Nanocomposites based on thermoplastic elastomers with functional basis of nano titanium dioxide

Nanocomposites based on a thermoplastic elastomer (TPE) (low-density polyethylene (LDPE) and 1,2-polybutadiene in a ratio of 60/40) with functional titanium dioxide nanoparticles of different nature, TiO{sub 2}/TPE, have been prepared and investigated by a complex of methods (X-ray diffraction analysis using X-ray and synchrotron radiation beams, scanning electron microscopy, transmission electron microscopy, and X-ray energy-dispersive spectroscopy). The morphology of the composites is found to be somewhat different, depending on the TiO{sub 2} characteristics. It is revealed that nanocomposites with cellular or porous structures containing nano-TiO{sub 2} aggregates with a large specific surface and large sizes of crystallites and nanoparticles exhibit the best deformation‒strength and fatigue properties and stability to the effect of active media under conditions of ozone and vapor‒air aging.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Experimental evaluation of low-pass shock isolation performance of elastomers using frequency-based Kolsky bar analyses

Elastomeric materials are used as shock isolation materials in a variety of environments to dampen vibrations and/or absorb energy from external impact to minimize energy transfer between two objects or bodies. Some applications require the shock isolation materials to behave as a low-pass mechanical filter to mitigate the shock/impact at high frequencies but transmit the energy at low frequencies with minimal attenuation. To fulfill this requirement, a shock isolation material needs to be carefully evaluated and selected with proper experimental design, procedures, and analyses. In this study, a Kolsky bar was modified with precompression (up to 15.5 kN) and confinement capabilities to evaluate low-pass shock isolation performance in terms of acceleration attenuation through a variety of elastomers. Also investigated were the effects of preload and specimen geometry on the low-pass shock isolation response.

36 MATERIALS SCIENCE↗

Effect of Filler Concentration on Thermal Stability of Vinyl Copolymer Elastomer (VCE) Composites

To study the thermal stability of vinyl copolymer elastomer (VCE) in its composite form, systematic TGA characterizations were conducted in both nonisothermal and isothermal modes. The effects of filler concentration on the aging behaviors of the VCE/filler composites were investigated under nitroplasticizer (NP) environment. FTIR characterization was used to probe the structural changes in the VCE polymer before and after the thermal treatments. This study suggests that the filler concentration significantly deteriorates the thermal stability of NP at a moderate temperature (< 70 °C). The degradation of NP, in turn, accelerates the aging process of the VCE polymer in its composite form.

36 MATERIALS SCIENCE↗

Performance of Bolted Closure Joint Elastomers Under Cask Aging Conditions

The bolted closure joint of a bare spent fuel cask is susceptible to age-related degradation and potential loss of confinement function under long-term storage conditions. Elastomeric seals, a component of the joint typically used to facilitate leak testing of the primary seal that includes the metallic seal and bolting, is susceptible to degradation over time by several mechanisms, principally via thermo-oxidation, stress-relaxation, and radiolytic degradation under time and temperature condition. Irradiation and thermal exposure testing and evaluation of an ethylene-propylene diene monomer (EPDM) elastomeric seal material similar to that used in the CASTOR® V/21 cask for a matrix of temperature and radiation exposure conditions relevant to the cask extended storage conditions, and development of semiempirical predictive models for loss of sealing force is in progress. A special insert was developed to allow Compressive Stress Relaxation (CSR) measurements before and after the irradiation and/or thermal exposure without unloading the elastomer. A condition of the loss of sealing force for the onset of leakage was suggested. The experimentation and modeling being performed could enable acquisition of extensive coupled aging data as well as an estimation of the timeframe when loss of sealing function under aging (temperature/radiation) conditions may occur.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Radiation-induced aging of PDMS Elastomer TR-55: a summary of constitutive, mesoscale, and population-based models

Filled and cross-linked elastomeric rubbers are versatile network materials with a multitude of applications ranging from artificial organs and biomedical devices to cushions, coatings, adhesives, interconnects, and seismic-isolation-, thermal-, and electrical barriers. External factors like mechanical stress, temperature fluctuations, or radiation are known to create chemical changes in such materials that can directly affect the molecular weight distribution (MWD) of the polymer between cross-links and alter the structural and mechanical properties. From a Materials Science point of view it is highly desirable to understand, effect, and manipulate such property changes in a controlled manner. In this report we summarize our modeling efforts on a polysiloxane elastomer TR-55, which is an important component in several of our systems, and representative of a wide class of filled rubber materials. The primary aging driver in this work has been γ-radiation, and a variety of modeling approaches have been employed, including constitutive, mesoscale, and population-based models. The work utilizes diverse experimental data, including mechanical stress-strain and compression set measurements, as well as MWD measurements using multiquantum NMR.

36 MATERIALS SCIENCE↗

A Modulated Differential Scanning Calorimetry Method for Characterization of Poly(ester urethane) Elastomer

A systematic series of experiments is presented utilizing MDSC to resolve the overlapping melt peaks found when analyzing poly(ester urethane) block copolymer elastomer by MDSC. Testing method parameters are idealized through diagnostic methods, leading to method parameters individualized to the material, which allow to optimize the MDSC method for the poly(ester urethane) characterization despite potentially problematic sample geometry. This is the second in a series of three reports on the degradation processes and physical properties of the materials used in polymer bonded explosive 9501.

36 MATERIALS SCIENCE↗

Evaluation of High Temperature Elastomers for Geothermal Wells

This report describes the extension of a performance screening study of elastomers for geothermal well applications. Elastomeric O-rings were subjected to compression while submerged in water at elevated temperatures and pressure to determine performance under more aggressive conditions. Following the experiment, the elastic moduli of the O-ring cross-sections were assessed for any changes which may affect O-ring function down-hole. All materials showed susceptibility to thermo-oxidative degradation at high temperatures and pressures. Type I FKM had the least amount of compression set of all materials tested at 150ºC while Kalrez FFKM O-rings had the least amount of edge hardening of all materials, regardless of aging temperature. Prior visual observation of materials aged in simulated environments revealed an unusual trend with EPDM and FEPM materials: the degradation and disintegration of these polymers in an oxidative thermal cycle environment, but the ability to maintain mechanical performance and shape during oxidative thermal cycling in the presence of steam. EPDM and FEPM were subjected to additional testing at SNL in order to better understand this aging anomaly. No abnormalities were observed in the chemical (oxidation rates, FTIR spectra, solvent uptake, gel content, and weight loss vs. temperature) or physical (modulus profiles) measurements that could explain the visually observed aging differences. SNL validated this observation through a secondary controlled aging test using only EPDM, where, once again, it was shown that thermo-oxidative conditions appear to cause more degradative damage (enhanced embrittlement) than did thermo-oxidative coupled with hydrolytic environments. From these data we conclude that water may favorably interfere with normal thermo-oxidative degradation processes via some type of inhibition pathway which has yet to be identified.

15 GEOTHERMAL ENERGY↗

Thermal Degradation Investigation of Polyurethane Elastomers using Thermal Gravimetric Analysis - Gas Chromatography/Mass Spectrometry

The thermal degradation of two polyurethane elastomers was investigated via thermal gravimetric analysis coupled with gas chromatography/ma ss spectrometry. Decomposition occur s in a multi - step fashion with similar onset temperatures for both materials. Apparent activation energy plots were calculated inside Model - Free Kinetics software and utilized to construct conversion and isothermal conversion tables . These tables predicted material degradation as a function of temperature and time. Isothermal experiments were performed and found to be in good agreement with the predictions made from the Model - Free Kinetic s software package. Volatile products evolved during the multistep decomposition were captured at various times and analyzed using the coupled gas chromatography/mass spectrometry system . This analysis demonstrated strong correlation between the degradation products and known decomposition mechanisms for polyurethanes.

36 MATERIALS SCIENCE↗

Silicone Elastomers with Novel Modified Filler for Increased Radiation Resistance

Radiation induced chemical aging behavior in filled silicone elastomers results in a decreased mechanical performance over time. This report describes chemical methodologies to reduce radiation aging via a surfacemodified filler. Four different modified fillers were incorporated into a silicone polymer matrix and subjected to accelerated radiation aging. Fillers modified with aryl group such as phenyl, styrl, and napthyl functionality should improve the radiation aging behavior of the composite material. A series of analytical methodologies were applied to determine the efficacy of the modified filler approach as a mitigation strategy for radiation damage. The results support that phenyl and napthyl modified fillers mitigated radiation damage when compared to control samples and samples with hexyl (non-aryl) modified filler.

36 MATERIALS SCIENCE↗

Challenges of accelerated aging techniques for elastomer lifetime predictions

Elastomers are often degraded when exposed to air or high humidity for extended times (years to decades). Lifetime estimates normally involve extrapolating accelerated aging results made at higher than ambient environments. Several potential problems associated with such studies are reviewed, and experimental and theoretical methods to address them are provided. The importance of verifying time–temperature superposition of degradation data is emphasized as evidence that the overall nature of the degradation process remains unchanged versus acceleration temperature. The confounding effects that occur when diffusion-limited oxidation (DLO) contributes under accelerated conditions are described, and it is shown that the DLO magnitude can be modeled by measurements or estimates of the oxygen permeability coefficient (P Ox ) and oxygen consumption rate (Φ). P Ox and Φ measurements can be influenced by DLO, and it is demonstrated how confident values can be derived. In addition, several experimental profiling techniques that screen for DLO effects are discussed. Values of Φ taken from high temperature to temperatures approaching ambient can be used to more confidently extrapolate accelerated aging results for air-aged materials, and many studies now show that Arrhenius extrapolations bend to lower activation energies as aging temperatures are lowered. Furthermore, best approaches for accelerated aging extrapolations of humidity-exposed materials are also offered.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Extensometer automatically measures elongation in elastomers

Extensometer, with a calibrated shaft, measures the elongation of elastomers and automatically records this distance on a chart. It is adaptable to almost any tensile testing machine and is fabricated at a relatively low cost.

Hooper, C. D.↗

Silazane elastomer remains resilient at 400 deg C

Smooth, unfoamed elastomer is unaffected by common acids, alkalies, and organic solvents. Its thermal stability, chemical resistance, and physical properties make it of interest for various applications.

Source record↗