Exploring Lithiation of Single Cathodic Nanoparticles using Scanning Probe Microscopy.
Abstract not provided.
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Abstract not provided.
Explore the source record for details and available documents.
Abstract not provided.
Metallic germanium is a promising anode material in secondary lithium-ion batteries (LIBs) due to its high theoretical capacity (1623 mAh/g) and low operating voltage, coupled with the high lithium-ion diffusivity and electronic conductivity of lithiated Ge. Here, the lithiation mechanism of micron-sized Ge anodes has been investigated with X-ray diffraction (XRD), pair distribution function (PDF) analysis, and in-/ex-situ high-resolution Li-7 solid-state nuclear magnetic resonance (NMR), utilizing the structural information and spectroscopic fingerprints obtained by characterizing a series of relevant Li(x)Gey model compounds. In contrast to previous work, which postulated the formation of Li9Ge4 upon initial lithiation, we show that crystalline Ge first reacts to form a mixture of amorphous and crystalline Li7Ge3 (space group P32(1)2). Although Li7Ge3 was proposed to be stable in a recent theoretical study of the Li-Ge phase diagram (Morris, A. J.; Grey, C. P.; Pickard, C. J. Phys. Rev. B: Condens. Matter Mater. Phys. 2014, 90, 054111), it had not been identified in prior experimental studies. Further lithiation results in the transformation of Li7Ge3, via a series of disordered phases with related structural motifs, to form a phase that locally resembles Li7Ge2, a process that involves the gradual breakage of the Ge-Ge bonds in the Ge-Ge dimers (dumbbells) on lithiation. Crystalline Li15Ge4 then grows, with an overlithiated phase, Li15+delta Ge4, being formed at the end of discharge. This study provides comprehensive experimental evidence, by using techniques that probe short-, medium-, and long-range order, for the structural transformations that occur on electrochemical lithiation of Ge; the results are consistent with corresponding theoretical studies regarding stable lithiated LixGey phases.
Linear (local) gyrokinetic predictions of edge microinstabilities in highly shaped, lithiated and non-lithiated NSTX discharges are reported using the gyrokinetic code GS2. Microtearing modes dominate the non-lithiated pedestal top. The stabilization of these modes at the lithiated pedestal top enables the electron temperature pedestal to extend further inwards, as observed experimentally. Kinetic ballooning modes are found to be unstable mainly at the mid-pedestal of both types of discharges, with un- stable trapped electron modes nearer the separatrix region. At electron wavelengths, ETG modes are found to be unstable from mid-pedestal outwards for η e, exp ~2.2 with higher growth rates for the lithiated discharge. Near the separatrix, the critical temperature gradient for driving ETG modes is reduced in the presence of lithium, re ecting the reduction of the lithiated density gradients observed experimentally. A preliminary linear study in the edge of non-lithiated discharges shows that the equilibrium shaping alters the electrostatic modes stability, found more unstable at high plasma shaping.
The lithium ion migration dynamics and the fast lithiation pathways in electrode materials are quite vital to the rate capability of lithium ion batteries (LIBs). To reveal the relationship between lithiation behavior and crystallographic orientations in layered MoSe 2 , its dynamic electrochemical reactions are investigated with in situ microscopy technique. Here, we report the crystallographic-orientation dependent lithium ion migration and reaction in MoSe 2 , where the preferential lithium-ion migration is observed along the $\langle10\bar{1}0\rangle$ orientations. These oriented-lithiation tips further assisted the surface to interior lithiation of layered MoSe 2 . At the same time, a phase transition from pristine 2H-MoSe 2 to 1T-Li x MoSe 2 and the following conversion reaction with the formation of Li2Se and Mo are observed during the first lithiation process. The lithiation induced stress and orientation-dependent interfacial reaction rate might be the main factor leading to the orientation-dependent lithiation behavior. The experimentally revealed crystallographic-orientation dependent lithium ion migration and reaction in layered MoSe 2 will provide intuitive understanding of the structural evolution during the discharge/charge cycling process, give guidance for the design of anode materials and can broaden the promising application of MoSe 2 in solid electrochemical devices.
Elastic strains are measured in operando in a nanostructured silicon-coated nickel inverse opal scaffold anode, using X-ray diffraction to study the Si (de)lithiation-induced Ni strains. The volume expansion upon lithiation of the Si in the anode is constrained by the surrounding Ni scaffold, causing mismatch stresses and strains in the Si and Ni phases during cycling. The Ni strains are measured in operando during (dis)charge cycles, using diffraction peak position and peak broadness to describe the distribution of strain in the Ni. During lithiation, compressive strains in the Ni first increase linearly with charge, after which a gradually decreasing strain rate is observed as the maximum lithiation state is approached; upon delithiation a similar process occurs. In-plane average compressive strains on the order of 990 ± 40 με are measured in the Ni scaffold during lithiation, corresponding to compressive stresses of 215 ± 9 MPa. Here, the decreasing strain rates and decreasing maximum and recovered strains suggest that plasticity in Ni and/or Si, as well as delamination between Ni and Si, may occur during cycling. Rate sensitivity in capacity is correlated with strain and a maximum Ni compressive stress of 230 ± 40 MPa is measured at the maximum state of lithiation.
Uniform intercalation is desired to enable next-generation Li-ion batteries. While we expect nonuniformity in materials undergoing a phase change, single-phase intercalation materials such as nickel manganese cobalt oxide are believed to lithiate uniformly at the particle/electrolyte interface. However, recent imaging reveals nonuniform lithiation. Motivated by this discrepancy, we examine if aspherical particle shape can cause such nonuniformity since the conventional belief is based on spherical particle theory. We obtain real particle geometries using rapid lab-based X-ray computed tomography and subsequently perform physics-based calculations accounting for electrochemical reactions at the particle/electrolyte interface and lithium transport inside the particle bulk. The aspherical geometry breaks the symmetry and causes nonuniform reaction distribution. Such nonuniformity is exacerbated as the particle becomes more aspherical. We report the proposed mechanism represents a fundamental limit on achievable lithiation uniformity in aspherical particles in the absence of other mechanisms causing inhomogeneity, such as grain structure, nonuniform carbon-binder coating, etc.
We report a first-principles atomic level assessment of the lithiation and reactivity of pre-lithiated Si clusters. Density functional theory formation energy calculations reveal that the pre-lithiated Li 16 Si 16 cluster exposed to two different Li fluxes can store Li between the concentrations of Li 2.5 Si and Li 3.5 Si. This increase in storage capacity is attributed to the start of an amorphization process in the cluster, and more importantly these results show that the intercalation reaction can be controlled by the flux of the Li-ions. However, in a real battery, the lithiation of the anode occurs simultaneously to the electrode-electrolyte reactions. Here we simulate the solid-electrolyte interphase (SEI) formation and simultaneous lithiation of a Li 16 Si 16 cluster in contact with two different electrolyte solutions: one with pure ethylene carbonate (EC), and another with a 1 M solution of LiPF 6 in EC. Our ab initio molecular dynamics simulations show that the solvent and salt are decomposed leading to the initial stages of the SEI layer formation and large part of the added Li becomes part of the SEI. Interestingly, the pure EC solution results in lower storage capacity and higher reactivity, whereas the presence of the salt causes the opposite effect: higher lithiation and reduced reactivity.
Recent reports have indicated that a manganese oxide spinel component, when embedded in a relatively small concentration in layered xLi2MnO3(1-x)LiMO2 (M=Ni, Mn, Co) electrode systems, can act as a stabilizer that increases their capacity, rate capability, cycle life, and first-cycle efficiency. These findings prompted us to explore the possibility of exploiting lithiated cobalt oxide spinel stabilizers by taking advantage of (1) the low mobility of cobalt ions relative to manganese and nickel ions in close-packed oxides and (2) their higher potential (~3.6 V vs. Li0) relative to manganese oxide spinels (~2.9 V vs. Li0) for the spinel-to-lithiated spinel electrochemical reaction. In particular, we have revisited the structural and electrochemical properties of lithiated spinels in the LiCo1-xNixO2 (0x0.2) system, first reported almost 25 years ago, by means of high-resolution (synchrotron) X-ray diffraction, transmission electron microscopy, nuclear magnetic resonance spectroscopy, electrochemical cell tests, and theoretical calculations. The results provide a deeper understanding of the complexity of intergrown layered/lithiated spinel LiCo1-xNixO2 structures, when prepared in air between 400 and 800 C, and the impact of structural variations on their electrochemical behavior. These structures, when used in low concentration, offer the possibility of improving the cycling stability, energy, and power of high energy (≥3.5 V) lithium-ion cells.
TiO 2 (B) exhibits unique electrochemical lithiation behavior where two closely spaced reduction and oxidation peaks, referred to as “double peaks,” are observed for 3-D forms of bulk and nanostructured TiO 2 (B) while a single broad redox peak is observed for 2-D nanosheet architectures. Here, we have used a combination of transmission electron microscopy (TEM), powder X-ray diffraction (XRD), Raman spectroscopy and cyclic voltammetry on TiO 2 (B) nanosheets as well as a series of thermally annealed nanosheets to map the morphological and phase transformation pathways that help clarify the structure-dependent lithiation behavior. We found that the double peak redox behavior only arises once a three dimensional nanocrystalline structure of TiO 2 (B) exists by observing nanoparticle growth on the TiO 2 (B) nanosheet surface via TEM at temperatures above 150 °C. This morphological transformation was also verified by Raman spectroscopy. The appearance of low-energy torsional modes at temperatures above 150 °C which are not observed in 2-D morphologies of TiO 2 (B) agrees well with TEM evidence of 3-D nanoparticle formation. Using scan rate dependent cyclic voltammetry we also verified that all lithiation behavior associated with TiO 2 (B) (either nanosheet or nanoparticle) is due primarily to a surface redox (pseudocapacitive) mechanism. The thermal annealing study also shows the phase transformation of surface nucleated TiO 2 (B) nanoparticles to anatase nanoparticles at temperatures above 200 °C. These studies clearly show how nano-morphological control can influence electrochemical lithiation behavior and help identify a possible mechanism to explain the double peak phenomenon observed for TiO 2 (B).
Linear (local) gyrokinetic predictions of edge microinstabilities in highly shaped, lithiated and non-lihiated NSTX discharges are reported using the gyrokinetic code GS2. Microtearing modes dominate the non-lithiated pedestal top. The stabilization of these modes at the lithiated pedestal top enables the electron temperature pedestal to extend further inwards, as observed experimentally. Kinetic ballooning modes are found to be unstable mainly at the mid-pedestal of both types of discharges, with unstable trapped electron modes nearer the separatrix region. At electron wavelengths, ETG modes are found to be unstable from mid-pedestal outwards for eta(e,exp)~2.2, with higher growth rates for the lithiated discharge. Near the separatrix, the critical temperature gradient for driving ETG modes is reduced in the presence of lithium, reflecting the reduction of the lithiated density gradients observed experimentally. A preliminary linear study in the edge of non-lithiated discharges shows that the equilibrium shaping alters the electrostatic modes stability, found more unstable at high plasma shaping.
Improved electrochemical performance of Si was recently reported by adding multivalent cation salts (such as Mg 2+ , Al 3+ , Ca 2+, etc.) in the electrolyte. This is achieved via the formation in an in situ manner of relatively more stable Li-M-Si ternary phases with less chemical reactivity. These phases stabilize Si anions and thus reduce side reactions with electrolytes at the surface and eventually benefit the overall electrochemistry. To understand the mechanism of ternary Zintl phase formation and its dynamics upon lithiation/delithiation, high-resolution solid-state 7 Li and 29 Si nuclear magnetic resonance (NMR) are utilized to directly probe the local Li and Si environments on Si electrodes harvested from coin and pouch cells at various states of (de)lithiation. The NMR spectra along with the electrochemical characterization reveal that lithiation of Si starts from the surface Si-O layer further confirmed by 7 Li– 29 Si cross-polarization NMR. Lithiation progresses with heterogeneous silicon clustering with Si -4 anions at high states of lithiation. At a fully lithiated state, the formation of overlithiated Si species is detected. At a low-voltage region (below 100 mV), direct evidence for Mg-ion insertion is found, postulated by two possible mechanisms: ion exchange with fully or overlithiated binary domains (Li 3.75+x Si) and/or a coinsertion with slightly underlithiated domains (similar to Li 3.55 Si). Upon delithiation, Li extraction starts from overlithiated Si domains. No evidence is found for electrochemical Mg removal. Evidence for a lithium-deficient Li y Mg 0.1 Si phase is found as a result of Li removal during charging. This investigation sheds light on the possible mechanisms of a new Si anode chemistry, which could enable the development of stable Si-based anodes for lithium-ion batteries.
Silicon offers high theoretical capacity as a negative electrode material for lithium-ion batteries; however, high irreversible capacity upon initial cycling and poor cycle life have limited commercial adoption. Herein, we report an operando isothermal microcalorimetry (IMC) study of a model system containing lithium metal and silicon composite film electrodes during the first two cycles of (de)lithiation. The total heat flow data are analyzed in terms of polarization, entropic, and parasitic heat flow contributions to quantify and determine the onset of parasitic reactions. These parasitic reactions, which include solid–electrolyte interphase formation, contribute to electrochemical irreversibility. Cycle 1 lithiation demonstrates the highest thermal energy output at 1509 mWh/g, compared to cycle 1 delithiation and cycle 2. To complement the calorimetry, operando X-ray diffraction is used to track the phase evolution of silicon. During cycle 1 lithiation, crystalline Si undergoes transformation to amorphous lithiated silicon and ultimately to crystalline Li 15 Si 4 . The solid-state amorphization process is correlated to a decrease in entropic heat flow, suggesting that heat associated with the amorphization contributes significantly to the entropic heat flow term. In conclusion, this study effectively uses IMC to probe the parasitic reactions that occur during lithiation of a silicon electrode, demonstrating an approach that can be broadly applied to quantify parasitic reactions in other complex systems.
Solutions for improving fast charging of lithium‐ion batteries have largely focused on alleviating through‐plane lithiation gradients while little is understood about in‐plane heterogeneities and how to resolve them. Herein, high‐speed synchrotron X‐ray diffraction (XRD) resolves graphite lithiation spatially and temporally during 6 C charging and 2 C discharging. At every point during operation, considerable differences in the state of lithiation across the pouch cell are present. Some regions are more responsive to operation than others, reaching full lithiation early during charge and full delithiation during discharge. Other regions within the cell never fully delithiate during discharge, despite a prolonged voltage hold at 2.8 V. Using time‐resolved XRD data, the calculated local current density (mA cm −2 ) at the graphite surface shows an unexpected occurrence of local inverted current densities where regions of graphite are observed to delithiate during charging and lithiate during discharging. A pseudo‐3D model is developed for the graphite electrode with spatially varying microstructural tortuosity to show how microstructural heterogeneity could influence spatial charge dynamics. The model could not predict the complex in‐plane charge behavior observed within the cell. Consequently physics‐based charging protocols based on homogeneous electrode assumptions may underestimate the local variations in charge dynamics and occurrence of lithium plating.
Conversion mechanism in lithium ion batteries provides higher capacity than intercalation mechanism since multiple numbers of electrons and lithium ions are associated. However, poor cycling stability, large voltage hysteresis, and low energy efficiency have been great challenges of conversion reaction. To address those issues, conversion-type electrode materials have been reformed via doping or substituting other elements. For example, iron fluorides (FeF 2 , FeF 3 ) have modified as iron oxyfluorides (FeF 1-x O x ), showing enhanced long-term stability. Furthermore, co-substituted (both anion and cation substituted) Fe 0.9 Co 0.1 OF (FeCoOF) was demonstrated excellent cycling stability. (capacity of 350 mAh g -1 at a current of 500 mA g -1 for 1000 cycles). Substituting anion and cation in iron fluoride has been suggested as an effective method to achieve better reversibility but understanding of lithiation reactions in co-substituted FeCoOF is not clear. This work takes advantage of ex-situ/ in-situ synchrotron X-ray based techniques and transmission electron microscopy to elucidate structural changes with lithium ion, which may provide fundamental insights into modifying conversion-type materials. Figure 1 presents discharge-charge curves and pair distribution function patterns acquired at each potential. As lithium ions were inserted, structural changes were noticed both at short-range and long-range. However, long-range ordering was nearly maintained even at 1 V, indicating absence of conversion reaction. Figure 2 shows lithiation induced structural evolution of a single FeCoOF nanorod observed in real time. As lithiation proceeds, the width of nanorods shows a stepwise increase, particularly A in figure 2d, which may indicate multiple steps of lithiation occur. Considering that conversion reaction takes place around 2 V in FeF 3 , co-substitution Co and O into iron fluoride may change thermodynamic features of lithiation reactions by lowering the initiation potential for conversion reaction. Instead, phase transformations occur at long-range order, which may help maintaining structural integrity during operation, eventually, achieving cycling stability.
Explore the source record for details and available documents.