Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “fracturing materials”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 307 records · Page 17

A very low shock alternative to conventional, pyrotechnically operated release devices

NiTiNOL is best known for its ability to remember a preset shape, even after being 'plastically' deformed. This is accomplished by heating the material to an elevated temperature up to 120 degrees C. However, NiTiNOL has other material and mechanical properties that provide a novel method of structural release. This combination of properties allows NiTiNOL to be used as a mechanical fuse between structural components. When electrical power is applied to the NiTiNOL fuse(s), the material is annealed reducing the mechanical strength to a small fraction of the as-wrought material. The preload then fractures the weakened NiTiNOL fuse(s) and releases the structure. This paper describes the mechanical characteristics of the NiTiNOL allow used in this invention, structural separation design concepts using the NiTiNOL material, and initial test data. Elimination of the safety hazard, high shock levels, and non-reusability inherent with pyrotechnic separation devices allows NiTiNOL actuated release devices to become a viable alternative for aerospace components and systems.

Robinson, Steven P.↗

Composite Materials Characterization and Development at AFWAL

The development of test methodology for characterizing matrix dominated failure modes is discussed emphasizing issues of matrix cracking, delamination under static loading, and the relationship of composite properties to matrix properties. Both strength characterization and classical techniques of linear elastic fracture mechanics were examined. Materials development studies are also discussed. Major areas of interest include acetylene-terminated and bismaleimide resins for 350 to 450 deg use, thermoplastics development, and failure resistant composite concepts.

Browning, C. E.↗

Numerical Evaluation of Mode 1 Stress Intensity Factor as a Function of Material Orientation For BX-265 Foam Insulation Material

Foam; a cellular material, is found all around us. Bone and cork are examples of biological cell materials. Many forms of man-made foam have found practical applications as insulating materials. NASA uses the BX-265 foam insulation material on the external tank (ET) for the Space Shuttle. This is a type of Spray-on Foam Insulation (SOFI), similar to the material used to insulate attics in residential construction. This foam material is a good insulator and is very lightweight, making it suitable for space applications. Breakup of segments of this foam insulation on the shuttle ET impacting the shuttle thermal protection tiles during liftoff is believed to have caused the space shuttle Columbia failure during re-entry. NASA engineers are very interested in understanding the processes that govern the breakup/fracture of this complex material from the shuttle ET. The foam is anisotropic in nature and the required stress and fracture mechanics analysis must include the effects of the direction dependence on material properties. Material testing at NASA MSFC has indicated that the foam can be modeled as a transversely isotropic material. As a first step toward understanding the fracture mechanics of this material, we present a general theoretical and numerical framework for computing stress intensity factors (SIFs), under mixed-mode loading conditions, taking into account the material anisotropy. We present mode I SIFs for middle tension - M(T) - test specimens, using 3D finite element stress analysis (ANSYS) and FRANC3D fracture analysis software, developed by the Cornel1 Fracture Group. Mode I SIF values are presented for a range of foam material orientations. Also, NASA has recorded the failure load for various M(T) specimens. For a linear analysis, the mode I SIF will scale with the far-field load. This allows us to numerically estimate the mode I fracture toughness for this material. The results represent a quantitative basis for evaluating the strength and fracture properties of anisotropic foam insulation material.

Knudsen, Erik↗

Fracture mechanics correlation of boron/aluminum coupons containing stress risers

The mechanical behavior of boron/aluminum near stress risers has been studied and reported. This effort was directed toward defining the tensile behavior of both unidirectional and (0/ plus or minus 45) boron/aluminum using linear elastic fracture mechanics (LEFM). The material used was 5.6-mil boron in 6061 aluminum, consolidated using conventional diffusion bonding techniques. Mechanical properties are reported for both unidirectional and (0/ plus or minus 45) boron/aluminum, which serve as control data for the fracture mechanics predictions. Three different flawed specimen types were studied. In each case the series of specimens remained geometrically similar to eliminate variations in finite size correction factors. The fracture data from these tests were reduced using two techniques. They both used conventional LEFM methods, but the existence of a characteristic flaw was assumed in one case and not the other. Both the data and the physical behavior of the specimens support the characteristic flaw hypothesis. Cracks were observed growing slowly in the (0/ plus or minus 45) laminates, until a critical crack length was reached at which time catastrophic failure occurred.

Adsit, N. R.↗

Materials

Materials science - brittleness, fatigue, and fracture mechanics - glass-reinforced plastic, high strength metals and alloys, and refractory materials

MATERIALS SCIENCE↗

Fracture Mechanics Properties of Fused Silicas Used for International Space Station Windowpanes

The fracture toughness and slow crack growth (SCG) parameters of a quartz-based silica and a high-purity fused silica were measured as part of a program to review the reliability of the International Space Station windows. The materials exhibit the same fracture toughness (.75 MPa m^(1/2) in N2) and very similar SCG parameters. The literature on fused silica indicates excellent agreement of fracture toughness, but a very wide range of SCG parameters, even from the same institution, with strength-based methods usually yielding a lower power law exponent than direct crack velocity measurements. Use of the exponential function is shown to provide better agreement between test methods, with velocity curves derived from strength tests of bare fiber and polished or ground test specimens paralleling those from wide-range, direct crack velocity observations, implying that constant stress rate tests can predict long lifetime via the exponential function. However, much variation still exists. SCG parameters for soda–lime silicate are much less sensitive to the test method than fused silica. Static load tests and stress intensity measurements resulted in a fatigue threshold of .3 MPa m^(1/2) for fused silica.

Silica, toughness, impact, crack growth, windows, ↗

Damage Mechanisms and Controlled Crack Propagation in a Hot Pressed Silicon Nitride Ceramic

The subcritical growth of cracks from pre-existing flaws in ceramics can severely affect the structural reliability of a material. The ability to directly observe subcritical crack growth and rigorously analyze its influence on fracture behavior is important for an accurate assessment of material performance. A Mode I fracture specimen and loading method has been developed which permits the observation of stable, subcritical crack extension in monolithic and toughened ceramics. The test specimen and procedure has demonstrated its ability to generate and stably propagate sharp, through-thickness cracks in brittle high modulus materials. Crack growth for an aluminum oxide ceramic was observed to be continuously stable throughout testing. Conversely, the fracture behavior of a silicon nitride ceramic exhibited crack growth as a series of subcritical extensions which are interrupted by dynamic propagation. Dynamic initiation and arrest fracture resistance measurements for the silicon nitride averaged 67 and 48 J/sq m, respectively. The dynamic initiation event was observed to be sudden and explosive. Increments of subcritical crack growth contributed to a 40 percent increase in fracture resistance before dynamic initiation. Subcritical crack growth visibly marked the fracture surface with an increase in surface roughness. Increments of subcritical crack growth loosen ceramic material near the fracture surface and the fracture debris is easily removed by a replication technique. Fracture debris is viewed as evidence that both crack bridging and subsurface microcracking may be some of the mechanisms contributing to the increase in fracture resistance. A Statistical Fracture Mechanics model specifically developed to address subcritical crack growth and fracture reliability is used together with a damaged zone of material at the crack tip to model experimental results. A Monte Carlo simulation of the actual experiments was used to establish a set of modeling input parameters. It was demonstrated that a single critical parameter does not characterize the conditions required for dynamic initiation. Experimental measurements for critical crack lengths, and the energy release rates exhibit significant scatter. The resulting output of the model produces good agreement with both the average values and scatter of experimental measurements.

Calomino, Anthony Martin↗

Evaluation of the Edge Crack Torsion (ECT) Test for Mode 3 Interlaminar Fracture Toughness of Laminated Composites

An analytical and experimental investigation was carried out on G40-800/R6376 graphite epoxy laminates to evaluate the Edge Crack Torsion (ECT) test as a candidate for a standard Mode 3 interlaminar fracture toughness test for laminated composites. The ECT test consists of a (90/(+/- 45)(sub 3)/(+/- 45)(sub 3)/90))(sub s) laminate with a delamination introduced by a non-adhesive film at the mid-plane along one edge and loaded in a special fixture to create torsion along the length of the laminate. Dye penetrate enhanced X-radiograph of failed specimens revealed that the delamination initiated at the middle of the specimen length and propagated in a self similar manner along the laminate mid-plane. A three-dimensional finite element analysis was performed that indicated that a pure Mode 3 delamination exists at the middle of specimen length away from both ends. At the ends near the loading point a small Mode 2 component exists. However, the magnitude of this Mode 2 strain energy release rate at the loading point is small compared to the magnitude of Mode 3 component in the mid-section of the specimen. Hence, the ECT test yielded the desired Mode 3 delamination. The Mode 3 fracture toughness was obtained from a compliance calibration method and was in good agreement with the finite element results. Mode 2 End-Notched Flexure (ENF) tests and Mode 1 Double Cantilever Beam (DCB) tests were also performed for the same composite material. The Mode 1 fracture toughness was much smaller than both the Mode 2 and Mode 3 fracture toughness. The Mode 2 fracture toughness was found to be 75% of the Mode 3 fracture toughness.

Li, Jian↗

The Merging of Fatigue and Fracture Mechanics Concepts: A Historical Perspective

The seventh Jerry L. Swedlow Memorial Lecture presents a review of some of the technical developments, that have occurred during the past 40 years, which have led to the merger of fatigue and fracture mechanics concepts. This review is made from the viewpoint of 'crack propagation.' As methods to observe the 'fatigue' process have improved, the formation of fatigue micro-cracks have been observed earlier in life and the measured crack sizes have become smaller. These observations suggest that fatigue damage can now be characterized by 'crack size.' In parallel, the crack-growth analysis methods, using stress-intensity factors, have also improved. But the effects of material inhomogeneities, crack-fracture mechanisms, and nonlinear behavior must now be included in these analyses. The discovery of crack-closure mechanisms, such as plasticity, roughness, and oxide/corrosion/fretting product debris, and the use of the effective stress-intensity factor range, has provided an engineering tool to predict small- and large-crack-growth rate behavior under service loading, conditions. These mechanisms have also provided a rationale for developing, new, damage-tolerant materials. This review suggests that small-crack growth behavior should be viewed as typical behavior, whereas large-crack threshold behavior should be viewed as the anomaly. Small-crack theory has unified 'fatigue' and 'fracture mechanics' concepts; and has bridged the cap between safe-life and durability/damage-tolerance design concepts.

Newman, James C., Jr.↗

Fracture Analysis of Semi-Elliptical Surface Cracks in Ductile Materials

Accurate life assessment of structural components may require advanced life prediction criteria and methodologies. Structural components often exhibit several different types of defects, among the most prevalent being surface cracks. A semi-elliptical surface crack subjected to monotonic loading will exhibit stable crack growth until the crack has reached a critical size, at which the crack loses stability and fracture ensues (Newman, 2000). The shape and geometry of the flaw are among the most influential factors. When considering simpler crack configurations, such as a through-the-thickness crack, a three-dimensional (3D) geometry may be modeled under the approximation of two-dimensional (2D) plane stress or plane strain. The more complex surface crack is typically modeled numerically with the Finite Element Method (FEM). A semi-elliptical surface crack is illustrated in Figure 1-1.

Daniewicz, S. R.↗

NiAl-based Polyphase in situ Composites in the NiAl-Ta-X (X = Cr, Mo, or V) Systems

Polyphase in situ composites were generated by directional solidification of ternary eutectics. This work was performed to discover if a balance of properties could be produced by combining the NiAl-Laves phase and the NiAl-refractory metal phase eutectics. The systems investigated were the Ni-Al-Ta-X (X = Cr, Mo, or V) alloys. Ternary eutectics were found in each of these systems and the eutectic composition, temperature, and morphology were determined. The ternary eutectic systems examined were the NiAl-NiAlTa-(Mo, Ta), NiAl-(Cr, Al) NiTa-Cr, and the NiAl-NiAlTa-V systems. Each eutectic consists of NiAl, a C14 Laves phase, and a refractory metal phase. Directional solidification was performed by containerless processing techniques in a levitation zone refiner to minimize alloy contamination. Room temperature fracture toughness of these materials was determined by a four-point bend test. Preliminary creep behavior was determined by compression tests at elevated temperatures, 1100-l400 K. Of the ternary eutectics, the one in the NiAl-Ta-Cr system was found to be the most promising. The fracture toughness of the NiAl-(Cr, Al)NiTa-Cr eutectic was intermediate between the values of the NiAl-NiAlTa eutectic and the NiAl-Cr eutectic. The creep strength of this ternary eutectic was similar to or greater than that of the NiAl-Cr eutectic.

Johnson, D. R.↗

On-Orbit Glass Stress Measurement Tool Development

Exposed window surfaces on-orbit are vulnerable to a variety of damage including impacts. These impacts impart stress into the panes and reduce the remaining life of the window. Spacecraft windows are evaluated before and after flight to determine the minimum strength of the glass prior to launch. Currently, no method exists to accurately evaluate the windows on-orbit. An on-orbit optical system is under development to evaluate spacecraft windowpane material for remaining flight life by directly measuring the stress in the glass. This optical system builds on the industry-standard practice of calculating the amount of impact-induced stress through birefringence measurement. In industry, the birefringence is imaged through the pane with a detector and light source on opposite sides. On-orbit, there is only access to one side of the pane. This system has been designed to image birefringence by reflecting the light off the pane to a detector on the same side of the glass. Previous studies have shown a correlation between material stress distribution and the associated K-value. This system is designed to determine low strength areas which can be caused by defects due to impact damage. Glass samples will be imaged and broken in order to correlate impact-induced stress to the fracture strength of the material. Once this correlation is determined, a quantitative assessment of the stress areas in spacecraft windows will occur prior to and during mission operations to reliably determine the overall strength of the glass.

Max J Schneiderman↗

Mechanics of fracture - Fundamentals and some recent developments

An overview is presented of the fundamental aspects of and recent developments in fracture mechanics. Reference is made to linear elastic fracture mechanics including the state of stresses and displacements in the vicinity of cracks, effects of crack geometry and orientation on stress intensity factors, energy balance of Griffith, Irwin's stress intensity concept, and linear elastic fracture mechanics testing for fracture toughness. Other aspects of this paper include the non-linear behavior of materials and their influence on fracture mechanics parameters, consideration of viscoelasticity and plasticity, non-linear fracture toughness parameters as C.O.D., R-curve and J-integral, and a non-linear energy method, proposed by Liebowitz. Finite element methods applied to fracture mechanics problems are indicated. Also, consideration has been given to slow crack growth, dynamic effects on K(IC), Sih's criterion for fracture, Lee and Liebowitz's criterion relating crack growth with plastic energy, and applications of fracture mechanics to aircraft design. Suggestions are offered for future research efforts to be undertaken in fracture mechanics.

Liebowitz, H.↗

A unifying strain criterion for fracture of fibrous composite laminates

Fibrous composite materials, such as graphite/epoxy, are light, stiff, and strong. They have great potential for reducing weight in aircraft structures. However, for a realization of this potential, designers will have to know the fracture toughness of composite laminates in order to design damage tolerant structures. In connection with the development of an economical testing procedure, there is a great need for a single fracture toughness parameter which can be used to predict the stress-intensity factor (K(Q)) for all laminates of interest to the designer. Poe and Sova (1980) have derived a general fracture toughness parameter (Qc), which is a material constant. It defines the critical level of strains in the principal load-carryng plies. The present investigation is concerned with the calculation of values for the ratio of Qc and the ultimate tensile strain of the fibers. The obtained data indicate that this ratio is reasonably constant for layups which fail largely by self-similar crack extension.

Poe, C. C., Jr.↗

A proposed standard round compact specimen for plane strain fracture toughness testing

A round, disk-shaped specimen is proposed as a standard test specimen for addition to ASTM Test for Plane-Strain Fracture Toughness of Metallic Materials (E 399-78A). The specimen is diametrically cracked, and loaded in the same way as the existing standard compact specimen. Tests and analyses were performed to verify that the proposed round compact specimen and associated stress intensity factor K solution are appropriate for a standard plane strain fracture toughness test. The use of the round compact specimen for other fracture tests is described.

Underwood, J. H.↗

TRIDENT Drill Validation at Mars and Lunar Analog Field Sites

Drilling on Earth is typically a human-intensive activity. Drilling on other planets is further complicated by the lack of prior local field surveys of their target area, hence blindly drilling into uncertain target rocks. Field conditions on the Moon or Mars are also different than for shallow drilling on Earth: lower temperatures and pressures, less power available, low masses (hence less weight-on-bit). Given the cost of transport from Earth, no drilling muds or working fluids are likely to be available to carry away cuttings. And impact-gardened regolith and dust vary mechanically and texturally from most terrestrial soils. The Regolith and Ice Drill for Exploration of New Terrains (TRIDENT) is a rotary-percussive 1m-class drill from Honeybee Robotics. It is low-power (rotary and percussive actuators are 200 W each) and lightweight (<20 kg) with the maximum weight on bit limited to 200 N. TRIDENT has been manifested for the Volatiles Investigating Polar Exploration Rover (VIPER) and PRIME-1 lunar south pole missions in 2024, has previously been field tested at a hot, dry analog site in the Atacama Desert, and in lunar conditions in thermal vacuum chamber tests. TRIDENT was also part of the 2019 Icebreaker Mars Discovery proposal, as well as in the Mars Life Explorer concept. During ARADS tests, drill control and fault recovery automation software enabled hands-off operations of a rover-mounted TRIDENT drill. TRIDENT Drill Analog Site Validation: Past TRIDENT tests in thermal vacuum (TVAC) chambers targeted containers of manufactured lunar simulants with added volatiles. 2022 TRIDENT ambient testing at NASA Ames drilled into cemented lunar simulant materials. Low cuttings-permeability led to cuttings buildup, and drill choking and binding was observed. The Atacama analog site in ARADS had desiccated unconsolidated sediments that did not challenge the TRIDENT design. However, lunar polar regolith is expected to be diverse and heterogeneous with varying clast sizes, with abundant impactites and perhaps subsurface ice deposits. Neither the simulants nor Atacama testing had completely covered the TRIDENT-targeted field characteristics, motivating further analog tests prior to the planned lunar missions. To gain more insight into the behavior of the TRIDENT hardware in diverse impactites and subsurface ice, and to verify the software automation in that environment, in August 2023 TRIDENT was brought to Haughton Crater, a field analog site in the Canadian Arctic. In September 2023 the same drill was brought to the Bishop Tuff in southern California to verify whether drilling binding behaviors previously seen in lunar simulant testing would be observed in naturally occurring fine-grained massive layers. The ~22 Ma Haughton Crater impact structure is located at 75 ̊22’ N, 89 ̊41’ W, on northwestern Devon Island, Nunavut, Canada. Numerous deposits of pale-grey crater-fill polymictic impact-melt breccia are found within the crater with a typical thickness reaching ~125 m or greater and covering ~60 km -2 . An approximately 600m-thick permafrost layer is also present with ice typically found within 0.5-0.6m of the surface. The volcanic tableland north of Bishop, CA exposes densely welded tuff laid down during the eruption that created the Long Valley Caldera at approximately 0.76 Ma. Extensional faults and the Owens River gorge expose cross-sections across the plateau. The area is viewed as an analog site for Mars features believed to be of pyroclastic origin. Results: Haughton Crater.Drilling tests were conducted 8-13 August 2023 at a previously undisturbed area separated 5-10 m from past years’ Drill Hill test sites (75.4208, -089.7613). In six days, TRIDENT drilled 8 holes to nearly 1 m depth each, totaling 7.80 m. The active layer/ice boundary was at ~67 cm depth, with a total of approximately 2.4 m drilled into ice or ice-cemented impact breccia. During drilling, five drill fault states were observed and successfully recovered. Holes 23-1, 4 and 7 were drilled under manual control, using Honeybee’s Thorax user interface. Holes 23-5, 6, and 8 were drilled with the Ames IBexec automated drilling control software. TRIDENT was observed to have little difficulty in the thawed uncemented impact breccia above the active layer boundary, but required percussion to make slower headway in the ice-cemented breccia. In Hole 23-7 (Fig.1), drilling slowed down in a massive unit just above the active-layer boundary (perhaps a large rock extending into the ice-cementation?), with only 7cm progress made in 27 minutes of high auger torque and constant percussion, leading to a choking fault and then a binding fault. A similar pattern had been observed in TRIDENT Rio Tinto test data from 2017 [6] as well as in the 2022laboratory tests.Bishop Tuff.A team from NASA Ames and the US Geological Survey deployed the same TRIDENT drill to Bishop Sites 1B and 1C (37.4203, -118.4289; 37.4265, -118.4215) on 13-16 September 2023, on the Bishop Tuff plateau. A third drill site was used 17-18 September 2023(37.4598, -118.3667) in an abandoned pumice mine. Four holes (totaling 2.5m depth) were drilled into the fine-grained, meters-thick tuff units at Sites 1B and 1C, and a further two boreholes (totaling 1.98m depth) were made at the pumice site. Drill behavior in the tuff below 10 cm depth was similar to that seen at 65-74 cm depth in Haughton Hole 23-7 (Fig. 1) and that seen in the 2022 lab simulant drilling. Drill safety torque limits were exceeded multiple times resulting in drill stops downhole. These freezes then required external added torques (with a pipe wrench) to resume rotation, to unstick the drill for withdrawal. To prevent this choking and binding behavior we found that more-frequent cuttings removal was necessary, e.g., reducing the “drill bite” size from the nominal 10 cm to 2 cm per bite --bringing the auger up to the surface more frequently, as seen in Bishop Site 1C Hole 2 (Fig.2). This permitted slow progress without drill binding and without external interventions. Conversely, TRIDENT drilling in the more porous pumice target material showed no cuttings buildup issue, and single bites as large as 40 cm were demonstrated. Discussion: We observed that TRIDENT easily penetrated unconsolidated heterogeneous soils (both above the active layer boundary at Haughton and previously in the Atacama). Cemented or consolidated targets that were cuttings-permeable (icy impact breccia, pumice) required more energy applied and percussion. However, in non-cuttings-permeable targets (welded microporous tuff, cemented simulants, boulder) TRIDENT was observed to be prone to excessive cuttings accumulation leading to choking/binding faults and stalling. The wedge cutting bit, used by TRIDENT in field tests and in its flight versions, pulverizes the target rock and creates fine cuttings that ideally are transported up the auger spirals for removal. In porous, fractured or vesicular target materials (such as at the Bishop pumice site) a significant portion of the cuttings are pushed aside, but for non-fractured, microporous targets the cuttings remain in the borehole and accumulate. Rock powder is relatively incompressible as a working fluid at only 100-200N downward force (TRIDENT limits) and hence eventual drilling progress slows or stops. Our recommended strategy for improving TRIDENT cuttings removal in massive target units with low cuttings-permeability is to reduce TRIDENT bite sizes when encountering these units, from 10cm to as little as 1-2cm, to effectively bail the accumulating cuttings. This approach was demonstrated to reduce choking and allowed slow progress to continue in cuttings-impermeable microporous target units (viz. the Bishop tuff in our September 2023 tests or cemented simulants in 2022 ambient tests).

robotic drilling↗

A Method for Combining Experimentation and Molecular Dynamics Simulation to Improve Cohesive Zone Models for Metallic Microstructures

Fracture processes within a material begin at the nanometer length scale at which the formation, propagation, and interaction of fundamental damage mechanisms occur. Physics-based modeling of these atomic processes quickly becomes computationally intractable as the system size increases. Thus, a multiscale modeling method, based on the aggregation of fundamental damage processes occurring at the nanoscale within a cohesive zone model, is under development and will enable computationally feasible and physically meaningful microscale fracture simulation in polycrystalline metals. This method employs atomistic simulation to provide an optimization loop with an initial prediction of a cohesive zone model (CZM). This initial CZM is then applied at the crack front region within a finite element model. The optimization procedure iterates upon the CZM until the finite element model acceptably reproduces the near-crack-front displacement fields obtained from experimental observation. With this approach, a comparison can be made between the original CZM predicted by atomistic simulation and the converged CZM that is based on experimental observation. Comparison of the two CZMs gives insight into how atomistic simulation scales.

Hochhalter, J. D.↗