At least 307 records · Page 17

Effect of Volumetric Energy Density on Microstructure and Properties of Grade 300 Maraging Steel Fabricated by Laser Powder Bed Fusion

Here this study investigated the effect of laser powder bed fusion process parameters on the microstructure and properties of maraging steel. The results show that the process parameters can be finetuned to achieve both a high build rate/low hardness and low build rate/high hardness during fabrication, enabling the co-design of components where property gradients are desirable such as an injection molding tool where surface hardness is desired to be higher than the bulk, which needs to have higher fracture toughness.

36 MATERIALS SCIENCE↗

High temperature high strength austenitic steel fabricated by laser powder-bed fusion

Extremely fast cooling rates during laser powder-bed fusion (LPBF) can result in materials with unique microstructures. For LPBF 316L stainless steel, the formation of sub-grain cellular structures with high dislocation density has been linked to superior tensile properties at room temperature. This cellular structure offers also a new route for the development of high temperature LPBF steels with the nucleation of nano-size strengthening carbides in the cell walls. HK30Nb steel (Fe-25Cr-20Ni-Nb-C) was, therefore, fabricated by LPBF to evaluate its potential for high temperature applications. Optimization of the fabrication parameters yielded material with density greater than 99.7%, with nano Nb-rich precipitates in the cell walls. Annealing at 800 °C for 5h resulted in the nucleation and growth of additional precipitates mainly in the cell walls and at grain boundaries. Furthermore, the high dislocation density led to yield strength at 20–900 °C two to three times higher than yield strength for cast HK30Nb and the nano carbides in the cell walls significantly improved the cellular structure stability at 800 °C.

36 MATERIALS SCIENCE↗

Long-term thermal aging behavior and strength reduction in a laser powder bed fusion 316H stainless steel

The long-term thermal stability of structural alloys is essential for ensuring the safe and reliable operation of nuclear reactors and other power plants. While extensive research has explored the effects of thermal aging on conventional stainless steels, the behavior of additively manufactured (AM) alloys remains less understood. This study examines the thermal aging response of laser powder bed fusion (LPBF) 316H stainless steel (SS) at temperatures ranging from 550 °C to 750 °C over durations of up to 10,000 h (approximately 1.14 years). Advanced characterization techniques, including electron microscopy and synchrotron X-ray diffraction, were used to investigate dislocation recovery and phase evolution. Based on these findings, a time-temperature-precipitation (TTP) diagram was developed for LPBF 316H SS, revealing a 10- to100-fold acceleration in precipitation kinetics compared to wrought 316H SS. A physics-informed model was calibrated using the short-term experimental data, enabling predictions of average precipitate sizes, volume fractions of M 23 C 6 and Laves phases, and changes in molybdenum solute concentration for aging up to 1 × 10⁶ h (114 years). These microstructural insights were further utilized to estimate yield strength and extrapolate strength reduction factors over the extended aging period. Despite the accelerated aging kinetics, LPBF 316H SS demonstrated superior yield strength retention compared to its wrought counterpart. In conclusion, this study establishes a framework for evaluating long-term performance using short-term experimental data and supports the accelerated qualification of AM materials for high-temperature structural applications.

Laser powder bed fusion↗

Mitigating keyhole pore formation by nanoparticles during laser powder bed fusion additive manufacturing

Keyhole pore formation is one of the most detrimental subsurface defects in the laser metal additive manufacturing process. However, effective ways to mitigate keyhole pore formation beyond tuning laser processing conditions during keyhole mode laser melting are still lacking. Here we report a novel approach to mitigate keyhole pore formation during laser powder bed fusion (LPBF) process by using stable nanoparticles. The critical keyhole depth for keyhole pore generation (i.e., the largest keyhole depth without keyhole pore formation) during LPBF of Al6061 increases from 246 µm to 454 µm (85% increase) after adding TiC nanoparticles. In-depth x-ray imaging studies and thermo-fluid dynamics simulation enable us to identify that two mechanisms work together to mitigate keyhole pore generation: (1) adding nanoparticles prevents the keyhole from collapsing by increasing the liquid viscosity to impede the protrusion development; (2) adding nanoparticles slows down the keyhole pore movement by increasing the liquid viscosity, resulting in the recapturing of the pore by the keyhole. We further demonstrate that adding TiC nanoparticles can also eliminate the keyhole fluctuation induced keyhole pore during LPBF of Al6061. Our research provides a potential way to mitigate keyhole pore formation for defect lean metal additive manufacturing.

36 MATERIALS SCIENCE↗

Process optimization of complex geometries using feed forward control for laser powder bed fusion additive manufacturing

Additive manufacturing (AM) enables the fabrication of complex designs that are difficult to create by other means. Metal parts manufactured by laser powder bed fusion (LPBF) can incorporate intricate design features and demonstrate desirable mechanical properties. However, printing a part that is qualified for its intended application often involves reprinting and discarding many parts to eliminate defects, improve dimensional accuracy, and increase repeatability. The process of iteratively converging on the appropriate build parameters increases the time and cost of creating functional LPBF manufactured parts. This work describes a fast, scalable method for part-scale process optimization of arbitrary geometries. Additionally, the computational approach uses feature extraction to identify scan vectors in need of parameter adaptation and applies results from simulation-based feed forward control models. This method provides a framework to quickly optimize complex parts through the targeted application of models with a range of fidelity and by automating the transfer of optimization strategies to new part designs. The computational approach and algorithmic framework are described, a software package is implemented, the method is applied to parts with complex features, and parts are printed on a customized open architecture LPBF machine.

3D printing↗

Correlations between thermal history and keyhole porosity in laser powder bed fusion

Additive manufacturing has the potential to revolutionize the production of metallic components as it yields near net shape parts with complex geometries and minimizes waste. At the present day, additively manufactured components face qualification and certification challenges due to the difficulty in controlling defects. This has driven a significant research effort aimed at better understanding and improving processing controls – yielding a plethora of in-situ measurements aimed at correlating defects with material quality metrics of interest. In this work, we develop machine-learning methods to learn correlations between thermal history and subsurface porosity for a variety of print conditions in laser powder bed fusion. Un-normalized surface temperatures (in the form of black-body radiances) are obtained using high-speed infrared imaging and porosity formation is observed in the sample cross-section through synchrotron x-ray imaging. To demonstrate the predictive power of these features, we present four statistical machine-learning models that correlate temperature histories to subsurface porosity formation in laser fused Ti-6Al4V powder.

36 MATERIALS SCIENCE↗

The origin and formation of oxygen inclusions in austenitic stainless steels manufactured by laser powder bed fusion

The origins of nano-scale oxide inclusions in 316L austenitic stainless steel (SS) manufactured by laser powder bed fusion (L-PBF) was investigated by quantifying the possible intrusion pathways of oxygen contained in the precursor powder, extraneous oxygen from the process environment during laser processing, and moisture contamination during powder handling and storage. When processing the fresh, as-received powder in a wellcontrolled environment, the oxide inclusions contained in the precursor powder were the primary contributors to the formation of nano-scale oxides in the final additive manufactured (AM) product. These oxide inclusions were found to be enriched with oxygen getter elements like Si and Mn. By controlling the extraneous oxygen level in the process environment, the oxygen level in AM produced parts was found to increase with the extraneous oxygen level. The intrusion pathway of this extra oxygen was found to be dominated by the incorporation of spatter particles into the build during processing. Moisture induced oxidation during powder storage was also found to result in a higher oxide density in the AM produced parts. SS 316L powder free of Si and Mn oxygen getters was processed in a well-controlled environment and resulted in a similar level of oxygen intrusion. Finally, microhardness testing indicated that the oxide volume fraction increase from extraneous oxygen did not influence hardness values. However, a marked decrease in hardness was found for the humidified and Si-Mn free AM processed parts.

36 MATERIALS SCIENCE↗

Types of spatter and their features and formation mechanisms in laser powder bed fusion additive manufacturing process

Spatter causes defect formation, powder redistribution and contamination in laser powder bed fusion (LPBF) additive manufacturing process. It is critical to distinguish different types of spatter and understand their features and formation mechanisms. This work reveals the features and formation mechanisms of five unique types of spatter during the LPBF process by in-situ high-speed, high-energy x-ray imaging. Spatters observed during LPBF testing are quantified by their speed, size, and direction. Distinct quantifiable characteristics for each type of spatter are identified. Finally, effects of the laser power, scan speed, and ambient pressure on spatter formation and features are unraveled. A spatter formation map for AlSi10Mg alloy is constructed.

36 MATERIALS SCIENCE↗

Towards improved speed and accuracy of laser powder bed fusion simulations via representation of multiple time scales

Here, we report the result of investigations into alternative representations of the temporal evolution of the laser powder bed fusion (LPBF) process. In order to provide the reader with sufficient context for the following discussion, the modeling challenge and its underlying cause, as well as current attempts to provide a satisfactory solution, will be discussed. Next, the author will describe two numerical methods (multirate time integration and parallel-in-time) to better represent the temporal scales of the problem. Finally, the results of applying these methods to a two-dimensional version of the heat transfer portion of the LPBF problem will be presented, reporting on both convergence and performance behavior, which indicate the possibility of significant speedup of solution calculations (40–100 times), along with well-characterized effects on solution accuracy.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Elucidating the effect of preheating temperature on melt pool morphology variation in Inconel 718 laser powder bed fusion via simulation and experiment

In laser powder bed fusion (L-PBF) additive manufacturing, the mechanical performance, microstructure and defects of fabricated parts are closely associated with the melt pool morphology, e.g., its dimension and shape through the building process. Past studies have largely focused on how the process parameters such as laser power and scan speed affect melt pool characteristics. In this study, the melt pool morphology variation as a function of preheating temperature in the conduction, transition, and keyhole regimes and the underlying mechanisms in each regime are investigated through ex-situ sample characterization and computation thermal fluid dynamics (CtFD) simulation. Single tracks with different combinations of laser power and scan speed are deposited on an Inconel 718 bare plate preheated to a temperature range of 100–500 °C in the experiment. Significant changes are observed in melt pool morphology as a function of preheating temperature from optical measurements of melt track cross sections. The depth of melt pool in the three regimes increases monotonically with preheating temperature, e.g., at 500 °C, the experimental melt pool depth is increased by 49% in conduction regime, 34% in transition regime and 33% in keyhole regime, respectively, while the variation of melt pool width in each regime does not all follow an increasing trend but depends on the melt pool regimes. Melt pool width variation in the conduction and transition regimes is found to depend on the enhanced heat conduction directly related to temperature dependent thermal properties. Through validated CtFD simulations, it is found that in the keyhole regime the evaporation mass, recoil pressure, and laser drilling effect is enhanced with higher preheating temperature, which gives rise to a deeper melt pool. The simulations also reveal that preheating temperature significantly elongates the melt track length due to the increased flow rate and strong recoil pressure that accelerates the backward flow.

36 MATERIALS SCIENCE↗

Effects of spatial energy distribution-induced porosity on mechanical properties of laser powder bed fusion 316L stainless steel

Laser powder bed fusion (LPBF) additive manufacturing (AM) offers a variety of advantages over traditional manufacturing, however its usefulness for manufacturing of high-performance components is currently hampered by internal defects (porosity) created during the LPBF process that have an unknown impact on global mechanical performance. By inducing porosity distributions through variations in print energy density and inspecting the resulting tensile samples using computed tomography, nearly 50,000 pores across 75 samples were identified. Porosity characteristics were quantitatively extracted from inspection data and compared with mechanical properties to understand the strength of relationships between porosity and global tensile performance. Useful porosity characteristics were identified for prediction of part performance. Results indicate that ductility and strain at ultimate tensile strength are the global tensile properties most significantly impacted by porosity and can be predicted with reasonable accuracy using simple porosity shape descriptors such as volume, diameter, and surface area. Moreover, it was found that the largest pores influenced behavior most significantly. Specifically, pores in excess of 125 µm in diameter were found to be a sufficient threshold for property estimation. These results establish an initial understanding of the complex defect-performance relationship in AM 316L stainless steel and can be leveraged to develop certification standards and improve confidence in part quality and reliability for the broader set of engineering alloys.

36 MATERIALS SCIENCE↗

Deformation and fracture behavior of a laser powder bed fusion processed stainless steel: In situ synchrotron x-ray computed microtomography study

Tensile plastic deformation and fracture behavior of a laser powder bed fusion processed 316L stainless steel alloy was investigated in situ using high-resolution synchrotron x-ray computed microtomography (sXCT). Three different cases were studied: (1) specimen A1, near full-density with initial porosity of 0.04%, (2) specimen B1, initial lack-of-fusion (LOF) porosity of about 3% with the major axis of defects aligned nearly perpendicular to the tensile loading direction (LD), and (3) specimen B, similar to B1 but with the major axis of LOF defects aligned nearly parallel to LD. The effects of type, density, and orientation of defects in as-printed samples on plastic deformation and failure modes were studied by analyzing sXCT image sequences and quantitative defect properties. Specifically, the evolutions of porosity, size, aspect ratio, and angle of gas pores and LOF defects were characterized as a function of applied strain. Moreover, interactions between as-printed defects and deformation-induced crack propagation were investigated. The tensile behavior of specimen A1 was comparable to that of a commercial wrought plate. Furthermore, the quantitative in-situ sXCT results showed a void-growth phenomenon in A1 but without noticeable coalescence, resulting in a ductile cup-cone failure. Specimen B1 showed damage-driven brittle failure with limited plasticity due to early and rapid propagation of open voids. On the other hand, specimen B, with a similar amount of LOF defects as B1, showed deceivingly strong and ductile tensile behavior similar to A1 without any major crack propagations due to the favorable orientation relationship between LOF defects and the LD.

36 MATERIALS SCIENCE↗

Effect of processing parameters and strut dimensions on the microstructures and hardness of stainless steel 316L lattice-emulating structures made by powder bed fusion

In this study, we present the effects of input processing parameters and strut thickness (in square struts) on microstructure and properties in laser powder bed fusion additively manufactured stainless steel 316L lattice-emulating structures. Lattice-emulating X-structures with square cross-sections of 1.5, 1.0, and 0.5 mm were fabricated using three different parameter sets with varying power, speed, and therefore, linear energy density. Grain size and morphology were shown to be dictated by epitaxial growth, which was dependent on weld pool morphology. Additionally, grain size and morphology were shown to change across the thickness direction of the struts (from the bottom inclined surface to the top inclined surface). The spatial variation in grain size was reflected by changes in hardness through the thickness of each strut. The 0.5 mm struts exhibited more significant grain elongation in the strut direction and larger sub-grain solidification cell diameters than their thicker counterparts. The larger sub-grain solidification cell diameters in the 0.5 mm samples resulted in correspondingly lower hardness values when compared to samples of higher thicknesses.

36 MATERIALS SCIENCE↗

Design of heterogeneous structured Al alloys with wide processing window for laser-powder bed fusion additive manufacturing

Required microstructural attributes of an alloy vary with structural applications. The microstructural fine-tuning capability of laser-powder bed fusion (L-PBF) additive manufacturing (AM) enables application specific manufacture of the components. Such manufacture with L-PBF AM requires alloys that exhibit wide processing window and are amenable to multiple deformation mechanisms. However, high hot cracking susceptibility of Al alloys poses a barrier to such printability-performance synergy. In this work we show that an integration of, a) grain refinement through heterogeneous nucleation, and b) eutectic solidification, leads to crack-free parts at wide range of process parameters, microstructural heterogeneity, and hierarchy in the Al-Ni-Ti-Zr alloy. Such an integration targets hot cracking at multiple stages of solidification in L-PBF as opposed to the contemporary alloy design strategies that target hot-cracking at only specific stages of solidification. The Al-Ni-Ti-Zr alloy exhibits excellent printability and a high as-built tensile performance. Due to the wide processing window and amenability to multiple deformation mechanisms, the alloy microstructure and subsequently the performance, can be fine-tuned. Here, such strategy opens the gateway for application-specific manufacture of Al alloys with L-PBF AM and establishes a fundamental shift in current methodologies for design of these alloys for L-PBF AM.

36 MATERIALS SCIENCE↗

Solidification texture, variant selection, and phase fraction in a spot-melt electron-beam powder bed fusion processed Ti-6Al-4V

The effect of a spot melt strategy on the solidification texture, variant selection, phase fraction, and their variations along the build height was investigated in comparison to a conventional linear melt strategy. Ti-6Al-4V alloy samples were manufactured by an electron-beam powder bed fusion process using two different melt strategies and characterized using high-energy synchrotron x-ray diffraction. The linear and spot melt cases resulted in β<100> cube and fiber textures, respectively, with the cube/fiber axis nearly parallel to the build direction. The α phase exhibited Burgers orientation relationship (BOR) with the parent β phase for both melt strategies. Although all of the key texture components and the BOR between the α and β phases were consistently observed in both cases along the build height, there were several measurable differences between the two. At the top of the build height, the β<100> build texture intensity was stronger in the linear case. However, the texture intensity in the linear case decreased gradually from the top to near the substrate, whereas the spot melt case did not show this trend. Moreover, the BOR was examined along the build height and the results showed that there is a distinct variant selection in the spot melt case, unlike the linear case. Specifically, the planar variants sharing ($\bar101$) β || (0002) α with [$\bar2\bar2\bar2$]β and [$2\bar22$]β were the most prominent in the spot melt, but no preference was identified in the directional variants. The β phase fraction was slightly lower in the spot melt case compared to the linear case. In both the cases, the β phase fraction decreased moving towards the substrate but remained significantly higher than that of the powder feedstock. Overall, the novel spot melt strategy produced a more homogeneous microstructure in terms of both the phase fraction and texture across the build height.

36 MATERIALS SCIENCE↗

A new procedure for implementing the modified inherent strain method with improved accuracy in predicting both residual stress and deformation for laser powder bed fusion

As a metal additive manufacturing (AM) process, laser powder bed fusion (L-PBF) has been widely used to produce parts with complex geometries. The large thermal gradient caused by the fast, intense, and repeated laser scanning induces significant residual deformation and stress to the as-built parts, which increase manufacturing difficulty and geometrical inaccuracy as a result. The modified inherent strain (MIS) method exploiting multiscale process simulations was developed to simulate residual deformation accurately and efficiently. However, the existing procedure of implementing the MIS method is found to give inaccurate residual stress prediction. Here in this work, a new implementation procedure for the MIS method is proposed to improve the simulation accuracy of residual stress without degrading the residual deformation prediction. The new procedure concerns the application of inherent strains to the part-scale layer-by-layer finite element model to obtain residual stress and deformation field. While the existing implementation of the part-scale MIS model involves only mechanical properties at ambient temperature, the new procedure adds one more solution step employing mechanical properties at an elevated temperature determined from the inherent strain extraction step. Both numerical and experimental studies are conducted to validate the proposed new implementation procedure. It shows that by using the new procedure, the MIS-based simulation can predict both residual stress and deformation of as-built L-PBF metal parts with good accuracy.

36 MATERIALS SCIENCE↗

Nanoparticle-enhanced absorptivity of copper during laser powder bed fusion

We report laser powder bed fusion (LPBF) of pure copper for thermal and electrical applications is hampered by its low near-infrared absorptivity and high thermal diffusivity. These material properties make it very difficult to localize the thermal energy needed to produce high density 3D printed parts. Modification of metal powders via nanoparticle additives is a promising approach to increasing absorptivity, but the effect of nanoparticles on absorptivity and melting behavior during LPBF is not well understood. In this study, we developed an in situ calorimetry system to measure effective absorptivity during LPBF on copper substrates. We decorated copper substrates using three nanoparticle systems (CuS, TiB 2 , multilayer graphene flakes) and demonstrated an enhanced absorptivity of the decorated substrates relative to pure copper. Graphene nanoflakes resulted in the highest improved absorption relative to pure copper from 0.09 to 0.48, due to their stability at high laser scanning powers. A thermomechanical model with convective heat transfer provided confidence in the measurements by reproducing the experimental melt pool traces. Full 3D cylindrical prints demonstrated an improvement in relative density of the copper-graphene powder prints (in the range of 0.930–0.992), relative to that of as-purchased copper powder prints (in the range of 0.854–0.972). This work provides a fundamental study of nanoparticle-enabled LPBF of highly reflective metals and demonstrates a viable route for expanding the library of reliably printable metals.

36 MATERIALS SCIENCE↗

Developing ductile and isotropic Ti alloy with tailored composition for laser powder bed fusion

Laser powder bed fusion (LPBF) is an advanced technology to create metallic components with complex geometry. Ti-6Al-4V (Ti64) is one of the most frequently used materials for LPBF. The intrinsic high cooling rates and ultra-high directional thermal gradient of melt, however, lead to a hierarchical structure composed of fine martensitic alpha' within columnar prior-beta grains in LPBF Ti64. This microstructure results in poor ductility and strong mechanical anisotropy in as-built Ti64 components, which largely limit their applications. Here, we report that the above shortcomings can be overcome by tailoring the alloy composition. Specifically, by reducing the aluminum content from 6 wt% to 4 wt%, the resultant LPBF Ti-4Al-4V (Ti44) alloy exhibits substantially improved ductility and mechanical isotropy. These improvements are attributed to grain refinement during solidification and the activation of multiple slip modes and twinning in the as-built material during deformation. This work offers a simple strategy to design new titanium alloys for LPBF with significantly improved ductility and isotropy.