Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SEI”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 325 records · Page 18

Single-phase local-high-concentration solid polymer electrolytes for lithium-metal batteries

Solid polymers are promising electrolytes for Li-metal batteries, but they have limitations: they cannot simultaneously achieve high ionic conductivity, good mechanical strength and compatibility with high-voltage cathodes while suppressing Li dendrites. Here, we design a class of locally high-concentration solid polymer electrolytes based on polymer blends, which are termed Li-polymer in F diluter (LPIFD). The Li-polymer (polymer-in-salt) ensures continuous Li-ion conduction channels and contributes to the solid electrolyte interphase (SEI), and the F diluter (inert fluorinated polymer) adds mechanical strength. Studies reveal that a single-phase LPIFD, which is based on a miscible polymer blend, lacks phase boundaries and forms an organic-less and LiF-rich SEI, effectively suppressing lithium dendrites. The single-phase LPIFD delivers ionic conductivity of 3.0 x 10 -4 S cm -1 and enables the Li anode to reach a high coulombic efficiency of 99.1% and a critical current density of 3.7 mA cm -2 . Furthermore, the ability to form an F-rich cathode electrolyte interphase allows LiNi 0.8 Co 0.1 Mn 0.1 O 2 ||Li cells to achieve a cycle life of 450 cycles at a high operating voltage of 4.5 V. In conclusion, this design will inspire efforts to commercialize polymer electrolytes for high-energy Li-metal batteries.

25 ENERGY STORAGE↗

Electro-chemo-mechanical evolution of sulfide solid electrolyte/Li metal interfaces: operando analysis and ALD interlayer effects

Sulfide solid electrolytes (SE) show promise for high-performance solid-state batteries because of their high ionic conductivity and ease of processing. However, sulfide electrolytes have suffered from chemical and electrochemical instability against Li metal anodes. In this paper, we use a suite of in situ/operando microscopy and spectroscopy techniques to demonstrate that Al 2 O 3 interlayers deposited using atomic layer deposition (ALD) delay degradation at the Li/LGPS interface by modifying the solid electrolyte interphase (SEI) chemistry and morphology. Optical and scanning electron microscopy are used to rationalize the electrochemical response of the system, which is attributed to a delayed onset of mechanical degradation at the interface when ALD interlayers are used. Operando X-ray photoelectron spectroscopy demonstrates that the dynamic evolution of SEI chemistry is impacted by the presence of the ALD interlayer. In situ Auger spectroscopy and operando optical microscopy provide visual evidence of spatial heterogeneity of Li plating, which is attributed to the chemo-mechanical degradation of the ALD interphase. The implications of these observations provide valuable insights toward the development of robust interlayers for solid-state batteries.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Tutorial review on structure – dendrite growth relations in metal battery anode supports

This tutorial review explains the emerging understanding of the surface and bulk chemistry – electrochemical performance relations in anode supports (aka secondary current collectors, substrates, templates, hosts) for lithium, sodium and potassium metal batteries (LMBs, SMBs or NMBs, and KMBs or PMBs). In relation to each section, the possible future research directions that may yield both new insight and improved cycling behavior are explored. Representative case studies from Li, Na and K metal anode literature are discussed. The tutorial starts with an overview of the solid electrolyte interphase (SEI), covering both the “classic” understanding of the SEI structure and the “modern” insights obtained by site-specific cryogenic stage TEM analysis. Next, the multiple roles of supports in promoting cycling stability are detailed. Without an optimized support architecture, the metal–electrolyte interface becomes geometrically unstable at a lower current density and cycle number. Taking into consideration the available literature on LMBs, SMBs and KMBs, it is concluded that effective architectures are geometrically complex and electrochemically lithiophilic, sodiophilic or potassiophilic, so as to promote conformal electrochemical wetting of the metal during plating/stripping. One way that philicity is achieved is through support oxygen surface chemistry, which yields a reversibly reactive metal–support interface. Examples of this include the well-known oxygen–carbon moieties in reduced graphene oxide (rGO), as well as classic ion battery reversible conversion reaction oxides such as SnO 2 . Unreactive surfaces lead to dewetted island growth of the metal, which is a precursor to dendrites, and possibly to non-uniform dissolution. Surveying the literature on various Li, Na and K metal supports, it is concluded that the key bulk thermodynamic property that will predict electrochemical wetting behavior is the enthalpy of infinite solution (Δ sol H ∞ ) of the metal (solute) into the support (solvent). Large and negative Δ sol H ∞ promotes uniform metal wetting on the support surface, corresponding to relatively low plating overpotential. Positive Δ sol H ∞ promotes dewetted islands and a relatively high overpotential. This simple rule explains a broad range of studies on Li, Na and K metal – support interactions, including the previously reported correlation between mutual solubility and wetting.

25 ENERGY STORAGE↗

Pursuing graphite-based K-ion O 2 batteries: a lesson from Li-ion batteries

The replacement of lithium metal by lithium intercalated graphite was crucial for developing safe lithium-ion batteries. Superoxide-based potassium–oxygen batteries represent an exciting metal–oxygen battery with the highest energy efficiencies. However, using potassium metal is a more serious safety threat than lithium. Herein, we explore the possibility of graphite-intercalation anodes for potassium-ion oxygen batteries (PIOBs) with enhanced safety. This work demonstrates for the first time that establishing an artificial potassium salt-rich solid electrolyte interphase (SEI) enables a reversible graphite-intercalation anode (249.6 mA h g -1 after 600 cycles) in a potassium bis(trifluoromethanesulfonyl)imide (KTFSI)-based localized high-concentration electrolyte. Such an electrolyte is stable with the superoxide cathode. The PIOB delivers energy efficiencies above 90% at a depth of discharge (DOD) of 25% for 80 cycles. A three-electrode measurement shows that its overpotential mainly comes from the anode. The lifespan is limited to the gradual degradation of the artificial SEI caused by oxygen crossover. This work represents a step towards achieving holistic anode–electrolyte–cathode compatibility in a PIOB and its realistic evaluation under a controlled DOD.

25 ENERGY STORAGE↗

Robust battery interphases from dilute fluorinated cations

Controlling solid electrolyte interphase (SEI) in batteries is crucial for their efficient cycling. Herein, we demonstrate an approach to enable robust battery performance that does not rely on high fractions of fluorinated species in electrolytes, thus substantially decreasing the environmental footprint and cost of high-energy batteries. In this approach, we use very low fractions of readily reducible fluorinated cations in electrolyte (~0.1 wt%) and employ electrostatic attraction to generate a substantial population of these cations at the anode surface. As a result, we can form a robust fluorine-rich SEI that allows for dendrite-free deposition of dense Li and stable cycling of Li-metal full cells with high-voltage cathodes. Our approach represents a general strategy for delivering desired chemical species to battery anodes through electrostatic attraction while using minute amounts of additive.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A comprehensive review on liquid electrolyte design for low-temperature lithium/sodium metal batteries

Lithium/sodium metal batteries (LMBs/SMBs) possess immense potential for various applications due to their high energy density. Nevertheless, LMBs/SMBs are highly susceptible to the detrimental effects of an unstable solid electrolyte interphase (SEI) and dendrites during practical applications, particularly pronounced in low-temperature environments. Furthermore, sluggish ion transportation further compromises the cycling stability of LMBs/SMBs at low temperatures. To achieve stable operation of LMBs/SMBs at low temperatures, researchers have made numerous efforts including electrolyte optimization aimed at creating stable SEIs and suppressing the metal dendrites under low temperature conditions. Despite the significant advancements made recently in the liquid electrolyte design, there remains considerable hurdle in electrolyte engineering for practical low-temperature, high energy density LMBs/SMBs, calling for a profound comprehension of the intricate interplay between the electrochemical reaction kinetics and electrolyte compositions. Here, this review provides a thorough overview of various strategies in optimizing liquid electrolytes covering weakly solvating electrolytes, concentration-designed electrolytes, and solvation structure-designed electrolytes, to address the challenges faced by LMBs/SMBs at low temperatures, including slow reaction kinetics and the difficulties in Li + /Na + solvation/desolvation. Furthermore, this review discusses future prospects for the advancement of this field, intending to provide valuable insights and support for subsequent research undertakings.

25 ENERGY STORAGE↗

Quantitative insights for diagnosing performance bottlenecks in lithium–sulfur batteries

Lithium–sulfur (Li–S) batteries hold significant promise for electric vehicles and aviation due to their high energy density and cost-effectiveness. However, understanding the root causes of performance degradation remains a formidable challenge, as the interplay of multiple factors obscures key failure mechanisms. A major limitation has been the inability to quantify soluble sulfur species within practical detection limits accurately and to correlate electrochemical processes with associated physical inventory changes. Here, we introduce the high-performance liquid chromatography-ultraviolet spectroscopy and gas chromatography sequential characterization (HUGS) toolkit, capable of precisely quantifying seven distinct sulfur and polysulfide species at concentrations as low as 40 ppb. HUGS has been successfully applied to practical coin and pouch cells without requiring cell modification. Furthermore, our self-developed software, Dr HUGS, enhanced the data analysis speed by over 30 times, enabling multi-source data integration and delivering comprehensive analysis results within minutes. Using HUGS, we identify significant capacity losses from inactive lithium and sulfur during initial cycles and sulfide-rich solid–electrolyte interphase (SEI) formation on the anode during later cycles. Notably, our findings reveal that soluble polysulfides have minimal contributions to capacity loss, challenging long-standing assumptions. Moreover, HUGS demonstrates that constant-pressure setups in Li–S pouch cells improve compositional uniformity compared to constant-gap configurations. For sulfurized polyacrylonitrile (SPAN) cathodes, unique issues such as non-sulfide SEI formation and lithium pulverization are observed, which can be mitigated through localized high-concentration electrolytes to enhance lithium inventory retention. By enabling precise quantification of critical inventory components, HUGS provides transformative insights into failure mechanisms across various electrolytes and cathode chemistries, guiding rational design strategies for next-generation energy storage systems.

25 ENERGY STORAGE↗

Enhanced cycling stability of Ni-rich Li-metal cells enabled by dual vinylene carbonate and tris(trimethylsilyl)borate electrolyte additives

NMC811 (LiNi 0.8 Co 0.1 Mn 0.1 O 2 ) and other high-Ni chemistries are promising cathode candidates for high-performance electric vehicles, owing to their high energy density and reduced cobalt content. However, their long-term cycling stability is hindered by surface degradation, particularly when paired with conventional electrolytes and a lithium metal anode. Electrolyte additives represent a practical approach to enhance interfacial stability and improve overall battery performance by promoting the formation of a robust electrolyte–electrode interphase (EEI). In this study, we revisit the effects of vinylene carbonate (VC) and tris(trimethylsilyl)borate (TMSB) additives on single-crystal SC-NMC811||Li cells. While TMSB only increases the open-circuit voltage and initial overpotential, it delivers superior capacity retention at C/3 compared to cells containing only VC or a dual additive system (VC and TMSB). Notably, under fast-charging conditions (1C, 2C, and 5C), the dual-additive system significantly outperforms other formulations, achieving markedly enhanced long-term capacity retention. Comprehensive electrochemical and spectroscopic analyses reveal that the VC/TMSB dual-additive system suppresses surface transition in NMC811, mitigates structural degradation by forming a thin, LiF-deficient cathode-electrolyte interface (CEI) layer. Moreover, they promote smooth and dense Li deposition and generate a LiF-deficient solid-electrolyte interphase (SEI). Consequently, the synergistic stabilization of both the CEI and SEI effectively limits the overall cell impedance growth during extended cycling. These findings provide key insights into co-additive strategies for engineering stable interfaces in high-energy Ni-rich Li-metal batteries.

36 MATERIALS SCIENCE↗

Mass spectral molecular mapping shows benefits of thermal evaporation in prelithiated silicon-based electrodes

Silicon based composites have become increasingly popular as potential anodes for lithium-ion batteries due to their large storage capacity and potential ability to generate batteries with energy densities greater than 350 Wh kg −1 . These anodes often see reduced initial columbic efficiency (ICE) due to disruptive volume expansionup to 300% and continuous solid electrolyte interphase (SEI) layer formation. Prelithiation, where an excess reservoir of Li is added to the electrode to compensate for irreversible SEI formation losses during their sample preparation, has proven to solve the issue of immediate capacity loss. Thermal evaporation is a prelithiation technique with limited studies on its effectiveness. In this study, time-of-flight secondary ion mass spectrometry (ToF-SIMS) is used to highlight the benefits of prelithiation via thermal evaporation. ToF-SIMS provides chemical mapping and spatial information in 2D and 3D visualizing the deposition of lithium, identifying Li x Si y alloy and Li x Si y O z silicate formation, and the distribution of lithium passivation into the electrodes. Passivation under different atmospheric conditions, such as inert Argon (Ar) and Ar/ carbon dioxide (CO 2 ), highlights the impact of the environment on the passivation effectiveness and formation of Li x Si y alloy and Li x Si y O z silicate. The ToF-SIMS molecular imaging and depth profiling results indicate that prelithiation via thermal evaporation effectively distributes lithium throughout the depth profile thickness of several hundred nanometers. It induces a greater degree of Li x Si y O z silicate formation over Li x Si y alloy. Our ToF-SIMS characterization results show the effectiveness of thermal evaporation in producing a more stable electrode and an electrode with an effective lithium reserve that can preserve its capacity.

Parker, Gabriel D. [Oak Ridge National Laboratory ↗

Localized high concentration electrolytes decomposition under electron-rich environments

Localized high concentration electrolytes have been proposed as an effective route to construct stable solid–electrolyte interphase (SEI) layers near Li-metal anodes. However, there is still a limited understanding of decomposition mechanisms of electrolyte components during SEI formation. In this work, we investigate reactivities of lithium bis(fluorosulfonyl)imide (LiFSI, salt), 1,2-dimethoxyethane (DME, solvent) and tris(2,2,2-trifluoroethyl)orthoformate (TFEO, diluent) species in DME+TFEO mixed solvents and 1M LiFSI/DME/TFEO solutions. By supplying excess of electrons into the simulation cell, LiFSI is initially reduced via a 4-electron charge transferring reaction yielding F - and N(SO 2 ) 2 3- . The local solvation environment has little effect on the subsequent TFEO reaction, which typically requires 6 |e| to decompose into F - , HCOO - , CH2CF and - OCH 2 CF 3 . Besides, TFEO dehydrogenation reaction mechanism under the attack of anions is also identified. Unlike salt and diluent, DME shows good stability with any excess of electrons. Here, the energetics of most relevant reactions are characterized. Most reactions are thermodynamically favorable with low activation barriers.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Probing the thermodynamics and kinetics of ethylene carbonate reduction at the electrode–electrolyte interface with molecular simulations

Understanding the formation of the solid-electrolyte interphase (SEI) in lithium-ion batteries (LIBs) is an ongoing area of research due to its high degree of complexity and the difficulties encountered by experimental studies. Herein, we investigate the initial stage of SEI growth, the reduction reaction of ethylene carbonate (EC), from both a thermodynamic and kinetic approach with theory and molecular simulation. We employed both the potential distribution theorem (PDT) and the SMD implicit solvent model to EC solvation for the estimation of reduction potentials of Li$^+$, EC, and Li$^+$-solvating EC (s-EC), as well as reduction rate constants of EC and s-EC. We find that solvation effects greatly influence these quantities of interest, particularly the Li$^+$/Li reference electrode potential in EC solvent. Further, we also compute the inner- and outer-sphere reorganization energies for both EC and s-EC at the interface of liquid EC and a hydroxyl-terminated graphite surface, where total reorganization energies are predicted to be 76.6 and 88.9 kcal/mol, respectively. With the computed reorganization energies, we estimate reduction rate constants across a range of overpotentials and show that EC has a larger electron transfer rate constant than s-EC at equilibrium, despite s-EC being more thermodynamically favorable. Furthermore, this manuscript demonstrates how ion solvation effects largely govern the prediction of reduction potentials and electron transfer rate constants at the electrode-electrolyte interface.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Stable metal anodes enabled by a labile organic molecule bonded to a reduced graphene oxide aerogel

Significance Rechargeable batteries based on metal anodes are highly desirable due to their high energy density. However, the electrochemical interface is generally not favorable for metal deposition, resulting in dendritic metal growth and an unstable solid–electrolyte interphase (SEI). We altered the interface using a labile organic molecule, benzenesulfonyl fluoride. This molecule was bonded to the surface of a reduced graphene oxide aerogel, which not only guides uniform metal deposition but also enables formation of a stable SEI layer. The lithium metal batteries showed stable cycling and excellent tolerance to low-temperature operation. Stable sodium and zinc anodes were also realized, demonstrating the versatility of this concept.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Design principles for self-forming interfaces enabling stable lithium-metal anodes

Significance It is possible to nearly double the energy density of existing lithium-ion batteries by using lithium metal anodes. However, it has been known for decades that the lithium dendrites and mossy lithium formed during charging (electrodeposition) limit the cycle life of the batteries. It is important to change the growth behavior of lithium metal, which is closely related to the properties of the solid–electrolyte interface (SEI) formed via spontaneous reactions between the lithium metal and the electrolyte. In this experimental-modeling integrated study, we reveal the design principles of the SEI that facilitates the dendrite-free and dense deposition of lithium and demonstrate one of the best cycling performances of lithium metal anode to date under practically relevant conditions.

25 ENERGY STORAGE↗

Multidimensional visualization of the dynamic evolution of Li metal via in situ/operando methods

The growing demands for high-energy density electrical energy storage devices stimulate the coupling of conversion-type cathodes and lithium (Li) metal anodes. While promising, the use of these “Li-free” cathodes brings new challenges to the Li anode interface, as Li needs to be dissolved first during cell operation. In this study, we have achieved a direct visualization and comprehensive analysis of the dynamic evolution of the Li interface. The critical metrics of the interfacial resistance, Li growth, and solid electrolyte interface (SEI) distribution during the initial dissolution/deposition processes were systematically investigated by employing multidimensional analysis methods. They include three-electrode impedance tests, in situ atomic force microscopy, scanning electrochemical microscopy, and cryogenic scanning transmission electron microscopy. The high-resolution imaging and real-time observations show that a loose, diffuse, and unevenly distributed SEI is formed during the initial dissolution process. This leads to the dramatically fast growth of Li during the subsequent deposition, deviating from Fick’s law, which exacerbates the interfacial impedance. The compactness of the interfacial structure and enrichment of electrolyte species at the surface during the initial deposition play critical roles in the long-term stability of Li anodes, as revealed by operando confocal Raman spectroscopic mapping. In conclusion, our observations relate to ion transfer, morphological and structural evolution, and Li (de)solvation at Li interfaces, revealing the underlying pathways influenced by the initial dissolution process, which promotes a reconsideration of anode investigations and effective protection strategies.

25 ENERGY STORAGE↗

Magnetically oriented nanosheet interlayer for dynamic regeneration in lithium metal batteries

Lithium (Li) metal has been recognized as a promising anode to advance the energy density of current Li-based batteries. However, the growth of the solid–electrolyte interphase (SEI) layer and dendritic Li microstructure pose significant challenges for the long-term operation of Li metal batteries (LMBs). Herein, we propose the utilization of a suspension electrolyte with dispersed magnetically responsive nanosheets whose orientation can be manipulated by an external magnetic field during cell operation for realizing in situ regeneration in LMBs. The regeneration mechanism arises from the redistribution of the ion flux and the formation of an inorganic-rich SEI for uniform and compact Li deposition. With the magnetic-field-induced regeneration process, we show that a Li||Li symmetric cell stably operates for 350 h at 2 mA cm −2 and 2 mA h cm −2 , ~5 times that of the cell with the pristine electrolyte. Furthermore, the cycling stability can be significantly extended in the Li||NMC full cell of 3 mA h cm −2 , showing a capacity retention of 67% after 500 cycles at 1C. The dynamic Li metal regeneration demonstrated here could bring useful design considerations for reviving the operating cells for achieving high-energy, long-duration battery systems.

Ju, Zhengyu↗