At different stages of deformation, diverse mechanisms were involved. These mechanisms include marstraining, detwinning accompanied by dislocation movement, and finally, severe plastic deformation, subdivision and amorphization of the matrix. Under increasing strains, high density lattice defects were generated and the morphology of B19’ became disordered. - Graphical abstract: The summary of microstructure changes of the martensite twins during tensile deformation in polycrystalline NiTi SMAs. - Highlights: • Initial elastic response, dislocation avalanche and deformation bands were studied. • < 011 > Type II twin accompanied by detwinned area after 2% cold work was observed. • Visible parallel fine stacking faults showed plastic flow of the material. • At higher strains, subgrains changed to recrystallized, finely amorphous structure.

36 MATERIALS SCIENCE↗

Epitaxial growth of hexagonal silicon polytypes on sapphire

The formation of a single-crystal silicon polytype is observed in silicon-on-sapphire structures by high-resolution transmission electron microscopy. The appearance of inclusions with a structure different from that of diamond is attributed to the formation of strong-twinning regions and the aggregation of stacking faults, which form their own crystal structure in the crystal lattice of silicon. It is demonstrated that the given modification belongs to the 9R silicon polytype.

36 MATERIALS SCIENCE↗

Heteroepitaxy of FCC-on-FCC systems of large misfit

Here, to understand the effects of lattice mismatch on heteroepitaxial growth, we have studied the equilibrium structure and orientation relationships (ORs) of FCC films grown epitaxially on FCC substrates, using molecular dynamics simulations in conjunction with embedded atom method potentials. Three film/substrate systems have been investigated, namely: Ag on Cu, Ag on Ni and Pb on Al. These systems cover a significant range of lattice mismatch, from 12.6% for Ag/Cu to 21.8% for Pb/Al. For each system, the ORs of films on six different substrate orientations, namely: (100), (511), (311), (211), (322) and (111), have been investigated. Films on these susbstrates cover a gradual transition from the oct-cube orientation relationship, which occurs only on (100) substrates, to the heterotwin orientation relationship, which often occurs on (111) substrates. It is found that the resulting ORs vary systematically with substrate orientation, but that the pattern of variation is almost identical for all three systems, and therefore largely independent of mismatch. However, the manner in which mismatch is accommodated does depend on the magnitude of mismatch. Simulations point to an important role for edge-to-edge matching and defects such as stacking faults. An analysis of these results in terms of transformation strains highlights the distinction between the ORs, which are largely independent of mismatch, and the local interfacial structure, which changes directly with mismatch.