Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “FLY ASH”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 325 records · Page 18

A green gem in the treasure state

The article describes a project conducted by researchers at the Western Transportation Institute (WTI) at Montana State University (MSU) into 100% fly ash concrete made with glass aggregate. Fly ash used is a Class C fly ash from the Corette Power Plant in Billings, Mont. Recycled pulverized glass of mixed color was used. Tests were carried out on two mix designs and then the material was used for load bearing beams by MacArthur, Means and Wells (MMW) Architects. 3 refs., 2 tabs., 6 photos.

01 COAL, LIGNITE, AND PEAT↗

Environmental chamber measurements of mercury flux from coal utilization by-products

An environmental chamber was constructed to measure the mercury flux from coal utilization by-product (CUB) samples. Samples of fly ash, FGD gypsum, and wallboard made from FGD gypsum were tested under both dark and illuminated conditions with or without the addition of water to the sample. Mercury releases varied widely, with 7-day experiment averages ranging from -6.8 to 73 ng/m2 h for the fly ash samples and -5.2 to 335 ng/m2 h for the FGD/wallboard samples. Initial mercury content, fly ash type, and light exposure had no observable consistent effects on the mercury flux. For the fly ash samples, the effect of a mercury control technology was to decrease the emission. For three of the four pairs of FGD gypsum and wallboard samples, the wallboard sample released less (or absorbed more) mercury than the gypsum.

20 FOSSIL-FUELED POWER PLANTS↗

Resistance of fly ash-Portland cement blends to thermal shock

Thermal-shock resistance of high-content fly ash-Portland cement blends was tested in the following ways. Activated and non-activated blends with 80-90 % fly ash F (FAF) were left to set at room temperature, then hydrated for 24 hours at 85°C and 24-more hours at 300°C and tested in five thermal-shock cycles (600°C heat - 25°C water quenching). XRD, and thermal gravimetric analyses, along with calorimetric measurements and SEM-EDX tests demonstrated that the activated blends form more hydrates after 24 hours at 300°C, and achieve a higher short-term compressive strength than do non-activated ones. Sodium meta-silicate and sodaash engendered the concomitant hydration of OPC and FAF, with the formation of mixed crystalline FAF-OPC hydrates and FAF hydrates, such as garranite, analcime, and wairakite, along with the amorphous FAF hydration products. In SS-activated and non-activated blends separate OPC (tobermorite) and FAF (amorphous gel) hydrates with no mixed crystalline products formed. The compressive strength of all tested blends decreased by nearly 50% after 5 thermal-shock test cycles. These changes in the compressive strength were accompanied by a marked decrease in the intensities of XRD patterns of the crystalline hydrates after the thermalshock. As a result, there was no significant difference in the performance of the blends with different activators

15 GEOTHERMAL ENERGY↗

Trace element partitioning in ashes from boilers firing pure wood or mixtures of solid waste with respect to fuel composition, chlorine content and temperature

Highlights: • Different solids waste incineration is discussed in grate fired and fluidized bed boilers. • We explained waste composition, temperature and chlorine effects on metal partitioning. • Excessive chlorine content can change oxide to chloride equilibrium partitioning the trace elements in fly ash. • Volatility increases with temperature due to increase in vapor pressure of metals and compounds. • In Fluidized bed boiler, most metals find themselves in fly ash, especially for wood incineration. - Abstract: Trace element partitioning in solid waste (household waste, industrial waste, waste wood chips and waste mixtures) incineration residues was investigated. Samples of fly ash and bottom ash were collected from six incineration facilities across Sweden including two grate fired and four fluidized bed incinerators, to have a variation in the input fuel composition (from pure biofuel to mixture of waste) and different temperature boiler conditions. As trace element concentrations in the input waste at the same facilities have already been analyzed, the present study focuses on the concentration of trace elements in the waste fuel, their distribution in the incineration residues with respect to chlorine content of waste and combustion temperature. Results indicate that Zn, Cu and Pb are dominating trace elements in the waste fuel. Highly volatile elements mercury and cadmium are mainly found in fly ash in all cases; 2/3 of lead also end up in fly ash while Zn, As and Sb show a large variation in distribution with most of them residing in the fly ash. Lithophilic elements such as copper and chromium are mainly found in bottom ash from grate fired facilities while partition mostly into fly ash from fluidized bed incinerators, especially for plants fuelled by waste wood or ordinary wood chips. There is no specific correlation between input concentration of an element in the waste fuel and fraction partitioned to fly ash. Temperature and chlorine content have significant effects on partitioning characteristics by increasing the formation and vaporization of highly volatile metal chlorides. Zinc and cadmium concentrations in fly ash increase with the incineration temperature.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Properties of mortars made by uncalcined FGD gypsum-fly ash-ground granulated blast furnace slag composite binder

Highlights: Black-Right-Pointing-Pointer The mortar with uncalcined FGD gypsum has suitable workability. Black-Right-Pointing-Pointer The strength of mortar with uncalcined FGD gypsum is higher than that of mortar without uncalcined FGD gypsum. Black-Right-Pointing-Pointer The dry shrinkage of mortar with uncalcined FGD gypsum is lower than that of mortar without uncalcined FGD gypsum. Black-Right-Pointing-Pointer The leaching of sulfate ion of mortar is studied. - Abstract: A series of novel mortars were developed from composite binder of uncalcined FGD gypsum, fly ash (FA) and ground granulated blast furnace slag (GGBFS) for the good utilization of flue gas desulphurization (FGD) gypsum. At a fixed ratio (20%) of GGBFS to the composite binder, keeping consistency of the mortar between 9.5 and 10.0 cm, the properties of the composite mortar were studied. The results show that higher water/binder (W/B) is required to keep the consistency when increasing the percentage of FGD gypsum. No obvious influences of the W/B and content of FGD gypsum on the bleeding of paste were observed which keeps lower than 2% under all experimental conditions tried. The highest compressive and flexural strengths (ratio is 20% FGD gypsum, 20% GGBFS and 60% FA) are 22.6 and 4.3 MPa at 28 days, respectively. Scanning electron microscopy (SEM) and X-ray diffraction (XRD) results indicate that massive ettringite crystals and C-S-H gels exist in the hydration products. At 90 days the mortars with FGD gypsum is dramatically smaller drying shrinkage (563-938 micro strain) than that without FGD gypsum (about 2250 micro strain). The release of the SO{sub 4}{sup 2-} from the mortar was analyzed, indicating that the dissolution of sulfate increases with FGD gypsum. The concentration of SO{sub 4}{sup 2-} releasing from the mortar with 10% FGD gypsum is almost equal to that obtained from the mortar without FGD gypsum. The release of SO{sub 4}{sup 2-} from the mortar with 20% FGD gypsum is 9200 mg{center_dot}m{sup -2}, which is lower than that from the mortar with 95% cement clinker and 5% FGD gypsum.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Degradation of Thermal Barrier Coatings from Deposits and Its Mitigation

Ceramic thermal barrier coatings (TBCs) used in gas-turbine engines afford higher operating temperatures, resulting in enhanced efficiencies and performance. However, in the case of syngas-fired engines, fly ash particulate impurities that may be present in syngas can melt on the hotter TBC surfaces and form glassy deposits. These deposits can penetrate the TBCs leading to their failure. In experiments using lignite fly ash to simulate these conditions we show that conventional TBCs of composition 93wt% ZrO 2 + 7wt% Y 2 O 3 (7YSZ) fabricated using the air plasma spray (APS) process are completely destroyed by the molten fly ash. The molten fly ash is found to penetrate the full thickness of the TBC. The mechanisms by which this occurs appear to be similar to those observed in degradation of 7YSZ TBCs by molten calcium-magnesium-aluminosilicate (CMAS) sand and by molten volcanic ash in aircraft engines. In contrast, APS TBCs of Gd 2 Zr 2 O 7 composition are highly resistant to attack by molten lignite fly ash under identical conditions, where the molten ash penetrates ~25% of TBC thickness. This damage mitigation appears to be due to the formation of an impervious, stable crystalline layer at the fly ash/Gd 2 Zr 2 O 7 TBC interface arresting the penetrating molten-fly-ash front. Additionally, these TBCs were tested using a rig with thermal gradient and simultaneous accumulation of ash. Modeling using an established mechanics model has been performed to illustrate the modes of delamination, as well as further opportunities to optimize coating microstructure. Transfer of the technology was developed in this program to all interested parties.

20 FOSSIL-FUELED POWER PLANTS↗

Construction of an embankment with a fly and bottom ash mixture: field performance study

Fly ash and bottom ash are coal combustion by-products (CCBPs) that are generated in large quantities throughout the world. It is often economical to dispose ash as mixtures rather than separately; that notwithstanding, only a few studies have been performed to investigate the behavior of fly and bottom ash mixtures, particularly those with high contents of fly ash. Also, there is very limited data available in the literature on the field performance of structures constructed using ash mixtures. This paper describes the construction and the instrumentation of a demonstration embankment built with an ash mixture (60:40 by weight of fly ash:bottom ash) on State Road 641, Terre Haute, Ind. Monitoring of the demonstration embankment was conducted for a period of 1 year from the start of construction of the embankment. The settlement of the embankment stabilized approximately 5 months after the end of its construction. According to horizontal inclinometer readings, the differential settlement at the top of the embankment is about 5 mm. Results from field quality control tests performed during construction of the demonstration embankment and monitoring data from vertical and horizontal inclinometers and settlement plates indicate that the ash mixture investigated can be considered an acceptable embankment construction material.

01 COAL, LIGNITE, AND PEAT↗

Alkali-activated Class F Fly Ash-rich Portland Cement Blends as Alternative Thermal Shock Resistant Cements

This study focused on evaluating the resistance of 300°C-autocalved alkali-activing Class F fly ash (FAF)-rich Type II Ordinary Portland Cement (OPC) blends with 80/20 and 90/10 FAF/OPC ratios to five thermal-shock (TS) fatigue cycles (one cycle, 600°C heat – 25°C water quenching). The factors to be evaluated included the hydration behaviors, crystalline/ amorphous phaseidentifications, -compositions and -transformations, and microstructural-developments andalterations for blended cements assembled by three different alkaline activators, sodium metasilicate (SMS), soda ash (SA), and sodium sulfate (SS). All factors were related directory to the changes in compressive strength after TS testing. The setting time of cement slurries at 25° and 85°C depended on the alkaline activators; SMS and SA contributing to a strong alkalinity hastened setting, while SS with moderate alkalinity extended the setting time. A more prolonged setting time was observed from non-activated cement. In this case, there were two separated hydration reactions: The first reaction was the hydration of OPC; the second one was associated with the dissolution and pozzolanic activity of FAF. In contrast, all alkali- activated cements engendered the concomitant hydration of OPC and FAF, thereby conferring a higher compressive strength on them than that of the non-activator one. The principal contributor to the development of strength of both the non-activated and activated cements at 300°C was the amorphous NaO 2 - or CaO-Al 2 O 3 - SiO 2 -H 2 O (N,C-A-S-H) phase formed by the interactions between alkaline activator, OPC, and FAF. This phase played an important role in minimizing the loss in strength after TS. On the other hand, adding SMS and SA introduced the mixed crystalline FAF-OPC hydrates, such as garranite and wairakite, as the major phases, into the autoclaved cement bodies. Also, these activators induced the formation of two FAF-related crystalline hydrates, analcime as the major phase and riversidelite (0.9 nm tobermorite) as the minor one. However, these identified phases were sensitive to TS, so converting the major phases into minor phases or vanishment. In contrast, three crystalline phases including calcite and anhydrous sodium sulfate as the major ones and 1.1 nm tobermorite as the minor one, that formed in non-activated and activated cements remained unchanged after TS. Additionally, SAactivated cement revealed porous microstructure created by the incorporation of copious amount of carbonate reaction products into the cement, raising concerns that cements might enhance the rate of water transportation and reduce compressive strength. Nevertheless, TS-insensitive amorphous N,C-A-S-H phase as the major cementitions structure coexisting with TS-insensitive crystalline products were responsible for sustaining the integrity of alkali-activated FAF-rich OPC cement systems in such harsh heat-cooling fatigue environments.

15 GEOTHERMAL ENERGY↗

Thermal Shock-resistant Cement

We studied the effectiveness of sodium silicate-activated Class F fly ash in improving the thermal shock resistance and in extending the onset of hydration of Secar #80 refractory cement. When the dry mix cement, consisting of Secar #80, Class F fly ash, and sodium silicate, came in contact with water, NaOH derived from the dissolution of sodium silicate preferentially reacted with Class F fly ash, rather than the #80, to dissociate silicate anions from Class F fly ash. Then, these dissociated silicate ions delayed significantly the hydration of #80 possessing a rapid setting behavior. We undertook a multiple heating -water cooling quenching-cycle test to evaluate the cement’s resistance to thermal shock. In one cycle, we heated the 200°C-autoclaved cement at 500°C for 24 hours, and then the heated cement was rapidly immersed in water at 25°C. This cycle was repeated five times. The phase composition of the autoclaved #80/Class F fly ash blend cements comprised four crystalline hydration products, boehmite, katoite, hydrogrossular, and hydroxysodalite, responsible for strengthening cement. After a test of 5- cycle heat-water quenching, we observed three crystalline phase-transformations in this autoclaved cement: boehmite → γ-Al 2 O 3 , katoite → calcite, and hydroxysodalite → carbonated sodalite. Among those, the hydroxysodalite → carbonated sodalite transformation not only played a pivotal role in densifying the cementitious structure and in sustaining the original compressive strength developed after autoclaving, but also offered an improved resistance of the #80 cement to thermal shock. In contrast, autoclaved Class G well cement with and without Class F fly ash and quartz flour failed this cycle test, generating multiple cracks in the cement. The major reason for such impairment was the hydration of lime derived from the dehydroxylation of portlandite formed in the autoclaved cement, causing its volume to expand.

15 GEOTHERMAL ENERGY↗

Degradation of TBC Systems in Environments Relevant to Advanced Gas Turbines for IGCC Systems

Air plasma sprayed (APS) thermal barrier coatings (TBCs) are used to provide thermal insulation for the hottest components in gas turbines. Zirconia stabilized with 7wt% yttria (7YSZ) is the most common ceramic top coat used for turbine blades. The 7YSZ coating can be degraded from the buildup of fly-ash deposits created in the power-generation process. Fly ash from an integrated gasification combined cycle (IGCC) system can result from coal-based syngas. TBCs are also exposed to harsh gas environments containing CO 2 , SO 2 , and steam. Degradation from the combined effects of fly ash and harsh gas atmospheres has the potential to severely limit TBC lifetimes. The main objective of this study was to use lab-scale testing to systematically elucidate the interplay between prototypical deposit chemistries (i.e., ash and its constituents, K 2 SO 4 , and FeS) and environmental oxidants (i.e., O 2 , H 2 O and CO 2 ) on the degradation behavior of advanced TBC systems. Several mechanisms of early TBC failure were identified, as were the specific fly-ash constituents responsible for degradation. The reactivity of MCrAlY bondcoats used in TBC systems was also investigated. The specific roles of oxide and sulfate components were assessed, together with the complex interplay between gas composition, deposit chemistry and alloy reactivity. Bondcoat composition design strategies to mitigate corrosion were established, particularly with regard to controlling phase constitution and the amount of reactive elements the bondcoat contains in order to achieve optimal corrosion resistance.

01 COAL, LIGNITE, AND PEAT↗

Radioactive Demonstration Of Mineralized Waste Forms Made From Hanford Low Activity Waste (Tank Farm Blend) By Fluidized Bed Steam Reformation (FBSR)

The U.S. Department of Energy’s Office of River Protection (ORP) is responsible for the retrieval, treatment, immobilization, and disposal of Hanford’s tank waste. A key aspect of the River Protection Project (RPP) cleanup mission is to construct and operate the Hanford Tank Waste Treatment and Immobilization Plant (WTP). The WTP will separate the tank waste into high-level and low-activity waste (LAW) fractions, both of which will subsequently be vitrified. The projected throughput capacity of the WTP LAW Vitrification Facility is insufficient to complete the RPP mission in the time frame required by the Hanford Federal Facility Agreement and Consent Order, also known as the Tri-Party Agreement (TPA), i.e. December 31, 2047. Supplemental Treatment is likely to be required both to meet the TPA treatment requirements as well as to more cost effectively complete the tank waste treatment mission. The Supplemental Treatment chosen will immobilize that portion of the retrieved LAW that is not sent to the WTP’s LAW Vitrification facility into a solidified waste form. The solidified waste will then be disposed on the Hanford site in the Integrated Disposal Facility (IDF). Fluidized Bed Steam Reforming (FBSR) offers a moderate temperature (700-750°C) continuous method by which LAW can be processed irrespective of whether the waste contain organics, nitrates, sulfates/sulfides, chlorides, fluorides, volatile radionuclides or other aqueous components. The FBSR technology can process these wastes into a crystalline ceramic (mineral) waste form. The mineral waste form that is produced by co-processing waste with kaolin clay in an FBSR process has been shown to be comparable to LAW glass, i.e. leaches Tc-99, Re and Na at <2g/m 2 during ASTM C1285 (Product Consistency) durability testing. Monolithing of the granular FBSR product was investigated to prevent dispersion during transport or burial/storage. Monolithing in an inorganic geopolymer binder, which is amorphous, macro-encapsulates the granules, and the monoliths pass ANSI/ANS 16.1 and ASTM C1308 durability testing with Re achieving a Leach Index (LI) of 9 (the Hanford Integrated Disposal Facility, IDF, criteria for Tc-99) after a few days and Na achieving an LI of >6 (the Hanford IDF criteria for Na) in the first few hours. The granular and monolithic waste forms also pass the EPA Toxicity Characteristic Leaching Procedure (TCLP) for all Resource Conservation and Recovery Act (RCRA) components at the Universal Treatment Standards (UTS). Two identical Benchscale Steam Reformers (BSR) were designed and constructed at SRNL, one to treat non-radioactive simulants and the other to treat actual radioactive wastes. The results from the non-radioactive BSR were used to determine the parameters needed to operate the radioactive BSR in order to confirm the findings of non-radioactive FBSR pilot scale and engineering scale tests and to qualify an FBSR LAW waste form for applications at Hanford. Radioactive testing commenced using SRS LAW from Tank 50 chemically trimmed to look like Hanford’s blended LAW known as the Rassat simulant as this simulant composition had been tested in the non-radioactive BSR, the non-radioactive pilot scale FBSR at the Science Applications International Corporation-Science and Technology Applications Research (SAIC-STAR) facility in Idaho Falls, ID and in the TTT Engineering Scale Technology Demonstration (ESTD) at Hazen Research Inc. (HRI) in Denver, CO. This provided a “tie back” between radioactive BSR testing and non-radioactive BSR, pilot scale, and engineering scale testing. Approximately six hundred grams of non-radioactive and radioactive BSR product were made for extensive testing and comparison to the non-radioactive pilot scale tests performed in 2004 at SAIC-STAR and the engineering scale test performed in 2008 at HRI with the Rassat simulant. The same mineral phases and off-gas species were found in the radioactive and non-radioactive testing. The granular ESTD and BSR products (radioactive and non-radioactive) were analyzed for total constituents and durability tested as a granular waste form. A subset of the granular material was stabilized in a clay based geopolymer matrix at 42% and 65% FBSR loadings and durability tested as a monolith waste form. The 65 wt% FBSR loaded monolith made with clay (radioactive) was more durable than the 67-68 wt% FBSR loaded monoliths made from fly ash (non-radioactive) based on short term PCT testing. Long term, 90 to 107 day, ASTM C1308 testing (similar to ANSI/ANS 16.1 testing) was only performed on two fly ash geopolymer monoliths at 67-68 wt% FBSR loading and three clay geopolymer monoliths at 42 wt% FBSR loading. More clay geopolymers need to be made and tested at longer times at higher FBSR loadings for comparison to the fly ash monoliths. Monoliths made with metakaolin (heat treated) clay are of a more constant composition and are very reactive as the heat treated clay is amorphous and alkali activated. The monoliths made with fly ash are subject to the inherent compositional variation found in fly ash as it is a waste product from burning coal and it contains unreactive components such as mullite. However, both the fly ash and the clay based monoliths perform well in long term ASTM C1308 testing.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

SALTSTONE MATRIX CHARACTERIZATION AND STADIUM SIMULATION RESULTS

SIMCO Technologies, Inc. was contracted to evaluate the durability of the saltstone matrix material and to measure saltstone transport properties. This information will be used to: (1) Parameterize the STADIUM{reg_sign} service life code, (2) Predict the leach rate (degradation rate) for the saltstone matrix over 10,000 years using the STADIUM{reg_sign} concrete service life code, and (3) Validate the modeled results by conducting leaching (water immersion) tests. Saltstone durability for this evaluation is limited to changes in the matrix itself and does not include changes in the chemical speciation of the contaminants in the saltstone. This report summarized results obtained to date which include: characterization data for saltstone cured up to 365 days and characterization of saltstone cured for 137 days and immersed in water for 31 days. Chemicals for preparing simulated non-radioactive salt solution were obtained from chemical suppliers. The saltstone slurry was mixed according to directions provided by SRNL. However SIMCO Technologies Inc. personnel made a mistake in the premix proportions. The formulation SIMCO personnel used to prepare saltstone premix was not the reference mix proportions: 45 wt% slag, 45 wt% fly ash, and 10 wt% cement. SIMCO Technologies Inc. personnel used the following proportions: 21 wt% slag, 65 wt% fly ash, and 14 wt% cement. The mistake was acknowledged and new mixes have been prepared and are curing. The results presented in this report are assumed to be conservative since the excessive fly ash was used in the SIMCO saltstone. The SIMCO mixes are low in slag which is very reactive in the caustic salt solution. The impact is that the results presented in this report are expected to be conservative since the samples prepared were deficient in slag and contained excess fly ash. The hydraulic reactivity of slag is about four times that of fly ash so the amount of hydrated binder formed per unit volume in the SIMCO saltstone samples is less than that expected for saltstone containing the reference amount of slag (45 wt.% of the total cementitious mixture versus 21 wt.% used in the SIMCO samples). Consequently the SIMCO saltstone samples are expected to have lower strengths, and tortuosity and higher porosity, water diffusivity, and intrinsic permeability compared to the reference case MCU saltstone. MCU reference saltstone contains nonradioactive salt solution with a composition designed to simulate the product of the Modular Caustic Side Solvent Extraction (MCU) Unit [Harbour, 2009]. The SIMCO saltstone samples were cast in molds and cured for three days under plastic with a source of water to prevent drying. Details of the sample preparation process are presented in Attachment 2. The molds were then removed and the samples were cured at a constant temperature (76 F, 24 C) and 100 percent relative humidity for up to one year. Selected samples were periodically removed and characterized the evolution of the matrix as a function of age. In order to preserve the age dependent microstructure at the specified curing times it is necessary to stop hydration. This was accomplished by immersing the samples in isopropanol for 5 days to replace water with alcohol. The microstructure of the matrix material was also characterized as a function of aging. This information was used as a base line for comparison with leached microstructures. After curing for 137 days, specimens were cut into 20 mm disks and exposed to deionized water with a pH maintained at 10.5. Microstructure and calcium sulfur leaching results for samples leached for 31 days are presented in this report. Insufficient leached material was generated during the testing to date to obtain physical and mineralogical properties for leached saltstone. Longer term experiments are required because the matrix alteration rate due to immersion in deionized water is slow.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Effect of Coal Properties and Operation Conditions on Flow Behavior of Coal Slag in Entrained Flow Gasifiers: A Brief Review

Integrated gasification combined cycle (IGCC) is a potentially promising clean technology with an inherent advantage of low emissions, since the process removes contaminants before combustion instead of from flue gas after combustion, as in a conventional coal steam plant. In addition, IGCC has potential for cost-effective carbon dioxide capture. Availability and high capital costs are the main challenges to making IGCC technology more competitive and fully commercial. Experiences from demonstrated IGCC plants show that, in the gasification system, low availability is largely due to slag buildup in the gasifier and fouling in the syngas cooler downstream of the gasification system. In the entrained flow gasifiers used in IGCC plants, the majority of mineral matter transforms to liquid slag on the wall of the gasifier and flows out the bottom. However, a small fraction of the mineral matter (as fly ash) is entrained with the raw syngas out of the gasifier to downstream processing. This molten/sticky fly ash could cause fouling of the syngas cooler. Therefore, it is preferable to minimize the quantity of fly ash and maximize slag. In addition, the hot raw syngas is cooled to convert any entrained molten fly slag to hardened solid fly ash prior to entering the syngas cooler. To improve gasification availability through better design and operation of the gasification process, better understanding of slag behavior and characteristics of the slagging process are needed. Slagging behavior is affected by char/ash properties, gas compositions in the gasifier, the gasifier wall structure, fluid dynamics, and plant operating conditions (mainly temperature and oxygen/carbon ratio). The viscosity of the slag is used to characterize the behavior of the slag flow and is the dominating factor to determine the probability that ash particles will stick. Slag viscosity strongly depends on the temperature and chemical composition of the slag. Because coal has varying ash content and composition, different operating conditions are required to maintain the slag flow and limit problems downstream. This report briefly introduces the IGCC process, the gasification process, and the main types and operating conditions of entrained flow gasifiers used in IGCC plants. This report also discusses the effects of coal ash and slag properties on slag flow and its qualities required for the entrained flow gasifier. Finally this report will identify the key operating conditions affecting slag flow behaviors, including temperature, oxygen/coal ratio, and flux agents.

01 COAL, LIGNITE, AND PEAT↗

Determining Coal Ash Impacts on Radium and Thorium Background Levels in Soil Using Rare Earth Element Analyses - 18604

One challenge at large remediation sites contaminated with radiological materials is differentiating between low-level site-related contamination and NORM. This is because sites contaminated with radiological materials, such as thorium processing and mining and milling facilities, often generate wastes that contain contaminants that are similar to NORM deposits. For sites in urban areas, this issue is further compounded due to the presence of historic industrial fill (historic fill) containing materials such as fly ash, coal ash, and red brick, that exhibit elevated radioactivity levels. These materials often have activity levels near, or even well above, a site's cleanup goal. At a large Superfund Site in the eastern US (Site), many of the suspected Site-related fill areas are commingled with coal and fly ash. As the cleanup criteria for the radionuclides of concern (ROC), radium (Ra) and thorium (Th), is 5 pico-Curies per gram above background, a four-pronged approach was developed to determine if the coal and fly ash are impacting the background levels of the ROCs. This evaluation included a review of boring logs to visually confirm the presence of historic fill, as well as coal fragments and coal ash; a literature review to establish the typical concentrations of Ra and Th found in coal and fly ash from US sources; the use of rare earth analyses to establish chemical signatures for non-Site related historic fill containing coal ash versus Site-related fill; and a quantitative analysis of Site-related data to determine if the radioactivity levels in historic fill containing coal were elevated. Soil samples were collected from two locations at the Site; fill areas containing coal ash that were not suspected to be impacted by Site activities, as well as fill areas containing coal ash that were associated with the former processing facility. These samples were analyzed for rare earth elements (REE), as well as Ra-228 and Th-232 and the ratios of lanthanum, cerium, and neodymium to Ra-228 and Th-232 were established for each sample. Based on a comparison of these data, a strong correlation was established between the rare earth/thorium decay chain ratios and the classification of material as either Site or non-Site related. These data were used to develop a higher background activity for fill areas containing non-Site related NORM. While the cleanup level defined in the Record of Decision remained unchanged, the higher background derived from the fly ash/coal ash material, as identified by REE analyses, resulted in higher project screening levels, which ensured that excavation activities did not 'chase' material that was not Site-related. To date, use of the coal ash background level has saved millions of dollars in cleanup costs since non-Site related contamination is not being remediated. Use of this approach to determine the appropriate background level for a site is relatively straightforward since it relies on visual observation of the soil for coal and fly ash, along with REE analyses, which is an inexpensive, quick, and established analytical method for soil samples. As long as a good rare earth profile of both contaminated and natural (in this case fly ash and coal ash) material can be established, the results can be quite definitive, which could result in significant volume reduction by minimizing the amount of material excavated and disposed of. This will lead to cost and time savings for what could be an otherwise costly and potentially complex excavation. Anyone performing environmental remediation of NORM contaminated sites may benefit from this paper and presentation. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Transformations and affinities for sulfur of Chinese Shenmu coal ash in a pulverized coal-fired boiler

The self-desulfurization efficiency of Shenmu coal with a high initial Ca/S molar ratio of 2.02 was measured in a 1,025 t/h pulverized coal-fired boiler. It increases from 29% to 32% when the power capacity decreases from 100% to 70%. About 60% of the mineral matter and calcium element fed into the furnace is retained in the fly ash, while less than 10% is retained in the bottom ash. About 70% of the sulfur element fed into the furnace is emitted as SO{sub 2} in the flue gas, while less than 10% is retained in the fly ash and less than 1% is retained in the bottom ash. The mineralogical compositions of feed coal, fly ash, and bottom ash were obtained by X-ray diffraction analysis. It is found that the initial amorphous phase content is 91.17% and the initial CaCO{sub 3} phase content is 2.07% in Shenmu coal. The vitreous phase and sulfation product CaSO{sub 4} contents are, respectively, 70.47% and 3.36% in the fly ash obtained at full capacity, while the retained CaCO{sub 3} and CaO contents are, respectively, 4.73% and 2.15%. However, the vitreous phase content is only 25.68% and no CaSO{sub 4} is detected in the bottom ash obtained at full capacity. When the power capacity decreases from 100% to 70%, the vitreous phase content in fly ash decreases from 70.47% to 67.41% and that in bottom ash increases from 25.68% to 28.10%.

01 COAL, LIGNITE, AND PEAT↗

Sulphate resistance of low‐clinker engineered cementitious composites examined by MicroXRF imaging

Abstract Engineered cementitious composites (ECC) are a class of high‐performing fibre‐reinforced cementitious materials recognised for their increased ductility and durability compared to conventional cement‐based materials, owing to their autogenously controlled tight crack widths, even when subjected to high strains. To reduce ECC's environmental impact, this research examines the use of a low‐clinker binder − limestone‐calcined clay cement (LC3) − as an alternative to portland cement (PC), along with fly ash to further reduce the clinker proportion and the embodied CO 2 of the formulations. In conventional concrete, LC3 hydrates to a denser microstructure resulting from the synergistic reaction between limestone and calcined clay. At the lower water contents typical of ECC and with the presence of fly ash, the influence of the binder composition on the microstructure is difficult to anticipate. To examine the influence of these compositional variables on microstructure, permeability and durability, the sulphate resistance of LC3‐based ECC is explored. Specifically, the ECC‐LC3 blends are designed with high clinker replacement rate of 75% by mass of binder and contain either conventional fly ash or reclaimed fly ash at 50% by mass of binder. Expansion of ECC‐LC3 samples subjected to standard sodium sulphate test conditions was measured up to 12 months and the depth of penetration of sulphates into the ECC‐LC3 of varying compositions was quantified using micro‐X‐Ray Fluorescence (microXRF) imaging and modelling. The expansion results show that the ECC‐LC3 formulations performed better than the PC samples and can provide adequate resistance to external sulphate attack, even when reclaimed fly ashes are used in place of the conventional ash. In addition, the shallow penetration of sulphate into these cementitious composites demonstrates the low diffusion coefficients values that were determined using the quantitative data from MicroXRF imaging.

Microscopy↗

Combustion Byproducts Recycling Consortium

The Combustion Byproducts Recycling Consortium (CBRC) program was developed as a focused program to remove and/or minimize the barriers for effective management of over 123 million tons of coal combustion byproducts (CCBs) annually generated in the USA. At the time of launching the CBRC in 1998, about 25% of CCBs were beneficially utilized while the remaining was disposed in on-site or off-site landfills. During the ten (10) year tenure of CBRC (1998-2008), after a critical review, 52 projects were funded nationwide. By region, the East, Midwest, and West had 21, 18, and 13 projects funded, respectively. Almost all projects were cooperative projects involving industry, government, and academia. The CBRC projects, to a large extent, successfully addressed the problems of large-scale utilization of CCBs. A few projects, such as the two Eastern Region projects that addressed the use of fly ash in foundry applications, might be thought of as a somewhat smaller application in comparison to construction and agricultural uses, but as a novel niche use, they set the stage to draw interest that fly ash substitution for Portland cement might not attract. With consideration of the large increase in flue gas desulfurization (FGD) gypsum in response to EPA regulations, agricultural uses of FGD gypsum hold promise for large-scale uses of a product currently directed to the (currently stagnant) home construction market. Outstanding achievements of the program are: (1) The CBRC successfully enhanced professional expertise in the area of CCBs throughout the nation. The enhanced capacity continues to provide technology and information transfer expertise to industry and regulatory agencies. (2) Several technologies were developed that can be used immediately. These include: (a) Use of CCBs for road base and sub-base applications; (b) full-depth, in situ stabilization of gravel roads or highway/pavement construction recycled materials; and (c) fired bricks containing up to 30%-40% F-fly ash. Some developed technologies have similar potential in the longer term. (3) Laboratory studies have been completed that indicate that much higher amounts of fly ash could be added in cement-concrete applications under some circumstances. This could significantly increase use of fly ash in cement-concrete applications. (4) A study of the long-term environmental effects of structural fills in a surface mine in Indiana was completed. This study has provided much sought after data for permitting large-volume management options in both beneficial as well as non-beneficial use settings. (5) The impact of CBRC on CCBs utilization trends is difficult to quantify. However it is fair to say that the CBRC program had a significant positive impact on increased utilization of CCBs in every region of the USA. Today, the overall utilization of CCBs is over 43%. (6) CBRC-developed knowledge base led to a large number of other projects completed with support from other sources of funding. (7) CBRC research has also had a large impact on CCBs management across the globe. Information transfer activities and visitors from leading coal producing countries such as South Africa, Australia, England, India, China, Poland, Czech Republic and Japan are truly noteworthy. (8) Overall, the CBRC has been a truly successful, cooperative research program. It has brought together researchers, industry, government, and regulators to deal with a major problem facing the USA and other coal producing countries in the world.

01 COAL, LIGNITE, AND PEAT↗

Synthesis and Functionalization of Coal Fly Ash-Derived Zeolites for Boron Removal From Wastewater

There are hundreds of both active and unused surface impoundments in the United States containing coal combustion residuals (CCRs) produced by coal-fired power plants which can leach toxic elements into surface and groundwater. Therefore, the development of efficient means for both the clean-up of surface impoundments and for deriving economically viable products from CCRs are urgent tasks for researchers. Herein, a microwave-assisted strategy is presented for converting a common coal combustion residual, coal fly ash (CFA), into zeolite-based sorbents for boron (B) removal from wastewater. Specifically, CFA constitutes the main source of Si and Al ions to produce zeolite type-A and the resulting sorbent subsequently undergoes simple cation exchange with Ca to enhance its B adsorption capacity. Structure and composition of the sorbents were characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDS), inductively coupled plasma (ICP)-mass spectrometry (MS), and ICP-optical emission spectroscopy (OES). The Ca-modified zeolite sorbent derived from CFA exhibits comparable B removal capacity with similar commercial zeolites.

Muldoon, Patrick↗