Analysis of Retrieved Hubble Space Telescope Thermal Control Materials

The mechanical and optical properties of the thermal control materials on the Hubble Space Telescope (HST) have degraded over the nearly seven years the telescope has been in orbit. Astronaut observations and photographs from the Second Servicing Mission (SM2) revealed large cracks in the metallized Teflon FEP, the outer-layer of the multi-layer insulation (MLI), in many locations around the telescope. Also, the emissivity of the bonded metallized Teflon FEP radiator surfaces of the telescope has increased over time. Samples of the top layer of the MLI and radiator material were retrieved during SM2, and a thorough investigation into the de-radiation followed in order to determine the primary cause of the damage. Mapping of the cracks on HST and the ground testing showed that thermal cycling with deep-layer damage from electron and proton radiation are necessary to cause the observed embrittlement. Further, strong, evidence was found indicating that chain scission (reduced molecular weight) is the dominant form of damage to the metallized Teflon FEP.

Townsend, Jacqueline A.↗

On-Orbit Teflon(R) FEP Degradation

During the Hubble Space Telescope (HST) Second Servicing Mission (SM2), degradation of unsupported Teflon(R) FEP (fluorinated ethylene propylene), used as the outer layer of the multi-layer insulation (MLI) blankets, was evident as large cracks on the telescope light shield. A sample of the degraded outer layer was retrieved during the mission and returned to Earth for ground testing and evaluation. The results of the Teflon(R) FEP sample evaluation and additional testing of pristine Teflon(R) FEP led the investigative team to theorize that the HST damage was caused by thermal cycling with deep-layer damage from electron and proton radiation which allowed the propagation of cracks along stress concentrations, and that the damage increased with the combined total dose of electrons, protons, UV and x-rays along with thermal cycling. This paper discusses the testing and evaluation of the Teflon(R) FEP.

Townsend, Jacqueline A.↗

Space Weathering of Genesis Mission Solar-wind Collectors with Inferences for Weathering on Airless Bodies

Samples from the Genesis Solar Wind Sample Return (NASA Discovery 5) are a unique opportunity to study the initial stages of space weathering, i.e., the physical and chemical effects of solar-wind irradiation. Arrays of collectors containing multiple materials were each exposed to a different solar-wind regime (fast, slow, bulk, or coronal mass ejection) at the L1 point for long durations (years). Materials exposed to the solar wind included metals, semiconductors, and insulators. Although the time of exposure was obviously short relative to samples having extraterrestrial origins, optical properties, surface chemical properties, and matrix structure have changed in many collectors due to exposure to solar wind. The thickness of amorphous zones, where present, appears to correspond with the depth of the peak of the solar-wind H distribution in each regime. Damage from high-energy particles was negligible because the collectors were 700 μm or less in thickness and shielded from the back by the spacecraft. Micrometeorite impacts and sputtering were also negligible because of the short exposure times. Our current results are preliminary: We hope future workers will extend this study both to support Genesis characterization efforts and to further understand space-weathering processes on a geologic timescale.

space weathering↗

Thermal Consideration of SWIFT XRT Radiator At-35C or Colder in Low Earth Orbit

The X-Ray Telescope (XRT) is an instrument on the National Aeronautics and Space Administration (NASA) SWIFT spacecraft. The thermoelectric cooler (TEC) for the charge coupled device (CCD) of the XRT requires a radiator temperature of -35 C or colder, and a goal of -55 C to minimize the damage by radiation. The waste heat rejected from the TEC to the radiator is in the 8 W to 20 W range. In the Phase A baseline design, the XRT radiator is mounted to the rear end of the XRT telescope tube and is very close to the bottom closeout of the spacecraft bus. The bottom closeout is multi-layer insulation (MLI) blankets. At sun angles between 90 deg and 180 deg, there is direct solar impingement on the bottom closeout. When the rolls +/- 5 deg, the XRT radiator is exposed to direct solar radiation. The radiator also has a view factor to the solar arrays. The results of thermal analysis showed that the flight temperature prediction of the radiator exceeds the temperature requirement of -35 C substantially at sun angles from 110 deg to 180 deg. A new location on the anti-sun side of the spacecraft is proposed for the radiator. It requires a heat pipe to couple the TEC and the radiator thermally. The results of thermal analysis show that the flight temperature prediction of the proposed radiator meets the temperature requirement at all sun angles.

Choi, Michael K.↗

Insights Developed Into the Damage Mechanism of Teflon FEP Thermal Control Material on the Hubble Space Telescope

Metalized Teflon FEP (DuPont; fluorinated ethylene propylene) thermal control material on the Hubble Space Telescope (HST) has been found to degrade in the space environment. Teflon FEP thermal control blankets retrieved during the first servicing mission were found to be embrittled on solar-facing surfaces and to contain microscopic cracks (the FEP surface is exposed to the space environment). During the second servicing mission, astronauts noticed that the FEP outer layer of the multilayer insulation blanketing covering the telescope was cracked in many locations. Large cracks were observed on the light shield, forward shell, and equipment bays. A tightly curled piece of cracked FEP from the light shield was retrieved during the second mission. This piece was severely embrittled, as witnessed by ground testing. A Failure Review Board was organized by NASA Goddard Space Flight Center to determine the mechanism causing the multilayer insulation degradation. This board included members of the Electro-Physics Branch of the NASA Glenn Research Center at Lewis Field. Density measurements of the retrieved materials obtained under the review board's investigations indicated that FEP from the first servicing mission was essentially unchanged from pristine FEP but that the second servicing mission FEP had increased in density in comparison to pristine FEP (ref. 1). The results were consistent with crystallinity measurements taken using x-ray diffraction and with results from solid-state nuclear magnetic resonance tests (see the table and ref. 1). Because the second servicing mission FEP was embrittled and its density and crystallinity had increased in comparison to pristine FEP, board researchers expected that the first servicing mission FEP, which was also embrittled, would also have increased in crystallinity and density, but it did not. Because the retrieved second servicing mission material curled while in space, it experienced a higher temperature extreme during thermal cycling (estimated at 200 C) than the first servicing mission material (estimated at 50 C). Therefore, Glenn initiated and conducted an investigation of the effects of heating pristine FEP and FEP that had been exposed on the Hubble Space Telescope. Samples of pristine and first and second servicing mission FEP were heated to 200 C and evaluated for changes in density and morphology. We hoped that the results would help explain why FEP degrades in the Hubble Space Telescope space environment.

deGroh, Kim K.↗

Hubble Space Telescope Metallized Teflon(registered trademark) FEP Thermal Control Materials: On-Orbit Degradation and Post-Retrieval Analysis

During the Hubble Space Telescope (HST) Second Servicing Mission (SM2), degradation of unsupported Teflon(Registered Trademark) FEP (fluorinated ethylene propylene), used as the outer layer of the multilayer insulation (MLI) blankets, was evident as large cracks on the telescope light shield. A sample of the degraded outer layer was retrieved during the mission and returned to Earth for ground testing and evaluation. The results of the Teflon(Registered Trademark) FEP sample evaluation and additional testing of pristine Teflon(Registered Trademark) FEP led the investigative team to theorize that the HST damage was caused by thermal cycling with deep-layer damage from electron and proton radiation which allowed the propagation of cracks along stress concentrations , and that the damage increased with the combined total dose of electrons, protons, UV and x-rays along with thermal cycling. This paper discusses the testing and evaluation of the retrieved Teflon(Registered Trademark) FEP.

Townsend, Jacqueline A.↗

Spectroscopic Behavior of Composite, Black Thermal Paint, Solar Cell, and Multi-Layered Insulation Materials in a GEO Simulated Environment

The population of objects orbiting Earth is dominated by orbital debris. The following study presents reflectance spectroscopic measurements and bidirectional reflectance distribution function (BRDF) evaluations taken on common spacecraft materials (Table 1), some of which are likely candidates in the orbital debris population. Their optical properties were assessed in their pristine conditions, as well as after exposure in a space environmental chamber used to simulate space weathering. The materials studied will prove that they have excellent properties in resisting the effects of damage that are common in both low Earth orbit and geosynchronous Earth orbit (GEO) based on the research discussed in this work.

Reyes, Jacqueline A.↗

Measurement of insulation integrity of IUE camera tube facsimiles by partial discharges method and diffusion of gases through various silicone rubbers

Several dummy tubes imitating the IUE Camera System design were encapsulated with Solithane 2, Conathane EN-11, Green and Black Hysols and SMRD 432. Various flaws were purposefully placed in some of these. Partial discharge testing in vacuum under direct voltage conditions was carried once a week for 12 weeks, 15 kv dc being applied during normal working hours for 40 hours duration per week. None of the units showed much damage during this time judging by the P.D. energy histograms. A more complete mathematical presentation is given on diffusion and permeation than previously. Measurements of diffusion constants for various silicone rubbers are carried out by the Time-Lag method and compared to other determinations in the literature. Calculations of the time required for diffusion through a thick wall are demonstrated in the long time approximation and for dimensions pertaining to void and wall sizes of a delamination problem in the LANDSAT-C vidicon tubes. An actual delaminated LANDSAT-C tube and some facsimiles are immersed in vacuum for long periods and tested for catastrophic breakdown due to diffusion of gas, by application of high voltage.

Bever, R. S.↗

Performance of uncoated AFRSI blankets during multiple Space Shuttle flights

Uncoated Advanced Flexible Reusable Surface Insulation (AFRSI) blankets were successfully flown on seven consecutive flights of the Space Shuttle Orbiter OV-099 (Challenger). In six of the eight locations monitored (forward windshield, forward canopy, mid-fuselage, upper wing, rudder/speed brake, and vertical tail) the AFRSI blankets performed well during the ascent and reentry exposure to the thermal and aeroacoustic environments. Several of the uncoated AFRSI blankets that sustained minor damage, such as fraying or broken threads, could be repaired by sewing or by patching with a surface coating called C-9. The chief reasons for replacing or completely coating a blanket were fabric embrittlement and fabric abrasion caused by wind erosion. This occurred in the orbiter maneuvering system (OMS) pod sidewall and the forward mid-fuselage locations.

Sawko, Paul M.↗

High-Temperature RF Probe Station For Device Characterization Through 500 deg C and 50 GHz

A high-temperature measurement system capable of performing on-wafer microwave testing of semiconductor devices has been developed. This high temperature probe station can characterize active and passive devices and circuits at temperatures ranging from room temperature to above 500 C. The heating system uses a ceramic heater mounted on an insulating block of NASA shuttle tile material. The temperature is adjusted by a graphical computer interface and is controlled by the software-based feedback loop. The system is used with a Hewlett-Packard 8510C Network Analyzer to measure scattering parameters over a frequency range of 1 to 50 GHz. The microwave probes, cables, and inspection microscope are all shielded to protect from heat damage. The high temperature probe station has been successfully used to characterize gold transmission lines on silicon carbide at temperatures up to 540 C.

Schwartz, Zachary D.↗

Development and testing of a solar flux heating freeze recovery system for molten salt parabolic troughs

A major obstacle preventing commercialization of molten salt parabolic trough plants is freeze protection and recovery of the solar field. One of the most common nitrate salt compositions under consideration allows for solar field outlet temperatures up to 565°C and begins solidifying above 240°C. Using molten salt directly in the solar field can significantly reduce thermal energy storage costs and the higher temperature compared to oil heat transfer fluids can power a more efficient power cycle, but the very high freezing point is cause for concern. This work builds on a previous modeling effort investigating different methods for melting Solar Salt frozen in the solar field, which suggested the viability of a novel solar heating method to lower costs of the freeze protection system. In this work higher fidelity models are developed to better investigate the melting process with a more detailed 3D geometry which includes the insulated bellows. The thermal-fluid model of the melting process is updated to include temperature dependent density and data for solid phase properties. In addition, a finite element model is developed to resolve thermal stresses at the point with highest thermal gradients. Results with the new model confirm the viability of using controllable solar flux heating to thaw salt frozen in the solar field without damaging the receiver; however, the presence of non-illuminated sections significantly slows down the melting process. Solar heating simulations with pauses off-sun of 120 and 60 s require 18.5 and 11.9 h to melt salt from a night-time temperature of 10°C with 1000 W m2 DNI, which results in maximum thermal stresses of 48.2 and 53.5 MPa, respectively. Adding 150 W m−1 to the solar heating simulation with a 60 s pause off-sun decreases both the melt time and thermal stresses due to the more uniform heating, suggesting a combined heating method may be the best option.

14 SOLAR ENERGY↗

Results of a FRSI material test under Space Shuttle ascent conditions in the Ames Research Center 9x7 foot supersonic wind tunnel (OS13). Space Shuttle aerothermodynamic data report

A test was conducted in the NASA/ARC 9 x 7 foot supersonic wind tunnel to verify the integrity of Felt Reusable Surface Insulation (FRSI) material in a panel flutter environment. A FRSI sample panel was subjected to the shocks, pressure gradients, and turbulence characteristics encountered at dynamic pressure 1.5 times the 3(sigma) dispersed trajectory flight conditions of the Space Shuttle. Static and fluctuating pressure data were obtained for Mach numbers ranging from 1.55 to 2.5 with dynamic pressures of 625 to 1250 psf. The FRSI panel suffered no appreciable damage as a result of the test.

Lemoine, P. L.↗

Potential for EMU Fabric Damage by Electron Beam and Molten Metal During Space Welding for the International Space Welding Experiment

As a consequence of preparations concerning the International Space Welding Experiment (ISWE), studies were performed to better understand the effect of molten metal contact and electron beam impingement with various fabrics for space suit applications. The question arose as to what would occur if the electron beam from the Ukrainian Universal Hand Tool (UHT) designed for welding in space were to impinge upon a piece of Nextel AF-62 ceramic cloth designed to withstand temperatures up to 1427 C. The expectation was that the electron beam would lay down a static charge pattern with no damage to the ceramic fabric. The electron beam is capable of spraying the fabric with enough negative charge to repel further electrons from the fabric before significant heating occurs. The static charge pattern would deflect any further charge accumulation except for a small initial amount of leakage to the grounded surface of the welder. However, when studies were made of the effect of the electron beam on the insulating ceramic fabric it was surprisingly found that the electron beam did indeed burn through the ceramic fabric. It was also found that the shorter electron beam standoff distances had longer burnthrough times than did some greater electron beam standoff distances. A possible explanation for the longer burnthrough times for the small electron beam standoff distance would be outgassing of the fabric which caused the electron beam hand-tool to cycle on and off to provide some protection for the cathodes. The electron beam hand tool was observed to cycle off at the short standoff distance of two inches likely due to vapors being outgassed. During the electron beam welding process there is an electron leakage, or current leakage, flow from the fabric. A static charge pattern is initially laid down by the electron beam current flow. The static charge makes up the current leakage flow which initially slightly heats up the fabric. The initially laid down surface charge leaks a small amount of current. The rate at which the current charge leaks from the fabric controls how fast the fabric heats up. As the ceramic fabric is heated it begins to outgass primarily from contamination/impurities atoms or molecules on and below the fabric surface. The contaminant gases ionize to create extra charge carriers and multiply a current of electrons. The emitted gas which ionized in the electron leakage flow promotes further leakage. Thus, the small leakage of charge from the fabric surface is enhanced by outgassing. When the electron beam current makes up the lost current, the incoming electrons heat the fabric and further enhance the outgassing. The additional leakage promotes additional heating up of the ceramic fabric. The electrons bound to the ceramic fabric surface leak off more and more as the surface gets hotter promoting even greater leakage. The additional electrons that result also gain energy in the field and produce further electrons. Eventually the process becomes unstable and accelerates to the point where a hole is burned through the fabric.

Fragomeni, James M.↗

Tethers as Debris: Simulating Impacts of Kevlar Tethers on Shuttle Tiles

In a previous paper I examined the effects of impacts of polymer tethers on aluminum plates using the SPHC hydrodynamic code. In this paper I apply tether models to a new target - models of Space Shuttle tiles developed during the STS 107 accident investigation. In this three-dimensional simulation, a short tether fragment strikes a single tile supported on an aluminum backing plate. A tile of the LI-900 material is modeled. Penetration and damage to the tile and the backwall are characterized for three normal impact velocities. The tether is modeled as a bundle of eight 1-mm strands, with the bundle having dimensions 2-mm x 4-mm x 20-cm. The bulk material properties used are those of Kevlar(TradeMark) 49, for which a Mie-Gruneisen multiphase equation of state (eos) is used. In addition, the strength model is applied in a linear sense, such that tensile loads along the strand length are supported, but there is no strength in the lateral directions. Tile models include the various layers making up the tile structure. The outermost layer is a relatively dense borosilicate glass, known as RCG, 0.5-mm thick. The RCG layer is present on the top and four sides of the tile. Below this coating is the bulk of the tile, 1.8- in thick, made of LI-900, a product consisting of rigidized fiberous silica with a density of 9 lWft3. Below the main insulating layer is a bottom layer of the same material that has been treated to increase its density by approximately 69% to improve its strength. This densified layer is bonded to a Strain Isolation Pad (SIP), modeled as a refractory felt fabric. The SIP is bonded to an aluminum 2024 wall 0.1-in thick. The tile and backwall materials use a Me-Gruneisen multiphase eos, with the exception of the SIP felt, which uses a fabric equation of state. Fabrics must be crushed to the full bulk material density before bulk material properties and a Mie-Gruneisen eos are applied. Tether fragment impact speeds of 3,7, and 10 km/s are simulated, with impact velocities normal to the tile face. Damage results are presented in tabular format.

Evans, Steven W.↗

Numerical investigation of thermomechanical response of multiscale porous Ultra-High Temperature Ceramics

Recent advances in Ultra-High Temperature Ceramics (UHTC) manufacturing have permitted the development of multiscale porous UHTC microstructures. Within the target application of hypersonic vehicles, dense UHTCs are suitable for thermal protection on leading edges, whereas porous UHTCs may find a role in providing thermally insulated interfaces for temperature-sensitive interior components. Designing vehicles incorporating porous UHTCs requires a characterization of their thermomechanical properties across the full range of expected operating temperatures spanning –20 °C–2500 °C. This research represents a preliminary study in performing this characterization. Several numerical experiments are performed using a coupled thermomechanical implementation of the Material Point Method to determine the temperature dependence of effective material properties both with and without damage. Furthermore, complex time-dependent boundary conditions derived from known hypersonic flight profiles are simulated in order to probe the various couplings between deformation, damage and heat transfer. It is shown that the model reveals the importance of micro-buckling in determining effective material stiffness and thermal conductivity.

36 MATERIALS SCIENCE↗

Mitigation of EMU Glove Cut Hazard by MMOD Impact Craters on Exposed ISS Handrails

Recent cut damages to crewmember extravehicular mobility unit (EMU) gloves during extravehicular activity (EVA) onboard the International Space Station (ISS) has been found to result from contact with sharp edges or pinch points rather than general wear or abrasion. One possible source of cut-hazards are protruding sharp edged crater lips from impact of micrometeoroid and orbital debris (MMOD) particles on external metallic handrails along EVA translation paths. During impact of MMOD particles at hypervelocity an evacuation flow develops behind the shock wave, resulting in the formation of crater lips that can protrude above the target surface. In this study, two methods were evaluated to limit EMU glove cut-hazards due to MMOD impact craters. In the first phase, four flexible overwrap configurations are evaluated: a felt-reusable surface insulation (FRSI), polyurethane polyether foam with beta-cloth cover, double-layer polyurethane polyether foam with beta-cloth cover, and multi-layer beta-cloth with intermediate Dacron netting spacers. These overwraps are suitable for retrofitting ground equipment that has yet to be flown, and are not intended to protect the handrail from impact of MMOD particles, rather to act as a spacer between hazardous impact profiles and crewmember gloves. At the impact conditions considered, all four overwrap configurations evaluated were effective in limiting contact between EMU gloves and impact crater profiles. The multi-layer beta-cloth configuration was the most effective in reducing the height of potentially hazardous profiles in handrail-representative targets. In the second phase of the study, four material alternatives to current aluminum and stainless steel alloys were evaluated: a metal matrix composite, carbon fiber reinforced plastic (CFRP), fiberglass, and a fiber metal laminate. Alternative material handrails are intended to prevent the formation of hazardous damage profiles during MMOD impact and are suitable for flight hardware yet to be constructed. Of the four materials evaluated, only the fiberglass formed a less hazardous damage profile than the baseline metallic target. Although the CFRP laminate did not form any noticeable crater lip, brittle protruding fibers are considered a puncture risk. In parallel with EMU glove redesign efforts, modifications to metallic ISS handrails such as those evaluated in this study provide the means to significantly reduce cut-hazards from MMOD impact craters.

Christiansen, Eric L.↗

High Temperature Resistant Organopolysiloxane Coating for Protecting and Repairing Rigid Thermal Insulation

Ceramics are protected from high temperature degradation, including high temperature, oxidative, aeroconvective degradation by a high temperature and oxidation resistant coating of a room temperature curing, hydrolyzed and partially condensed liquid polyorganosiloxane to the surface of the ceramic. The liquid polyorganosiloxane is formed by the hydrolysis and partial condensation of an alkyltrialkoxysilane with water or a mixture of an alkyltrialkoxysilane and a dialkyldialkoxysilane with water. The liquid polyorganosiloxane cures at room temperature on the surface of the ceramic to form a hard, protective, solid coating which forms a high temperature environment, and is also used as an adhesive for adhering a repair plug in major damage to the ceramic. This has been found useful for protecting and repairing porous, rigid ceramics of a type used on reentry space vehicles.

Leiser, Daniel B.↗

Investigation of Teflon FEP Embrittlement on Spacecraft in Low Earth Orbit

Teflon(registered trademark) FEP (fluorinated ethylene-propylene) is commonly used on exterior spacecraft surfaces in the low Earth orbit (LEO) environment for thermal control. Silverized or aluminized FEP is used for the outer layer of thermal control blankets because of its low solar absorptance and high thermal emittance. FEP is also preferred over other spacecraft polymers because of its relatively high resistance to atomic oxygen erosion. Because of its low atomic oxygen erosion yield, FEP has not been protected in the space environment. Recent, long term space exposures such as on the Long Duration Exposure Facility (LDEF, 5.8 years in space), and the Hubble Space Telescope (HST, after 3.6 years in space) have provided evidence of LEO environmental degradation of FEP. These exposures provide unique opportunities for studying environmental degradation because of the long durations and the different conditions (such as differences in altitude) of the exposures. Samples of FEP from LDEF and from HST (retrieved during its first servicing mission) have been evaluated for solar induced embrittlement and for synergistic effects of solar degradation and atomic oxygen. Micro-indenter results indicate that the surface hardness increased as the ratio of atomic oxygen fluence to solar fluence decreased for the LDEF samples. FEP multilayer insulation (MLI) retrieved from HST provided evidence of severe embrittlement on solar facing surfaces. Micro-indenter measurements indicated higher surface hardness values for these samples than LDEF samples, but the solar exposures were higher. Cracks induced during bend testing were significantly deeper for the HST samples with the highest solar exposure than for LDEF samples with similar atomic oxygen fluence to solar fluence ratios. If solar fluences are compared, the LDEF samples appear as damaged as HST samples, except that HST had deeper induced cracks. The results illustrate difficulties in comparing LEO exposed materials from different missions. Because the HST FEP appears more damaged than LDEF FEP based on depth of embrittlement, other causes for FEP embrittlement in addition to atomic oxygen and ultraviolet (UV) radiation, such as thermal effects and the possible role of soft x-ray radiation, need to be considered. FEP that was exposed to soft x-rays in a ground test facility, showed embrittlement similar to that witnessed in LEO, which indicates that the observed differences between LDEF and HST FEP might be attributed to the different soft x-ray fluences during these two missions.

deGroh, Kim K.↗