At least 307 records · Page 17

High-temperature oxidation and quenching of chromium-coated zirconium alloy ATF cladding tubes with and w/o pre-damage

Chromium-coated zirconium alloys are one of the promising candidates for accident-tolerant fuel cladding (ATF) tubes for light water reactors (LWRs). In this study, the high temperature oxidation and degradation of two types of Cr coatings (cold spray and physical vapor deposition) with and without pre-damage by scratches were investigated on prototype rod segment samples filled with ZrO 2 pellets and tightly sealed with welded end caps. Isothermal tests at 1100 and 1200 °C were terminated by quenching with water; transient tests were performed up to 1500–1600 °C until complete coating failure. The positive effect of both types of Cr coatings was observed in all tests. Pre-damaged specimens showed only locally increased oxidation of the scratched zone, but no negative effects on the adjacent Cr coating. Finally, the behavior of the two types of coatings is compared and the degradation mechanisms are discussed based on hydrogen release data, extensive metallographic post-test examinations, and the current state of global research.

36 MATERIALS SCIENCE↗

Synergies between H, He and radiation damage in dual and triple ion irradiation of candidate fusion blanket materials

Three ferritic/martensitic alloys were studied to understand the synergistic effect between single ion beam (Fe 2+ ), dual ion beam (Fe 2+ +He 2+ and Fe 2+ +H + ), and triple ion beam (Fe 2+ +He 2+ +H + ) irradiations on cavity evolution. A commercial alloy, F82H, a castable nanostructured alloy, CNA3, and a high purity model alloy, Fe8Cr2W, were irradiated at 400°C to 600°C to a damage level of 50 dpa at a damage rate of 1 × 10 –3 dpa/s with He and H injection rates of 10 and 40 appm/dpa, respectively. Post-irradiation characterization via bright field transmission electron microscopy and high-angle annular dark-field scanning transmission electron microscopy was performed on all irradiated conditions to characterize the cavity size distribution and determine the effects of H/He injection on cavity microstructure. In all three alloys, hydrogen co-injection with helium resulted in an increased cavity number density and maximum cavity size, producing an increase in swelling over that from helium injection alone. Swelling in F82H appears to peak between 450°C and 500°C. At 600°C, swelling was minimal and cavities of high density and small size were confined to grain boundaries and dislocations while at 400°C, swelling is also low with a nearly homogeneous, high density, distribution of very small cavities throughout. Swelling was least in the commercial alloy F82H due to the high sink strength. The CNA3 alloy underwent dissolution of precipitates that lowered the sink strength and resulted in higher swelling than F82H, but less than the model alloy. Electron energy loss spectroscopy (EELS) elemental mapping revealed hydrogen forming a halo-like structure about the periphery of the cavities and helium residing within the cavities themselves. Finally, this observation suggests that hydrogen reduces the surface energy of helium-filled cavities which results in both increased cavity number density and cavity size in triple beam irradiation over dual beam irradiation.

36 MATERIALS SCIENCE↗

Intense cyclic heating effects on thermo-fracture and thermal shock of solid tungsten and open-cell tungsten foam

Here we investigate here the effects of transient (cyclic) arc-jet plasma and laser heating on fracture behavior of W-foam and solid tungsten. The two key parameters that control the foam thermomechanical response are its density and mean cell size expressed in Pores Per Inch (PPI). Tungsten foam samples were fabricated with Chemical Vapor Deposition (CVD) with variety of PPI and relative density. These were tested under two types of qualitatively different conditions: (1) high-enthalpy arc-jet, and (2) high-power cyclic laser heating. None of the foam samples showed macroscopic through-thickness cracks. However, distributed micro-cracks were observed on ligaments and their triple junctions. Under the same loading conditions, W-foam and solid tungsten showed similar crack network pattern and characteristic length-scale. However, Crack Opening Displacement (COD) was twice as large in solid W as compared to W-foam. Foam samples that have been previously exposed to a low-pressure helium plasma showed significant changes in their surface forming nano-texture fuzz which was removed by subsequent testing in the arc-jet. Extensive fracture and re-crystallization were observed in the thin solid W disk that was fully-constrained from expansion. Thicker and fully-constrained solid W disks did not display recrystallization, grain growth, and extensive cracking. However, thicker disks that were free to expand showed some recrystallization and extensive through-thickness cracks due to less effective cooling and thus higher temperatures. Laser beam testing showed no visible damage formation at 0.19 GW/m 2 and 0.38 GW/m 2 for both low-density (23%) and high-density (43%) foams at low pulses (100-1000). Micro-cracks were observed after 10,000 pulses at 0.19 GW/m 2 in both foams, and in low-density foam after 100,000 at 0.38 GW/m 2 . The nature of thermomechanical damage in W-foam exposed to extreme power (GW/m 2 ) short-duration laser pulses was found to be qualitatively similar to that of high power (MW/m 2 ) long-duration arc-jet.

36 MATERIALS SCIENCE↗

Corrosion behavior of a series of combinatorial physical vapor deposition coatings on SiC in a simulated boiling water reactor environment

Here, the simulated boiling water condition corrosion properties of multilayer and combinatorial physical vapor deposition metal coatings (Zr, Cr, and/or Ti) deposited on a SiC f -SiC composite were investigated. Various compositions within the ternary system were corroded to the most suitable composition preventing underlying SiC f -SiC from further attack. Mass measurements and visual observations were conducted to identify which coatings formed protective oxides and which coatings spalled. Transmission electron microscopy was conducted to observe the microstructure of the physical vapor deposition metal layer before and after corrosion as well as identify the oxide which were forming.

36 MATERIALS SCIENCE↗

Hydrogen trapping energetics at BCC iron-helium interfaces

Density functional theory (DFT) calculations have been performed to assess the trapping and segregation strength of hydrogen (H) to helium (He) interfaces in BCC (Fe) as a function of He density and surface orientation. The He density ranges from 0 to 2 He/V which corresponds to equilibrium bubbles that are expected to form in the structural components in a fusion reactor environment. The DFT calculations consist of a slab of BCC metal and an initial lattice of FCC He. Here, the report on the binding energy of H to these interfaces as well as the migration barriers into and away from the surface, which together provide information on the de-trapping energy for H at He bubbles. It was found that the binding energy of H to He-Fe interfaces decreases with increasing He density. Migration barriers are also modified due to the He density, which are sensitive to the surface orientation as well as the diffusion pathway. These results provide valuable first-principles energetics that are necessary for higher-order, mesoscale models, and provide insight into the extent to which He bubbles may trap tritium in fusion structural materials.

42 ENGINEERING↗

A fusion relevant data-driven engineering void swelling model for 9Cr tempered martensitic steels

The UCSB database on cavity evolution in 9-12Cr tempered martensitic steels (TMS), includes the results for both dual heavy and helium ion (DII), and High Flux Isotope Reactor (HFIR) in situ helium injection (ISHI) neutron irradiations at 500°C. These results were combined with literature single ion and fission neutron irradiation data to derive a model for the void volume fraction, f v , as a function of displacements per atom (dpa) and transmutant helium concentrations in atomic parts per million (appm). The scientific foundation for the paper is described in a companion paper entitled “Cavity Evolution and Void Swelling in Dual Ion Irradiated Tempered Martensitic Steels”. Here, in this study, we show that f v (dpa, He/dpa) is described by the incubation dose, dpa i , for the onset of void growth, and the post-incubation growth rate, f v ’(%/dpa). Both dpa i and f v ’ decrease with increasing He/dpa at > ~ 5. The dpa i is also lower for the ISHI neutron irradiations at the same He/dpa. Single heavy ion and fission reactor neutron irradiations, with low He/dpa ratios, have a much larger dpa i . Based on a combined analysis of DII, single ion, ISHI and fission neutron data, we further show that the post-incubation f v data analyzed here have a common empirical curve shape, with f v ’ reaching up to ~ 0.2%/dpa at very high dpa. We also show that f v ’ can be predicted based on a physical model of defect partitioning between evolving sinks. At 500°C and fusion relevant He/dpa ≈ 10, the best-fit model predicts nominal swelling, S = f v /(1-f v ), of ~ 1.1, 4.9 and 16% at 50, 100 and 200 dpa, respectively. The physically motivated, data-driven model includes estimated uncertainties for both dpa i and f v ’.

36 MATERIALS SCIENCE↗

A quantitative method to determine the region not influenced by injected interstitial and surface effects during void swelling in ion-irradiated metals

We propose and demonstrate a microstructurally-based experimental method to quantitively determine the depth regions in self-ion-irradiated metals that are affected by the injected interstitial effect and various surface effects, focusing on the choice of safe analysis zones to minimize the impact of these phenomena. The goal is to define the depth ranges where extracted data can be confidently applied to ion-neutron correlations for reactor application. Since ion energies in the range of 1–5 MeV are most frequently employed by the radiation effects community, irradiations were conducted at four energies in this range, all proceeding at 475 °C. The experiment was conducted on relatively pure single crystal iron to focus only on physical phenomena, avoiding the influence of possibly confounding chemical or segregation processes. Care was also taken to minimize the influence of other physical factors such as crystalline orientation. It was shown that, at 475 °C, ion energies of ≤1 MeV were too shallow in penetration and did not yield a safe depth range, but irradiations at 2.5 MeV and above yielded useful safe zones with predicted swelling behavior becoming independent of ion energy. The surface-affected zone width was found to be roughly twice that of the void-denuded zone width and to be independent of accumulated displacement dose. The largest injected-interstitial effect arises from the injected interstitial depression of void nucleation and growth. The interstitial-affected region starts at about one half of the projected range and does not show any “spreading” of its influence in depth as the peak damage level increases from 50 to 100 dpa. This study provides some confidence that enhances the credibility of ion simulation when applied to prediction of void swelling in neutron environments.

36 MATERIALS SCIENCE↗

Cavity evolution and void swelling in dual ion irradiated tempered martensitic steels

Microstructural evolutions in two variants of the F82H 8 wt%Cr tempered martensitic steel under dual (He + plus Fe 3+ ) ion irradiations at 500 °C have been characterized by transmission electron microscopy. Emphasis is on understanding the combined effects of displacements per atom (dpa) and the helium/dpa ratio (He/dpa) on cavity evolution and void swelling (f v ). The dual ion database includes 231 alloy-dpa-He/dpa conditions for irradiations up to ~ 82 dpa and 3700 appm helium. Here, we hypothesize that the large “scatter” observed in the f v data is primarily due to local microstructural variations, especially those that shield regions at shallower depths from the effects of injected interstitial atoms, which would otherwise reduce f v . More generally, our hypothesis is that the highest f v data, at a specified dpa and He/dpa, provides the most appropriate estimate of swelling for fusion neutron irradiation conditions. The dose dependence of f v can be described by an incubation dpa i , marking the onset of significant void growth, and a post-incubation swelling rate, f v ’ = Δf v /Δdpa. Both dpa i and f v ’ decrease with increasing He/dpa. The f v ’ data are quantitatively consistent with a simple model for defect partitioning between evolving bubble, void, and dislocation sinks strengths and biases. Most notably, the model correctly predicts both the incubation dpa i , and the subsequent f v ’, in spite of the fact that they reflect somewhat different physics. Our analysis also suggests that defect recombination is modest at 500 °C. Along with other considerations, this supports the hypothesis that, even at high dpa rates, dual ion irradiations can be used to reasonably emulate void nucleation and growth for a range of fusion-relevant neutron irradiation service conditions. A companion paper incorporates the results of this study in a reduced-order, data-driven void swelling model.

36 MATERIALS SCIENCE↗

Development of hydrothermal corrosion model and BWR metal coating for CVD SiC in light water reactors

SiC/SiC fiber composites with CVD SiC overcoats are potential candidates for light water reactor advanced accident tolerant cladding materials. Understanding its corrosion kinetics in Light Water Reactor (LWR) conditions is essential to evaluate the concept's viability. Existing models only account for the temperature and oxygen concentration effect on the hydrothermal corrosion behavior applicable to LWR operating conditions. However, the development of a general corrosion rate for CVD SiC that accounts for the impact of irradiated microstructure, flow rate, electrical resistivity, pH, and surface roughness is critical for the practical realization of SiC/SiC-based cladding concepts. After a rigorous experimental campaign, this work updates the existing hydrothermal corrosion model to predict hydrothermal corrosion in LWRs. Numerical radiation and coolant chemistry analysis for LWRs conducted based on the updated corrosion kinetic models suggests that CVD SiC is likely a viable environmental barrier coating for Pressurized Water Reactors while questionable for Boiling Water Reactors (BWR) when the effect of irradiation damage on SiC corrosion is considered. An effective mitigation strategy for the double-layer metal coating is proposed for BWR applications. The double-layer metal coating comprising a FeCrAl overcoat with an intermediate Cr bond coating was observed to provide a stable protective barrier against SiC dissolution in BWR conditions. Finally, the proposed metal coating was also fully adherent following quench and burst tests.

36 MATERIALS SCIENCE↗