Anomalous Hall effect in the noncollinear antiferromagnet Mn{sub 5}Si{sub 3}

Metallic antiferromagnets with noncollinear orientation of magnetic moments provide a playground for investigating spin-dependent transport properties by analysis of the anomalous Hall effect. The intermetallic compound Mn{sub 5}Si{sub 3} is an intinerant antiferromagnet with collinear and noncollinear magnetic structures due to Mn atoms on two inequivalent lattice sites. Here, magnetotransport measurements on polycrstalline thin films and a single crystal are reported. In all samples, an additional contribution to the anomalous Hall effect attributed to the noncollinear arrangment of magnetic moments is observed. Furthermore, an additional magnetic phase between the noncollinear and collinear regimes above a metamagnetic transition is resolved in the single crystal by the anomalous Hall effect.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of cold working and isothermal aging on the precipitation of sigma phase in 2205 duplex stainless steel

A comprehensive understanding of the formation of the sigma phase resulting from the eutectoid reaction ({delta} {yields} {sigma} + {gamma}{sub 2}) is required. The kinetics necessary for the eutectoid reaction are closely related to the amount of plastic deformation in DSS. This work investigates the microstructural evolution of the {sigma} phase in a 22Cr-5Ni SAF 2205 DSS after subsequent plastic deformation and isothermal aging. The precipitation of the {sigma} phase resulted from the higher driving force for precipitating intermetallic compounds and the higher diffusion rate of their elements by cold-rolling, as well as the sufficient supply of molybdenum. The maximum amount of {sigma} phase precipitation remarkably increased with an increasing cold deformation, as compared with the non-cold-rolled materials. - Highlights: Black-Right-Pointing-Pointer The microstructural evolution of sigma phase has been characterized. Black-Right-Pointing-Pointer The chemical compositions of sigma phases were analyzed using TEM-EDX. Black-Right-Pointing-Pointer The effect of cold deformation on the precipitation of sigma phase was investigated.

36 MATERIALS SCIENCE↗

Multi-scale mechanical modeling of Al-steel resistance spot welds

A multi-scale finite element modeling approach was developed to study the deformation and fracture behavior of Al-steel resistance spot welds. First, a micro-scale model was applied to simulate the mechanical responses of the intermetallic compound (IMC) layer having various morphologies and thicknesses under tensile and shear loading conditions. Second, the predicted tensile and shear strength of the IMC layer, that varied along the joint interface per the IMC layer morphology and thickness variation, was then introduced into 3D macro-scale models to predict the overall mechanical performance of weld coupons under coach peel, lap shear and cross-tension testing conditions. In conclusion, the numerical predictions agreed reasonably well with the experimental data.

36 MATERIALS SCIENCE↗

Understanding of Void Formation in Cu/Sn-Sn/Cu System During Transient Liquid Phase Bonding Process Through Diffusion Modeling

Transient Liquid Phase (TPL) bounding of Sn foil sandwiched between two Cu foils involves, in the temperature range above the melting point of Sn (232 °C) and below 350 °C, the formation and the growth of two intermetallic compounds (IMCs) Cu{sub 6}Sn{sub 5} and Cu{sub 3}Sn and mostly unintended micro-pores. The present study aims to analyze the mechanism of void development during the soldering process through an experimental and modeling approach of diffusion-controlled IMC transformation. This modeling couples the diffusion process and the interface motion with the volume shrinkage induced by the difference of partial molar volumes of atoms between each phase. We also consider two types of inter-diffusion transports: (i) inter-diffusion based on the exchange of Cu and Sn atoms and (ii) inter-diffusion of Sn atoms with vacancies allowing Kirkendall void formation. The simulations of IMC growth performed correspond to a sequence of planar phase layers, where the distinctive scallop morphology of the Cu{sub 6}Sn{sub 5} layer is described through an analytical function allowing to quantify the grain boundary diffusion pathway. We take into account of the volume diffusion mechanism for Cu{sub 3}Sn intermetallic. For Cu{sub 6}Sn{sub 5} intermetallic two mechanisms are considered, volume diffusion and grain boundary diffusion, limited by grain growth. The simulations of IMC growth kinetics, for different transport scenarios, are compared to the experimental evolving morphologies to determine the most likely mechanism of micro-void formation.

36 MATERIALS SCIENCE↗

Influence of Annealing on the Properties of Explosively Welded Titanium Grade 1—AW7075 Aluminum Alloy Bimetals

Explosive welding of titanium Grade 1 to AW7075 aluminum alloy arranged in parallel setup was performed. The annealing of produced bimetals at the temperatures of 450, 500 and 550 °C for times ranging from 20 to 100 h was carried out after explosive welding. The produced bimetal was characteristic by its wavy interface typical for that bonding process. Increase in the microhardness at the interface was recorded due to work hardening. Delamination of titanium Grade 1 flyer sheet was firstly observed when annealing temperature of 500 °C for 40 h was carried out. Annealing at 550 °C also resulted in delamination of upper sheet. The intermetallic compound (IMC) layer was observed at the interface after annealing of bimetals. The higher the annealing temperature and time, the higher the thickness of continuous IMC layer. The maximum measured thickness of IMC layer averaged 13 µm. Energy dispersive x-ray spectroscopy (EDS) and x-ray diffraction (XRD) analyses revealed that the interface layer is consisted of Al{sub 18}Ti{sub 2}Mg{sub 3} IMC. Microhardness at the interface increased dramatically up to 439 HV0.1 after annealing of bimetal due to the presence of above-mentioned IMC.

36 MATERIALS SCIENCE↗

Electron-irradiation-induced crystallization at metallic amorphous/silicon oxide interfaces caused by electronic excitation

Irradiation-induced crystallization of an amorphous phase was stimulated at a Pd-Si amorphous/silicon oxide (a(Pd-Si)/SiO{sub x}) interface at 298 K by electron irradiation at acceleration voltages ranging between 25 kV and 200 kV. Under irradiation, a Pd-Si amorphous phase was initially formed at the crystalline face-centered cubic palladium/silicon oxide (Pd/SiO{sub x}) interface, followed by the formation of a Pd{sub 2}Si intermetallic compound through irradiation-induced crystallization. The irradiation-induced crystallization can be considered to be stimulated not by defect introduction through the electron knock-on effects and electron-beam heating, but by the electronic excitation mechanism. The observed irradiation-induced structural change at the a(Pd-Si)/SiO{sub x} and Pd/SiO{sub x} interfaces indicates multiple structural modifications at the metal/silicon oxide interfaces through electronic excitation induced by the electron-beam processes.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Phase relations and structural properties of the ternary narrow gap semiconductors Zn{sub 5}Sb{sub 4}In{sub 2-{delta}}({delta}=0.15) and Zn{sub 9}Sb{sub 6}In{sub 2}

A systematic study of the Zn-rich corner of the ternary system Zn-Sb-In revealed the presence of two ternary compounds: stable Zn{sub 5}Sb{sub 4}In{sub 2-{delta}}({delta}=0.15) and metastable Zn{sub 9}Sb{sub 6}In{sub 2} with closely related crystal structures. Their common motif is a tetragonal basic structure of 3{sup 2}434 nets formed by the Sb atoms. The nets are stacked in antiposition to yield layers of square antiprisms sharing edges plus intervening tetracapped tetrahedra (tetreadersterns). The majority of Zn atoms occupy peripheral tetrahedra of such tetraedersterns, which produces frameworks with a composition 'ZnSb'. These frameworks represent orthorhombic superstructures: (2x1x1) for Zn{sub 5}Sb{sub 4}In{sub 2-{delta}}(Z=4) and (2x3x1) for Zn{sub 9}Sb{sub 6}In{sub 2} (Z=8) with respect to the tetragonal arrangement of Sb atoms. The In and remaining Zn atoms are distributed in the channels formed by the square antiprisms. Phase relations in the Zn-Sb-In system are complex. Crystals of metastable Zn{sub 9}Sb{sub 6}In{sub 2} are regularly intergrown with various amounts of Zn{sub 5}Sb{sub 4}In{sub 2-{delta}}. Additionally, a monoclinic variant to orthorhombic Zn{sub 9}Sb{sub 6}In{sub 2} could be identified. Zn{sub 9}Sb{sub 6}In{sub 2} decomposes exothermically into a mixture of Zn{sub 5}Sb{sub 4}In{sub 2-{delta}}, Zn{sub 4}Sb{sub 3} and elemental Zn at around 480 K. Both Zn{sub 5}Sb{sub 4}In{sub 2-{delta}}and Zn{sub 9}Sb{sub 6}In{sub 2} are poor metals with resistivity values that are characteristic of heavily doped or degenerate semiconductors (0.2-3 m {Omega} cm at room temperature). - Graphical abstract: A metastable intermetallic compound with the composition Zn{sub 9}Sb{sub 6}In{sub 2} has been identified in the ternary system Zn-Sb-In. Its structure relates to tetragonal CuAl{sub 2} in that it contains 3{sup 2}434 nets (formed by the Sb atoms) that are stacked in antiposition orientation.

36 MATERIALS SCIENCE↗

The sequence of intermetallic formation and solidification pathway of an Al–13Mg–7Si–2Cu in-situ composite

The phase transformation sequence and solidification behaviour of an Al–13Mg–7Si–2Cu in-situ composite was examined using a combination of computer-aided cooling curve thermal analysis and interrupted quenching techniques. Five different phases were identified by analysing the derivative cooling curves, the X-ray diffraction profile, optical and scanning electron microscopy images and the corresponding energy dispersive spectroscopy. It has been found that the solidification of this alloy begins with primary Mg{sub 2}Si precipitation and continues with the formation of eutectic Al–Mg{sub 2}Si, followed by Al{sub 5}FeSi and simultaneous precipitation of Al{sub 5}Cu{sub 2}Mg{sub 8}Si{sub 6} and Al{sub 2}Cu complex intermetallic phases. The formation of the last three intermetallic compounds changes the solidification behaviour of these composites remarkably due to their complex eutectic formation reactions. The solidification of the alloy, calculated using the Factsage thermochemical analysis software, has demonstrated a good agreement with the experiments in terms of compound prediction, their weight fractions and reaction temperatures. - Highlights: • Solidification path of a commercial Al-13Mg-7Si-2Cu composite was characterized. • Five different phases were identified and then confirmed with EDS and XRD results. • Mg{sub 2}Si, Al-Mg{sub 2}Si,Al{sub 5}FeSi (β),Al{sub 5}Cu{sub 2}Mg{sub 8}Si{sub 6} (Q) and Al{sub 2}Cu(θ) precipitated respectively. • Solidification was predicted using the Factsage thermochemical analysis software.

36 MATERIALS SCIENCE↗

Investigation on Microstructure and Mechanical Properties of TA10–Q245R Composite Plate Formed by Explosive Welding

The titanium alloy TA10 and the carbon steel Q245R are welded by explosive welding, and post-weld heat treatment (PWHT) is carried out for the TA10–Q245R composite plate. Microstructure and mechanical properties of the composite plate are investigated both in as-welded (AW) condition and after PWHT, respectively. Results show that, in AW condition, the bonding interface of composite plate presents wavy morphology, and at both sides of the interface plastic deformation is generated to a certain degree. Near the interface interdiffusion zone of alloying elements exists, and no Fe-Ti intermetallic compound is produced at the interface. SEM images indicate that the tensile fracture of composite plate presents the characteristic of ductile fracture, and no defects such as gas pores or impurities are found on the surface of shear fracture. After PWHT, the interfacial microstructure of the composite plate is obviously changed. Compared with the mechanical properties of the composite plate in AW condition, both tensile strength and shear strength of the composite plate are decreased to a certain extent after PWHT. With various factors into consideration, the suitable heat treatment procedure of TA10–Q245R composite plate is determined as follows: 550 °C × 1.5 h.

36 MATERIALS SCIENCE↗

Effect of Different Heat Treatments on the Microstructural Evolution and Mechanical Properties of Ni-Cr-Si Alloy Fabricated by Laser Additive Manufacturing

Ni-Cr-Si alloy samples were fabricated on mild steel via laser additive manufacturing technology. The microstructural evolution and mechanical properties of the samples were studied systematically in as-deposited conditions and under three different types of heat-treated conditions. The scanning electron microscopy, energy-dispersive x-ray spectroscopy and x-ray diffraction results showed that the structures of the as-deposited samples were mainly dendritic matrices of γ(Ni, Fe), continuous interdendritic eutectics of γ + Ni{sub 3}B and discrete Cr-rich carbides and borides. After solid solution treatment, carbides (Cr{sub 7}C{sub 3}) and borides (CrB) precipitated on the boundary of the eutectic structure, distributing discretely in the matrix. In the solution plus aging heat-treated conditions, the interdendritic eutectics formed Ni{sub 3}Fe intermetallic compounds with a layered distribution. After annealing, the grains were refined, and the hard phases (CrB) were uniformly dispersed along the grain boundary. Among the tested samples, the as-deposited specimens exhibited the highest microhardness and good wear ability at room temperature; however, the wear resistance of the as-deposited sample obviously decreased at 250 °C. The mechanical properties of the specimens were not greatly improved by solution treatment or solution plus aging treatment. The sample subjected to annealing treatment exhibited excellent wear resistance both at room temperature and at a service temperature of 250 °C.

36 MATERIALS SCIENCE↗

Diffusion bonding titanium to stainless steel using Nb/Cu/Ni multi-interlayer

By using Nb/Cu/Ni structure as multi-interlayer, diffusion bonding titanium to austenitic stainless steel has been conducted. The effects of bonding temperature and bonding time on the interfacial microstructure were analyzed by scanning electron microscope equipped with energy dispersive spectroscope, and the joint strength was evaluated by tensile test. The results showed that Ni atoms aggregated at the Cu-Nb interface, which promoted Cu solution in Nb. This phenomenon forms a Cu-Nb solution strengthening effect. However, such effect would decay by using long bonding time that dilutes Ni atom aggregation, or be suppressed by using high bonding temperature that embrittles the Cu-Nb interface due to the formation of large grown intermetallic compounds. The sound joint was obtained by promoted parameters as 850 Degree-Sign C for 30-45 min, under which a bonding strength around 300 MPa could be obtained. - Highlights: Black-Right-Pointing-Pointer Titanium was diffusion bonded to stainless steel using Nb/Cu/Ni multi-interlayer. Black-Right-Pointing-Pointer The effects of bonding parameters on microstructure and joint strength were studied. Black-Right-Pointing-Pointer Nickel aggregation promotes Cu solution in Nb which can strengthen the joint. Black-Right-Pointing-Pointer The sound joint with strength of around 300 MPa was obtained by promoted parameters.

36 MATERIALS SCIENCE↗

The synthesis and air oxidation behavior of U-Si-Al and U-Si-B compositions

Uranium silicide intermetallic compounds are currently under investigation by the DOE-NE Advanced Fuels Campaign as candidate accident tolerant nuclear fuel concepts for light water reactors. While many U-Si compounds offer benefits compared to reference UO{sub 2} in terms of heavy metal density and thermal conductivity, they have been shown to display poor resistance to oxidizing atmospheres above 400 Celsius degrees. The general oxidation behavior of all U-Si compounds is oxidation of uranium; formation of UO{sub 2} followed by U{sub 3}O{sub 8} leads to rapid pulverization of the material. It is hypothesized that introducing an additional compositional degree of freedom by exploring U-Si-X (X=Al or B) ternary systems may provide the means to design a candidate nuclear fuel which optimizes the benefits of each binary. Phase analysis and preliminary oxidation testing were performed on four compositions containing alloying additions to U{sub 3}Si{sub 2} and U{sub 3}Si{sub 5}. Aluminum additions to U{sub 3}Si{sub 2} were observed to increase the oxidation resistance by delaying the onset of oxidation during synthetic air ramp testing. U{sub 3}Al{sub 2}Si{sub 3} delayed the onset of oxidation to T>650 C. degrees. During a 10 hour isothermal hold at 400 C. degrees in air the compound gained very little mass, indicating that it could be stable at reactor operating temperatures. Further analysis of this material is necessary to determine its oxidation behavior in steam and determine the specific mechanism that is providing the delayed oxidation. Boron additions to U{sub 3}Si{sub 5} do not appear to provide any additional oxidation resistance to the compound as tested in this work. The 1.67 at.% addition of B produced primarily single-phase composition. Melting and sintering studies followed by further compositional and thermal analyses are required to advance this composition as a candidate composite fuel additive. Lastly, the nominally U{sub 3}BSi{sub 4} composition produced a multi-phase system which provided no additional oxidation resistance following either a synthetic air ramp oxidation test or a pre-passivation isothermal hold at 800 C. degrees.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Influence of Indium on Microstructure and Properties of Sn-Pb Binary Alloy Applied in Photovoltaic Ribbon

In this work, the conductivity, melting point, microstructure, spreading behavior, and mechanical properties of three types of Sn-Pb-In(indium) alloys are investigated along with Sn60Pb40 alloy as a reference. The results show that the In element improves the comprehensive properties of the Sn-Pb alloys. The maximum conductivity of the Sn-Pb-In alloys is 7.08 MS/m when the content of the In element is 3 wt.%. With an increasing content of the In element, the melting points of the Sn-Pb-In alloys gradually decrease from 183 to 166 °C. The microstructures of the alloys are refined with the addition of In. The intermetallic compound (IMC) InSn{sub 4} is only found in Sn60Pb34In6, except for the α-Pb and β-Sn phases. A spread test shows that only IMC Cu{sub 6}Sn{sub 5} is present at the Cu/solder interface of the solder joints. The Sn60Pb34In3 solder joint shows the highest ultimate tensile strength of 54 MPa. The microhardness of the alloys slightly increases from 12.76 HV{sub 0.05} to 13.56 HV{sub 0.05} with the In content increasing from 0 to 3 wt.%, while a sharp increase to 15.53 HV{sub 0.05} is observed when the amount of In exceeds 3 wt.%.

36 MATERIALS SCIENCE↗

Sample dependence of giant magnetocaloric effect in a cluster-glass system Ho{sub 5}Pd{sub 2}

In order to investigate the effect of vacancy on the magnetocaloric effect in Ho{sub 5}Pd{sub 2}, we have carried out X-ray diffraction, magnetization, and specific heat measurements in the rare-earth intermetallic compound Ho{sub 5+x}Pd{sub 2}(−0.4 ≤ x ≤ 0.4). The maximum magnetic entropy change −ΔS{sub m}{sup max}, the maximum adiabatic temperature change ΔT{sub ad}{sup max}, and the relative cooling power of Ho{sub 5+x}Pd{sub 2} take large values at x = 0−0.4 for the field change of 5 T. The paramagnetic Curie temperature θ{sub p} increases with an increase of x. This fact suggests that the enhancement of ferromagnetic coupling among the correlated spins leads to the increase of magnetocaloric effect.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Investigating stainless steel/aluminum bimetallic structures fabricated by cold metal transfer (CMT)-based wire-arc directed energy deposition

Here, this study investigated the process of fabricating a bimetallic structure of 316L stainless steel (SS) and 4043 aluminum (Al) using wire-arc directed energy deposition (DED) based on the cold metal transfer (CMT) process. The impact of heat input on the fabricated structure’s geometry, porosity, and microstructures at the interface, with a specific emphasis on the intermetallic compound (IMC) formation, and the subsequent impact on the joint strength of the structure, were studied. The IMC layer at the interface was predominantly comprised of FeAl 2 Si. For the various heat input conditions studied, the IMC layer's thickness varied from 5 µm to 18 µm. The tensile strength reached up to approximately 130 MPa, which is among the highest reported in the literature for steel/Al bimetallic structures. The specimens fabricated with high heat input conditions had a thicker IMC layer at the steel/Al interface, resulting in a more brittle interface and degradation of the mechanical properties.

36 MATERIALS SCIENCE↗

Electromigration induced Kirkendall void growth in Sn-3.5Ag/Cu solder joints

Effects of electric current flow on the Kirkendall void formation at solder joints were investigated using Sn-3.5Ag/Cu joints specially designed to have localized nucleation of Kirkendall voids at the Cu{sub 3}Sn/Cu interface. Under the current density of 1 × 10{sup 4} A/cm{sup 2}, kinetics of Kirkendall void growth and intermetallic compound thickening were affected by the electromigration (EM), and both showed the polarity effect. Cu{sub 6}Sn{sub 5} showed a strong susceptibility to the polarity effect, while Cu{sub 3}Sn did not. The electromigration force induced additional tensile (or compressive) stress at the cathode (or anode), which accelerated (or decelerated) the void growth. From the measurements of the fraction of void at the Cu{sub 3}Sn/Cu interface on SEM micrographs and analysis of the kinetics of void growth, the magnitude of the local stress induced by EM was estimated to be 9 MPa at the anode and −7 MPa at the cathode.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of Ag3Sn nanoparticles and temperature on Cu6Sn5 IMC growth in Sn-xAg/Cu solder joints

Highlights: • The number density of Ag{sub 3}Sn grains precipitated upon Cu{sub 6}Sn{sub 5}, increases with Ag content and reflow temperature (T). • Raising of wt. % of Ag in solder and lowering of T can cause an increase in grain diameter of Ag{sub 3}Sn nanoparticles. • The blockading effect of Ag{sub 3}Sn particles on Cu{sub 6}Sn{sub 5} IMC growth is more pronounced in Sn-3Ag and Sn-3.5Ag alloys. • IMC suppressing nanoparticles can be utilized for solder materials design. - Abstract: The growing importance of Pb-free Sn-xAg solders and high cost of Ag has attracted the attention of researchers to perform experiment with solders with varied content of Ag element. In this study, Sn-xAg(0,1,2,3.5) solder balls on Cu substrate have been reflowed at 250/275/300 °C for 60 s and air cooled. Finite element method has been utilized to simulate the concentration and temperature during cooling. The experimental results suggest that the Cu flux through grain boundary diffusion is the dominant mechanism for Cu{sub 6}Sn{sub 5} intermetallic compound growth in Pure Sn and Sn-1Ag solders. When the Ag content is increased, as in case of Sn-3Ag and Sn-3.5Ag alloys; the shielding effect of Ag{sub 3}Sn nanoparticles is the determinant factor for affecting the thickness of Cu{sub 6}Sn{sub 5} IMC. Both Cu influx rate and shielding effect of Ag{sub 3}Sn nanoparticles are enhanced with the raise in pre-cooled isothermal reflow temperature. Sn-1Ag solder is observed to have the thickest Cu{sub 6}Sn{sub 5} IMC.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Enormous electron-electron scattering in the filled-cage cubic compound B a 10 T i 24 B i 39

Cubic intermetallic compound Ba 10 Ti 24 Bi 39 has a Ba 6 Bi 16 polyhedral cage with a Bi guest atom encapsulated inside. The compound can be formulated as Ba 5 Ti 12 Bi$_{19+x}$ when $x$ signifies the extra Bi atoms filling cages. It crystallizes in a complex noncentrosymmetric cubic structure in space group $P-43m$ with cell parameter $a = 12.6787(4)Å$. The guest Bi atoms distribute diffusely in the cages and seem to play a role in stabilizing the crystal structure. The magnetic susceptibility of this compound shows a weak temperature dependence with a positive slope coefficient. The charge transport properties as a function of temperature exhibit two competing components which are in charge of positive and negative magnetoresistances. Electronic band-structure calculations reveal the complex multiband hybridization of Ti/Bi orbitals near the Fermi surface, which may play a role in the enormous electron-electron scattering in this material evidenced by the large Kadowaki-Woods ratio.

36 MATERIALS SCIENCE↗