At least 325 records · Page 18

Stress corrosion in high-strength aluminum alloys

Report describes results of stress-corrosion tests on aluminum alloys 7075, 7475, 7050, and 7049. Tests compare performance of original stress-corrosion-resistant (SCR) aluminum, 7075, with newer, higher-strength SCR alloys. Alloys 7050 and 7049 are found superior in short-transverse cross-corrosion resistance to older 7075 alloy; all alloys are subject to self-loading effect caused by wedging of corrosion products in cracks. Effect causes cracks to continue to grow, even at very-low externally applied loads.

Dorward, R. C.↗

Compound oxidized styrylphosphine

A process is described for preparing flame resistant, nontoxic vinyl polymers which contain phosphazene groups and which do not emit any toxic or corrosive products when they are oxidatively degraded. Homopolymers, copolymers, and terpolymers of a styrene based monomer are prepared by polymerizing at least one oxidized styrylphosphine monomer from a group of organic azides, or by polymerizing p-diphenylphosphinestyrene and then oxidizing that monomer with an organoazide from the group of (C6H5)2P(O)N3, (C6H5O)2P(O)N3, (C6H5)2C3N3(N3), and C6H5C3N3(N3)2. Copolymers can also be prepared by copolymerizing styrene with at least one oxidized styrylphosphine monomer.

Paciorek, K. J. L.↗

A basic design fault in ceramic flat packs

Recent moisture resistance tests of various multilayer top brazed ceramic flat packs and leaded and unleaded chip carriers has revealed a serious design defect. These packages, which utilize a tungsten interconnect system, in the presence of high humidity, suffer a galvanic corrosion which anodically consumes the tungsten. This process can continue until the package suffers an open circuit. The test results indicate that the lead plating system does not adequately seal off the interface area where the tungsten stripe egresses from the inside of the package. Leaded and leadless chip carrier packages were also subjected to the moisture resistance test. The familiar red and green corrosion products were visible after the test was completed. Careful sectioning of the chip carriers has revealed that the tungsten interconnect stripe instead of exiting under the castellations, exits at the top of the castellation and is thus vulnerable to the attack of moisture. These basic design faults severely impact the reliability of these packages.

Drotman, B.↗

Fire extinguishment and inhibition in spacecraft environments

It was concluded that it is essential that NASA develop a comprehensive approach to fire extinguishment and inerting in spacecraft environments. Electronic equipment might be easily protected through use of an onboard inert gas generating system. The use of Halon 1301 presents serious technological challenges for agent cleanup and removal of the toxic and corrosive products of combustion. Nitrogen pressurization, while effective, probably presents a serious weight penality. The use of liquid water sprays appears to be the most effective approach to general purpose spacecraft fire protection.

Deris, John↗

Chemical durability of high-temperature superconductor YBa2Cu3O(7-x) in aqueous environments

The stability of YBa2Cu3O(7-x) in water and 100-percent humidity has been investigated at three temperatures, using pH measurements, X-ray diffraction, and scanning electron microscopy. The oxide-ceramic superconductor is highly unstable; it reacts rapidly with water and degrades in moisture. Dissolution of the oxide perovskite in water is highly incongruent. The corrosion products are found to be BaCO3, CuO, O2, etc. Barium hydroxide is first formed and further reacts with atmospheric CO2 to form needle-shaped crystals of BaCO3. For any practical applications, devices made from these materials would have to be protected with an impermeable coating to prevent deterioration from atmosphere.

Bansal, Narottam P.↗

Reactions of silicon-based ceramics in mixed oxidation chlorination environments

The reaction of silicon-based ceramics with 2 percent Cl2/Ar and 1 percent Cl2/1 percent to 20 percent O2/Ar at 950 C was studied with thermogravimetric analysis and high-pressure mass spectrometry. Pure Si, SiO2, several types of SiC, and Si3N4 were examined. The primary corrosion products were SiCl4(g) and SiO2(s) with smaller amounts of volatile silicon oxychlorides. The reactions appear to occur by chlorine penetration of the SiO2 layer, and gas-phase diffusion of the silicon chlorides away from the sample appears to be rate limiting. Pure SiO2 shows very little reaction with Cl2, SiC with excess Si is more reactive than the other materials with Cl2, whereas SiC with excess carbon is more reactive than the other materials with Cl2/O2. Si3N4 shows very little reaction with Cl2. These differences are explained on the basis of thermodynamic and microstructural factors.

Marra, John E.↗

Environmental fatigue in aluminum-lithium alloys

Aluminum-lithium alloys exhibit similar environmental fatigue crack growth characteristics compared to conventional 2000 series alloys and are more resistant to environmental fatigue compared to 7000 series alloys. The superior fatigue crack growth behavior of Al-Li alloys 2090, 2091, 8090, and 8091 is due to crack closure caused by tortuous crack path morphology and crack surface corrosion products. At high R and reduced closure, chemical environment effects are pronounced resulting in accelerated near threshold da/dN. The beneficial effects of crack closure are minimized for small cracks resulting in rapid growth rates. Limited data suggest that the 'chemically small crack' effect, observed in other alloy system, is not pronounced in Al-Li alloys. Modeling of environmental fatigue in Al-Li-Cu alloys related accelerated fatigue crack growth in moist air and salt water to hydrogen embrittlement.

Piascik, Robert S.↗

Analyzing For Light Elements By X-Ray Scattering

Nondestructive method of determining concentrations of low-atomic-number elements in liquids and solids involves measurements of Compton and Rayleigh scattering of x rays. Applied in quantitative analysis of low-atomic-number constituents of alloys, of contaminants and corrosion products on surfaces of alloys, and of fractions of hydrogen in plastics, oils, and solvents.

Ross, H. Richard↗

Standardization of surface contamination analysis systems

Corrosion products, oils and greases can potentially degrade material bonding properties. The Marshall Space Flight Center (MSFC) Surface Contamination Analysis Team (SCAT) utilizes a variety of analytical equipment to detect identify and quantify contamination on metallic and non-metallic substrates. Analysis techniques include FT-IR Microscopy (FT-IR), Near Infrared Optical Fiber Spectrometry (NIR), Optically Stimulated Electron Emission (OSEE), Ultraviolet Fluorescence (UVF) and Ellipsometry. To insure that consistent qualitative and quantitative information are obtained, standards are required to develop analysis techniques, to establish instrument sensitivity to potential contaminants, and to develop calibration curves. This paper describes techniques for preparing and preserving contamination standards. Calibration of surface contamination analysis systems is discussed, and methods are presented for evaluating the effects of potential contaminants on bonding properties.

Boothe, Richard E.↗

Burner Rig Hot Corrosion of a Single Crystal Ni-48Al-Ti-Hf-Ga Alloy

The hot corrosion resistance of a single crystal Ni-48Al-1Ti-0.5Hf-0.2Ga alloy was examined in a Mach 0.3 burner rig at 900 C for 300 hours. The combustion chamber was doped with 2 ppmw synthetic sea salt. The hot corrosion attack produced a random mound morphology on the surface. Microstructurally, the hot corrosion attack appeared to initiate with oxide-filled pits which were often broad and shallow. At an intermediate stage, the pits increased in size to incorporate unoxidized Ni islands in the corrosion product. The rampant attack stage, which was observed only at sharp sample corners, was characterized by rapid inward growth of alumina in finger-like protrusions incorporating significant amounts of Al-depleted Ni islands. Aluminum consumption in the oxide fingers resulted in the growth of a gamma' layer ahead of the advancing oxide fingers.

Nesbitt, James A.↗

Design Through Simulation of a Molecular Sieve Column for Treatment of MON-3

The presence of water in propellant-grade MON-3 is a concern in the Aerospace Industry. NASA Johnson Space Center (JSC), White Sands Test Facility (WSTF) Propulsion Department has evaluated many types of molecular sieves for control of iron, the corrosion product of water in Mixed Oxides of Nitrogen (MON-3). In 1995, WSTF initiated laboratory and pilot-scale testing of molecular sieve type 3A for removal of water and iron. These tests showed sufficient promise that a series of continuous recycle tests were conducted at WSTF. Periodic samples of the circulating MON-3 solution were analyzed for water (wt %) and iron (ppm, wt). This test column was modeled as a series of transfer units; i. e., each unit represented the height equivalent of a theoretical plate. Such a model assumes there is equilibrium between the adsorbent material and the effluent stream from the unit. Operational and design parameters were derived based on the simulation results. These parameters were used to predict the design characteristics of a proposed molecular sieve column for removal of water and iron from MON-3 at the NASA Kennedy Space Center (KSC). In addition, these parameters were used to simulate a small, single-pass operation column at KSC currently used for treating MON-3. The results of this work indicated that molecular sieve type 3A in 1/16 in. diameter pellets, in a column 2.5 ft. in diameter, 18 ft. in height, and operated at 25 gpm is adequate for the required removal of water and iron from MON-3.

Swartz, A. Ben↗

Opaque Mineral Assemblages at Chondrule Boundaries in the Vigarano CV Chondrite: Evidence for Gas-Solid Reactions Following Chondrule Formation

Recent studies of opaque minerals in primitive ordinary chondrites suggest that metal grains exposed at chondrule boundaries were corroded when volatile elements recondensed after the transient heating event responsible for chondrule formation. Metal grains at chondrule boundaries in the Bishunpur (LL3.1) chondrite are rimmed by troilite and fayalite. If these layers formed by gas solid reaction, then the composition of the corrosion products can provide information on the chondrule formation environment. Given the broad similarities among chondrules from different chondrite groups, similar scale layers should occur on chondrules in other primitive meteorite groups. Here I report on metal grains at chondrule boundaries in Vigarano (CV3).

Lauretta, Dante S.↗

Internal Active Thermal Control System (IATCS) Sodium Bicarbonate/Carbonate Buffer in an Open Aqueous Carbon Dioxide System and Corollary Electrochemical/Chemical Reactions Relative to System pH Changes

The International Space Station (ISS) Internal Active Thermal Control System (IATCS) experienced a number of chemical changes driven by system absorption of CO2 which altered the coolant’s pH. The natural effects of the decrease in pH from approximately 9.2 to less than 8.4 had immediate consequences on system corrosion rates and corrosion product interactions with specified coolant constituents. The alkalinity of the system was increased through the development and implementation of a carbonate/bicarbonate buffer that would increase coolant pH to 9.0 – 10.0 and maintain pH above 9.0 in the presence of ISS cabin concentrations of CO2 up to twenty times higher than ground concentrations. This paper defines how a carbonate/bicarbonate buffer works in an open carbon dioxide system and summarizes the analyses performed on the buffer for safe and effective application in the on-orbit system. The importance of the relationship between the cabin environment and the IATCS is demonstrated as the dominant factor in understanding the system chemistry and pH trends before and after addition of the carbonate/bicarbonate buffer. The paper also documents the corollary electrochemical and chemical reactions the system has experienced and the rationale for remediation of these effects with the addition of the carbonate/bicarbonate buffer.

Stegman, Thomas W.↗

Bounding Pressure and Flammability Evaluations for a Department of Energy Standard Canister Loaded with Aluminum-Clad Spent Fuel

This report presents bounding pressurization and flammability evaluations from the radiolytic gas generation expected during extended (>50 years) dry storage of aluminum-clad spent nuclear fuel (ASNF) elements in a sealed Department of Energy (DOE) Standard Canister. The primary questions involving extended ASNF dry storage center around the adequacy of dry storage conditioning processes (i.e., drying) and the behavior of residual hydrated aluminum oxides on the cladding—specifically, the radiolytic breakdown of chemically bound water in these corrosion products. The objectives of the presented work include providing a bounding assessment of the pressure with respect to the DOE Standard Canister’s structural integrity limits and identifying the potential for forming flammable or explosive gas mixtures (i.e., exceedance of the lower flammability limit of the molecular hydrogen [H2] and oxygen [O2] concentrations). The evaluation results confirm the findings of previous, more complex M&S work. That is, the structural integrity of the canister remains unchallenged by a wide margin. Nevertheless, it is important to recognize that the presented pressure calculations consider a full breakdown of the chemisorbed water, including a consequent release of all available H2. In reality, the breakdown of water in these systems will likely remain incomplete, due to competing chemical and radiolytic reactions, thereby attaining an equilibrium in the storage environment.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Examination of long-stored uranium metal

A small quantity of unirradiated uranium from Magnox fuel elements is currently held in archive storage. Some of these samples date back to the late fifties. This material has been stored, untreated, in unsealed containers in air at ambient temperature, humidity and pressure conditions. Such conditions are relevant to those that may exist in a passive storage facility. A sample of this material has been subject to optical, electron-optical and Raman spectroscopic examination to determine the extent of corrosion and the composition of corrosion product arising from long-term, low-temperature oxidation of uranium metal in air. The examinations have established that, even after a period in excess of 40 years, there was no observable spalling of uranium oxide from the sample during storage. The extent of oxidation of the metal, derived by SEM analysis, was slight and insignificant in relation to overall structural stability of the material. Raman spectroscopy data showed that the bulk of the oxide layer was comprised of hyper-stoichiometric UO{sub 2}, with U{sub 4}O{sub 9} being the dominant component. The oxygen/uranium ratio was observed to be decreased at the metal/oxide interface, with a very thin layer that consisted of mainly UO{sub 2} at the metal surface. At the oxide/air interface, a very thin U{sub 3}O{sub 8} layer was detected. U{sub 4}O{sub 9} is relatively mechanically stable, due to a significantly higher density than UO{sub 2} and U{sub 3}O{sub 8}. It is likely that the lower internal stresses in the thick U{sub 4}O{sub 9} layer have resulted in less oxide film cracking than would be expected from UO{sub 2} or U{sub 3}O{sub 8} and hence the low oxidation rate observed. These results suggest that storage of uranium metal in air over decades is a safe and credible option. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Decommissioning and PIE of the MEGAPIE spallation target

A key experiment in the Accelerated Driven Systems roadmap, the MEGAwatt PIlot Experiment (MEGAPIE) (1 MW) was initiated in 1999 in order to design and build a liquid lead-bismuth spallation target, then to operate it into the Swiss spallation neutron facility SINQ at Paul Scherrer Institute. The target has been designed, manufactured, and tested during integral tests, before irradiation carried out end of 2006. During irradiation, neutron and thermo hydraulic measurements were performed allowing deep interpretation of the experiment and validation of the models used during design phase. The decommissioning, Post Irradiation Examinations and waste management phases were defined properly. The phases dedicated to cutting, sampling, cleaning, waste management, samples preparation and shipping to various laboratories were performed by PSI teams: all these phases constitute a huge work, which allows now to perform post-irradiation examination (PIE) of structural material, irradiated in relevant conditions. Preliminary results are presented in the paper, they concern chemical characterization. The following radio-nuclides have been identified by γ-spectrometry: {sup 60}Co, {sup 101}Rh, {sup 102}Rh, {sup 108m}Ag, {sup 110m}Ag, {sup 133}Ba, {sup 172}Hf/Lu, {sup 173}Lu, {sup 194}Hg/Au, {sup 195}Au, {sup 207}Bi. For some of these nuclides the activities can be easily evaluated from γ-spectrometry results ({sup 207}Bi, {sup 194}Hg/Au), while other nuclides can only be determined after chemical separations ({sup 108m}Ag, {sup 110m}Ag, {sup 195}Au, {sup 129}I, {sup 36}Cl and α-emitting {sup 208-210}Po). The concentration of {sup 129}I is lower than expected. The chemical analysis already performed on spallation and corrosion products in the lead-bismuth eutectic (LBE) are very relevant for further applications of LBE as a spallation media and more generally as a coolant.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Bounding Pressure and Flammability Evaluations of Aluminum-Clad Spent Nuclear Fuel Department of Energy Standard Canisters

This paper presents bounding pressure and flammability evaluations for DOE Standard Canister loaded with DOE-managed aluminum-clad spent nuclear fuel (ASNF). The objective of these evaluations is to gain confidence in the safety and feasibility of possible loading configurations for extended (>50 years) periods of dry storage, with particular focus on the dry storage canister pressures and potential for formation of a flammable atmosphere. The primary concern about the extended dry storage of ASNF is radiolytic gas generation. The aluminum cladding of these materials tends to corrode, and these corrosion products—typically aluminum oxides, such as boehmite, bayerite, or gibbsite—could carry water. This makes ASNF dry storage canisters difficult to dry. The gamma radiation field in dry storage environments could cause a radiolytic breakdown of residual water, forming chemical species such as molecular hydrogen (H2). The release of these species could increase the canister pressure and lead to the generation of a flammable canister atmosphere. The bounding evaluations presented within this study surmise conservative, but credible, conditions and processes. This includes the assumption of a full breakdown of a large quantity of free, physisorbed, and chemisorbed water (bound in a trihydrate, i.e., Al2O3 • 3H2O, layer). The considered dry storage configurations include a ~3 m (10 ft) long, ~46 cm (18 in) diameter (10 x 18) DOE Standard Canister loaded with 32 Advanced Test Reactor (ATR) ASNF elements, and a ~3 m (10 ft) long, ~61 cm (24 in) (10 x 24) diameter DOE Standard Canister loaded with 40 ATR ASNF elements. While the results of this study indicate the possibility of atmospheric hydrogen concentrations above the lower flammability limit, insufficient concentrations of oxygen will prevent the formation of flammable atmospheres. The maximum credible pressures remain well within the structural limits of the DOE Standard Canister.