Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “FERRITE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 307 records · Page 17

Stability of Y–Ti–O precipitates in friction stir welded nanostructured ferritic alloys

Nanostructured ferritic alloys, which have complex microstructures which consist of ultrafine ferritic grains with a dispersion of stable oxide particles and nanoclusters, are promising materials for fuel cladding and structural applications in the next generation nuclear reactor. This paper evaluates microstructure of friction stir welded nanostructured ferritic alloys using electron microscopy and atom probe tomography techniques. Atom probe tomography results revealed that nanoclusters are coarsened and inhomogeneously distributed in the stir zone and thermomechanically affected zone. Three hypotheses on coarsening of nanoclusters are presented. Finally, the hardness difference in different regions of friction stir weld has been explained.

36 MATERIALS SCIENCE↗

Technical Letter Report on the Cracking of Irradiated Cast Stainless Steels with Low Ferrite Content

Crack growth rate and fracture toughness J-R curve tests were performed on CF-3 and CF-8 cast austenite stainless steels (CASS) with 13-14% of ferrite. The tests were conducted at ~320°C in either high-purity water with low dissolved oxygen or in simulated PWR water. The cyclic crack growth rates of CF-8 were higher than that of CF-3, and the differences between the aged and unaged specimens were small. No elevated SCC susceptibility was observed among these samples, and the SCC CGRs of these materials were comparable to those of CASS alloys with >23% ferrite. The fracture toughness values of unirradiated CF-3 were similar between unaged and aged specimens, and neutron irradiation decreased the fracture toughness significantly. The fracture toughness of CF-8 was reduced after thermal aging, and declined further after irradiation. It appears that while lowering ferrite content may help reduce the tendency of thermal aging embrittlement, it is not very effective to mitigate irradiation-induced embrittlement. Under a combined condition of thermal aging and irradiation, neutron irradiation plays a dominant role in causing embrittlement in CASS alloys.

36 MATERIALS SCIENCE↗

Effect of High-Density Nanoparticles on Recrystallization and Texture Evolution in Ferritic Alloys

Ferritic alloys are important for nuclear reactor applications due to their microstructural stability, corrosion resistance, and favorable mechanical properties. Nanostructured ferritic alloys having a high density of Y-Ti-O rich nano-oxides (NOs < 5 nm) are found to be extremely stable at high temperatures up to ~1100 °C. This study serves to understand the effect of a high density of nano-particles on texture evolution and recrystallization mechanisms in ferritic alloys of 14YWT (14Cr-3W-0.4Ti-0.21Y-Fe wt %) having a high density of nano-particles and dispersion-free FeCrAl (13Cr-5.2Al-0.05Y-2Mo-0.2Si-1Nb wt %). In order to investigate the recrystallization mechanisms in these alloys, neutron diffraction, electron backscattered diffraction, and in situ and ex situ transmission electron microscopy have been utilized. It has been observed that even though the deformation textures of both the 14YWT and FeCrAl alloys evolved similarly, resulting in either the formation (in FeCrAl alloy) or increase (in 14YWT) in γ-fiber texture, the texture evolution during recrystallization is different. While FeCrAl alloy keeps its γ-fiber texture after recrystallization, 14YWT samples develop a ε-fiber as a result of annealing at 1100 °C, which can be attributed to the existence of NOs. In situ transmission electron microscopy annealing experiments on 14YWT show the combination and growth of the lamellar grains rather than nucleation; however, the recrystallization and growth kinetics are slower due to NOs compared to FeCrAl.

36 MATERIALS SCIENCE↗

Benchmarking a 9Cr-2WVTa Reduced Activation Ferritic Martensitic Steel Fabricated via Additive Manufacturing

Reduced activation ferritic (RAF) martensitic steels are promising candidates for the first wall of fusion reactors. However, current manufacturing capabilities call for these components to be made by welding wrought plates. This limits design freedom and necessitates the use of post-weld heat treatments (PWHT) in accordance with the boiler and pressure vessel code. Additive manufacturing (AM) can offer a unique solution to solve this challenge by leveraging the layer-wise deposition strategy to come up with temper bead deposition techniques to eliminate post-processing heat treatments (PPHT). However, it is necessary to benchmark the properties of RAF steels fabricated by AM with their wrought counterparts to identify the process-structure-property correlation, which is the goal of this study. The study demonstrates that while tensile properties at room temperature and high temperatures are satisfactory, the as fabricated and samples after PPHT have significant heterogeneity in tensile elongation. This has been attributed to the presence of discontinuities in the build. The as-fabricated samples have an average tensile strength of 1190 + 12 MPa and an average elongation of 15 + 5% at room temperature and 658 ± 20 MPa ultimate tensile strength (UTS) and 14 ± 7% at 600 °C. After the post-weld heat treatment, mechanical properties decrease to around 600–650 MPa and an elongation between 20–25% at room temperature to 300 MPa UTS and 25–28% elongation at 600 °C. The characterization of microstructures at various length scales demonstrates that the as-fabricated structure has a significant fraction of delta ferrite in a lath martensitic matrix. No precipitates could be identified in the as-fabricated structure. PPHT led to a decrease in the area fraction of delta ferrite and precipitation of M 23 C 6 and MX. Detailed characterization clearly demonstrates that the lack of precipitates in the as-fabricated structure could be due to the slow tempering response of the alloy. Finally, the needs to develop new alloys to achieve the objectives stated above are articulated.

36 MATERIALS SCIENCE↗

Hard–Soft Core–Shell Architecture Formation from Cubic Cobalt Ferrite Nanoparticles

Cubic bi-magnetic hard–soft core–shell nanoarchitectures were prepared starting from cobalt ferrite nanoparticles, prevalently with cubic shape, as seeds to grow a manganese ferrite shell. The combined use of direct (nanoscale chemical mapping via STEM-EDX) and indirect (DC magnetometry) tools was adopted to verify the formation of the heterostructures at the nanoscale and bulk level, respectively. The results showed the obtainment of core–shell NPs (CoFe 2 O 4 @MnFe 2 O 4 ) with a thin shell (heterogenous nucleation). In addition, manganese ferrite was found to homogeneously nucleate to form a secondary nanoparticle population (homogenous nucleation). This study shed light on the competitive formation mechanism of homogenous and heterogenous nucleation, suggesting the existence of a critical size, beyond which, phase separation occurs and seeds are no longer available in the reaction medium for heterogenous nucleation. These findings may allow one to tailor the synthesis process in order to achieve better control of the materials’ features affecting the magnetic behaviour, and consequently, the performances as heat mediators or components for data storage devices.

36 MATERIALS SCIENCE↗

Coexistence of Low Damping and Strong Magnetoelastic Coupling in Epitaxial Spinel Ferrite Thin Films

Low‐loss magnetization dynamics and strong magnetoelastic coupling are generally mutually exclusive properties due to opposing dependencies on spin–orbit interactions. So far, the lack of low‐damping, magnetostrictive ferrite films has hindered the development of power‐efficient magnetoelectric and acoustic spintronic devices. Here, magnetically soft epitaxial spinel NiZnAl‐ferrite thin films with an unusually low Gilbert damping parameter (<3 × 10 −3 ), as well as strong magnetoelastic coupling evidenced by a giant strain‐induced anisotropy field (≈1 T) and a sizable magnetostriction coefficient (≈10 ppm), are reported. This exceptional combination of low intrinsic damping and substantial magnetostriction arises from the cation chemistry of NiZnAl‐ferrite. At the same time, the coherently strained film structure suppresses extrinsic damping, enables soft magnetic behavior, and generates large easy‐plane magnetoelastic anisotropy. These findings provide a foundation for a new class of low‐loss, magnetoelastic thin film materials that are promising for spin‐mechanical devices.

Emori, Satoru↗

Influence of Molybdenum on Rapid Solidification Microstructure and Microsegregation in Primary Ferrite Solidified Stainless Steel

Due to the widespread use and familiarity of austenitic stainless steels in many industries these alloys are often the first materials used when adapting new processing techniques. The rapid cooling and solidification rates that occur during fusion based additive manufacturing processes like powder bed fusion cause a fundamental shift in the solidification behavior of the material. While the effects that Cr and Ni have on the microstructure have been fairly well documented across a range of solidification conditions, the impact of alloying elements like Mo are not as well understood at rapid solidification rates. For this study, four custom stainless steel alloy feedstocks were made with targeted modification of the Cr and Mo concentrations to maintain a constant Cr/Ni eq ratio of ~1.7. Two-piston splat quenching was used to produce rapidly solidified samples and the solidification mode, phase, and cell size were investigated. Solidification rates were estimated to be between 0.4 and 1.5m/s. A comparison of the microsegregation and partitioning behavior of Cr, Ni and Mo in ferrite solidified material was also performed for the different alloy compositions. Variations of the Mo concentration between each feedstock showed no measurable influence on the solidification/cooling rates, solidification morphology, or the partitioning of Mo. Furthermore, higher concentrations of Mo were found to significantly increase the amount of ferrite phase in the microstructure by suppressing the ferrite to austenite massive transformation.

36 MATERIALS SCIENCE↗

Investigation of Iron-Chromium-Niobium-Titanium Ferritic Stainless Steel for Solid Oxide Fuel Cell Interconnect Applications

As part of an effort to develop cost-effective ferritic stainless steel-based interconnects for solid oxide fuel cell (SOFC) stacks, AL 441 HPTM was studied in terms of its metallurgical characteristics, oxidation behavior, and electrical performance. Minor alloying elements (Nb and Ti) captured interstitials such as C by forming carbides, stabilizing the ferritic structure and mitigating the risks of sensitization and inter-granular corrosion. Laves phases rich in Nb and Si precipitated along grain boundaries during high temperature exposure, improving the steel’s high temperature mechanical strength. The capture of Si in the Laves phase minimized the Si activity in the steel substrate and prevented formation of an insulating silica layer at the scale/metal interface. However, the relatively high oxidation rate, and thus increasing ASR over time, necessitates the application of a conductive protection layer on the steel. In particular, Mn1.5Co1.5O4 spinel protection layers drastically improved the electrical performance of the ferritic stainless steel 441, acting as barriers to chromium outward and oxygen inward diffusion.

Solid oxide fuel cell, interconnect, oxidation, co↗

Effect of austenite grain size on acicular ferrite transformation in a HSLA steel

Highlights: • The fraction of acicular ferrite increases with reduced austenite grain sizes. • The reduction of austenite grain size refines and homogenises the microstructure. • There is a limit to increase the acicular ferrite fraction by reducing austenite size. • An equation relating effective grain sizes with processing parameters was proposed. - Abstract: Austenite grain size is well known to have a significant influence on various phase transformations in steels. Although the effects of many thermomechanical processing parameters on acicular ferrite (AF) transformation in HSLA steels have been investigated, little attention has been paid to the influence of austenite grain size. Therefore, in this research, different parameters of solid-solution heat treatment and rough deformation were adopted to generate austenite with different grain sizes and the effects of austenite grain size before deformation on the AF transformation and grain refinement were investigated. It was found that the reduction of prior-austenite grain size (PAGS) from 62.8 μm to 37.0 μm before austenite deformation promotes the AF transformation and simultaneously refines and homogenises the transformed microstructures. A reciprocally increased density of deformation induced dislocations with the reduction of PAGS was proposed to account for these results, which not only increase the nucleation sites of AF but also suppress the lengthening of BF laths. Further reducing PAGS from 37.0 μm to 22.3 μm, the fraction of AF is not increased and the transformed microstructure is not refined. Possible differences in the type, distribution, and density of austenite deformation substructures between austenite with PAGSs of 37.0 μm and 22.3 μm were argued to be responsible for the cease of grain refinement. The relationship between effective grain sizes and the S{sub v} parameter was investigated and an equation relating effective grain sizes with processing parameters was also proposed.

36 MATERIALS SCIENCE↗

Mesoporous palladium–copper ferrites as highly efficient and magnetically separable catalysts for Suzuki coupling reaction

Highlights: • Mesoporous Cu–Pd ferrites were prepared by a facile, mild and environment-friendly route. • The catalysts have shown great efficiencies in Suzuki coupling reaction and up to 36.9 × 10{sup 3} h{sup −1} TOF can be obtained. • The catalyst can be magnetically separated easily and have shown prominent recyclability. - Abstract: Mesoporous Cu–Pd ferrites were prepared by using MCM-41 and SBA-15 mesoporous molecular sieves as hard templates and well characterized by X-ray diffraction (XRD), transmission electron microscopy (TEM), ICP-atomic emission spectroscopy, N{sub 2} adsorption–desorption and X-ray photoelectric spectroscopy (XPS). Compared with samples prepared by the sol–gel auto-combustion methods, the as-prepared mesoporous ferrites have shown uniform pore size and much higher specific surface areas. The samples showed a remarkably high activity in connection with the Suzuki coupling reaction, especially Cu{sub 0.99}Pd{sub 0.01}Fe{sub 2}O{sub 4} prepared by using MCM-41 as template obtained an excellent TOF as high as 36.9 × 10{sup 3} h{sup −1} and no obvious decrease in the activity was observed after ten consecutive runs.

36 MATERIALS SCIENCE↗

Synthesis and optimization of the magnetic properties of aligned strontium ferrite nanowires

Highlights: • Dip coating method was used to synthesize strontium ferrite nanowires in template. • Size of nanowires was controlled via anodization parameters. • Fe/Sr ratio was optimized in precursor. • Magnetic properties of nanowires and nanopowders were compared. - Abstract: High aspect ratio strontium hexaferrite nanowires were fabricated by dip coating in alumina template. Fe/Sr ratio was changed from 10 to 12 in precursor, and the samples were annealed at a range of temperatures 500–900 °C in order to optimize the magnetic properties of strontium ferrite in the form of nanowires. Field emission scanning electron microscope (FESEM) proved the formation of nanowires in the templates, while TEM images revealed a high degree of crystallinity. The ferrites were further characterized by X-ray diffraction (XRD) and energy dispersive X-ray spectrometer (EDS). Magnetic properties of the specimens were studied by a SQUID at 10–300 K. The results showed that the coercivity of packed density nanowires in the template was much less than that of the nanopowders. On the other hand, the coercivity of nanowires at ambient temperature was less than low temperature coercivity.

36 MATERIALS SCIENCE↗

Characterization of phase properties and deformation in ferritic-austenitic duplex stainless steels by nanoindentation and finite element method

The phase properties and deformation behavior of the δ–ferrite and γ–austenite phases of CF–3 and CF–8 cast duplex stainless steels were characterized by nanoindentation and microstructure-based finite element method (FEM) models. We evaluated the elastic modulus of each phase and the results indicate that the mean elastic modulus of the δ–ferrite phase is greater than that of the γ–austenite phase, and the mean nanoindentation hardness values of each phase are approximately the same. Furthermore, the elastic FEM model results illustrate that greater von Mises stresses are located within the δ–ferrite phase, while greater von Mises strains are located in the γ–austenite phase in response to elastic deformation. The elastic moduli calculated by FEM agree closely with those measured by tensile testing. Finally, the plastically deformed specimens exhibit an increase in misorientation, deformed grains, and subgrain structure formation as measured by electron backscatter diffraction (EBSD).

36 MATERIALS SCIENCE↗

Ultrafast Spin Crossover in a Room-Temperature Ferrimagnet: Element-Specific Spin Dynamics in Photoexcited Cobalt Ferrite

Transition metal complexes capable of photoinduced spin crossover have been greatly investigated because of their potential to enable ultrafast optical control of information processing. Yet, any real application of photoswitchable molecules requires that spin crossover be paired with additional functionality such as long-range magnetic order. Important advances combining these functions are notably reported for a number of bimetallic Prussian Blue analogues; however, to date, PBA-based magnetic photoswitches can only operate below 150 K due to loss of magnetic order. In contrast, cobalt ferrite is a ferrimagnetic semiconductor with a Curie temperature of 790 K and extremely favorable magnetic properties by comparison to state-of-the-art PBAs. The mixed valence electronic structure of cobalt ferrite is reminiscent of cobalt–iron PBA, which is a well-known photoswitch. To investigate the potential for photoswitching in this material, we employ transient XUV spectroscopy to probe charge and spin dynamics with element-specific resolution on the femtosecond time scale. Results show that 400 nm light excites a metal-to-metal charge transfer transition, which drives the crossover of high-spin Co 2+ to low-spin Co 3+ with a time constant of 405 ± 29 fs and an internal quantum efficiency of unity. This result establishes the existence of efficient photoswitching in a new class of robust ferrimagnetic spinel ferrites.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Temperature dependence of magnetic behaviour in very fine grained, spark plasma sintered NiCuZn ferrites

Recently, using spark plasma sintering technique, a family of very fine grained, fully dense NiCuZn ferrites have been produced, which show constant permeability up to several 10 MHz. These ferrites can be used for filtering purposes in high frequency applications where a wide frequency band is required. In this paper, we study the magnetization processes taking place in these nano grained materials, in the frequency interval of 100 kHz to 5 MHz. Using a fluxmetric hysteresis graph, permeability, loss, and BH loops are measured at different temperatures, from -5 deg. C to 110 deg. C. Results are compared to the behavior of micrometric grain size ferrites, which are commonly used for power electronic and high frequency applications.

36 MATERIALS SCIENCE↗

Structure dependent electrical properties of Ni-Mg-Cu nano ferrites

Nano ferrites with the general chemical formula Ni{sub 0.5}Mg{sub x}Cu{sub 1-x} Fe{sub 2}O{sub 4} were synthesized by chemical route. They were characterized by x-ray diffraction by powder method. The diffraction patterns confirm the formation of single phase ferrites. The particle size is calculated by Scherrer formula which varies between 20nm to 60nm. DC resistivity was measured as a function of composition from room temperature to 700{sup o} C by two probe method. These ferrites show higher resistivity than those synthesized by ceramic method, due to control over composition and morphology. This leads to the elimination of domain wall resonance so that the materials can work at higher frequencies. AC resistivity was measured as a function of frequency at room temperature. Dielectric dispersion obeys Maxwell - Wagner model, in accordance with Koop’s phenomenological theory. The variation of loss angle follows the variation of ac resistivity with frequency and composition. The change in ac conductivity with frequency obeys the power law σ{sub a} = B.ω{sup n}. Such a behavior suggests that conductivity is due to polarons in all the samples.

36 MATERIALS SCIENCE↗

Structure–property relations of binary ferrite melts

Molten ferrite systems are used in the smelting and refining processes in steelmaking, to reduce the loss of metals in slags and to accelerate reaction rates. Here, high-energy x-ray diffraction experiments have been performed on aerodynamically levitated molten spheres of 43BaO–57FeO X and 43SrO–57FeO X at 1873 K using laser beam heating. The composition was varied within the range of x = 1–1.5 by changing the oxygen partial pressure of the levitation gas. The corresponding x-ray pair distribution functions have been interpreted using empirical potential structure refinement (EPSR) modeling. In oxygen-rich melts (x = 1.5), our EPSR models indicate very similar structures for the different alkaline-earth liquids, with both the Ba–O and Sr–O coordination numbers to be ∼8.4 and the total Fe–O coordination numbers ∼5.7. However, our models show that in reducing environments, the Fe 3+ and Fe 2+ ions exhibit very different behaviors in the Ba- and Sr-ferrite liquids. In the Ba-ferrite melt, the Fe 3+ –O coordination number decreases from 5.7 (at x = 1.5) to 5.2 (at x = 1.07), whereas Fe 2+ –O remains constant at ∼5.0 across the same compositional range. In the Sr melts, both the Fe 2+ –O and Fe 3+ –O coordination numbers rise from ∼5.7 (at x = 1.5) to 6.3 (at x = 1.07). All models show the structures to be heterogeneous with intertwined nanometer sized clusters or channels of Ba/Sr–O and Fe–O polyhedra that grow as oxygen content is reduced. Changes in the viscosity and electrical properties are interpreted in terms of the number of bridging and non-bridging oxygens associated with FeO 4 tetrahedra and concentration of charge carriers, respectively.

Benmore, Chris J. [Argonne National Laboratory (AN↗

Wet chemistry-synthesized Fe/mixed ferrite soft magnetic composites for high-frequency power conversion

State-of-the-art soft magnetic (SM) alloy systems such as electrical steels and permalloys exhibit large eddy current losses at high-frequency (kHz range and above), limiting their application in fast switching devices. Eddy current losses can be reduced for metallic alloys through a decrease in characteristic length scale or embedding them in an insulation layer. This work proposes the development of fine-scale core materials consisting of metallic SM nano/microparticles with magnetic, inorganic insulation layers, and their synthesis using a wet chemistry-based, scalable method for high frequency and high-power applications. More specifically, a magnetic ferrite coating (Ni 0.5-x Mn x Zn 0.5 Fe 2 O 4 , x = 0.0–0.5) was applied via deposition of ferrite powder produced using a “wet chemistry-based” co-precipitation method; the ferrite was distributed through the Fe micropowder via either ball milling or ultrasonic mixing. Powder cores were prepared by compaction of the synthesized composites. Relative magnetic permeability and core loss were measured at excitation frequencies to 200 kHz. A core loss of 127 kW/m 3 was measured at excitation frequency of 100 kHz and magnetization of 0.02 T. This value improves on the 199.3 kW/m 3 reported in literature at identical excitation conditions for a compact formed from a composite comprising Fe microparticles coated with low-permeability Ni 0.5 Zn 0.5 Fe 2 O 4 . Ultrasonic mixing resulted in slightly lower core loss than ball milling, possibly because ball milling causes loss-increasing deformation of the Fe micropowder. XRD and SEM were used to observe composite composition and core cross-section microstructure.

36 MATERIALS SCIENCE↗

Design and optimization of cancellation coil topologies for a ferrite-less wireless EV charging pad

Ferrite cores are widely used in conventional wireless EV charging pads to reduce stray EMF emissions, but they can be brittle, heavy, and expensive. This work furthers the development of ferrite-less wireless charging pads by comparing an active and two distinct passive cancellation coil topologies as candidates to replace the ferrite. Using the software packages FEMM and MATLAB, each topology is optimized to find the best winding positions and radii to minimize leakage at a specified position under the side of the vehicle. The optimized designs are compared for shielding effectiveness, induced current, and efficiency. All three topologies are able to sufficiently reduce the leakage field below the ICNIRP limit of 27 μTrms with just one turn. Interestingly, we find that an array of simple passive cancellation loops performs similar to the more widely studied passive cancellation coil.

Scher, Aaron D.↗