Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “MOLYBDATES”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 307 records · Page 17

Spectral properties of Tm{sup 3+}:NaGd(MoO{sub 4}){sub 2} crystal

The Tm{sup 3+}:NaGd(MoO{sub 4}){sub 2} crystal with dimensions of {phi} 15 x 38 mm{sup 2} was grown by Czochralski method. Polarized absorption and fluorescence spectra at room temperature were investigated. The absorption bands attributed to {sup 3}H{sub 6} {yields} {sup 3}H{sub 4} transition have large absorption cross-sections, which are 3.99 x 10{sup -20} and 2.36 x 10{sup -20} cm{sup 2} for {sigma}- and {pi}-polarization, respectively. The emission bands corresponding to the {sup 3}H{sub 4} {yields} {sup 3}H{sub 6} transition are strong and broad with emission cross-sections of 1.33 x 10{sup -20} and 1.20 x 10{sup -20} cm{sup 2} for {sigma}- and {pi}-polarization, respectively. The correlative full widths at half maximum are 35 nm for {sigma}-polarization and 36 nm for {pi}-polarization. The fluorescence lifetime for the {sup 3}H{sub 4} {yields} {sup 3}F{sub 4} transition is 146 {mu}s and the luminescent quantum efficiency is 76.8%.

36 MATERIALS SCIENCE↗

Synthesis and upconversion luminescence properties of Yb{sup 3+}/Er{sup 3+} codoped BaGd{sub 2}(MoO{sub 4}){sub 4} powder

Synthesis and upconversion luminescence properties of the new BaGd{sub 2}(MoO{sub 4}){sub 4}:Yb{sup 3+},Er{sup 3+} phosphor were reported in this paper. The phosphor powder was obtained by the traditional high temperature solid-state method, and its phase structure was characterized by the XRD pattern. Based on the upconversion luminescence properties studies, it is found that, under 980 nm semiconductor laser excitation, BaGd{sub 2}(MoO{sub 4}){sub 4}:Yb{sup 3+},Er{sup 3+} phosphor exhibits intense green upconversion luminescence, which is ascribed to {sup 2}H{sub 11/2} {yields} {sup 4}I{sub 15/2} and {sup 4}S{sub 3/2} {yields} {sup 4}I{sub 15/2} transition of Er{sup 3+}. While the observed much weaker red emission is due to the non-radiative relaxation process of {sup 4}S{sub 3/2} {yields} {sup 4}F{sub 9/2} and {sup 4}F{sub 9/2} {yields} {sup 4}I{sub 15/2} transition originating from the same Er{sup 3+}. The concentration quenching effects for both Yb{sup 3+} and Er{sup 3+} were found, and the optimum doping concentrations of 0.5 mol% Yb{sup 3+} and 0.08 mol% Er{sup 3+} in the new BaGd{sub 2}(MoO{sub 4}){sub 4} Gd{sup 3+} host were established.

36 MATERIALS SCIENCE↗

New red phosphor for near-ultraviolet light-emitting diodes with high color-purity

New red phosphors, Na{sub 5}Eu(MoO{sub 4}){sub 4} doped with boron oxide were prepared by the solid-state reaction. Their structure and photo-luminescent properties were investigated. With the introduction of boron oxide, the red emission intensity of the phosphors under 395 nm excitation is strengthened, with high color-purity (x = 0.673, y = 0.327). The single red light-emitting diode was obtained by combining InGaN chip with the red phosphor, bright red light can be observed by naked eyes from the red light-emitting diodes under a forward bias of 20 mA.

36 MATERIALS SCIENCE↗

Photoluminescence properties of NaGd(MoO{sub 4}){sub 2}:Eu{sup 3+} nanophosphors prepared by sol-gel method

NaGd(MoO{sub 4}){sub 2}:Eu{sup 3+} (hereafter NGM:Eu) phosphors have been prepared by sol-gel method. The properties of the resulting phosphors are characterized by X-ray diffraction (XRD), scanning electron microscope (SEM), photoluminescence (PL) spectra and decay curve. The excitation spectra of NGM:Eu phosphors are mainly attributed to O {yields} Mo charge-transfer (CT) band at about 282 nm and some sharp lines of Eu{sup 3+} f-f transitions in near-UV and visible regions with two strong peaks at 395 and 465 nm, respectively. Under the 395 and 465 nm excitation, intense red emission peaked at 616 nm corresponding to {sup 5}D{sub 0} {yields} {sup 7}F{sub 2} transition of Eu{sup 3+} are observed for 35 at.% NGM:Eu phosphors as the optimal doping concentration. The luminescence properties suggest that NGM:Eu phosphor may be regarded as a potential red phosphor candidate for near-UV and blue light-emitting diodes (LEDs).

36 MATERIALS SCIENCE↗

Solution combustion synthesis of {gamma}(L)-Bi{sub 2}MoO{sub 6} and photocatalytic activity under solar radiation

Highlights: {yields} Solution combustion technique was used to synthesize {gamma}(L)-Bi{sub 2}MoO{sub 6}. {yields} The material was in crystalline orthorhombic phase. {yields} High photocatalytic activity under solar radiation was observed. -- Abstract: The facile method of solution combustion was used to synthesize {gamma}(L)-Bi{sub 2}MoO{sub 6}. The material was crystallized in a purely crystalline orthorhombic phase with sizes varying from 300 to 500 nm. Because the band gap was 2.51 eV, the degradation of wide variety of cationic and anionic dyes was investigated under solar radiation. Despite the low surface area (<1 m{sup 2}/g) of the synthesized material, {gamma}(L)-Bi{sub 2}MoO{sub 6} showed high photocatalytic activity under solar radiation due to its electronic and morphological properties.

36 MATERIALS SCIENCE↗

Low temperature synthesis and photoluminescent properties of CaMoO{sub 4}:Eu{sup 3+} red phosphor with uniform micro-assemblies

Highlights: {yields} Synthesis of Eu{sup 3+}-doped CaMoO{sub 4} red phosphor via a facile hydrothermal method. {yields} The morphology of the materials was manipulated using different alkaline sources. {yields} Micro-structures were assembled by small nanostructures. {yields} Luminescent investigations confirmed that the Eu{sup 3+} ions have been effectively doped into the nanostructures. {yields} Schematic diagram for the energy transfer clearly reveals the photoluminescent mechanism. -- Abstract: Scheelite-type Eu{sup 3+}-doped CaMoO{sub 4} red phosphor with uniform micro-assemblies has been successfully synthesized via a facile hydrothermal method at 120 {sup o}C for 10 h. The Eu{sup 3+}-doped CaMoO{sub 4} microstructures were assembled by small nanostructures and the morphology of materials was found to be manipulated by dropping different alkalis into the stock solution for the first time. The structure, morphology, and luminescent property were characterized and investigated by techniques of X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), transmission electron microscopy (TEM), high-resolution transmission electron microscopy (HRTEM), and photoluminescence (PL). The luminescent investigations confirmed that the Eu{sup 3+} ions have been effectively doped into CaMoO{sub 4} nanostructures. The successfully achieved Eu{sup 3+}-doped CaMoO{sub 4} nanostructures will be potential in technological applications on near UV chip-based white light emitting diode (WLED).

36 MATERIALS SCIENCE↗

Tuning of crystal phase and luminescence properties of Gd{sub 2}(MoO{sub 4}){sub 3}:Dy{sup 3+} phosphors

Graphical abstract: The optical properties of Dy{sup 3+} were found to be sensitive to the crystal phase of the as-synthesized Gd{sub 2}(MoO{sub 4}){sub 3}:Dy{sup 3+} phosphors, especially the distinct features of the charge transfer (CT) transition. The mechanism involved was discussed in detail based on the experiments and theoretic calculations. Highlights: ► The crystal phase of Gd{sub 2}(MoO{sub 4}){sub 3}:Dy{sup 3+} was tuned by changing the pH value of the solution in hydrothermal system. ► The optical properties of Dy{sup 3+} were found to be sensitive to the crystal phase of Gd{sub 2}(MoO{sub 4}){sub 3}:Dy{sup 3+}. ► The mechanisms of different crystal phases affected on the luminescence properties of Gd{sub 2}(MoO{sub 4}){sub 3}:Dy{sup 3+} were discussed. -- Abstract: The orthorhombic and monoclinic Gd{sub 2}(MoO{sub 4}){sub 3}:Dy{sup 3+} were successfully synthesized by a hydrothermal process with a subsequent annealing treatment at 800 °C for 4 h. The crystal phase of Gd{sub 2}(MoO{sub 4}){sub 3}:Dy{sup 3+} was controlled as a function of the pH value of the solution. The crystallization and microstructures of the samples were characterized by Powder X-ray diffraction (XRD) and scanning electron micrograph (SEM). Furthermore, the optical properties were investigated by the diffuse reflection, excitation and emission spectra. The mechanisms of different crystal phases affected on the luminescence properties of Gd{sub 2}(MoO{sub 4}){sub 3}:Dy{sup 3+} were discussed. The electric dipole–dipole interaction between Dy{sup 3+} ions was identified as the main mechanism for the concentration quenching of the two structures. Finally, the chromatic natures of all the samples were analyzed in detail. The results indicate that the orthorhombic phosphor Gd{sub 1.84}(MoO{sub 4}){sub 3}:Dy{sub 0.16}{sup 3+} can be considered as a suitable candidate for white light emitting diodes (W-LEDs).

36 MATERIALS SCIENCE↗

Controlled synthesis, characterization and photoluminescence property of olive-like tetragonal α-Nd{sub 2}(MoO{sub 4}){sub 3}

Highlights: ► The olive-like tetragonal α-Nd{sub 2}(MoO{sub 4}){sub 3} was gained with EDTA assisted hydrothermal method. ► The product was characterized by XRD, XPS, FTIR, FESEM, and PL. ► The possible formation mechanism for olive-like α-Nd{sub 2}(MoO{sub 4}){sub 3} was proposed. ► The PL in visible region of the olive-like α-Nd{sub 2}(MoO{sub 4}){sub 3} was studied. -- Abstract: The olive-like tetragonal α-Nd{sub 2}(MoO{sub 4}){sub 3} was obtained by a convenient and facile complex agent assisted hydrothermal method. The product was characterized by X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS), Fourier transform infrared (FTIR) spectroscopy, field-emission scanning electron microscopy (FESEM) and photoluminescence (PL). The possible formation mechanism of the olive-like α-Nd{sub 2}(MoO{sub 4}){sub 3} was proposed. The photoluminescence property in visible region of the olive-like tetragonal α-Nd{sub 2}(MoO{sub 4}){sub 3} was studied.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Magnetic properties and homogeneous distribution of Gd{sup 3+} ions in gadolinium molybdenum borate glass with high Gd{sub 2}O{sub 3} content

Highlights: ► The magnetic susceptibility of Gd{sub 2}O{sub 3}–MoO{sub 3}–B{sub 2}O{sub 3} glass was examined in T = 1.8–300 K. ► The effective magnetic moment was μ{sub eff} = 7.87 μ{sub B}. ► The Weiss constant was θ = −0.7 K. ► Gd{sup 3+} ions are distributed homogeneously as paramagnetic ions down to T = 1.8 K. -- Abstract: The magnetic susceptibility and specific heat of 21.25Gd{sub 2}O{sub 3}–63.75MoO{sub 3}–15B{sub 2}O{sub 3} (mol%) glass showing the crystallization of ferroelastic β′-Gd{sub 2}(MoO{sub 4}){sub 3} crystals are examined in the temperature range of T = 1.8–300 K to clarify magnetic and distribution states of Gd{sup 3+} ions. The magnetic susceptibility obeys the Curie–Weiss law, giving the effective magnetic moment of μ{sub eff} = 7.87 μ{sub B} and the Weiss constant of θ = −0.7 K. Any peak such as λ-type anomaly is not observed in the temperature dependence of specific heat in T = 1.8–5 K. It is suggested that Gd{sup 3+} ions in the glass with a high Gd{sub 2}O{sub 3} content of 21.25 mol% are distributed homogeneously and randomly as paramagnetic ions down to T = 1.8 K without inducing any strong magnetic interaction. The present study suggests that glasses based on the MoO{sub 3}–B{sub 2}O{sub 3} system are good hosts for the homogeneous solubility of a large amount of rare-earth oxides.

36 MATERIALS SCIENCE↗

The red-emitting phosphors of Eu{sup 3+}-activated MR{sub 2}(MoO{sub 4}){sub 4} (M = Ba, Sr, Ca; R = La{sup 3+}, Gd{sup 3+}, Y{sup 3+}) for light emitting diodes

Graphical abstract: The luminescence quantum efficiencies of Eu{sup 3+}-doped MY{sub 2−x}Eu{sub x}(MoO{sub 4}){sub 4} show the dependence on the Eu{sup 3+} doping (x) for M = Ca (a), Sr (b), Ba (c). Display Omitted Highlights: ► Eu{sup 3+}-activated MY{sub 2}(MoO{sub 4}){sub 4} (M = Ba, Sr, Ca) were firstly prepared. ► Comprehensive investigations of QEs and thermal stabilities of Eu{sup 3+}-activated MR{sub 2}(MoO{sub 4}){sub 4} (M = Ba, Sr, Ca; R = La, Gd). ► BaYEu(MoO{sub 4}){sub 4}, SrY0.6Eu1.4(MoO{sub 4}){sub 4} and CaEu{sub 2}(MoO{sub 4}){sub 4} are the best choice for solid state lighting because of high QEs and thermal stabilities. -- Abstract: A series of red-emitting phosphors of MR{sub 2}(MoO{sub 4}){sub 4}:Eu{sup 3+} (M = Ba, Sr, Ca; R = La{sup 3+}, Gd{sup 3+}, Y{sup 3+}) were prepared by solid-state reaction. The photoluminescence excitation and emission spectra were investigated. The phosphors can be efficiently excited by the near UV light and exhibit a red luminescence corresponding to the electric dipole transition {sup 5}D{sub 0} → {sup 7}F{sub 2} at 615 nm. The optimum doping in MY{sub 2−x}Eu{sub x}(MoO{sub 4}){sub 4} (M = Ba, Sr, Ca) were investigated by the dependence of luminescence quantum efficiency (QE) on the Eu{sup 3+} concentrations. The absolute luminescence quantum efficiencies were measured for all the samples. The luminescence thermal satiability was checked by measuring the temperature-dependent luminescence intensities in temperature region of 10–450 K. The results indicate that the three phosphors of BaYEu(MoO{sub 4}){sub 4}, SrY{sub 0.6}Eu{sub 1.4}(MoO{sub 4}){sub 4} and CaEu{sub 2}(MoO{sub 4}){sub 4} are the best choice for white-LEDs to be used for lighting. This was evaluated in details by taking into account of the properties such as the excitation spectra, the luminescence QEs, the red color coordinates, the luminescence quenching of Eu{sup 3+}-doping concentrations and the thermal stability.

36 MATERIALS SCIENCE↗

Effects of the solvent on the structure, morphology and photocatalytic properties of Bi{sub 2}MoO{sub 6} in the solvothermal process

Graphical abstract: Various nanostructure Bi{sub 2}MoO{sub 6} photocatalysts have been prepared by a solvothermal process via simply altering the used solvent. It is revealed that the type of solvents has a strong influence on the morphology of Bi{sub 2}MoO{sub 6}. This could be understood in terms of the reaction media effect on the crystal growth. The photocatalytic experiments for the decomposition of RhB demonstrate that the samples prepared by different solvents show different photocatalytic activity. The highest photocatalytic activity is obtained by the sample with glycol as solvent. Highlights: ► The used solvent in the synthesis can affect the morphology and size of Bi{sub 2}MoO{sub 6}. ► Different solvent in the reaction leads to different surface area and pore size. ► The highest photocatalytic activity is obtained by the sample prepared in glycol. ► The high activity is mainly due to the large surface area and small particle size. - Abstract: Visible-light-driven photocatalyst Bi{sub 2}MoO{sub 6} was prepared by a solvothermal process with different kinds of solvent including water, isopropanol and ethylene glycol. The obtained samples were characterized by X-ray diffraction technique, N{sub 2}-sorption, UV–vis diffuse reflectance spectra, transmission electron microscopy and Fourier transform infrared spectroscopy. The results revealed that the type of solvent has a strong influence on the morphologies and physico-chemical properties of Bi{sub 2}MoO{sub 6}. Meanwhile, the formation mechanism of Bi{sub 2}MoO{sub 6} with various morphologies was discussed. The photocatalytic activities of Bi{sub 2}MoO{sub 6} photocatalysts were evaluated by the decomposition of rhodamine B (RhB) under visible light irradiation (λ > 420 nm). It was found that the sample prepared with glycol as solvent showed the best performance in the photodegradation of RhB under visible light irradiation. This could be ascribed to the large surface area, unique morphology and small particle size.

36 MATERIALS SCIENCE↗

Negative thermal expansion correlated with polyhedral movements and distortions in orthorhombic Y{sub 2}Mo{sub 3}O{sub 12}

Graphical abstract: Our work confirms the negative thermal expansion (NTE) behavior of the orthorhombic Y{sub 2}Mo{sub 3}O{sub 12} in this range 0–1000 K. The orthorhombic Y{sub 2}Mo{sub 3}O{sub 12} has an open framework structure where MoO{sub 4} tetrahedra and YO{sub 6} octahedra are connected by oxygen atoms. The previous mechanisms for the NTE behavior of orthorhombic Y{sub 2}Mo{sub 3}O{sub 12} are that the translational mode (see (b)) of the O bridge atoms in Y-O-Mo linkages will cause the linkages to be bent, reducing the space between polyhedra and making the volumetric shrinkage. Furthermore, the internal polyhedral distortions have been reported experimentally. It is necessary to reveal the relationship between NTE and polyhedral movements, distortions. From the vibrational properties, we get that the different vibrational eigenvectors of oxygen atoms relative to Y or Mo atoms can lead internal polyhedra to distort unevenly (see (c)). Herein, an extended 3D model of the connected unit YO{sub 6}-MoO{sub 4} based on the Y-O-Mo linkage is proposed (see (a)). It presents a simultaneous dynamic process, i.e. the YO{sub 6} octahedra and MoO{sub 4} tetrahedra distort unevenly, along with both polyhedra being closer which makes the volumetric contraction. This model is helpful to improve the mechanisms of NTE and may be applied in the whole A{sub 2}M{sub 3}O{sub 12} family. - Highlights: • The NTE properties of Y{sub 2}Mo{sub 3}O{sub 12} are confirmed using a first-principles calculation. • The optical branch with the lowest frequency is most responsible for the NTE. • The relationship between NTE and polyhedral movements, distortions is elucidated. • An extended 3D model of the connected unit YO{sub 6}-MoO{sub 4} is proposed. - Abstract: The internal polyhedral distortions have been reported experimentally in orthorhombic Y{sub 2}Mo{sub 3}O{sub 12} as a negative thermal expansion (NTE) material. To reveal the relationship between NTE and polyhedral movements, distortions, the vibrational properties of Y{sub 2}Mo{sub 3}O{sub 12} have been studied using first-principles calculations. The lowest optical branch corresponding to translational mode of the O bridge atom in Y-O-Mo linkage has the largest negative Grüneisen parameter and therefore contributes most to the NTE behavior. The different vibrational eigenvectors of oxygen atoms relative to Y or Mo atoms can cause internal polyhedral to distort unevenly. Herein, an extended 3D model of the connected unit YO{sub 6}-MoO{sub 4} based on the Y-O-Mo linkage presents a simultaneous dynamic process, i.e. the YO{sub 6} octahedra and MoO{sub 4} tetrahedra distort unevenly, along with both polyhedra being closer which makes the volumetric contraction. This model is helpful to improve the mechanisms of NTE and may be applied in the whole A{sub 2}M{sub 3}O{sub 12} family.

36 MATERIALS SCIENCE↗

A facile mixed-solvothermal route to γ-Bi{sub 2}MoO{sub 6} nanoflakes and their visible-light-responsive photocatalytic activity

Graphical abstract: γ-Bi2MoO6 nanoflakes were successfully synthesized by a mixed-solvothermal process. The visible-light-responsive photocatalytic activities of the obtained γ-Bi2MoO6 nanoflakes were evaluated by photodegradation of Rhodamie B under visible light. The high degradation efficiency of RhB was attributed to the good crystallization and flake-like morphology of γ-Bi2MoO6 nanostructures, which is in accord with the photocurrent result. - Highlights: • γ-Bi{sub 2}MoO{sub 6} nanoflakes were obtained by a mixed-solvothermal process with SDBS as surfactant. • The photocurrent test was taken to characterize the photocatalytic activity. • The nanopowders exhibit high efficient photocatalytic activity under visibile-light irradiation. - Abstract: γ-Bi{sub 2}MoO{sub 6} nanoflakes were successfully synthesized by a mixed-solvothermal process with SDBS involved in the reaction. The as-prepared γ-Bi{sub 2}MoO{sub 6} was characterized by X-ray diffraction (XRD), transmission electron microscopy (TEM), and UV–vis absorption spectroscopy. The effect of different ratio of solvents on the resulting products was investigated. The visible-light-responsive photocatalytic activities of the obtained γ-Bi{sub 2}MoO{sub 6} nanoflakes were evaluated by photodegradation of Rhodamie B under visible light (λ > 400 nm). The high degradation efficiency of RhB was attributed to the good crystallization and flake-like morphology of γ-Bi{sub 2}MoO{sub 6} nanostructures, which is in accord with the photocurrent result.

36 MATERIALS SCIENCE↗

The photocatalysis of Bi{sub 2}MoO{sub 6} under the irradiation of blue LED

Graphical abstract: - Highlights: • ·OH trap and hole sink were involved to investigate the active radicals. • Holes play a more important role in the degradation of RhB. • The ·OH were related to the decomposition of phenol. • The ·O{sub 2}-played a leading role in the photodegradation of phenol. • Blue LED is competitive and promising alternative for the future application. - Abstract: Bi{sub 2}MoO{sub 6} has been reported as a promising photocatalyst in wastewater treatment. The active radicals generated over the Bi{sub 2}MoO{sub 6} during the photocatalytic process were thought to be hydroxyl radical (·OH) but have not been proved. Herein, Bi{sub 2}MoO{sub 6} with nanoplate like morphology was synthesized and its photocatalytic performances in the degradation of rhodamine B (RhB) and phenol as colored and colorless model pollutants respectively were evaluated under the irradiation of blue light emitting diode (LED). The tert-butyl alcohol (TBA) as a ·OH trap and ethylene diamine tetraacetic acid (EDTA) as a hole sink were involved to investigate the main active groups that are generated on Bi{sub 2}MoO{sub 6} and function during the photodegradation of RhB and phenol. In addition, it is a competitive and promising alternative plan to use blue LED as light source for the future practical application in environmental remediation.

36 MATERIALS SCIENCE↗

A novel Bi-based phosphomolybdate photocatalyst K{sub 2}Bi(PO{sub 4})(MoO{sub 4}): Crystal structure, electronic structure and photocatalytic activity

Graphical abstract: - Highlights: • A new type of phosphomolybdate K{sub 2}Bi(PO{sub 4})(MoO{sub 4}) photocatalyst was successfully synthesized. • The products synthesized at 600 °C were mainly composed of nano-cubes. • The indirect band gap of K{sub 2}Bi(PO{sub 4})(MoO{sub 4}) has been determined to be 2.93 eV. • K{sub 2}Bi(PO{sub 4})(MoO{sub 4}) synthesized at 600 °C exhibits the highest photocatalytic activity. • The electronic structure was calculated by density functional calculations. - Abstract: A novel phosphomolybdate photocatalyst K{sub 2}Bi(PO{sub 4})(MoO{sub 4}) has been successfully developed via a solid-state reaction. The products were characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM), high-resolution transmission electron microscopy (HRTEM), diffuse reflectance spectrum (DRS) and photoluminescence (PL) spectra. The photocatalytic activities of the samples prepared at different temperature were determined by the photooxidative decomposition of methylene blue (MB) in aqueous solution. The results revealed that K{sub 2}Bi(PO{sub 4})(MoO{sub 4}) can be used as an effective photocatalyst under UV–vis irradiation and the nanocubes obtained at 600 °C exhibits the highest photocatalytic activity. The photodegradation of MB by K{sub 2}Bi(PO{sub 4})(MoO{sub 4}) nanocrystals followed the first-order kinetics. Theoretical calculations on electronic structure confirmed the indirect optical transitions property in the absorption edge region of K{sub 2}Bi(PO{sub 4})(MoO{sub 4}), and the orbital constitutions of CB and VB were also analyzed.

36 MATERIALS SCIENCE↗

NaYF{sub 4}:Er,Yb/Bi{sub 2}MoO{sub 6} core/shell nanocomposite: A highly efficient visible-light-driven photocatalyst utilizing upconversion

Highlights: • Design and synthesis of NaYF{sub 4}:Er,Yb/Bi{sub 2}MoO{sub 6} based on upconversion. • NaYF{sub 4}:Er,Yb/Bi{sub 2}MoO{sub 6} nanocomposite was prepared for the first time. • Core–shell structure benefits the properties. • Upconversion contributed to the enhanced photocatalytic activity. • Helps to understand the functionality of new type photocatalysts. - Abstract: NaYF{sub 4}:Er,Yb/Bi{sub 2}MoO{sub 6} core/shell nanocomposite was designed and prepared for the first time based on upconversion. The products were characterized by X-ray diffraction (XRD), transmission electron microscopy (TEM), high resolution TEM (HRTEM), energy dispersive X-ray spectroscopy (EDS) and diffuse reflectance spectra (DRS). The results revealed that the as-synthesized NaYF{sub 4}:Er,Yb/Bi{sub 2}MoO{sub 6} consisted of spheres with a core diameter of about 26 nm and a shell diameter of around 6 nm. The core was upconversion illuminant NaYF{sub 4}:Er,Yb and the shell was Bi{sub 2}MoO{sub 6} around the core, which was confirmed by EDS. The NaYF{sub 4}:Er,Yb/Bi{sub 2}MoO{sub 6} exhibited higher photocatalytic activity for the photodecomposition of Rhodamine B (RhB) under the irradiation of Xe lamp and green light emitting diode (g-LED). The mechanism of the high photocatalytic activity was discussed by photoluminescence spectra (PL), which is mainly attributed to upconversion of NaYF{sub 4}:Er,Yb in the NaYF{sub 4}:Er,Yb/Bi{sub 2}MoO{sub 6} nanocomposite and the core–shell structure.

36 MATERIALS SCIENCE↗

Transformation of Mo and W thiosalts into unsupported sulfide catalysts: A temperature dependent in-situ spectroscopic investigation

Highlights: • TPD–MS results suggest that the majority of S remains in the solid sample after decomposition. • Decomposition of the (CH{sub 3}){sub 4}N is not directly correlated with that of the MS{sub 4}{sup 2−} species. • Surface of materials does not track directly with the bulk at various treatment temperatures. • ATT-derived materials retained a significant amount of +6 state consistent with the precursor. - Abstract: The thermal decomposition of ammonium thiomolybdate (ATM), ammonium thiotungstate (ATT), tetramethylammonium thiomolybdate (TMATM) and tetramethylammonium thiotungstate (TMATT) are investigated as a function of temperature by using thermogravimetric analysis (TGA), temperature-programmed decomposition with mass spectroscopy (TPS–MS), in-situ Fourier transform infrared (FTIR) and Raman spectroscopies, and X-ray photoelectron spectroscopy (XPS). The results allow for correlations to be made between the changes in the bulk and surface structures of the materials, and the evolution of gas-phase decomposition products. The major difference between the ammonium and tetramethylammonium precursors is the complexity of the thermal decomposition profile, which is found to follow two steps over a wide temperature range for the former, but one step over a relatively narrow range for the latter materials. Raman and FTIR spectra reveal the decomposition of the ammonium and tetramethylammonium groups, along with the decomposition of the initial sulfide structures to metal disulfides. For both sets of precursors, XPS results show that the surface of the resulting materials at various temperatures of treatment does not track directly with the state of the bulk material. While the ATM, TMATM, and TMATT-derived material surfaces are reduced to the 4{sup +} state at the highest temperature, indicating disulfides, the ATT-derived materials still retained a significant amount of W{sup 6+} state consistent with the starting precursor.

36 MATERIALS SCIENCE↗

Sodium citrate (Na{sub 3}Cit)-assisted hydrothermal synthesis of uniform spindle-like SrMoO{sub 4}:Eu{sup 3+} phosphors

Graphical abstract: A facile hydrothermal method for the synthesis of uniform spindle-like SrMoO{sub 4}:Eu{sup 3+} phosphors with the assistance of sodium citrate (Na{sub 3}Cit). - Highlights: • Well-crystallized spindle-like SrMoO{sub 4}:Eu{sup 3+} phosphors have been synthesized. • The influence of the reaction temperature and reaction time were clearly shown. • The dosage of Na{sub 3}Cit has a strong effect on the spindle-like SrMoO{sub 4}:Eu{sup 3+} phosphors. • The growth mechanism for the formation of final samples was proposed. - Abstract: Highly uniform spindle-like SrMoO{sub 4}:Eu{sup 3+} phosphors have been prepared by a facile hydrothermal method using sodium citrate (Na{sub 3}Cit) as the chelating reagent. X-ray powder diffraction (XRD), field emission scanning electron microscopy (FE-SEM), energy-dispersive X-ray spectrum (EDS), transmission electron microscopy (TEM), X-ray photoelectron spectra (XPS), Fourier transform-infrared spectroscopy (FT-IR) and photoluminescence spectra (PL) were used to characterize the resulting samples. The dosage of sodium citrate, reaction temperature and reaction time play key roles in the formation of the final samples. The possible formation mechanism for SrMoO{sub 4}:Eu{sup 3+} phosphors has been proposed. Upon excitation by ultraviolet radiation, the as-synthesized SrMoO{sub 4}:Eu{sup 3+} phosphors show the characteristic {sup 5}D{sub 0}–{sup 7}F{sub J} (J = 1, 2, 3, 4) emission lines with red emission {sup 5}D{sub 0}–{sup 7}F{sub 2} (613 nm) as the most prominent group.

36 MATERIALS SCIENCE↗