Sulfur Species in Zinc-Rich Condylar Zones of a Rat Temporomandibular Joint

We performed synchrotron-based micro-X-ray absorption near-edge spectroscopy (µ-XANES) coupled with micro-X-ray fluorescence (µ-XRF) for the identification of elements that included biometal zinc (Zn) and nonmetal sulfur (S) (and its species) in the condylar zones of a rat temporomandibular joint (TMJ). Zone-specific spatial localization of biometal Zn and nonmetal S from a materials viewpoint when correlated with hypoxia inducible factor-1α (HIF-1α) (a surrogate for tissue oxygenation) can provide insights into Zn-specific redox pathways at the vulnerable subchondral interface. Histologic localization of Zn, HIF-1α, and sulfur-rich proteoglycans (PGs) were mapped using an optical microscope. The µ-XRF maps coupled with site-specific micro-X-ray diffraction (µ-XRD) patterns were used to underline Zn-incorporated biological apatite in the subchondral bone and the bone of a rat TMJ condyle. Results demonstrated an association between Zn, PG, and HIF-1α histologic maps with µ-XRF, µ-XANES, and µ-XRD data and provided insights into plausible biological S species in Zn-enriched zones of a rat TMJ condyle. Spatially localized Zn and S underscore their roles in cell and tissue functions in a zone-specific manner. Elemental Zn with organic and inorganic S species at the cartilage-bone interface and the biomineral phase of Zn-enriched biological apatite from subchondral bone to condylar bone were ascertained using µ-XRF-XANES and µ-XRF-XRD. The coupled µ-XRF-XANES in situ complemented with µ-XRF-XRD in situ and immunohistochemistry provided valuable biological insights into zone-specific biological pathways in rat TMJ condyles. Based on these data, we present a workflow to reliably map and correlate S species within Zn-enriched regions of cartilage, bone, and their interface. We suggest the use of this correlative and complementary microspectroscopic spatial information for zone-specific localization of biometal Zn and nonmetal S to gain insights into plausible microanatomy-specific oxidative stress in the TMJ.

apatites↗

Zinc Speciation and Propane Dehydrogenation in Zn/H-ZSM-5 Catalysts

Zn/H-ZSM-5 catalysts have been frequently investigated for propane dehydrogenation (PDH); however, the active site remains unresolved due to the complexity of the system. We employed in situ FTIR spectroscopy and a kinetics method to correlate the Zn speciation and PDH activity in Zn/H-ZSM-5 with two Si/Al ratios (15 and 39) and a range of Zn/Al ratios (0–1.7). Incremental additions of zinc show that Zn 2+ sites are preferentially formed on H-ZSM-5 over a fraction of paired Al sites followed by [Zn-O-Zn] 2+ and [ZnOH] + sites and then ZnO x clusters. The [Zn-OH] + and [Zn-O-Zn] 2+ sites in H-ZSM-5 are more active and selective than isolated Zn 2+ for PDH. [Zn-OH] + species sublimate over time on stream, leading to catalyst deactivation, while [Zn-O-Zn] 2+ species are stable even after high-temperature reduction (750 °C for 60 min). Three distinct Zn sites ([Zn-O-Zn] 2+ , Zn 2+ , and [ZnOH] + ) show a similar propane reaction order (close to 1) and H 2 reaction order (close to 0). Combined with the lack of Zn hydride when propane flows over the catalyst at 550 °C, it is concluded that propane adsorption and dissociation is a rate-determining step and H 2 desorption is fast. This work indicates that the preparation of H-ZSM-5 with abundant Al pairs may be a strategy to form stable and selective Zn/H-ZSM-5 catalysts for propane dehydrogenation. Furthermore, it is also highlighted that examining the effect of both metal/Al ratios and Al distribution of the zeolite is crucial in identifying the metal cations in metal–zeolite systems.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Rechargeable Alkaline Zinc/Copper Oxide Batteries

Resurrecting a battery chemistry thought to be only primary, we demonstrate the first example of a rechargeable alkaline zinc/copper oxide battery. With the incorporation of a Bi 2 O 3 additive to stabilize the copper oxide-based conversion cathode, Zn/(CuO–Bi 2 O 3 ) cells are capable of cycling over 100 times at >124 W h/L, with capacities from 674 mA h/g (cycle 1) to 362 mA h/g (cycle 150). The crucial role of Bi 2 O 3 in facilitating the electrochemical reversibility of Cu 2 O, Cu(OH) 2 , and Cu o was supported by scanning and transmission electrochemical microscopy, cyclic voltammetry, and rotating ring-disc electrode voltammetry and monitored via operando energy-dispersive X-ray diffraction measurements. Bismuth was identified as serving two roles, decreasing the cell resistance and promoting Cu(I) and Cu(II) reduction. Additionally, to mitigate the capacity losses of long-term cycling CuO cells, we demonstrate two limited depth of discharge (DOD) strategies. First, a 30% DOD (202 mA h/g) retains 99.9% capacity over 250 cycles. Second, the modification of the CuO cathode by the inclusion of additional Cu metal enables performance at very high areal capacities of ~40 mA h/cm 2 and unprecedented energy densities of ~260 W h/L, with near 100% Coulombic efficiency. This work revitalizes a historically primary battery chemistry and opens opportunity to future works in developing copper-based conversion cathode chemistries for the realization of low-cost, safe, and energy-dense secondary batteries.

25 ENERGY STORAGE↗

Zn acceptors in β-Ga 2 O 3 crystals

Electron paramagnetic resonance (EPR) is used to identify and characterize neutral zinc acceptors in Zn-doped β-Ga 2 O 3 crystals. Two EPR spectra are observed at low temperatures, one from Zn ions at tetrahedral Ga(1) sites (the $Zn$$^{0}_{Ga 1}$ acceptor) and one from Zn ions at octahedral Ga(2) sites (the $Zn$$^{0}_{Ga 2}$ acceptor). These Zn acceptors are small polarons, with the unpaired spin localized in each case on a threefold coordinated oxygen O(I) ion adjacent to the Zn ion. Resolved hyperfine interactions with neighboring 69 Ga and 71 Ga nuclei allow the EPR spectra from the two acceptors to be easily distinguished: $Zn$$^{0}_{Ga 1}$ acceptors interact equally with two Ga(2) ions and $Zn$$^{0}_{Ga 2}$ acceptors interact unequally with a Ga(1) ion and a Ga(2) ion. The as-grown crystals are compensated, with the Zn ions initially present as singly ionized acceptors ($Zn$$^{-}_{Ga 1}$ and $Zn$$^{-}_{Ga 2}$). Exposing a crystal to 325 nm laser light, while being held at 140 K, primarily produces neutral $Zn$$^{0}_{Ga 2}$ acceptors when photoinduced holes are trapped at $Zn$$^{-}_{Ga 2}$ acceptors. This suggests that there may be significantly more Zn ions at Ga(2) sites than at Ga(1) sites. Warming the crystal briefly to room temperature, after removing the light, destroys the EPR spectrum from the shallower $Zn$$^{0}_{Ga 2}$ acceptors and produces the EPR spectrum from the more stable $Zn$$^{0}_{Ga 1}$ acceptors. Furthermore, the $Zn$$^{0}_{Ga 2}$ acceptors decay in the 240–260 K region with a thermal activation energy near 0.65 eV, similar to $Mg$$^{0}_{Ga 2}$ acceptors, whereas the slightly deeper $Zn$$^{0}_{Ga 1}$ acceptors decay close to room temperature with an approximate thermal activation energy of 0.78 eV.

36 MATERIALS SCIENCE↗