Instability in Rotating Machinery

The proceedings contain 45 papers on a wide range of subjects including flow generated instabilities in fluid flow machines, cracked shaft detection, case histories of instability phenomena in compressors, turbines, and pumps, vibration control in turbomachinery (including antiswirl techniques), and the simulation and estimation of destabilizing forces in rotating machines. The symposium was held to serve as an update on the understanding and control of rotating machinery instability problems.

Source record↗

Linear elastic fracture mechanics primer

This primer is intended to remove the blackbox perception of fracture mechanics computer software by structural engineers. The fundamental concepts of linear elastic fracture mechanics are presented with emphasis on the practical application of fracture mechanics to real problems. Numerous rules of thumb are provided. Recommended texts for additional reading, and a discussion of the significance of fracture mechanics in structural design are given. Griffith's criterion for crack extension, Irwin's elastic stress field near the crack tip, and the influence of small-scale plasticity are discussed. Common stress intensities factor solutions and methods for determining them are included. Fracture toughness and subcritical crack growth are discussed. The application of fracture mechanics to damage tolerance and fracture control is discussed. Several example problems and a practice set of problems are given.

Wilson, Christopher D.↗

More About Brazing Or Welding NiAl Without Filler

Two reports present additional information about two processes for joining, brazing, or welding workpieces made of nickel aluminide alloys, without use of filler metal. Joining processes involve uniform heating in vacuum-controlled furnace. Eliminates internal thermal gradients in workpieces joined and greatly reduces tendency toward cracking.

Moore, Thomas J.↗

The Test and Evaluation of a Non-Chromate Finishing Agent

This research is focused on the design, development and implementation of an industry, military and commercial standard testing cell for surface coatings, which focuses on advanced non-chromate materials technology and their commercialization. Currently, within both private and commercial sectors, chromates are used in the corrosion prevention. processes. However, there is a great demand for chromate-free systems that are able to provide equal protection. At the end of this effort, it is intended that a patented alternative to chromate conversion coatings would be tested and processed for commercialization. Thus far, research studies have been concerned primarily with current corrosion knowledge and testing methods. Corrosion can be classified into five categories: The first type is uniform corrosion which is dominated by a uniform thinning due to an even and regular loss of metal. The second type is called localized corrosion in which most of the loss occurs in discrete areas. The third type, metallurgically influenced corrosion is a form of attack where metallurgy plays a significant role. The fourth type, titled mechanically assisted degradation is a form of attack where velocity, abrasion, and hydrodynamics control the corrosion process. The last type of corrosion is defined as environmentally induced cracking which occurs when cracks are produced under specific, premeditated stress. Oddly enough, with these varying classifications, there are not as many standardized corrosion testing sites. Two of the most common testing methods for corrosion are salt spray testing and filiform. Although neither has proven to be absolute, in terms of the resulting observations, our research aims to help provide data that may be used to support the standardization for corrosion testing. We would acquire and use a Singleton Cyclic Corrosion Testing Chamber. Singleton test chambers perform a wide range of commonly used catalytic corrosion tests. They are used throughout the industry, some of which are - automotive, aerospace, electronic and many more. In addition to this, Singleton test chambers are fully expandable to accommodate cyclic corrosion testing needs. Singleton chambers are also designed for complete compliance and conformity with ASTM (American Society for Testing and Materials), military and commercial standards.

Gulley, H.↗

Stressed Oxidation Life Prediction for C/SiC Composites

The residual strength and life of C/SiC is dominated by carbon interface and fiber oxidation if seal coat and matrix cracks are open to allow oxygen ingress. Crack opening is determined by the combination of thermal, mechanical and thermal expansion mismatch induced stresses. When cracks are open, life can be predicted by simple oxidation based models with reaction controlled kinetics at low temperature, and by gas phase diffusion controlled kinetics at high temperatures. Key life governing variables in these models include temperature, stress, initial strength, oxygen partial pressure, and total pressure. These models are described in this paper.

Levine, Stanley R.↗

The Tensile Properties of Advanced Nickel-Base Disk Superalloys During Quenching Heat Treatments

There is a need to increase the temperature capabilities of superalloy turbine disks. This would allow full utilization of higher temperature combustor and airfoil concepts under development. One approach to meet this goal is to modify the processing and chemistry of advanced alloys, while preserving the ability to use rapid cooling supersolvus heat treatments to achieve coarse grain, fine gamma prime microstructures. An important step in this effort is to understand the key high temperature tensile properties of advanced alloys as they exist during supersolvus heat treatments. This could help in projecting cracking tendencies of disks during quenches from supersolvus heat treatments. The objective of this study was to examine the tensile properties of two advanced disk superalloys during simulated quenching heat treatments. Specimens were cooled from the solution heat treatment temperatures at controlled rates, interrupted, and immediately tensile tested at various temperatures. The responses and failure modes were compared and related to the quench cracking tendencies of disk forgings.

Gabb, Timothy P.↗

Oxidation Through Coating Cracks of SiC-Protected Carbon/Carbon

The oxidation of SiC-protected carbon/carbon through machined slots and naturally occurring craze cracks in the SiC was studied. The slot and crack geometries were characterized, and the subsurface oxidation of the carbon/carbon substrate at temperatures of 1000 to 1300 C in air was assessed using weight change, x-ray computed tomography, and optical microscopy of sections. Rate constants were derived from these measurements and compared with a two-step diffusion control model of carbon oxidation. Oxidation kinetic measurements on both the specimens with machined slots and with naturally occurring craze cracks showed good agreement with the model.

Jacobson, Nathan S.↗

Oxidation Through Coating Cracks of SiC-Protected Carbon/Carbon

The oxidation of SiC-protected carbon/carbon through machined slots and naturally occurring craze cracks in the SiC was studied. The slot and crack geometries were characterized, and the subsurface oxidation of the carbon/carbon substrate at temperatures of 1000 to 1300 C in air was assessed using weight change, x-ray computed tomography, and optical microscopy of sections. Rate constants were derived from these measurements and compared with a two-step diffusion control model of carbon oxidation. Oxidation kinetic measurements on both the specimens with machined slots and with naturally occurring craze cracks showed good agreement with the model.

Jacobson, Nathan S.↗

Oxidation Through Coating Cracks of SiC-Protected Carbon/Carbon

The oxidation of SiC-protected carbon/carbon through machined slots and naturally occurring craze cracks in the SiC was studied. The slot and crack geometries were characterized, and the subsurface oxidation of the carbon/carbon substrate at temperatures of 1000 to 1300 C in air was assessed using weight change, x-ray computed tomography, and optical microscopy of sections. Rate constants were derived from these measurements and compared with a two-step diffusion control model of carbon oxidation. Oxidation kinetic measurements on both the specimens with machined slots and with naturally occurring craze cracks showed good agreement with the model.

Jacobson, Nathan S.↗

Injection Parameters That Promote Branching of Hydraulic Cracks

Fluid injection into rock formations can either produce complex branched hydraulic fractures, create simple planar fractures, or be dominated by porous diffusion. Currently, the optimum injection parameters to create branched fractures are unknown. We conducted repeatable hydraulic fracturing experiments using analog-rock samples with controlled heterogeneity to quantify the fluid parameters that promote fracture branching. A large range of injection rates and fluid viscosities were used to investigate their effects on induced fracture patterns. Paired with a simple analytical model, our results identify the threshold at which fracture transitions from an isolated planar crack to branched cracks when closed natural fractures exist. These results demonstrate that this transition can be controlled by injection rate and fluid viscosity. In relation to the field practices, the present model predicts slickwater and lower viscosity fluid injections promote fracture branching, with the Marcellus shale used as an example.

58 GEOSCIENCES↗

Failure Mechanisms During Isothermal Fatigue of SiC/Ti-24Al-11Nb Composites

Failure mechanisms during isothermal fatigue of unidirectional SiC/Ti-24Al-11Nb (at.%) composites have been determined by microstructural analysis of samples from tests interrupted prior to the end of life and from tests conducted to failure. Specimens from three regions of life were examined based on the maximum strain from a fatigue life diagram: Region 1 (high strain), Region 2 (mid-strain) and Region 3 (low strain). Crack lengths were also measured from interrupted samples and compared based on temperature (23-815 C), region of life and numbers of cycles. Region 1 was controlled by fiber-dominated failure. A transition zone was observed between Regions 1 and 2 due to competition between failure mechanisms. Failure in Region 2 was generally described as surface-initiated cracking with varying amounts of fiber bridging. However, the specific descriptions of crack propagation through the fibers and matrix varied with strain and temperature over this broad region. Region 3 exhibited endurance behaviour at 23 C with no cracking after lO(exp 6) cycles. However at 425 C, surface-initiated cracking was observed after 10(exp 6) cycles with fractured fibers in the crack wake. If endurance behaviour exists for conditions of isothermal fatigue in air at temperatures of greater than or equal to 425 C, it may only be found at very low strains and at greater than 10(exp 6) cycles.

Brindley, P. K.↗

Oxygen Diffusion and Reaction Kinetics in Continuous Fiber Ceramic Matrix Composites

Previous stressed oxidation tests of C/SiC composites at elevated temperatures (350 C to 1500 C) and sustained stresses (69 MPa and 172 MPa) have led to the development of a finite difference cracked matrix model. The times to failure in the samples suggest oxidation occurred in two kinetic regimes defined by the rate controlling mechanisms (i.e. diffusion controlled and reaction controlled kinetics). Microstructural analysis revealed preferential oxidation along as-fabricated, matrix microcracks and also suggested two regimes of oxidation kinetics dependent on the oxidation temperature. Based on experimental results, observation, and theory, a finite difference model was developed. The model simulates the diffusion of oxygen into a matrix crack bridged by carbon fibers. The model facilitates the study of the relative importance of temperature, the reaction rate constant, and the diffusion coefficient on the overall oxidation kinetics.

Halbig, Michael C.↗

Inversion-based correction of Double-Torsion (DT) subcritical crack growth tests for crack profile geometry

Because of its simplicity and the ability to produce a stable, slow-propagating crack, the Double-Torsion (DT) method has been used widely for investigating the critical and subcritical propagation of a slow-propagating tensile (mode-I) crack. However, to determine the complex relationship between the crack velocity $\mathcal{v_c}$ vs. the strain energy release rate $\mathscr{G}$ (or the stress intensity factor K) from laboratory measurements, several corrections must be made to account for the impact of sample and crack geometry. Particularly, DT test typically produces a crack with a curved edge profile instead of a straight line, causing the local $\mathcal{v_c}$ and $\mathscr{G}$ vary along the crack front. The experimentally measured $\mathcal{v_c}$ and $\mathscr{G}$ data merely reflect collective, averaged behavior of the crack. This makes inversion for the intrinsic, “true” crack growth kinetics necessary, based upon the knowledge of the crack geometry. Simple and effective correction methods have been proposed and validated for the slow, chemical-reaction-controlled part (Region I) of the $\mathcal{v_c}$-$\mathscr{G}$ curve. However, reliable methods for the highly nonlinear, transport-dominated part (Region II) and its sudden transition to the dynamic propagation part (Region III) are still lacking. Here we propose a method for determining the intrinsic $\mathcal{v_c}$-$\mathscr{G}$ relationship across all three Regions based upon DT test data, using a simple model function and its numerical inversion. The performance of this approach is examined and demonstrated using both synthetic and laboratory data for subcritical crack growth in soda lime glass.

42 ENGINEERING↗

Fabrication of yttrium hydride for high-temperature moderator application

We report given the superior thermal stability and highly attainable hydrogen density, yttrium hydride is an excellent high-temperature moderator material in advanced thermal neutron spectrum reactors that require small core volumes. Large-scale, crack-free, bulk yttrium hydride is in high demand; however, fabrication of yttrium hydride is challenging and has not been demonstrated for nearly half century. The associated challenges are discussed herein. In response to these challenges, a hydriding system was designed and constructed at Oak Ridge National Laboratory and was used to successfully fabricate crack-free yttrium hydride in complex geometries at large scales. This was accomplished by precisely controlling the hydrogen’s partial pressure and the retort temperature, which was informed by the well-established thermodynamic properties of the binary H–Y system. Hydrogen content in as-fabricated hydride was determined by weight change, an approach which was considered reliable based on the use of ultra–high-purity yttrium, the absence of oxide phases up to levels detectable using x-ray diffraction (XRD), and the significant weight gain. Hydrogen distribution along one yttrium hydride rod was evaluated with XRD analysis on materials extracted from different locations on the rod. The results indicated a relatively homogeneous hydrogen distribution along the hydride rod, with <3% uncertainty in the fraction of the δ-phase hydride. In addition, significant efforts are being dedicated to establish a complete database summarizing the thermomechanical and physical properties of as-fabricated yttrium hydride and the irradiation response to facilitate its deployment as a high-temperature moderator in advanced nuclear reactors.

36 MATERIALS SCIENCE↗

Physical and Thermomechanical Properties of Yttrium Hydride from Large Scale Bulk Metal Hydriding Furnace

Given the superior thermal stability and highly attainable hydrogen density, yttrium hydride is an excellent high-temperature moderator material in advanced thermal neutron spectrum reactors that require small core volumes. Yttrium hydride has been selected as the moderator material for the Transformational Challenge Reactor, which was launched at Oak Ridge National Laboratory (ORNL) in 2019. However, fabrication of large-scale crack-free yttrium hydride is challenging and very limited efforts have been committed to the characterization of bulk yttrium hydride in response to the need to establish a complete database of the thermomechanical properties of YHx. In this report, the challenges associated with fabricating large-scale crack-free yttrium hydride are discussed herein. In response to those challenges, a hydriding system was designed and constructed at ORNL and was used to successfully fabricate crack-free yttrium hydride in complex geometries at large scales. This was accomplished by precisely controlling the hydrogen’s partial pressure and the retort temperature, which was informed by the well-established thermodynamic properties of the binary H-Y system. Hydrogen content in as-fabricated hydride was determined by the weight change method and vacuum hot extraction technique, complemented by the X-ray diffraction (XRD). In addition, significant efforts are being dedicated to establishing a complete database of the thermomechanical properties of as-fabricated yttrium hydride. In FY2020, we investigated the thermophysical properties of yttrium hydrides as a function of temperature (room temperature to 700°C) and hydrogen concentration (H/Y ratio ranges from 1.52 to 1.93). The results indicate that at the temperatures below 300 °C, the hydrogen content did not have a significant influence on the thermal expansion, while the specific heat capacity, the thermal diffusivity, and the calculated thermal conductivity were slightly higher for the higher H/Y ratio. Between 300°C and 700 °C, a reversible second-order endothermic transition in all measured thermal properties was observed. It was also found that the onset temperatures of the observed transition varied, with the composition having inverse dependence on the hydrogen content. An attempt was made to explain the behavior of the thermophysical properties at higher temperatures by considering the order– disorder transition as a result of hydrogen redistribution. In addition, nanoindentation was employed to determine the elastic modulus and hardness and to capture the crystal orientation dependence of these parameters. Vickers hardness was also reported. The final section of the report introduces ongoing neutron irradiation campaign of yttrium hydride.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Friction, deformation and fracture of single-crystal silicon carbide

Friction experiments were conducted with hemispherical and conical diamond riders sliding on the basal plane of silicon carbide. The results indicate that, when deformation is primarily elastic, the friction does not depend on crystallographic orientation and there is no detectable fracture or cracking. When, however, plastic deformation occurs, silicon carbide exhibits anisotropic friction and deformation behavior. Surface fracture crack patterns surrounding wear tracks are observed to be of three types. The crack-geometries of two types are generally independent of orientation, the third crack, however, depends on the orientation. All surface cracks extend into subsurface. Anisotropic friction, deformation and fracture on the basal plane are primarily controlled by the slip system and cleavage.

Miyoshi, K.↗

The thermal fatigue resistance of H-13 Die Steel for aluminum die casting dies

The effects of welding, five selected surface coatings, and stress relieving on the thermal fatigue resistance of H-13 Die Steel for aluminum die casting dies were studied using eleven thermal fatigue specimens. Stress relieving was conducted after each 5,000 cycle interval at 1050 F for three hours. Four thermal fatigue specimens were welded with H-13 or maraging steel welding rods at ambient and elevated temperatures and subsequently, subjected to different post-weld heat treatments. Crack patterns were examined at 5,000, 10,000, and 15,000 cycles. The thermal fatigue resistance is expressed by two crack parameters which are the average maximum crack and the average cracked area. The results indicate that a significant improvement in thermal fatigue resistance over the control was obtained from the stress-relieving treatment. Small improvements were obtained from the H-13 welded specimens and from a salt bath nitrogen and carbon-surface treatment. The other surface treatments and welded specimens either did not affect or had a detrimental influence on the thermal fatigue properties of the H-13 die steel.

Source record↗

Large-displacement structural durability analyses of simple bend specimen emulating rocket nozzle liners

Large-displacement elastic and elastic-plastic, finite-element stress-strain analyses of an oxygen-tree high-conductivity (OFHC) copper plate specimen were performed using an updated Lagrangian formulation. The plate specimen is intended for low-cost experiments that emulate the most important thermomechanical loading and failure modes of a more complex rocket nozzle. The plate, which is loaded in bending at 593 C, contains a centrally located and internally pressurized channel. The cyclic crack initiation lives were estimated using the results from the analyses and isothermal strain-controlled low-cycle fatigue data for OFHC copper. A comparison of the predicted and experimental cyclic lives showed that an elastic analysis predicts a longer cyclic life than that observed in experiments by a factor greater than 4. The results from elastic-plastic analysis for the plate bend specimen, however, predicted a cyclic life in close agreement with experiment, thus justifying the need for the more rigorous stress-strain analysis.

Arya, Vinod K.↗