Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Crack control”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 325 records · Page 18

Simplified data reduction methods for the ECT test for mode 3 interlaminar fracture toughness

Simplified expressions for the parameter controlling the load point compliance and strain energy release rate were obtained for the Edge Crack Torsion (ECT) specimen for mode 3 interlaminar fracture toughness. Data reduction methods for mode 3 toughness based on the present analysis are proposed. The effect of the transverse shear modulus, G(sub 23), on mode 3 interlaminar fracture toughness characterization was evaluated. Parameters influenced by the transverse shear modulus were identified. Analytical results indicate that a higher value of G(sub 23) results in a low load point compliance and lower mode 3 toughness estimation. The effect of G(sub 23) on the mode 3 toughness using the ECT specimen is negligible when an appropriate initial delamination length is chosen. A conservative estimation of mode 3 toughness can be obtained by assuming G(sub 23) = G(sub 12) for any initial delamination length.

Li, Jian↗

In-Plane Tensile Properties, Creep Behavior and Failure Mechanisms of CVI and PIP SiC/SiC Composites at Temperatures to 1,650⁰C in Air

The in-plane tensile and creep properties of 2D woven CVI and PIP SiC/SiC composites with SylramicTM-iBN SiC fibers were measured at temperatures to 16500C in air and the data compared with the literature. Batch-to-batch variations in the tensile and creep properties, influence of thermal treatment on creep, creep parameters, damage mechanisms and failure modes for these composites were studied. Under the tested conditions, the CVI SiC/SiC composites exhibited both matrix and fiber dominated creep depending on stress, whereas the PIP SiC/SiC composites displayed only fiber dominated creep. Creep durability in both composite systems is controlled by the most creep resistant phase as well as oxidation of the fibers via cracked matrix. The Larson-Miller parameter and Monkman-Grant relationship were used wherever applicable for analyzing and predicting creep durability.

SiC-SiC Composites, CVI, PIP, Creep, In-plane tens↗

Factors Controlling Stress Rupture of Fiber-Reinforced Ceramic Composites

The successful application of fiber-reinforced ceramic matrix composites (CMC) depends strongly on maximizing material rupture life over a wide range of temperatures and applied stresses. The objective of this paper is to examine the various intrinsic and extrinsic factors that control the high-temperature stress rupture of CMC for stresses below and above those required for cracking of the 0 C plies (Regions I and II, respectively). Using creep-rupture results for a variety of ceramic fibers and rupture data for CMC reinforced by these fibers, it is shown that in those cases where the matrix carries little structural load, CMC rupture conditions can be predicted very well from the fiber behavior measured under the appropriate test environment. As such, one can then examine the intrinsic characteristics of the fibers in order to develop design guidelines for selecting fibers and fiber microstructures in order to maximize CMC rupture life. For those cases where the fiber interfacial coatings are unstable in the test environment, CMC lives are generally worse than those predicted by fiber behavior alone. For those cases where the matrix can support structural load, CMC life can even be greater provided matrix creep behavior is properly controlled. Thus the achievement of long CMC rupture life requires understanding and optimizing the behavior of all constituents in the proper manner.

DiCarlo, J. A.↗

High temperature fatigue behavior of tungsten copper composites

The high temperature fatigue behavior of a 9 vol percent, tungsten fiber reinforced copper matrix composite was investigated. Load-controlled isothermal fatigue experiments at 260 and 560 C and thermomechanical fatigue (TMF) experiments, both in phase and out of phase between 260 and 560 C, were performed. The stress-strain response displayed considerable inelasticity under all conditions. Also, strain ratcheting was observed during all the fatigue experiments. For the isothermal fatigue and in-phase TMF tests, the ratcheting was always in a tensile direction, continuing until failure. The ratcheting during the out-of-phase TMF test shifted from a tensile direction to a compressive direction. This behavior was thought to be associated with the observed bulging and the extensive cracking of the out-of-phase specimen. For all cases, the fatigue lives were found to be controlled by damage to the copper matrix. Grain boundary cavitation was the dominant damage mechanism of the matrix. On a stress basis, TMF loading reduced lives substantially, relative to isothermal cycling. In-phase cycling resulted in the shortest lives, and isothermal fatigue at 260 C, the longest.

Verrilli, Michael J.↗

Experimental and theoretical study of the restrained shrinkage cracking of early age well cement

The shrinkage cracking occurring in oil & gas well cement material is a major factor that reduces the cement sheath integrity and impairs the durability of an underground well. Shrinkage mainly takes place in the early hydration period of the cement, and the resulting restrained shrinkage cracking can form a leaking network for oil & gas or carbon dioxide stored in an underground reservoir. It is thus important to understand the early age behavior of well cement and the leaking pathway formation in the well. This study describes the application of the digital image correlation (DIC) method as a tool to measure the strain development and crack distributions of well cement in the lab during early phase changes. A theoretical model is presented to calculate the stress distribution built up in the cement sheath during early ages of well cement hydration, which helps to interpret the experimental observations and determine the major factors influencing the cracking sequences. This study presents the whole hydration – drying shrinkage – and cracking mechanism of early age well cement under restrained ring conditions experimentally and theoretically. Finally, the results offer useful insights on the key material and geometric parameters which control the fracture of a well cementing structure.

36 MATERIALS SCIENCE↗

In-line measurements of below-the-surface food deformation during drying with an interference-based optical fiber strain sensor

Real-time measurements of food deformation are important for quality control in drying, yet they pose significant challenges. In this study, we developed an interference-based optical fiber strain sensor to enable in-line, continuous, below-the-surface strain measurements in drying of soft food samples. Compared to a strain resolution of 8 × 10 -4 at zero strain and 7.2 × 10 -3 at 0.20 strain reported in our previously published work, the present study achieves markedly improved resolutions of 1.3 × 10 -4 at zero strain and 7.8 × 10 -4 at 0.25 strain, which strains are the lower and higher boundaries of the dynamic range, respectively. This nearly order-of-magnitude improvement is attributed to the unique interference-based sensing mechanism, no need for calibration to convert optical signals to strain, and the system-design-enabled immunity to fiber-disk misalignments and light source intensity fluctuations. To demonstrate the in-line process monitoring, deformation measurements of fresh banana slices and sugar cookie doughs were carried out in a benchtop oven and an industrial-scale hot-air pilot dryer, respectively. In both dryers, strain measurements were continuously measured during the whole drying process at various depths and radii below the sample surfaces, with the strains up to 25%. Computer vision was used only in the benchtop drying to confirm the faithfulness of the fiber sensor measurements and cannot provide below-the-surface measurements. The measured spatiotemporal deformation allowed us to confirm the shell-hardening effect and to determine the speed and location of large deformation changes in the whole drying process, the latter of which is related to the sample cracking. To the best of the authors’ knowledge, this study is the first to report on an interferometry-based fiber sensor to measure food deformation. This sensor and the sensing mechanism have high potential for real-time process monitoring and control to prevent over-drying or cracking during drying processes.

47 OTHER INSTRUMENTATION↗

System definition study of deployable, non-metallic space structures

The state of the art for nonmetallic materials and fabrication techniques suitable for future space structures are summarized. Typical subsystems and systems of interest to the space community that are reviewed include: (1) inflatable/rigidized space hangar; (2) flexible/storable acoustic barrier; (3) deployable fabric bulkhead in a space habitat; (4) extendible tunnel for soft docking; (5) deployable space recovery/re-entry systems for personnel or materials; (6) a manned habitat for a space station; (7) storage enclosures external to the space station habitat; (8) attachable work stations; and (9) safe haven structures. Performance parameters examined include micrometeoroid protection; leakage rate prediction and control; rigidization of flexible structures in the space environment; flammability and offgassing; lifetime for nonmetallic materials; crack propagation prevention; and the effects of atomic oxygen and space debris. An expandable airlock for shuttle flight experiments and potential tethered experiments from shuttle are discussed.

Stimler, F. J.↗

Effect of Crystal Orientation on Analysis of Single-Crystal, Nickel-Based Turbine Blade Superalloys

High-cycle fatigue-induced failures in turbine and turbopump blades is a pervasive problem. Single-crystal nickel turbine blades are used because of their superior creep, stress rupture, melt resistance, and thermomechanical fatigue capabilities. Single-crystal materials have highly orthotropic properties making the position of the crystal lattice relative to the part geometry a significant and complicating factor. A fatigue failure criterion based on the maximum shear stress amplitude on the 24 octahedral and 6 cube slip systems is presented for single-crystal nickel superalloys (FCC crystal). This criterion greatly reduces the scatter in uniaxial fatigue data for PWA 1493 at 1,200 F in air. Additionally, single-crystal turbine blades used in the Space Shuttle main engine high pressure fuel turbopump/alternate turbopump are modeled using a three-dimensional finite element (FE) model. This model accounts for material orthotrophy and crystal orientation. Fatigue life of the blade tip is computed using FE stress results and the failure criterion that was developed. Stress analysis results in the blade attachment region are also presented. Results demonstrate that control of crystallographic orientation has the potential to significantly increase a component's resistance to fatigue crack growth without adding additional weight or cost.

Swanson, G. R.↗

Stress Corrosion Evaluation of NiTiHf Alloy for the International Space Station Environmental Control and Life Support System

A stress corrosion evaluation was performed on NiTiHf alloy because this material is considered a bearing material candidate for the Environmental Control and Life Support System. Stressed round tensile specimens survived exposures to alternate pretreat, alternate brine, baseline pretreat, baseline brine, and 3.5% NaCl alternate immersion. Metallographic evaluations did not detect stress corrosion on exposed samples. The ultimate tensile strength values varied significantly for this material, which is common for bearing materials. This variation was observed on both, exposed and nonexposed specimens. The results of this work indicate that this material has potential applications as a bearing material.

International Space Station (ISS)↗

Impact of Plate Thickness and Joint Geometry on Residual Stresses in 347H Stainless Steel Welds

Weldments of 347H stainless steel are potentially susceptible to stress relaxation cracking at elevated service temperatures. Mitigation of stress relaxation cracking susceptibility within a multipass weld requires a good understanding of welding practices and manufacturing techniques to control high tensile residual stresses. Here in this work, the dependence of residual stress distribution in 347H stainless steel on base plate thickness, joint geometry design, and preheating condition was systematically investigated by using three-dimensional finite element models. The finite element models were validated through good agreement between neutron diffraction measurements and calculated elastic strains. The single-V-groove welds with and without a preheating step all produced similar peak von Mises residual stresses, above 450 MPa, within both the fusion zone and heat-affected zone (HAZ). In plates thicker than 0.5 in. (12.7 mm), high tensile residual stress could be observed in a relatively large area, from the middle of the plate thickness to underneath the top surface. A double-V groove shifted the high tensile stress area to the middle thickness of the weld. A single-J-groove weld was able to confine the residual stress to a very small region near the middle thickness within the fusion zone and suppressed the von Mises residual stress within the HAZ to below 400 MPa.

14 SOLAR ENERGY↗

Tidal Control of Jet Eruptions Observed by Cassini ISS

Observations by Cassini's Imaging Science Subsystem (ISS) of Enceladus' south polar region at high phase angles has revealed jets of material venting into space. Observations by Cassini's Composite Infrared Spectrometer (CIRS) have also shown that the south polar region is anomalously warm with hotspots associated with geological features called the Tiger Stripes. The Tiger Stripes are large rifts near the south pole of Enceladus, which are typically about 130 km in length, 2 km wide, with a trough 500 m deep, and are l1anked on each side by 100m tall ridges. Preliminary triangulation of jets as viewed at different times and with different viewing geometries in Cassini ISS images taken between 2005 and 2007 have constrained the locations of eight major eruptions of material and found all of them associated with the south polar fractures unofficially the 'Tiger Stripes', and found four of them coincident with the hotspots reported in 2006 by CIRS. While published ISS observations of jet activity suggest that individual eruption sites stay active on the timescale of years, any shorter temporal variability (on timescales of an orbital period, or 1.3 Earth days, for example) is more difficult to establish because of the spotty temporal coverage and the difficulty of visually isolating one jet from the forest of many seen in a typical image. Consequently, it is not known whether individual jets are continuously active, randomly active, or if they erupt on a predictable, periodic schedule. One mechanism that may control the timing of eruptions is diurnal tidal stress, which oscillates between compression/tension as well as right and left lateral shear at any given location throughout Enceladus' orbit and may allow the cracks to open and close regularly. We examine the stresses on the Tiger Stripe regions to see how well diurnal tidal stress caused by Enceladus' orbital eccentricity may possibly correlate with and thus control the observed eruptions. We then identify possible mechanisms by which tidal stress can provide access to the surface for volatile material and implications for observed jet activity.

Hurford, T. A.↗

Slow Strain Rate Testing of A537 Tank Wall Material

At Savannah River Site (SRS), High-Level Waste is stored in below-grade carbon steel tanks. This waste in part consists of sludge, salt cake, and/or supernate. Preparation of this waste for future processing involves dissolution of the salt cake layer. The salt dissolution process can create conditions that leave the carbon steel tanks susceptible to localized corrosion. The salt to be dissolved contains high concentrations of nitrate, that once released, create an environment that may be conducive to pitting corrosion and/or stress corrosion cracking (SCC) of carbon steel. The salt dissolution process also liberates interstitial liquid trapped between the salt crystals. This liquid is initially high in nitrite and hydroxide concentration. High pH and greater ratios of nitrite to nitrate act as inhibitors to minimize corrosion of carbon steel in high nitrate environments. However, as dissolution proceeds, the concentration of nitrate will increase, while the hydroxide and nitrite concentration of the interstitial liquid will deplete and become insufficient to prevent the onset of corrosion attack. Tank blending and the addition of inhibitors are used to ensure adequate concentrations of hydroxide and nitrite. However, this is not desirable during salt dissolution as it can reduce process efficiency and increase the amount of waste that needs processing. This testing program was designed to examine the risk of SCC associated with utilizing the pitting factor (PF) and nitrite/nitrate (NO 2 - /NO 3 - ) ratio limits for handling dissolved salt solutions at an elevated temperature in the carbon steel waste tanks. The previously identified limits are a PF of 1.2 and an NO 2 - /NO 3 - ratio of 0.15. The results indicate that as long as the NO 2 - /NO 3 - ratio exceeds 0.1 and the PF is above approximately 0.8, there is a discernible safety margin between the open circuit potential (OCP) and the critical cracking potential (CCP) observed during applied potential testing. However, this margin, defined by the difference between the OCP and CCP, is relatively narrow, ranging from 0.1 to 0.25 volts. This small margin raises concerns about potential shifts in OCP during waste retrieval operations, which could inadvertently increase the risk of SCC if the OCP approaches or exceeds the CCP. These results confirm that dissolved salt solutions provide a potent chemistry that, under certain conditions, makes carbon steel susceptible to SCC. The next question to consider is the influence these results have on decisions for storage and retrieval of waste from the tanks. For Type III/IIIA waste tanks, the risk of SCC remains very low. First, and most importantly, the post-weld stress relief of the tanks has reduced the residual stress near the welds. Thus, without the stress component, SCC risk is minimized. The material of construction (A537 Carbon steel) for the Type III/IIIA tanks is superior to the steel in its resistance to SCC than the steel that was utilized for the Type I, II, and IV tanks (A285 carbon steel). From a chemistry control standpoint for a Type III/IIIA tank directly involved with handling dissolved salt solutions, the PF and NO 2 - /NO 3 - ratio limits may be utilized wherein chemistry control provides an extra layer of defense against SCC. Chemistry control for a Type III/IIIA tank minimizes the risk for a tank that may receive the dissolved salt solution, particularly if that tank is a Type I, II, or IV waste tank. On the other hand, if the dissolved salt solution is handled by a Type I, II, or IV waste tank the risk of SCC is real. The potent chemistry, absence of stress relief, and inferior material result in a condition that is conducive to cracking. Efforts should be made to either avoid transferring waste that may not meet the PF and NO 2 - /NO 3 - ratio criteria to one of these tanks or if it is unavoidable, take measures to minimize the consequences of a leak. As shown by these tests, even if the PF and NO 2 - /NO 3 - ratio criteria are met, there is a risk that the tank potential may be disturbed in the positive direction and the risk of SCC increase.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Effect of microstructure on fatigue crack propagation in additive manufactured nickel-based superalloy Haynes 282: an experiment and crystal plasticity study

Haynes 282 is a γ' precipitation-strengthened nickel-based superalloy known for its exceptional high-temperature creep resistance and excellent fabricability. Recent advancements in powder-bed fusion-based additive manufacturing (PBF-AM) have enabled the fabrication of Haynes 282 with accurate, site-specific control of the grain orientation and morphology at the microscale. This ability opens up new avenues for microstructure design, to improve the material’s fatigue crack resistance and service life. This paper investigates the fatigue crack growth behavior of hybrid microstructure Haynes 282 fabricated via PBF-AM. Previous experiments revealed a higher crack propagation rate in the coarse columnar-grained microstructural regions when compared against fine-grained areas. Here, a strain gradient crystal plasticity model was adapted to study the fracture-related mechanical fields at the crack tip in the two microstructures. The simulation results showed a consistent influence of grain structure and texture on crack propagation, as was seen in the experiment. The model analysis revealed higher crack propagation driving force along crack direction in the coarse-grained sharply textured microstructure and higher driving force for crack kinking in fine-grained more diffusely textured microstructure, which is ascribed to the combined effect of yield stress, hardening rate, texture and grain morphology. The presented modeling approach will facilitate the development of the AM-based accurate microstructure design by deepening the fundamental study in AM-specific microstructure-properties relations.

36 MATERIALS SCIENCE↗

The relative stress-corrosion-cracking susceptibility of candidate aluminum-lithium alloys for aerospace applications

Stress corrosion tests of Al-Li-Cu powder metallurgy alloys are described. Alloys investigated were Al-2.6% Li-1.4% and Al-2.6% Li-1.4% Cu-1.6% Mg. The base properties of the alloys were characterized. Process, heat treatment, and size/orientational effects on the tensile and fracture behavior were investigated. Metallurgical and electrochemical conditions are identified which provide reproducible and controlled parameters for stress corrosion evaluation. Preliminary stress corrosion test results are reported. Both Al-Li-Cu alloys appear more susceptible to stress corrosion crack initiation than 7075-T6 aluminum, with the magnesium bearing alloy being the most susceptible. Tests to determine the threshold stress intensity for the base and magnesium bearing alloys are underway. Twelve each, bolt loaded DCB type specimens are under test (120 days) and limited crack growth in these precracked specimens has been observed. General corrosion in the aqueous sodium chloride environment is thought to be obscuring results through crack tip blunting.

Pizzo, P. P.↗

Development of Testing Methods to Predict Cracking in Photovoltaic Backsheets

In recent years there have been some significant failures of photovoltaic backsheets resulting from inadequacies of design that are not detected in current versions of the qualification standards. In some cases, this has resulted in catastrophic failure in less than 5 y of deployment. In this work, we develop a test sample construction and evaluate accelerated exposure conditions necessary to duplicate the cracking field failure of backsheets using a small and manageable coupon. This sample uses a piece of solder wire to put some controlled topology and stress into the backsheet. Through exposure to different environmental stressors it was found that the application of thermal cycling stresses, after ultraviolet radiation exposure, is of primary importance to duplicate field failures.

14 SOLAR ENERGY↗

Oxidation Behavior of Binary Niobium Alloys

This investigation concludes a study to determine the effects of up to 25 atomic percent of 55 alloying additions on the oxidation characteristics of niobium. The alloys were evaluated by oxidizing in an air atmosphere for 4 hours at 1000 C and 2 hours at 1200 C. Titanium and chromium improved oxidation resistance at both evaluation conditions. Vanadium and aluminum improved oxidation resistance at 1000 C, even though the V scale tended to liquefy and the Al specimens became brittle and the scale powdery. Copper, cobalt, iron, and iridium improved oxidation resistance at 1200 C. Other investigations report tungsten and molybdenum are protective up to about 1000 C, and tantalum at 1100 C. The most important factor influencing the rate of oxidation was the ion size of the alloy additions. Ions slightly smaller than the Nb(5+) ion are soluble in the oxide lattice and tend to lower the compressive stresses in the bulk scale that lead to cracking. The solubility of the alloying addition also depends on the valence to some extent. All of the elements mentioned that improve the oxidation resistance of Nb fit this size criterion with the possible exception of Al, whose extremely small size in large concentrations would probably lead to the formation of a powdery scale. Maintenance of a crack-free bulk scale for as long as possible may contribute to the formation of a dark subscale that ultimately is rate- controlling in the oxidation process. The platinum-group metals, especially Ir, appear to protect by entrapment of the finely dispersed alloying element by the incoming Nb2O5 metal-oxide interface. This inert metallic Ir when alloyed in a sufficient amount with Yb appears to give a ductile phase dispersed in the brittle oxide. This scale would then flow more easily to relieve the large compressive stresses to delay cracking. Complex oxide formation (which both Ti and Zr tend to initiate) and valence effects, which probably change the vacancy concentration in the scale, are masked by the overriding tendency for a porous scale.

Barrett, Charles A.↗

An analysis for crack layer stability

The problem of uncontrolled crack propagation and crack arrest is considered with respect to crack layer (CL) translational stability. CL propagation is determined by the difference between the energy release rate and the amount of energy required for material transformation, and necessary and sufficient conditions for CL instability are derived. CL propagation in polystyrene is studied for two cases. For the case of remotely applied fixed load fatigue, the sufficient condition of instability is shown to be met before the necessary condition, and the necessary condition controls the stability. For the fixed displacement case, neither of the instability conditions are met, and CL propagation remains stable, resulting in crack arrest.

Sehanobish, K.↗

Surface protection of graphite fabric/PMR-15 composites subjected to thermal oxidation

Graphite fabric/PMR-15 laminates develop matrix cracks during long-term exposure in air at temperatures in the range of 500 to 600 F. This study was performed to demonstrate the effectiveness of incorporating graphite mat surface plies as a means of reducing the developing of matrix cracks. Celion 3000 graphite fabric/PMR-15 laminates were fabricated with graphite or graphite mat/325-mesh boron powder surface plies. Laminates without mat surface plies were also fabricated for control purposes. Composite flexural strength, flexural modulus, and interlaminar shear strength were determined at 288 C before and after long-term exposure (up to 1500 hr) in air at 316 C. The results of this study showed that the incorporation of graphite mat surface plies reduces matrix cracking and improves the elevated temperature mechanical property retention characteristics of the composites.

Hanson, M. P.↗