Tribological behavior of few-nanometer-thick MoS2 prepared by low-temperature conversion of atomic layer deposited MoOx films
Not Available
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Not Available
Growing concerns over energy and environmental sustainability have lately sparked worldwide interest in more efficient and cleaner transportation systems and industrial activities. Friction roughly consumes one-fifth of all energy used worldwide. One-third of all energy used in transportation goes to overcome friction. At the same time, the fruits of decades of dedicated research on all-electric vehicles powered by advanced batteries are paving the way toward a much cleaner and sustainable transportation future. In this article, we provide a short overview of what are the energy efficiency and environmental impacts of current transportation, industrial, and residential systems and how much of that efficiency is adversely affected by friction and wear losses in moving mechanical parts and components. We also touch upon recent advances in new materials, lubricants, and design changes that could reduce energy losses by 18–40%, mainly resulting from friction and wear. The savings would be up to 8.7% of the total global energy use and 1.4% of the gross national products (GNP). Finally, we calculate the energy consumption and friction losses in battery-powered electric passenger cars and show the benefit of electric cars where the total energy use is in average 3.4 times lower compared to combustion engine powered cars. The CO 2 emissions are 4.5 times higher for a combustion engine car compared to an electric car when the electricity comes from renewable energy sources. Moving from fossil to renewable energy sources may cut down the energy losses due to friction in energy production by more than 60%.
Sliding friction and wear characteristics of aluminum alloys against AISI 52100 steel lubricated by ionic liquids (ILs) were investigated at both room and elevated temperatures. The tested aluminum alloys include a commercially pure aluminum Al 1100, a wrought alloy Al 6061-T6511, and a cast alloy Al 319-T6. The lubricating performance of two ILs with the same anion, one ammonium-based [C8H17]3NH.Tf2N and one imidazolium-based C10mim.Tf2N, were compared each other and benchmarked against that of a conventional fully-formulated engine oil. Significant friction (up to 35%) and wear (up to 55%) reductions were achieved by the ammonium IL when lubricating the three aluminum alloys compared to the engine oil. The imidazolium IL performed better than the oil but not as well as the ammonium IL for Al 1100 and 319 alloys. However, accelerated wear was unexpectedly observed for Al 6061 alloy when lubricated by C10mim.Tf2N. Surface chemical analyses implied complex tribochemical reactions between the aluminum surfaces and ILs during the wear testing, which has been demonstrated either beneficial by forming a protective boundary film or detrimental by causing severe tribo-corrosion. The effects of the IL cation structure, aluminum alloy composition, and tribo-testing condition on the friction and wear results have been discussed.
Abstract not provided
This paper describes the friction and wear behavior of a Co–Cr alloy sliding on a Ta–W alloy. Measurements were performed in a pin-on-flat configuration with a hemispherically tipped Co-base alloy pin sliding on a Ta–W alloy flat from ambient to 430°C. Focused ion beam-scanning electron microscopy (FIB-SEM) and cross-sectional transmission electron microscopy (TEM) were used to identify the friction-induced changes to the chemistry and crystal structure in the subsurface regions of wear tracks. During sliding contact, transfer of material varied as a function of the test temperature, either from pin-to-flat, flat-to-pin, or both, resulting in either wear loss and/or volume gain. Friction coefficients (μ) and wear rates also varied as a function of test temperature. The lowest friction coefficient (μ=0.25) and wear rate (1×10 –4 mm 3 /N•m) were observed at 430°C in argon atmosphere. This was attributed to the formation of a Co-base metal oxide layer (glaze), predominantly (Co, Cr)O with Rocksalt crystal structure, on the pin surface. Part of this oxide film transferred to the wear track on Ta–W, providing a self-mated oxide-on-oxide contact. Once the oxide glaze is formed, it is able to provide friction reduction for the entire temperature range of this study, ambient to 430°C. Furthermore, the results of this study indicate that glazing the surfaces of Haynes alloys with continuous layers of cobalt chrome oxide prior to wear could protect the cladded surfaces from damage.
Not Available
This paper presents an experimental study of friction and wear performance of quaternary CrSiCN coatings deposited on a hardened H-13 steel substrate by a plasma enhanced magnetron sputtering (PEMS) technique. Friction and wear tests were conducted with a reciprocating line contact between a hardened 4370 steel roller and coated and uncoated flat specimens under dry and lubricated conditions. The effects of coating thickness (1, 3.5 and 7.5 μm) on the mechanical properties, friction and wear performance were also assessed. In dry sliding, the friction of coated surfaces was about the same as for uncoated surfaces, except for the 1-μm coating, which had higher friction. Friction for coated surfaces under lubricated contact was in general higher than for uncoated surfaces. There was no measurable wear on any of the coated surfaces, under either dry or lubricated conditions. However, wear was higher on the steel roller counterface sliding against the coated surfaces, with the amount of wear proportional to the mating coating thickness. The effectiveness of formulated lubricant additives was also modified by the coating, resulting in major effects on friction and wear behavior. Finally, this reduction in lubricant additive efficacy is due to the fact that the additives were designed and optimized for ferrous surfaces.
Mathematical models suggest that the strain along the film formed by parallel passes of a nanoindentation probe in contact with the film can be either homogenous or heterogeneous, depending on contact pressure and spacing between passes. Here, in this study, a 1 µm copper thin film was worn with a cono-spherical diamond probe with normal loads ranging from 25 to 800 µN and wear box edge lengths of 40, 60, and 80 µm. The nanoindenter counterface was rastered across the surface to mimic dry sliding wear. To determine potential strain field changes, 10-step quasi-static indents (200–2000 µN) were performed using nanoindentation inside the wear boxes created at various loads to determine if a strain field alteration could be observed in changes in hardness of the copper thin film. It was shown that there was a softening effect in the hardness for normal loads < 400 µN used during nanowear compared to the as-deposited copper. Normal loads ≥ 400 µN had a similar or higher hardness than the as-deposited copper. This is believed to have occurred due to a relaxation in the residual stresses created during deposition in the copper thin films at lower loads, which caused a decrease in hardness. Conversely, at the higher loads, increased deformation leads to an increase in hardness. Lastly, all of the wear boxes displayed a higher estimated strain hardening exponent than the as-deposited material.
Anti-wear additives (AWs), like zinc dialkyldithiophosphates (ZDDPs), have been used in lubricants for more than a half-century, and more effective candidate AWs, like oil-soluble ionic liquids (ILs), are emerging. However, there is a lack of fundamental understanding of how the AW concentration impacts the tribochemical activities at the contact interface. This study systematically investigated the friction and wear behavior in correlation to the tribofilm morphology and composition as a function of the concentration of a ZDDP, a phosphonium-alkylphosphate IL, and an IL+ZDDP combination. The ZDDP concentration rising from 0.4 to 6.4 wt% caused a proportionally increased friction coefficient, which was well correlated to a thicker, rougher, and more brittle tribofilm. This was further understood by the decreasing phosphates but increasing sulfur compounds in the ZDDP tribofilm. In contrast, the IL and IL+ZDDP maintained a low and stable friction coefficient at 0.5 wt% or above. There was no sulfur in the IL tribofilm, and the sulfur compounds were maintained at a low level in the tribofilm for IL+ZDDP even at high concentrations. Results suggested minimizing the sulfur content in the tribofilm would be an effective way to control the friction. An interesting V-shape relationship between the AW concentration and the wear loss was observed for both the IL-containing AWs, with an optimum at 2 wt% for the IL alone and 0.46–0.92 wt% for the IL+ZDDP, respectively. A unique heat map was created using the phosphorus binding energy distribution to reveal the phosphate polymerization at different depths of the tribofilms, which provided additional insight for the tribofilm evolution.
Here, this research investigates the feasibility of hybrid aluminum metal matrix composites (MMC) incorporating TiB 2 particles for brake rotor applications. The composites were produced by incorporating both in-situ, submicron-sized TiB 2 particles and regular micron-sized TiB 2 powders via stir and squeeze casting techniques into A206 aluminum alloy matrix. Systematic adjustments in the fractions of in-situ and ex-situ TiB 2 particles were conducted to evaluate their impact on wear behavior and mechanisms. Combination of both particle types allowed composites with up to 10 vol% of reinforcements. Composites with higher proportions of ex-situ particles demonstrated increased wear resistance compared to those solely composed of in-situ particles, control specimens without TiB 2 , and conventional cast iron counterparts. The lowest wear rate for the hybrid composites sliding against phenolic brake pads was 1.1 × 10 -5 mm 3 /Nm, signifying a 3-fold reduction relative to cast iron sliding against the same pads. Wear analysis elucidated distinctive mechanisms within the hybrid composites, characterized by mild fragmented abrasive wear, adhesive wear, and plastic deformation, accompanied by the formation of an intermixed tribo-oxide layer.
Not Available
Deposition of molybdenum disulfide (MoS 2 ) coatings using physical vapor deposition (PVD) and mechanical burnishing has been widely assessed for solid lubricants in space applications but still suffers from line-of-sight constraints on complex geometries. Here, we highlight one of the first demonstrations of electrodeposited Mo x S y O z and Mo x S y O z /Ni thin-film coatings from aqueous solutions of ammonium tetrathiomolybdate for solid lubricant applications and their remarkable ability to provide low coefficients of friction and high wear resistance. Characterization of the coating morphology shows amorphous microstructures with a high oxygen content and cracking upon drying. Even so, electrodeposited Mo x S y O z can achieve low steady-state coefficients of friction (μ ∼ 0.05–0.06) and wear rates (2.6 × 10 –7 mm 3 /(N m)) approaching those of physical vapor deposited coatings (2.3 × 10 –7 mm 3 /(N m)). Additionally, we show that adding dopants such as nickel increased the wear rate (7.5 × 10 –7 mm 3 /(N m)) and initial coefficient of friction (μ i = 0.23) due to compositional modifications such as dramatic sub-stoichiometry (S/Mo ∼ 1) and expression of a NiO x surface layer, although doping did reduce the degree of cracking upon drying.
Not Available