Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Dendrites”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 307 records · Page 17

Supercooling and structure of levitation melted Fe-Ni alloys

A study has been made of the effect of supercooling, quenching rate, growth inhibitors, and grain refiners on the structure of levitation-melted Fe- 25 pct Ni alloys. A combination of three morphologies, dendritic, spherical, and mixed dendritic and spherical, is observed in samples superheated or supercooled by less than 175 K. At larger supercooling, however, only the spherical morphology is observed. The grain size and the grain boundary shape are found to be strongly dependent on the subgrain morphology but not on the quenching temperature. Considerable grain growth is evident in samples with spherical and mixed morphologies but not in the dendriitic samples. The average cooling rates during solidification and the heat transfer coefficients at the metal-quenching medium boundary are calculated. For samples solidified in water, molten lead, and ceramic molds, the heat transfer coefficients are 0.41, 0.52, and 0.15 w/sq cm, respectively.

Abbaschian, G. J.↗

Some fundamental aspects of solidification in a supercooled melt

A model of dendritic growth in both supercooled pure and alloy melts is presented. In a pure melt, dendrite morphology is determined by the value of the dimensionless parameter sigma = 2 alpha (L)d(o)/sq Rr(t) whereas, in an alloy melt it is determined by the parameter sigma = 2 lambda (c)D(L)/sq Rr(t). The application of the above analysis to cylindrical and spherical growth morphologies obtained in highly supercooled melts has been discussed. An upper and lower bound for the particle or tip radius in this case has been obtained in terms of the growth rate and the initial bath supercooling.

Laxmanan, V.↗

Orientation and Morphology Effects in Rapid Silicon Sheet Solidification

Radial growth anisotropies and equilibrium forms of point nucleated, dislocation free silicon sheets spreading horizontally on the free surface of a silicon melt were measured for (100), (110), (111), and (112) sheet planes. The growth process was recorded. Qualitative Wulff surface free energy polar plots were deduced from the equilibrium shapes for each sheet plane. Predicted geometries for the tip shape of unidirectional, dislocation free, horizontally grown sheets growing in various directions within the planes were analyzed. Polycrystalline sheets and dendrite propagation were analyzed. For dendrites, growth rates on the order of 2.5 m/min and growth rate anisotropies of 25 are measured.

Ciszek, T. F.↗

The potential for bulk undercooling as an industrial process

The main focus is on solidification occurring in highly supercooled melts. Solidification rates in such melts are extremely high, an attractive feature from a commercial standpoint. Thus, the reported growth velocities for pure Ni and Co dendrites at a supercooling of 175 K are in excess of 180 km/hr. Rapidly quenched crystalline alloys produced by various atomization processes (e.g., centrifugal atomization or inert gas atomization) or melt spinning are examples of solidification processes, currently being intensively explored commercially, wherein extremely high solidification rates are achieved. Estimated dendrite tip growth rates are about 2 km/hr in a binary Al-4.5 wt % alloy, with a heat transfer coefficient of 6.4x10 sub 5 w/sq cm K or 15 cal/cu cm sK. In the limit, when the solidification rate exceeds a critical value, a glassy microstructure is obtained even in highly alloyed melts, which under normal conditions would solidity to form one or more crystalline phases. Glassy metals, also called metallic glasses, are candidate materials for distribution transformers because of their very low energy losses and are also being used in brazing and soldering applications.

Laxmanan, V.↗

Dynamics of interfacial pattern formation

A phenomenological model of dendritic solidification incorporating interfacial kinetics, crystalline anisotropy, and a local approximation for the dynamics of the thermal diffusion field is proposed. The preliminary results are in qualitative agreement with natural dendrite-like pattern formation.

Ben-Jacob, E.↗

The growth of metastable peritectic compounds

The effects of directional solidification processing on the microstructural, compositional, and magnetic properties of high-melting-temperature, commercially important alloys which form from the liquid state via peritectic or eutectic type reactions were determined. Emphasis was placed on ferromagnetic compounds of the commercially important Co-Sm and Al-Mn systems. The primary dendrite spacing for eutectic Sm2Co17/Co scaled with negative square root of V and varied from approximately 50 microns for V 20 cm/h to hundreds of microns for V 10 cm/h. Since the crystal growth mechanism was dendritic rather than cooperative, the assoicated permanent magnet properties were rather poor. Magnetization as a function of sample orientation indicates that the easy axis of magnetization was primarily along the direction of solidification for the eutectic Sm2Co17/Co and peritectic SmCo5/Sm2Co17 compositions. For the Al-Mn case, magnetization and microstructural characterization suggest isotropic, polycrystalling growth for all solidification velocities studied.

Pirich, R. G.↗

Solid/melt interface studies of high-speed silicon sheet growth

Radial growth-rate anisotropies and limiting growth forms of point nucleated, dislocation-free silicon sheets spreading horizontally on the free surface of a silicon melt have been measured for (100), (110), (111), and (112) sheet planes. Sixteen-millimeter movie photography was used to record the growth process. Analysis of the sheet edges has lead to predicted geometries for the tip shape of unidirectional, dislocation-free, horizontally growing sheets propagating in various directions within the above-mentioned planes. Similar techniques were used to study polycrystalline sheets and dendrite propagation. For dendrites, growth rates on the order of 2.5 m/min and growth rate anisotropies on the order of 25 were measured.

Ciszek, T. F.↗

Studies of the Crystallization Process of Aluminum-Silicon Alloys Using a High Temperature Microscope

It is shown that primary silicon crystals grow polyhedral in super-eutectic AlSi melts and that phosphorus additives to the melt confirm the strong seeding capacity. Primary silicon exhibits strong dendritic seeding effects in eutectic silicon phases of various silicon alloys, whereas primary aluminum does not possess this capacity. Sodium addition also produces a dendritic silicon network growth in the interior of the sample that is attributed to the slower silicon diffusion velocity during cooling.

Justi, S.↗

Metals Electroprocessing in Molten Salts

The present study seeks to explain the poor quality of solid electrodeposits in molten salts through a consideration of the effects of fluid flow of the electrolyte. Transparent cells allow observation of electrolyte circulation by a laser schlieren optical technique during the electrodeposition of solid zinc from the molten salt electrolyte, ZnCl2 - LiCl-KCl. Experimental variables are current, density, electrolyte composition, and cell geometry. Based on the results of earlier electrodeposition studies as well as reports in the literature, these parameters are identified as having the primary influence on cell performance and deposit quality. Experiments are conducted to measure the fluid flow patterns and the electrochemical cell characteristics, and to correlate this information with the morphology of the solid electrodeposit produced. Specifically, cell voltage, cell current, characteristic time for dendrite evolution, and dendrite growth directions are noted. Their relationship to electrolyte flow patterns and the morphology of the resulting electrodeposit are derived. Results to date indicate that laser schlieren imaging is capable of revealing fluid flow patterns in a molten salt electrolyte.

Sadoway, D. R.↗

Surface film effects on drop tube undercooling studies

The effects of various gaseous atmospheric constituents on drop-tube solidified samples of elemental metals were examined from a microstructural standpoint. All specimens were prepared from the purest available elements, so effects of impurities should not account for the observed effects. The drop-tube gas has a definite effect on the sample microstructure. Most dramatically, the sample cooling rate is effected. Some samples receive sufficient cooling to solidify in free fall while others do not, splating at the end of the drop tube in the sample catcher. Gases are selectively absorbed into the sample. Upon solidification gas can become less soluble and as a result forms voids within the sample. The general oxidation/reduction characteristics of the gas also affect sample microstructures. In general, under the more favorable experimental conditions including reducing atmospheric conditions and superheatings, examination of sample microstructures indicates that nucleation has been suppressed. This is indicated by underlying uniform dendrite spacings throughout the sample and with a single dendrite orientation through most of the sample. The samples were annealed yielding a few large grains and single or bi-crystal samples were commonly formed. This was especially true of samples that were inadvertently greatly superheated. This is in contrast with results from a previous study in which surface oxides were stable and contained numerous sites of nucleation. The number of nucleation events depends upon the surface state of the specimen as determined by the atmosphere and is consistent with theoretical expectations based upon the thermodynamic stability of surface oxide films. Oxide-free specimens are characterized by shiny surfaces, with no observable features under the scanning electron microscope at 5000X.

Ethridge, E. C.↗

Silicon material and JPL Web Team

Silicon material activities are described. Topics discussed include: fluidized bed technology, model predictions (reaction kinetics and grid design parameters), seed-particle cleaning procedure, runaway nucleation, thermal analysis of dendritic ribbons, and residual stress in dendritic ribbons.

Lutwack, R.↗

Process research of non-Cz material

Efforts were aimed at achieving a simultaneous front and back junction. Lasers and other heat sources were tried. Successful results were gained by two different methods: laser and flash lamp. Polymer dopants were applied to both sides of dendritic web cells. Rapid heating and cooling avoided any cross contamination between two junctions after removal of the dendrites. Both methods required subsequent thermal annealing in an oven to produce maximum efficiency cells.

Campbell, R. B.↗

Microstructure and stability of melt spun INCONEL 713 LC

The alloy IN-714LC was used in an investigation of the effect of process parameters on the microstructure of a rapidly solidified melt-spun material. The resultant ribbon microstructure consisted of several distinct regions, each of which corresponds to a different thermal history during processing. A chill zone of equiaxed randomly-oriented grains exists in a region of the foil which was in contact with the wheel during casting. This zone develops into a dendritic growth morphology with distance away from the lower ribbon surface. Dendrites inclined in the direction of wheel rotation result from growth into a flowing stream. TEM studies showed that a cell structure formed, the cell size decreasing with increasing wheel speed. Aging studies indicated that the cell structure plays an important role in gamma prime precipitation. Results relating to heat treatments (as would be encountered in compaction and use) and the stability of the melt-spun structure are considered.

Antolovich, S. D.↗

A study of the microstructure of a rapidly solidified nickel-base superalloy modified with boron

The microstructures of melt-spun superalloy ribbons with variable boron levels have been studied by transmission electron microscopy. The base alloy was of approximate composition Ni-11% Cr-5%Mo-5%Al-4%Ti with boron levels of 0.06, 0.12, and 0.60 percent (all by weight). Thirty micron thick ribbons display an equiaxed chill zone near the wheel contact side which develops into primary dendrite arms in the ribbon center. Secondary dendrite arms are observed near the ribbon free surface. In the higher boron bearing alloys, boride precipitates are observed along grain boundaries. A concerted effort has been made to elucidate true grain shapes by the use of bright field/dark field microscopy. In the low boron alloy, grain shapes are often convex, and grain faces are flat. Boundary faces frequently have large curvature, and grain shapes form concave polygons in the higher boron level alloys. It is proposed that just after solidification, in all of the alloys studied, grain shapes were initially concave and boundaries were wavy. Boundary straightening is presumed to occur on cooling in the low boron alloy. Boundary migration is precluded in the higher boron alloys by fast precipitation of borides at internal interfaces.

Speck, J. S.↗

Comparison of structures of gas atomized and of emulsified highly undercooled Ni-Sn alloy droplets

A comparison is made of microstructures of droplets of Ni-Sn alloys rapidly solidified by gas atomization and in a glass emulsifying medium. Cooling rate of the gas atomized particles ranged from 10 to the 3rd to 10 to the 6th K/s depending on droplet diameter (20-230 microns). In the hypoeutectic alloy studied, /Ni-(25 wt pct Sn)/, most particles showed a dendritic structure. These same particles, melted and resolidified in a glass medium using DTA (Differential Thermal Analysis), showed undercoolings up to 280 K: the structures were dendritic at low undercoolings and nondendritic at undercoolings above 220 K. It is concluded that the gas atomized particles exhibited little or no undercooling before nucleation; the solidification time of the undercooled emulsified droplets is substantially less than that of gas atomized droplets, and the undercooling required to achieve nondendritic structure depends on sample size.

Yamamoto, M.↗

Local convective flows in partly solidified alloys

Channel formation in a dendritic mushy zone is examined with reference to experimental results obtained for an acqueous system, NH4Cl-H2O, and a low-melting metallic system, Pb-Sn. The problems of channel nucleation, propagation, and prevention are considered for a configuration in which heat flow is directed downwards and growth occurs upwards into a positive temperature gradient. It is found that channels nucleate at the growth front by double diffusive perturbations into the quiescent bulk liquid, and not by perturbations within the dendritic framework of the mushy zone.

Hellawell, A.↗

Solidification of undercooled Ni-Sn eutectic alloy under microgravity conditions in the Space Shuttle

The Space Shuttle Columbia carried an Alloy Undercooling Experiment on its STS 61-C mission in January, 1986. The experiment was performed in an electromagnetic levitator. A sample of Ni-32.5 wt pct Sn eutectic was melted and solidified under microgravity conditions in the Space Shuttle. The specimen achieved only a fairly small undercooling, probably less than 30 K. The specimen was examined by optical and scanning electron microscopy. The surface and cross-sectional microstructures were primarily composed of normal lamellar eutectic, but showed several interesting features, including an apparent surface nucleation site, curved dendrites with nonorthogonal secondary arms, dendrite fragments with extremely fine arm spacing, submicron precipitates, and faceted crystals. The results of the space experiment are presented and compared with ground-based results obtained with the same alloy.

Piccone, T. J.↗

Rapid solidification of levitation melted Ni-Sn alloy droplets with high undercooling

Experimental results obtained by high-speed optical temperature sensing for the rapid solidification of highly undercooled, levitation-melted Ni-Sn alloy droplets are presented. These data suggest a solidification model proceeding according to overlapping steps: (1) dendritic growth within the bulk undercooled melt, (2) continued recalescence as supersaturation of the interdendritic liquid dissipates, (3) fine-scale remelting within the dendrites, (4) ripening of the fine structure, and (5) solidification of remaining liquid at the end of recalescence.

Shiohara, Yuh↗