Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “solid electrolyte”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 307 records · Page 17

Voltage-Dependent First-Principles Barriers to Li Transport within Li-Ion Battery Solid Electrolyte Interphases

Charging a Li-ion battery requires Li-ion transport between the cathode and the anode. This Li-ion transport is dependent on (among other factors) the electrostatic environment that the ion encounters within the solid electrolyte interphase (SEI), which separates the anode from the surrounding electrolyte. A previous first-principles work has illuminated the reaction barriers through likely atomistic SEI environments but has had difficulty accurately reflecting the larger electrostatic potential landscape that an ion encounters moving through the SEI. In this work, we apply the recently developed quantum continuum approximation (QCA) technique to provide an equilibrium electronic potentiostat for first-principles interface calculations. Using QCA, we calculate the potential barrier for Li-ion transport through LiF, Li 2 O, and Li 2 CO 3 SEIs along with LiF–LiF and LiF–Li 2 O grain boundaries, all paired with Li metal anodes. Here, we demonstrate that the SEI potential barrier is dependent on the electrochemical potentials of the anode in each system. Finally, we use these techniques to estimate the change in the diffusion barrier for a Li ion moving in a LiF SEI as a function of the anode potential. We find that properly accounting for interface and electronic voltage effects significantly lowers reaction barriers compared with previous literature results.

25 ENERGY STORAGE↗

Taming Metal–Solid Electrolyte Interface Instability via Metal Strain Hardening

Abstract Solid-state lithium metal batteries have emerged as a promising technology for electric vehicles due to their high specific energy and safety potential. Obtaining intimate contact between Li and electrolyte during cell fabrication, however, remains challenging. Adequate fabrication pressure is required to promote close contact, but this pressure can cause Li deformation and penetration into the electrolyte, resulting in poor battery performance. Here, a strategy for addressing this problem is presented by incorporating 3 at% Mg into Li. Unlike pure Li which obeys the Voce hardening law and allows unconstrained deformation, Li–Mg alloy follows the Swift hardening law and strengthens with strain under compression stress. Because of the constrained deformation of Li–Mg, intimate contact with solid electrolytes is possible even at high fabrication pressure (50–65 MPa), resulting in high critical current densities. These findings underscore the importance of understanding Li metal deformation properties to improve solid-state battery performance.

25 ENERGY STORAGE↗

Impacts of Dissolved Ni 2+ on the Solid Electrolyte Interphase on a Graphite Anode

Transition metal (e.g. Ni) ions dissolved from layered-structured Ni-rich cathodes can migrate to the anode side and accelerate the failure of lithium-ion batteries. The investigations of the impact and distribution of Ni species on the solid electrolyte interphase (SEI) on the anode are crucial to understand the failure mechanism. Herein, we used time-of-flight secondary ion mass spectroscopy (TOF-SIMS) coupled with multivariate curve resolution (MCR) analysis to intuitively characterize the distribution of Ni species in the SEI. We find that the SEI on the graphite electrode using an EC-based electrolyte exhibits a multi-stratum structure. During accelerated aging of the LiNi 0.88 Co 0.08 Mn 0.04 O 2 /graphite full cell, the dissolution of Ni aggravates significantly upon cycling. A strong correlation between the dissolved-Ni and organic species in the SEI on graphite is illustrated. Here, the ion-exchange reaction between Ni 2+ and Li + ions in the SEI is demonstrated to be the main reason for the increase of SEI resistivity.

25 ENERGY STORAGE↗

Delineating the Impact of Transition‐Metal Crossover on Solid‐Electrolyte Interphase Formation with Ion Mass Spectrometry

Abstract Lithium‐metal batteries (LMB) employing cobalt‐free layered‐oxide cathodes are a sustainable path forward to achieving high energy densities, but these cathodes exhibit substantial transition‐metal dissolution during high‐voltage cycling. While transition‐metal crossover is recognized to disrupt solid‐electrolyte interphase (SEI) formation on graphite anodes, experimental evidence is necessary to demonstrate this for lithium‐metal anodes. In this work, advanced high‐resolution 3D chemical analysis is conducted with time‐of‐flight secondary‐ion mass spectrometry (TOF‐SIMS) to establish spatial correlations between the transition metals and electrolyte decomposition products found on cycled lithium‐metal anodes. Insights into the localization of various chemistries linked to crucial processes that define LMB performance, such as lithium deposition, SEI growth, and transition‐metal deposition are deduced from a precise elemental and spatial analysis of the SEI. Heterogenous transition‐metal deposition is found to perpetuate both heterogeneous SEI growth and lithium deposition on lithium‐metal anodes. These correlations are confirmed across various lithium‐metal anodes that are cycled with different cobalt‐free cathodes and electrolytes. An advanced electrolyte that is stable to higher voltages is shown to minimize transition‐metal crossover and its effects on lithium‐metal anodes. Overall, these results highlight the importance of maintaining uniform SEI coverage on lithium‐metal anodes, which is disrupted by transition‐metal crossover during operation at high voltages.

Chemistry↗

The Chemistry, Formation and Passivation of Solid-Electrolyte Interphase (SEI) from FSI- Breakdown at Li-metal Potential

LiFSI-based liquid electrolytes are promising for realizing high Coulombic efficiency (CE) and long cycle life of next-generation high-energy Li metal battery. Nevertheless, the fundamentals of both the chemistry and formation of solid-electrolyte interphase (SEI) in these electrolytes have remained elusive. Herein, we extensively combine electrochemistry and X-ray photoelectron spectroscopy (XPS) to illustrate the reaction pathways of electrolyte decomposition, especially FSI- breakdown, as well as the dissolution trend of various inorganic SEI components. The SEI-forming reactions at Cu/electrolyte interface manifest a potential (E) dependence, driven by direct electron-transfer (ET) and Li underpotential-deposition (Li UPD) at high and low E regions, respectively. By closely correlating the XPS data obtained with and without solvent washing, we demonstrate that not all the products derived from SEI reactions are incorporated into forming a passivating surface layer, with a notable portion dissolving into liquid electrolyte instead. Importantly, high-CE electrolyte dictated by the chemical identity of solvent, is found to exhibit minimized interfacial reactivity of SEI formation enabling more effective interphasial passivation, via preferential integration of passivating ingredients such as LiF. Overall, this work formulates a systematic understating of bridging the SEI chemistry, formation and passivation while identifying key characteristics of high-performance electrolyte for guiding future design.

Bao, Zhenan [SLAC National Accelerator Laboratory ↗

Solid Electrolytes in the Spotlight

This virtual issue is targeted to students and researchers, and highlights 32 research articles published over the past 5 years (from July 2016 to July 2021) in Chemistry of Materials (CM). Here, the compilation of papers summarizes the latest advances in the field of solid-state electrolytes for lithium (Li)-, sodium (Na)-, and multivalent-ion (not among the 32 articles discussed) all-solid-state batteries (ASSBs), with a focus on inorganic materials and excluding hybrid systems, e.g., polymer/ceramic composites or systems including liquid media. A total of 125 articles reporting exciting experimental and/or theoretical findings on solid electrolytes were considered for this issue. During 2017–2019, there were about 25–30 papers published per year on this topic, but 2020 and 2021 saw a significant increase, with 26 publications in the first half of 2021 alone. Submissions came from many countries around the world, as shown in Figure 1. While most papers were led by research groups located in the United States, Germany and Japan follow closely, and Austria, the United Kingdom, Canada, and China are also well represented.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Recovering carbon losses in CO 2 electrolysis using a solid electrolyte reactor

The practical implementation of electrochemical CO 2 reduction technology is greatly challenged by notable CO 2 crossover to the anode side, where the crossed-over CO 2 is mixed with O 2 , via interfacial carbonate formation in traditional CO 2 electrolysers. Here we report a porous solid electrolyte reactor strategy to efficiently recover these carbon losses. Furthermore, by creating a permeable and ion-conducting sulfonated polymer electrolyte between cathode and anode as a buffer layer, the crossover carbonate can combine with protons generated from the anode to re-form CO 2 gas for reuse without mixing with anodic O 2 . Using a silver nanowire catalyst for CO 2 reduction to CO, we demonstrated up to 90% recovery of the crossover CO 2 in an ultrahigh gas purity form (>99%), while delivering over 90% CO Faradaic efficiency under a 200 mA cm -2 current. A high continuous CO 2 conversion efficiency of over 90% was achieved by recycling the recovered CO 2 to the CO 2 input stream.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A Self-Healing, Flowable, Yet Solid Electrolyte Suppresses Li-Metal Morphological Instabilities

In this article, lithium metal (Li 0 ) solid-state batteries encounter implementation challenges due to dendrite formation, side reactions, and movement of the electrode–electrolyte interface in cycling. Notably, voids and cracks formed during battery fabrication/operation are hot spots for failure. Here, a self-healing, flowable yet solid electrolyte composed of mobile ceramic crystals embedded in a reconfigurable polymer network is reported. This electrolyte can auto-repair voids and cracks through a two-step self-healing process that occurs at a fast rate of 5.6 µm h -1 . A dynamical phase diagram is generated, showing the material can switch between liquid and solid forms in response to external strain rates. The flowability of the electrolyte allows it to accommodate the electrode volume change during Li 0 stripping. Simultaneously, the electrolyte maintains a solid form with high tensile strength (0.28 MPa), facilitating the regulation of mossy Li 0 deposition. The chemistries and kinetics are studied by operando synchrotron X-ray and in situ transmission electron microscopy (TEM). Solid-state NMR reveals a dual-phase ion conduction pathway and rapid Li + diffusion through the stable polymer-ceramic interphase. This designed electrolyte exhibits extended cycling life in Li 0 –Li 0 cells, reaching 12 000 h at 0.2 mA cm -2 and 5000 h at 0.5 mA cm -2 . Furthermore, owing to its high critical current density of 9 mA cm -2 , the Li 0 –LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) full cell demonstrates stable cycling at 5 mA cm -2 for 1100 cycles, retaining 88% of its capacity, even under near-zero stack pressure conditions.

25 ENERGY STORAGE↗

A Facile Potential Hold Method for Fostering an Inorganic Solid‐Electrolyte Interphase for Anode‐Free Lithium‐Metal Batteries

Abstract Anode‐free lithium batteries are regarded as an ultimate form of high‐energy‐density lithium‐ion batteries. Unfortunately, irreversible lithium loss during cycling plays a major role in degrading the overall cell performance in the anode‐free configuration. To alleviate the deterioration, building a robust solid‐electrolyte interface on an anode current collector is an indispensable requirement. Here, we present a facile in‐situ electrochemical method of a potential hold during the first charge to guide more salt‐derived (less solvent‐derived) decomposition on the anode interface. We show the distinctive decomposition potential of lithium salts and ether/carbonate solvents, where the Li‐solvation structures with salt contact‐ion‐pairs preferentially decompose to form LiF‐rich and less organic components, leading to enhanced lithium Coulombic efficiency in Li||Cu cells as well as mitigating the capacity fade of Cu||LiFePO 4 and Cu||LiNi 0.8 Mn 0.1 Co 0.1 O 2 cells.

Shin, Woochul↗

Salt-rich solid electrolyte interphase for safer high-energy-density Li metal batteries with limited Li excess

We propose a carbonate-based electrolyte optimized with dual cations and ionic liquid for high-efficiency Li metal batteries with a high-voltage cathode. An average coulombic efficiency of Li deposition of 99.6% is achieved due to the salt-rich solid electrolyte interphase and Na guided uniform Li plating. The Li||NCM811 cells can be cycled with limited Li (N/P = 1) over 90 cycles. An additional advantage is that it improves the thermal stability of the NCM811 cathode.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Toward quantifying capacity losses due to solid electrolyte interphase evolution in silicon thin film batteries

To understand the origins of failure and limited cycle life in lithium-ion batteries (LIBs), it is imperative to quantitatively link capacity-fading mechanisms to electrochemical and chemical processes. This is extremely challenging in real systems where capacity is lost during each cycle to both active material loss and solid electrolyte interphase (SEI) evolution, two indistinguishable contributions in traditional electrochemical measurements. Here, we have used a model system in combination with (1) precision measurements of the overall Coulombic efficiency via electrochemical experiments and (2) x-ray reflectivity measurements of the active material losses. The model system consisted of a 515 Å thick amorphous silicon (a-Si) thin film on silicon carbide in half-cell geometry using a carbonate electrolyte with LiPF6 salt. This approach allowed us to quantify the capacity lost during each cycle due to SEI evolution. Combined with electrochemical analysis, we identify SEI growth as the major contribution to capacity fading. Specifically, the continued SEI growth results in increasing overpotentials due to increased SEI resistance, and this leads to lower extent of lithiation when the cutoff voltage is reached during lithiation. Our results suggest that SEI grows more with increased time spent at low voltages where electrolyte decomposition is favored. Finally, we extracted a proportionality constant for SEI growth following a parabolic growth law. Our methodology allows for the quantitative determination of lithium-ion loss mechanisms in LIBs by separately tracking lithium ions within the active materials and the SEI and offers a powerful method of quantitatively understanding LIB loss mechanisms.

25 ENERGY STORAGE↗

Solvation Rule for Solid‐Electrolyte Interphase Enabler in Lithium‐Metal Batteries

Abstract Despite the exceptionally high energy density of lithium metal anodes, the practical application of lithium‐metal batteries (LMBs) is still impeded by the instability of the interphase between the lithium metal and the electrolyte. To formulate a functional electrolyte system that can stabilize the lithium‐metal anode, the solvation behavior of the solvent molecules must be understood because the electrochemical properties of a solvent can be heavily influenced by its solvation status. We unambiguously demonstrated the solvation rule for the solid‐electrolyte interphase (SEI) enabler in an electrolyte system. In this study, fluoroethylene carbonate was used as the SEI enabler due to its ability to form a robust SEI on the lithium metal surface, allowing relatively stable LMB cycling. The results revealed that the solvation number of fluoroethylene carbonate must be ≥1 to ensure the formation of a stable SEI in which the sacrificial reduction of the SEI enabler subsequently leads to the stable cycling of LMBs.

Su, Chi‐Cheung↗

A room temperature rechargeable Li 2 O-based lithium-air battery enabled by a solid electrolyte

Lithium-air batteries have scope to compete with gasoline in terms of energy density. However, in most systems, the reaction pathways either involve one- or two-electron transfer, leading to lithium peroxide (Li 2 O 2 ) or lithium superoxide (LiO 2 ), respectively. Kondori et al. investigated a lithium-air battery that uses a ceramic-polyethylene oxide–based composite solid electrolyte and found that it can undergo a four-electron redox reaction through lithium oxide (Li 2 O) formation and decomposition (see the Perspective by Dong and Lu). The composite electrolyte embedded with Li 10 GeP 2 S 12 nanoparticles shows high ionic conductivity and stability and high cycle stability through a four-electron transfer process.

25 ENERGY STORAGE↗

Modeling the influence of the solid electrolyte interphase on the sand’s time and dendrite formation on lithium metal electrodes

Lithium metal is a sought after battery material for its high energy density due to the low electrochemical potential and density. However, lithium metal is also highly reactive, which results in a strong propensity for dendrite formation. The Sand’s time has previously been used to predict the time of dendrite initiation on metals that do not form a solid-electrolyte interphase (SEI), but it has been shown that the Sand’s time is not accurate for lithium electrodes when using transport parameters associated with the electrolyte. Thus, we built a numerical model to simulate lithium ion transport through a growing SEI to predict the Sand’s time. The numerical model is shown to be more accurate than previous analytical solutions, especially for low current densities. We then analyze the sensitivity of the Sand’s time to different SEI properties and the chemical potential gradients present in the SEI, driving lithium transport. The results showed that high lithium concentration has a greater impact at high current density, while fast diffusivity is more important at low current density. Lastly, we modeled the influence of surface roughness on the plating evolution and chemical potential gradients when an SEI is present in comparison to the electrolyte. As a result, we demonstrate that the SEI plays a critical role in lithium electrode stability, and that improved characterization techniques are needed to better understand transport through the SEI and increase lithium metal utilization in energy storage devices.

Chemistry↗

Multi-scale stabilization of high-voltage LiCoO 2 enabled by nanoscale solid electrolyte coating

LiCoO 2 (LCO) possess a high theoretical specific capacity of 274 mAh g -1 , and currently LCO charged to 4.48 V with a capacity of ~190–195 mAh g -1 is penetrating the commercial markets. Scalable strategies to further enhance the performance of LCO are highly attractive. Here, we develop a scalable ball-milling and sintering method to tackle this long-standing challenge by modifying LCO surface with only 1.5–3.5% ceramic solid electrolyte nanoparticles, specifically Li 1.5 Al 0.5 Ge 1.5 (PO 4 ) 3 (LAGP) as an example. Consequently, the atomic-to-meso multiscale structural stabilities have been significantly improved, even with a high cut-off voltage of 4.5 V vs. Li/Li + , leading to excellent electrochemical stabilities. The nano-LAGP modified Li|LCO cell exhibits high discharge capacity of 196 mAh g -1 at 0.1 C, capacity retention of 88% over 400 cycles, and remarkably enhanced rate capability (163 mAh g -1 at 6 C). These results show significant improvement compared to the Li|LCO cells. The as-prepared graphite|LAGP-LCO full cells also show steady cycling with 80.4% capacity retention after 200 cycles with a voltage cut-off of 4.45 V. This work provides a simple and scalable approach to achieve stable cycling of LCO at high voltage with high energy density.

25 ENERGY STORAGE↗

Suppressing Atmospheric Degradation of Sulfide-Based Solid Electrolytes via Ultrathin Metal Oxide Layers

Sulfide-based solid-state electrolytes (SSEs) are promising materials with superior Li-ion conductivity; however, their poor atmospheric stability limits commercial manufacturing at scale. Here, we investigate the impact of ultrathin metal oxide layers deposited via atomic layer deposition (ALD) on the stability of Li 6 PS 5 Cl (LPSCl). Al 2 O 3 layers grown directly on LPSCl particles significantly stabilize the surface chemistry and Li-ion transport properties relative to uncoated material upon exposure to both an ambient atmosphere (22% relative humidity, RH) and humidified O 2 (100% RH). Detailed investigations indicate that coatings impede the surface and bulk degradation kinetics of exposed materials, even for coatings as thin as ∼1 Å. Furthermore, this suggests that stabilization is due to more than just a physical barrier. Shifts in valence band edge positions of coated LPSCl indicate that ALD coatings alter the surface electronic structure and resulting oxidation tendency of underlying LPSCl, suggesting new avenues to improving the environmental stability of sulfide SSEs.

Atmospheric chemistry↗

A solid electrolyte interphase to protect the sulfurized polyacrylonitrile (SPAN) composite for Li–S batteries: computational approach addressing the electrolyte/SPAN interfacial reactivity

This study addresses the reactivity of multiple solvents and lithium bis(fluorosulfonyl)imide (LiFSI) at the interface with sulfurized polyacrylonitrile (SPAN) in multiple stages of lithiation via ab initio molecular dynamics simulations. Here, both ether 1,3-dioxolane (DOL) and dimethyl carbonate (DMC) proved stable on the lithiated SPAN surface regardless of the lithium content, meaning that neither of these species likely contributes to growing a solid electrolyte interphase (SEI) coating to protect the SPAN composite. Conversely, cyclic carbonates, ethylene carbonate (EC) and fluoroethylene carbonate (FEC) are shown to be very active. The EC reduction occurs only on a highly lithiated surface with a 3.0 Li/S molar ratio, the equivalent of the SPAN composite in an over-discharge regime with voltages close to 0.0 V vs. Li/Li + . The FEC reduction starts with a 2.0 Li/S molar ratio and above, suggesting that FEC could act as a useful additive in electrolyte formulations with EC. Both EC and FEC follow multiple reduction mechanisms to produce complex reduction products and LiF in the FEC case. We provide a mechanistic description for each detected decomposition path. The LiFSI salt also proves reactive against the lithiated SPAN surface. The FSI – defluorination is the dominant reduction path. However, the SO 2 NSO 2 F – and SO 2 NSO 2 2– species proved stable against S–N cleavage. This behavior makes the LiFSI salt a potential candidate for SPAN-based Li–S batteries because it produces LiF without releasing SO 2 .

25 ENERGY STORAGE↗