Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ALUMINIZATION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 307 records · Page 17

Reflective Packaging

The aluminized polymer film used in spacecraft as a radiation barrier to protect both astronauts and delicate instruments has led to a number of spinoff applications. Among them are aluminized shipping bags, food cart covers and medical bags. Radiant Technologies purchases component materials and assembles a barrier made of layers of aluminized foil. The packaging reflects outside heat away from the product inside the container. The company is developing new aluminized lines, express mailers, large shipping bags, gel packs and insulated panels for the building industry.

Source record↗

A Multilayer Model for Alumina Inclusion Transformation by Calcium in the Ladle Furnace

Calcium wire injection is widely used for modification of solid alumina inclusions to liquid or partially liquid calcium aluminate. In the present work, a multilayer growth model is proposed for modification of alumina inclusions. Diffusion through a multiphase product layer and mass transfer of solute through the boundary layer to the inclusion are taken into account in this model. It is assumed that the outer surface of the inclusion is thermodynamically in equilibrium with the local steel composition. The results show that the mass transfer of calcium through the boundary layer and within the inclusion is complete in a matter of seconds; furthermore, once the liquid calcium aluminate forms, it quickly consumes the other solid calcium aluminate phases. Because the calcium is so rapidly consumed by the inclusions, the rate of transformation in a calcium treatment process is controlled by the rate that calcium is supplied to the steel by the calcium bubbles.

36 MATERIALS SCIENCE↗

Electronic structural and lattice thermodynamic properties of MAlO2 and M5AlO4 (M = Li, Na, K) sorbents for CO2 capture applications

Abstract The electronic properties and thermal stabilities of MAlO 2 and M 5 AlO 4 (M = Li, Na, K) are investigated by density functional theory and lattice phonon dynamics. Based on the calculated electronic and lattice thermodynamic properties, their abilities to capture CO 2 as solid sorbents are analyzed. The calculated electronic structural properties of MAlO 2 and M 5 AlO 4 indicate that all these alkali aluminates are semiconductors with a bandgap range of 2.4 ~ 6.4 eV. The 1st valence bands of these alkali aluminates are located 0 ~ − 6 eV under Fermi levels and are mainly contributed by p orbitals of O, s and p orbitals of Al and M. The phonon vibrational frequencies of M 5 AlO 4 spread at a lower frequency range compared to their MAlO 2 phases. With increasing temperature, the calculated phonon free energies of M 5 AlO 4 decrease faster than their corresponding MAlO 2 while their entropies have opposite trends. The reaction 2MAlO 2 + CO 2 = M 2 CO 3 + Al 2 O 3 has higher reaction heat and Gibbs free energy change than those of corresponding reaction 2 / 5 M 5 AlO 4 + CO 2 = M 2 CO 3 + 1 / 5 Al 2 O 3 , which shows the former reaction possesses lower turnover temperature. Among the alkali aluminates studied, the β-NaAlO 2 , lt-KAlO 2 , and γ-LiAlO 2 are better candidates that could be applied for CO 2 capture technologies. Graphical Abstract

36 MATERIALS SCIENCE↗

Compliant alkali silicate sealing glass for solid oxide fuel cell applications: the effect of protective alumina coating on electrical stability in dual environment

An alkali-containing silicate glass was recently proposed as a potential sealant for solid oxide fuel cells (SOFC). The glass contains appreciable amount of alkalis and retains its glassy microstructure at elevated temperatures over time. It is more compliant as compared to conventional glass-ceramics sealants and could potentially heal cracks during thermal cycling. In previous papers the thermal cycle stability, thermal stability and chemical compatibility were reported with yttria-stabilized zirconia (YSZ) electrolyte and YSZ-coated ferritic stainless steel interconnect. In this paper, we report the electrical stability of the compliant glass with aluminized AISI441 interconnect material under DC load in dual environment at 700-800oC. Apparent electrical resistivity was measured with a 4-point method for the glass sealed between two aluminized AISI441 metal coupons as well as plain AISI441 substrates. The results showed good electrical stability with the aluminized AISI441 substrate, while unstable behavior was observed for un-coated substrates. In addition, interfacial microstructure was examined with scanning electron microscopy and correlated with the measured resistivity results. Overall, the alumina coating demonstrated good chemical stability with the alkali-containing silicate sealing glass under DC loading.

aluminization↗

Structural characterization of C-S-H and C-A-S-H samples-Part II: Local environment investigated by spectroscopic analyses

Spectroscopic studies ({sup 1}H, {sup 23}Na and {sup 27}Al MAS NMR and Raman spectroscopy) have been used to characterize three series of C-S-H samples (0.8<Ca/Si<1.7): one C-S-H series, one aluminum inserted C-S-H series (named C-A-S-H series), and one sodium and aluminum inserted C-S-H series (named C-N-A-S-H series). Previous Rietveld analyses have been performed on the two first series and have clearly shown that (1) a unique 'tobermorite M defect' structural model allows to describe the C-S-H structure whatever the Ca/Si ratio and (2) the insertion of aluminum into the C-S-H structure led to the degradation of the crystallinity and to a systematic increase of the basal spacing of about 2 A regardless the Ca/(Si+Al) ratio (at a constant Al/Si ratio of 0.1). Spectroscopic investigations indicate that the main part of the Al atoms is readily incorporated into the interlayer region of the C-S-H structure. Al atoms are mainly inserted as four-fold coordinated aluminates in the dreierketten silicate chain (either in bridging or paired tetrahedra) at low Ca/Si ratio. Four-fold aluminates are progressively replaced by six-fold coordinated aluminates located into the interlayer region of the C-S-H structure and bonded to silicate chains. Investigation of the hydrogen bonding in C-S-H indicates that the main part of the hydrogen bonds is intra-main layer, and thus explains the low stacking cohesion of the C-S-H structure leading to its nanometric crystal size and the OD character of the tobermorite like structures. - Graphical abstract: The insertion of aluminum atoms into the C-S-H structure has been investigated by spectroscopic analyses ({sup 27}Al and {sup 1}H MAS NMR and Raman). The previously determined structural continuity, when increasing the C/S ratio from the C-S-H(I) type to the C-S-H(II) type, has been confirmed even in the presence of aluminum.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Study of photoluminescence properties of CaAl{sub 2}O{sub 4}: Eu{sup 2+} prepared by combustion synthesis method

Eu{sup 2+} doped alkaline earth metals such as strontium aluminate, calcium aluminate and barium aluminate prepared by using modified combustion synthesis method at 600°C with Urea as fuel. Crystal structure is determined by using XRD and the sample confirmation by using the FTIR. The effect of the host material on the photoluminescence (PL) and phosphorescence properties were studied by using the Hitachi F-7000 spectrofluorimeter equipped with a 450W Xenon lamp, in the range 200-650 nm. The emission spectra of Eu{sup 2+} range from 450 to 500 nm in the Blue to aqua region and the transition 4f{sup 7}-4f{sup 6} 5d{sup 1}. The observed emission in CaAl{sub 2}O{sub 4} is 440 nm.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

MEASUREMENT OF SPECIFIC HEAT CAPACITY OF SALTSTONE

One of the goals of the Saltstone variability study is to identify (and quantify the impact of) the operational and compositional variables that control or influence the important processing and performance properties of Saltstone grout mixtures. The heat capacity of the Saltstone waste form is one of the important properties of Saltstone mixes that was last measured at SRNL in 1997. It is therefore important to develop a core competency for rapid and accurate analysis of the specific heat capacity of the Saltstone mixes in order to quantify the impact of compositional and operational variations on this property as part of the variability study. The heat capacity, coupled with the heat of hydration data obtained from isothermal calorimetry for a given Saltstone mix, can be used to predict the maximum temperature increase in the cells within the vaults of the Saltstone Disposal Facility (SDF). The temperature increase controls the processing rate and the pour schedule. The maximum temperature is also important to the performance properties of the Saltstone. For example, in mass pours of concrete or grout of which Saltstone is an example, the maximum temperature increase and the maximum temperature difference (between the surface and the hottest location) are controlled to ensure durability of the product and prevent or limit the cracking caused by the thermal gradients produced during curing. This report details the development and implementation of a method for the measurement of the heat capacities of Saltstone mixes as well as the heat capacities of the cementitious materials of the premix and the simulated salt solutions used to batch the mixes. The developed method utilizes the TAM Air isothermal calorimeter and takes advantage of the sophisticated heat flow measurement capabilities of the instrument. Standards and reference materials were identified and used to validate the procedure and ensure accuracy of testing. Heat capacities of Saltstone mixes were {approx} 55% higher than the previous measurement of specific heat capacity on a reference Saltstone mix in 1997. Values of mixes prepared using Deliquification, Dissolution and Adjustment (DDA), Modular Caustic Side Solvent Extraction Unit (MCU) and Salt Waste Processing Facility (SWPF) simulants and premix at 0.60 w/cm ratio were {approx} 1.95 J/g/{sup o}C and were equivalent within experimental error. The simple law of mixtures was used to predict the heat capacities of the Saltstone and the results were in excellent agreement with experimental data. This simple law of mixtures can therefore be used to predict the heat capacities of Saltstone mixes in those cases where measurements have not been made. The time dependence of the heat capacity is important as an input to the modeling of temperature increase in Saltstone vaults. The heat capacity of a mix of MCU and premix at 0.60 w/cm ratio was measured immediately after initial mixing and then periodically up to times greater than 100 days. Within experimental error, the heat capacity did not change with time. Therefore, the modeling is not complicated by requiring a time dependent function for specific heat capacity. The water to cementitious material (w/cm) ratio plays a key role in determining the value of the heat capacity. Both experimental and predictive values for SWPF mixes as function of the w/cm ratio were obtained and presented in this report. Predictions of the maximum temperatures of the Saltstone mixes were made using the heat of hydration data from previous isothermal measurements and the newly measured heat capacities for DDA, MCU and SWPF mixes. The maximum temperature increase ranged from 37 to 48 C for these mixes. The presence of aluminate at 0.33 M produced a temperature increase of 68 C which is close to the adiabatic temperature rise of 74 C observed by Steimke and Fowler in 1997 for a mix containing 0.35 M aluminate. Aluminum dissolution of the sludge will increase the aluminate in the DSS which in turn will result in a larger temperature increase in the Saltstone vaults during the curing period. The initial temperature of the Saltstone mixes in the Saltstone Production Facility (SPF) can be predicted using the specific heat capacities of Decontaminated Salt Solutions (DSS), the specific heat capacities of cementitious materials, and the initial temperatures of the DSS and the premix. This initial mix temperature is dominated by the DSS temperature due to its high heat capacity relative to the cementitious materials. Therefore, controlling the initial temperature of the DSS to lower temperatures will lead to lower maximum temperatures in the vault for a given batch of Saltstone.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Real-time high-resolution X-ray imaging and nuclear magnetic resonance study of the hydration of pure and Na-doped C3A in the presence of sulfates

This study details the differences in real-time hydration between pure tricalcium aluminate (cubic C{sub 3}A or 3CaO {center_dot} Al{sub 2}O{sub 3}) and Na-doped tricalcium aluminate (orthorhombic C{sub 3}A or Na{sub 2}Ca{sub 8}Al{sub 6}O{sub 18}), in aqueous solutions containing sulfate ions. Pure phases were synthesized in the laboratory to develop an independent benchmark for the reactions, meaning that their reactions during hydration in a simulated early age cement pore solution (saturated with respect to gypsum and lime) were able to be isolated. Because the rate of this reaction is extremely rapid, most microscopy methods are not adequate to study the early phases of the reactions in the early stages. Here, a high-resolution full-field soft X-ray imaging technique operating in the X-ray water window, combined with solution analysis by {sup 27}Al nuclear magnetic resonance (NMR) spectroscopy, was used to capture information regarding the mechanism of C{sub 3}A hydration during the early stages. There are differences in the hydration mechanism between the two types of C{sub 3}A, which are also dependent on the concentration of sulfate ions in the solution. The reactions with cubic C{sub 3}A (pure) seem to be more influenced by higher concentrations of sulfate ions, forming smaller ettringite needles at a slower pace than the orthorhombic C{sub 3}A (Na-doped) sample. The rate of release of aluminate species into the solution phase is also accelerated by Na doping.

36 MATERIALS SCIENCE↗

Properties of impurity-bearing ferrihydrite I. Effects of Al content and precipitation rate on the structure of 2-line ferrihydrite

The association of Al with ferrihydrite (Fh) may have a considerable effect on the composition, structure, and surface properties of Fh nanoparticles, and thus impact its reactivity and interaction with pollutant species. Aluminous Fh is abundant in natural environments, but the mode of association of Al with this nanomineral is not yet fully understood. Al{sup 3+} speciation may vary from true chemical substitution for Fe{sup 3+}, to adsorption or surface precipitation, and/or to formation of a mixture of two (or more) individual nanoscale phases. The conditions of formation (i.e. slow vs. rapid precipitation) may also affect the nature of Fh nanoparticles in terms of their crystallinity, phase purity, and Al speciation. In this study we used a variety of laboratory (TEM, NMR, ICP-AES) and synchrotron-based techniques (X-ray total scattering and PDF analysis, scanning transmission X-ray microscopy, Al K-edge XANES spectroscopy) to characterize two synthetic Al-bearing Fh series formed at different precipitation rates in the presence of 5-40 mol% Al. We find that Al is dominantly octahedrally coordinated in the synthetic Fh samples and that up to 20-30 mol% Al substitutes for Fe in the Fh structure, regardless of the synthesis method we used. Formation of separate aluminous phases (e.g., gibbsite) was most significant at Al concentrations above 30 mol% Al in slowly precipitated samples. However, small amounts (<6% of total Al) of Al-hydroxide phases were also detected by NMR spectroscopy in samples with lower Al content (as low as 15 mol% Al), particularly in the Fh series that was precipitated slowly. Furthermore, it appears that the amount of Al incorporated in Fh is not affected by the synthesis methods we used and is more likely controlled by the accumulated strain caused by Al substitution in the Fh lattice. Given the prevalence of naturally occurring aluminous ferrihydrite, assumptions about ferrihydrite reactivity in natural environments should consider the impact of Al substitution on reduction potential, Fe bioavailability, as well as sorption reactions.

58 GEOSCIENCES↗

Tritium trapping in silicon carbide in contact with solid breeder under high flux isotope reactor irradiation

The trapping of tritium in silicon carbide (SiC) injected from ceramic breeding materials was examined via tritium measurements using imaging plate (IP) techniques. Monolithic SiC in contact with ternary lithium oxide (lithium titanate and lithium aluminate) as a ceramic breeder was irradiated in the High Flux Isotope Reactor (HFIR) in Oak Ridge, Tennessee, USA. The distribution of photo-stimulated luminescence (PSL) of tritium in SiC was successfully obtained, which separated the contribution of 14C ß-rays to the PSL. The tritium incident from ceramic breeders was retained in the vicinity of the SiC surface even after irradiation at 1073 K over the duration of ~3000 h, while trapping of tritium was not observed in the bulk region. The PSL intensity near the SiC surface in contact with lithium titanate was higher than that obtained with lithium aluminate. The amount of the incident tritium and/or the formation of a Li2SiO3 phase on SiC due to the reaction with lithium aluminate under irradiation likely were responsible for this observation.

99 GENERAL AND MISCELLANEOUS↗

Formation of Aluminide Coatings on Fe-Based Alloys by Chemical Vapor Deposition

Aluminide and Al-containing coatings were synthesized on commercial ferritic (P91) and austenitic (304L) alloys via a laboratory chemical vapor deposition (CVD) procedure for rigorous control over coating composition, purity and microstructure. The effect of the CVD aluminizing parameters such as temperature, Al activity, and post-aluminizing anneal on coating growth was investigated. Two procedures involving different Al activities were employed with and without including Cr-Al pellets in the CVD reactor to produce coatings with suitable thickness and composition for coating performance evaluation. The phase constitution of the as-synthesized coatings was assessed with the aid of a combination of X-ray diffraction, electron probe microanalysis, and existing phase diagrams. The mechanisms of formation of these CVD coatings on the Fe-based alloys are discussed, and compared with nickel aluminide coatings on Ni-base superalloys. In addition, Cr-Al pellets were replaced with Fe-Al metals in some aluminizing process runs and similar coatings were achieved.

36 MATERIALS SCIENCE↗

Microstructural evolution of an aluminide coating on alloy 625 during wet air exposure at 900 °C and 1000 °C

The microstructural changes of the aluminized alloy 625 during cyclic oxidation in air + 6% H 2 O at 900 °C and 1000 °C were analyzed using optical metallography (OM), scanning electron microscopy (SEM) with energy and wave length dispersive X-ray analysis (EDX/WDX) as well as electron backscatter diffraction (EBSD). An in-house developed thermodynamic-kinetic procedure was employed to predict the microstructural evolution of aluminized alloy 625 during high temperature exposure by considering simultaneously occurring surface oxidation and interdiffusion processes. Because of the lack of mobility data for the relevant alloying elements in the σ-phase, assumptions for the mobilities were made based on the value of the mobilities in α-Cr. Despite these assumptions, the calculated results were found to be in good agreement with experimental observations. The complete depletion of β-NiAl in the coating observed during exposure at 1000 °C was correctly predicted by the model. The model was also able to infer dissolution of the precipitate phases α-Cr and σ in the interdiffusion zone during exposures at 900 °C and 1000 °C. The model was yet unable to predict the formation of the μ-phase in the alloy after 1000 h of exposure at 1000 °C. The developed modelling method offers the potential to predict microstructural changes of aluminized nickel base alloys thus reducing cost and time consuming experimental efforts.

36 MATERIALS SCIENCE↗

Screening of binders for pelletization of CaO-based sorbents for CO{sub 2} capture

CaO-based CO{sub 2} looping cycle technology is a promising method for separation of CO{sub 2} from flue gas and syngas at high temperatures. The process of CO{sub 2} capture is expected to take place in fluidized-bed combustion (FBC) systems, which implies significant attrition and elutriation of the solid sorbent. Hence, both reactivation of spent sorbent and preparation of modified CaO-based sorbent may be required to maximize the performance of the sorbent. We present initial results on the screening of suitable binders for pelletization. Two types of bentonite (Na- and Ca-bentonite) and four types of commercial calcium aluminate cements (CA-14, CA-25, Secar 51, and Secar 80) were investigated here, with a primary focus of maintaining a high CO{sub 2}-capture capacity over 30-35 cycles. The tests were carried out using a thermogravimetric analyzer (TGA), and the results showed that the presence of bentonites led to faster decay in activity as a result of the formation of calcium-silica compounds with low melting points, which leads to enhanced sintering. This is confirmed by scanning electron microscopy (SEM) and also X-ray diffraction (XRD), which showed the presence of spurrite (Ca{sub 5}(SiO{sub 4}){sub 2}CO{sub 3}) as the dominant compound in the pellet after this series of cycles. Better results were obtained with no binder, i.e., by hydration of lime, where Ca(OH){sub 2} plays the role of the binder. Promising results were obtained also with calcium aluminate cements, where no effect of sintering because of the presence of these binders was noticed. Thus, on the basis of this study, the use of calcium aluminate cements for pelletization of CaO-based sorbent is recommended. 39 refs., 9 figs., 2 tabs.

01 COAL, LIGNITE, AND PEAT↗

Multifunctional cement for geothermal wells

This report compiles the work of BNL in support of Thermal Shock Resistant Cement evaluations (TSRC) by Schlumberger. BNL has worked on the formulation of thermal-shock resistant cement since 2011. All the materials on the blend including publications and presentations are in public domain and were sent to Schlumberger for review prior the beginning of the evaluations. Initial efforts focused on achieving long and controlled thickening time of TSRC at 85°C in thickening time tests in a pressurized consistometer. Since the results of BNL set control were not reproduced by Schlumberger technical feedback on Schlumberger testing was among the main efforts of the BNL team in the beginning of the collaboration. When it became clear that the main reason of results deviation was the difference in the mode of retarder addition (dry-blended at BNL and pre-dissolved at Schlumberger) the efforts shifted to the possible decrease in the cost of the formulation by changing concentrations and nature of the alkali activator as well as evaluating performance of more economical formulations with calcium-aluminate cement, Secar #51, Secar #71 and Ciment Fondu, suggested by Schlumberger based on communications with Kerneos (supplier of calcium aluminate cements). Another piece of information obtained by Schlumberger from Kerneos that prompted evaluations of different calcium-aluminate cements in the composition of TSRC was the fact that originally used Secar#80 contains some performance-improving additives that may interfere with the set control and rheological properties of the slurries. In summary, the report contains the following information: 1. Review of the setting behavior of TSRC slurries prepared by dry-blending TA powder or pre dissolving it in mix water in calorimetric tests at 85°C; 2. Results of evaluation of different alkali activators for improved compressive strength development and cost reduction; 3. Results of evaluation of Secar #51, 71 and cement Fondu as an alternative to Secar #80 in TSRC formulation – thermal shock tests and phases’ analyses of set cement; 4. A brief discussion of early-compressive-strength-development test conditions appropriate for geothermal wells.

15 GEOTHERMAL ENERGY↗

Multifunctional Cement for Geothermal Wells

This report compiles the work of BNL in support of Thermal Shock Resistant Cement evaluations (TSRC) by Schlumberger. BNL has worked on the formulation of thermal-shock resistant cement since 2011. All the materials on the blend including publications and presentations are in public domain and were sent to Schlumberger for review prior the beginning of the evaluations. Initial efforts focused on achieving long and controlled thickening time of TSRC at 85°C in thickening time tests in a pressurized consistometer. Since the results of BNL set control were not reproduced by Schlumberger technical feedback on Schlumberger testing was among the main efforts of the BNL team in the beginning of the collaboration. When it became clear that the main reason of results deviation was the difference in the mode of retarder addition (dry-blended at BNL and pre-dissolved at Schlumberger) the efforts shifted to the possible decrease in the cost of the formulation by changing concentrations and nature of the alkali activator as well as evaluating performance of more economical formulations with calcium-aluminate cement, Secar #51, Secar #71 and Ciment Fondu, suggested by Schlumberger based on communications with Kerneos (supplier of calcium aluminate cements). Another piece of information obtained by Schlumberger from Kerneos that prompted evaluations of different calcium-aluminate cements in the composition of TSRC was the fact that originally used Secar#80 contains some performance-improving additives that may interfere with the set control and rheological properties of the slurries. In summary, the report contains the following information: 1. Review of the setting behavior of TSRC slurries prepared by dry-blending TA powder or pre dissolving it in mix water in calorimetric tests at 85°C; 2. Results of evaluation of different alkali activators for improved compressive strength development and cost reduction; 3. Results of evaluation of Secar #51, 71 and cement Fondu as an alternative to Secar #80 in TSRC formulation – thermal shock tests and phases’ analyses of set cement; 4. A brief discussion of early-compressive-strength-development test conditions appropriate for geothermal wells.

36 MATERIALS SCIENCE↗

Tribological Behavior of Structural Materials in High Temperature Helium Gas-Cooled Reactor Environments

The High-Temperature Gas-cooled Reactor (HTGR) is a Generation IV concept designed to produce electricity and hydrogen at high efficiencies via high operating temperatures (700 °C or higher). Helium, the primary coolant for HTGRs, contains impurities (e.g., CO, H2O and CH4) that can induce corrosion reactions at high temperatures such as oxidation and (de)carburization, which in turn can affect the tribological behavior of components. Incoloy® 800HT (Ni-Fe-Cr austenitic solid-solution alloy) and Inconel® 617 (Ni-Cr-Co-Mo solid-solution alloy) are two high-temperature superalloys currently selected as candidate structural materials for the HTGR. The objective of this study is to evaluate the high-temperature tribological performance of these two candidate alloys after conditioning them in HTGR environments. Four regimes of corrosion were considered: a non-conditioned regime (Regime I), an oxidizing regime (Regime II), a carburizing and oxidizing regime (Regime III), and a carburizing regime (Regime IV). To simulate oxidation in HTGR, samples were conditioned for 22 days at elevated temperatures in a once-through helium loop with 4 ppmv H2O. Carburization of the samples was achieved by the commercial process, Kolsterising®. In addition, two surface treatments – shot peening and aluminization – were considered as potential routes of improving the alloys’ wear resistance. Surface-treated samples were tested both before and after conditioning in Regime II. Tribological testing of the samples was performed via a pin-on-disk tribometer at elevated temperatures in ambient environment – 650 and 750°C for 800HT; 850 and 900°C for 617 – with applied loads of 1N, 2N and 5N. The wear behavior of the alloys was assessed via wear volume and friction coefficient measurements, supported by morphological, structural and compositional analyses of the wear tracks. Conditioning the samples in Regime II led to the formation of a chromium oxide on both alloys. This protective scale increased the wear resistance compared to that of as-received samples (Regime I) due to the formation of a compacted ‘glaze’ oxide layer during sliding, rendering the wear track nearly undistinguishable from the unworn background and resulting in wear volumes below the detection limits of the measurement technique. The variability of the friction coefficients of the conditioned samples was also considerably reduced compared to that of the as-received samples due to the glaze layer. Additionally, the initial friction coefficients of the samples conditioned in Regime II were reduced by 45% and 54% compared to those of as-received samples for alloys 800HT and 617, respectively. Carburizing the samples (Regime IV) hardened the surfaces of both alloys and promoted the formation of an iron oxide on 800HT during tribological testing, thereby increasing the wear resistance and decreasing the initial friction coefficient by a factor of two compared to those of as-received 800HT. Alloy 617 exhibited an enhanced wear resistance but similar initial friction coefficient compared to those of as-received samples due to the increased surface hardness. The Mn-Cr oxide developed during Regime III conditioning of 800HT did not develop a glaze layer during tribotesting, even at lower loads. Thus, it was not as protective as the oxide produced during conditioning of Regime II samples, leading to lower wear resistance of 800HT in Regime III compared to that measured in the Regime II condition. 800HT benefited from the aluminization surface treatment, particularly before conditioning in Regime II, due to the promotion of a wear-resistant aluminum oxide layer during testing and the increase in surface hardness due to the presence of a FeAl intermetallic phase. The presence of this phase caused an order-of-magnitude reduction in wear volumes compared to those of as-received 800HT. Aluminization of 617 decreased its wear resistance, particularly after conditioning in Regime II, due to significant wear of the aluminum oxide via a ceramic wear mechanism. This aluminum oxide was removed during sliding, causing the wear volumes to increase by a factor of five compared to those of 617 conditioned in Regime II. Shot-peened 800HT exhibited a tribological behavior similar to that of as-received 800HT, despite an enhancement in the rate of chromium oxide formation. Shot-peened 800HT conditioned in Regime II showed lower wear resistance compared to that of 800HT conditioned in Regime II due to the poor adhesion between the oxide and the underlying metal, preventing the formation of the glaze layer during sliding. Shot peening of 617 increased its wear resistance at higher load, reducing worn volumes by 60% compared to that measured with as-received 617. Tribotesting of shot-peened 617 in Regime II revealed that the glaze-oxide layer was formed at every load, resulting in negligible wear, similar to what was observed from testing 617 after conditioning in Regime II. Overall, alloy 617 exhibited tribologically superior behavior compared to that of alloy 800HT, as demonstrated by its lower friction coefficients and its order-of-magnitude lower wear volumes when measurable.

36 MATERIALS SCIENCE↗

Effect of aluminum substitution on the reflectance spectra of hematite

Hematite and aluminous hematite were synthesized and the diffuse reflectance spectra were recorded for the region between 0.35 and 1.20 microns. Results show that the near-IR based minimum for the aluminous hematite is shifted longward by about 0.02 microns and is much more shallow. Also, the aluminous specimen is considerably more reflective shortward of approximately 0.55 microns where the ferritic specimen is strongly absorbing. This is noteworthy since the visible slope and the red shoulder are often used in the construction of false color and band ratio images.

Morris, R. V.↗