Burning rate and flame structure of cocrystals of CL-20 and a polycrystalline composite crystal of HMX/AP
Explore the source record for details and available documents.
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
Highlights: • High quality ZnO thin films grown on different p-Si substrates were successful obtained by sol–gel process. • PL measurement revealed that ZnO thin film grown on porous Si has the better optical quality. • I–V characteristics for all heterojunctions exhibit successful diode formation. • The diode ZnO/PSi shows a better photovoltaic effect under illumination with a maximum {sub Voc} of 0.2 V. - Abstract: In this study, ZnO thin films are deposited by sol–gel technique on p-type crystalline silicon (Si) with [100] orientation, etched silicon and porous silicon. The structural analyses showed that the obtained thin films were polycrystalline with a hexagonal wurtzite structure and preferentially oriented along the c-axis direction. Morphological study revealed the presence of rounded and facetted grains irregularly distributed on the surface of all samples. PL spectra at room temperature revealed that ZnO thin film grown on porous Si has a strong UV emission with low defects in the visible region comparing with ZnO grown on plat Si and etched Si surface. The heterojunction parameters were evaluated from the (I–V) under dark and illumination at room temperature. The ideality factor, barrier height and series resistance of heterojunction grown on different p-Si substrates are determined by using different methods. Best electrical properties are obtained for ZnO layer deposited on porous silicon.
The electronic structures and thermoelectric properties of a polycrystalline Mg{sub 2}Si thin film have been investigated by first-principle density-functional theory (DFT) and Boltzmann transport theory calculations within the constant-relaxation time approximation. The polycrystalline thin film has been simulated by assembling three types of slabs each having the orientation (001), (110) or (111) with a thickness of about 18 Å. The effect of applying the relaxation procedure to the thin film induces disorder in the structure that has been ascertained by calculating radial distribution functions. For the calculations of the thermoelectric properties, the energy gap has been fixed at the experimental value of 0.74 eV. The thermoelectric properties, namely the Seebeck coefficient, the electrical conductivity and the power factor, have been determined at three temperatures of 350 K, 600 K and 900 K with respect to both the energy levels and the p-type and n-type doping levels. The best Seebeck coefficient is obtained at 350 K: the S{sub yy} component of the tensor amounts to about ±1000 μV K{sup −1}, depending on the type of charge carriers. However, the electrical conductivity is much too small which results in low values of the figure of merit ZT. Structure–property relationship correlations based on directional radial distribution functions allow us to tentatively draw some explanations regarding the anisotropy of the electrical conductivity. Finally, the low ZT values obtained for the polycrystalline Mg{sub 2}Si thin film are paralleled with those recently reported in the literature for bulk chalcogenide glasses. - Graphical abstract: Structure of the polycrystalline thin film of Mg{sub 2}Si. - Author-Highlights: • Polycrystalline Mg{sub 2}Si film has been modelled by DFT approach. • Thermoelectric properties have been evaluated by semi-classical Boltzmann theory. • The structure was found to be slightly disordered after relaxation. • The highest value of Seebeck coefficient reaches −1000 μV/K at 350 K. • The ZT value is estimated between 0.0175 at 350 K and 0.2 at 900 K.
Polycrystalline samples of Mg{sub 0.5}Zn{sub 0.5−x}Co{sub x}Fe{sub 2}O{sub 4} (0 ≤ x ≤ 0.5) with x varying from 0.0-0.5 synthesized by sol-gel auto ignition method. The X-ray diffraction analysis with Retvield refinement reveals the formation of single phase cubic spinel structure. The frequency dependent of real part of dielectric constant has been measured at room temperature and at 100 °C by using an ac impedance analyzer. Except x = 0.5, an increase in the dielectric constant is observed with increase in Co{sup 2+} substitution. Magnetic response has been seen by vibrating sample magnetometer (VSM) at room temperature. The saturation magnetization (M{sub S}) and coercivity (H{sub C}) increase with increasing the Co{sub 2+} substitution. The cation distribution estimated by Mössbauer spectroscopy shows that Co{sub 2+} and Mg{sub 2+} ions have their preference towards octahedral B site, on the other hand Zn{sub 2+} ions preferentially occupy tetrahedral A site, whereas Fe{sub 3+} ions are randomly distributed over A- and B-site. The as obtained results indicated that the substitution of Co{sub 2+} has brought the significant changes in the structural, electrical and magnetic properties of as prepared Mg-Zn-Co multioxide nanocrystals.
The growth-temperature dependency and interface structure effects on the thermal conductivity of the highly textured AlN thin films on (001) Si substrates were systematically studied by characterizing the crystal structures, surface morphologies, interface structures, chemical compositions, and thermal conductivity using x-ray diffraction analysis, atomic force microscopy, high resolution transmission electron microscopy, x-ray photoelectron spectroscopy, and 3-omega method, respectively. By optimizing the interface microstructure and the growth temperature, thermal conductivity of polycrystalline AlN thin films can be greatly enhanced from 9.9 to 26.7 W/mK, when the growth temperature increases from 330 to 560 Degree-Sign C. This achievement is considered to be associated with the diminishment of the amorphous and disordered layer at the AlN/Si interface.
Zinc oxide (ZnO) Thin films were deposited on glass substrate using Spin coating method. Zinc acetate dehydrate, Carbinol and Mono-ethanolamine were used as the precursor, solvent and stabilizer respectively to prepare ZnO Thin-films. The molar ratio of Monoethanolamine to Zinc acetate was maintained as approximately 1. The thickness of the films was determined by Interference technique. The optical properties of the films were studied by UV Vis-Spectrophotometer. From transmittance and absorbance curve, the energy band gap of ZnO is found out. Electrical Conductivity measurements of ZnO are carried out by two probe method and Activation energy for the electrical conductivity of ZnO are found out. The crystal structure and orientation of the films were analyzed by XRD. The XRD patterns show that the ZnO films are polycrystalline with wurtzite hexagonal structure.
Polycrystalline ceramic samples of Zirconium (Zr)-doped GaFeO{sub 3} (GaFe{sub 1-x}Zr{sub x}O{sub 3}) were studied using powder X-ray diffraction, complex impedance spectroscopy and Raman spectroscopic measurements to understand the effect of Zr doping on the structural and dielectric properties. The samples with varying Zr content were prepared by Sol-Gel method. X-ray data analysis confirmed the formation of single phase material without formation of any secondary phases and all are crystallized in Pc2{sub 1}n orthorhombic symmetry. Rietveld refinement of the X-ray data suggested an increase in the lattice constants due to size effect and decreases on x = 0.15 due to the effect of change in interplanner spacing. Impedance studies on the samples showed that the dielectric constant increases while loss tangent decrease as the Zr content increases. Raman scattering on GaFe{sub 1-x}Zr{sub x}O{sub 3} (x = 0, 0.05, 0.10, & 0.15) used to understand the composition dependence on phonon modes at room temperature. On Zr doping, Raman modes frequencies shifts to lower energies consistent with the X-ray data.
The solid solution Sr{sub 1−x}Pb{sub x}WO{sub 4} based on luminescent tungstates SrWO{sub 4} and PbWO{sub 4} has been synthesized by solid-state reaction for all compositions 0≤x≤1. Using Rietveld method, the structural data of all polycrystalline samples have been refined and crystal cell parameters exhibited a linear behavior as a function of x. All substituted structures are of scheelite type. Scanning electron microscopy showed that a high level of crystallization characterized the samples, with modifications in sizes and shapes depending on composition x. Infrared and Raman spectroscopy have been performed to characterize the evolution of vibrational modes with substitution rate. Finally, a systematic study of luminescence under X-ray excitation has been performed: in the composition range x=0.2 to 0.4, intensities of emission exhibited increased values. The luminescence profiles have been interpreted in terms of four Gaussian components, two of them depending on substitution rate. - Graphical abstract: Photoluminescence under X-ray excitation of Sr{sub 1−x}Pb{sub x}WO{sub 4} solid solution: (left) decomposition of emission large band into four components for composition x=0.3; (right) variation of total emission intensity with composition x. - Highlights: • Structural study of solid solution Sr{sub 1−x}Pb{sub x} WO{sub 4} using Rietveld analyses. • Variation of Debye–Waller factor with composition x, disorder parameter. • Existence of four components of luminescence under X-ray excitation. • Effect of substitution of Sr by Pb on two components, due to Pb–O–W interactions. • Enhancement of luminescence intensity in a specific composition range.
The 1144 phase (Ae1A1Fe4As4) shows a strong advantage of engineering fabrication among Fe Iron)-based superconductor (FBS) family due to the robustness of its superconducting properties with respect to chemical inhomogeneities, granted by its uniform crystalline-layered structure. This regularity is furthermore associated to crystalline defects capable of acting as efficient pinning centers, which high critical currents achieved at high fields for these superconductors. Like other FBS phases, its lossless current-carrying capability can be remarkably degraded by distractions at grain boundaries (GBs). GB oxidation is an issue of upmost importance to the realization of the practical FBS application for high field (> 20T) magnet. In this study, we explore oxidized grain boundary and intrinsic grain structural properties of 1144 polycrystalline samples by applying analytical electron microscopy such as atomic resolution scanning transmission electron microscopy and atom probe tomography. These structural properties of samples produced by a mechanochemically assisted synthesis are evaluated following the degradation of superconducting properties due to oxidation. We observe a strong correlation between the contamination at grain boundaries and the decrease of transport properties of the bulk sample, while the crystallin structure seems to be not affected by the oxidation.
Grain boundaries strongly affect many materials properties in polycrystalline materials. Yet, very few structure–property models exist for grain boundaries, due in large part to the complicated and poorly understood way in which the properties of grain boundaries vary with their crystallographic structure. Here, we infer grain boundary structure–property correlations from measurements of the effective properties of a polycrystal. We refer to this method as grain boundary properties localization. We apply this technique to a simple model system of grain boundary diffusivity in a two-dimensional microstructure, and infer the properties of low- and high-angle grain boundaries from the effective diffusivity of the grain boundary network. The generalization and use of these methods could greatly reduce the computational and experimental effort required to establish structure–property correlations for grain boundaries. More broadly, the technique of properties localization could be used to infer the properties of many microstructural constituents in complex microstructures.
The polycrystalline ceramic samples of layer structured Aurivillius oxide of general formula Ba{sub 2}Bi{sub 4}Ti{sub 5}O{sub 18}(BBTO) have been prepared by high temperature solid state reaction technique. The formation of the compound as well as its structural refinement have been carried out using X-ray diffraction followed by Rietveld refinement analysis. There is a good agreement between observe and calculated d-values. The calculated lattice parameters are better than the earlier report. The dielectric constant and loss and hence a.c. conductivity have been measured as a function of frequency (100 Hz-2 MHz) and temperature (RT to 370 deg. C). The dielectric constant shows an anomaly at around 335 deg. C. The results are discussed in detail.
Tungsten doped tin oxide (WTO) and Molybdenum doped tin oxide (MoTO) thin film were deposited on corn glass by thermal evaporation method. The films were annealed at 350°C for one hour. Structural analysis using Xray diffraction data shows both the films are polycrystalline in nature with monoclinic structure of tin oxide, Sn{sub 3}O{sub 4}, corresponding to JCPDS card number 01-078-6064. SEM photograph showed that both the films have spherical grains with size in the range of 20–30 nm. Compositional analysis was carried out using EDS which reveals the presence of Sn, O and the dopant Mo/W only thereby indicating the absence of any secondary phase in the films. The films are found to contain nearly 6 wt% of Mo, 8 wt% of W as dopants respectively. The transmission pattern for both the films in the spectral range 200 – 2000 nm shows that W doping gives a transparency of nearly 80% from 380 nm onwards while Mo doping has less transparency of 39% at 380nm. Film hardness measurement using Triboscope shows a film hardness of about 9–10 GPa for both the films. It indicates that W or M doping in tin oxide provides the films the added advantage of withstanding the mechanical wear and tear due to environmental fluctuations By optimizing the optical and electrical properties, W/Mo doped tin oxide films may be explored as window layers in opto-electronic applications such as solar cells.
Nb 3 Sn is considered as a potential candidate for superconducting radiofrequency cavities for particle acceleration due to its higher transition temperature of 18.3 K and higher superheating field of 400 mT. Nb 3 Sn films can be grown inside the surface of a Nb cavity by sequentially sputtering multiple layers of Nb and Sn thin films followed by annealing at 950 °C for 3 h. We report on the properties of Nb 3 Sn films grown on Nb substrates by magnetron sputtering. The films’ crystal structure, surface morphology, and composition were characterized by X-ray diffraction, scanning electron microscopy, and energy-dispersive X-ray spectroscopy. The films had a polycrystalline Nb 3 Sn structure with a fine-grain surface and an atomic Sn composition of ~23%. The RF surface resistance of the films was measured for different temperatures at 7.4 GHz to understand the feasibility of this method for the SRF application. The RF surface resistance of the films was 5 mΩ at 12 K, which is about 2 orders of magnitude higher than 60 μΩ previously measured in Nb 3 Sn films grown by Sn vapor diffusion. Finally, the sputtered film had a superconducting transition at 17.2 K, which is also lower than 17.9 K observed in Nb 3 Sn film prepared by vapor diffusion.
AgSbSe{sub 2} semiconducting thin films are successfully deposited using reactive evaporation technique at a substrate temperature of 398K. X-ray diffraction studies reveal that the films are polycrystalline in nature. The structural parameters such as average particle size, dislocation density, and number of crystallites per unit have been evaluated. Atomic Force Microscopy is used to study the topographic characteristics of the film including the grain size and surface roughness. The silver antimony selenide thin films have high absorption coefficient of about 10{sup 5} cm{sup −1} and it has an indirect band gap of 0.64eV.
Tin selenide (SnSe) has been the subject of great attention in the last years due to its highly efficient thermoelectricity and its possibilities as a green material, free of Pb and Te. Here, we report for the first time a thermoelectricity and transport study of individual SnSe micro- and nano-wires with diameters in the range between 130nm and 1.15μm. X-ray diffraction and transmission electron microscopy analyses confirm an orthorhombic SnSe structure with Pnma (62) symmetry group and 1:1 Sn:Se atomic ratio. Electrical and thermal conductivity and the Seebeck coeficient were measured in each individual nanowire using a specialized suspended microdevice in the 150–370K temperature range, yielding a thermal conductivity of 0.55Wm -1 K -1 at room temperature and ZT~0.156 at 370K for the 130nm diameter nanowire. The measured properties were correlated with electronic information obtained by model simulations and with phonon scattering analysis. The results confirm these structures as promising building blocks to develop efficient temperature sensors, refrigerators and thermoelectric energy converters. The thermoelectric response of the nanowires is compared with recent reports on crystalline, polycrystalline and layered bulk structures.
Graphical abstract: Hexagonal Mg(OH){sub 2} nanoflakes were synthesized via hydrothermal method in the presence of PEG-20,000. Results show that PEG-20,000 plays an important role in the formation of this kind of nanostructure. The SAED patterns taken from the different positions on a single hexagonal Mg(OH){sub 2} nanoflake yielded different crystalline structures. The structure of the nanoflakes are polycrystalline and the probable formation mechanism of Mg(OH){sub 2} nanoflakes is discussed. - Highlights: • Hexagonal Mg(OH){sub 2} nanoflakes were synthesized via hydrothermal method. • PEG-20,000 plays an important role in the formation of hexagonal nanostructure. • Mg(OH){sub 2} nanoflakes show different crystalline structures at different positions. • The probable formation mechanism of hexagonal Mg(OH){sub 2} nanoflakes was reported. - Abstract: Hexagonal magnesium hydroxide (Mg(OH){sub 2}) nanoflakes were successfully synthesized via hydrothermal method in the presence of the surfactant polyethylene glycol 20,000 (PEG-20,000). Results show that PEG-20,000 plays an important role in the formation of this kind of nanostructure. The composition, morphologies and structure of the Mg(OH){sub 2} nanoflakes were characterized by X-ray diffraction (XRD), field-emission scanning electron microscopy (FE-SEM), high-resolution transmission electron microscopy (HRTEM), and selected area electron diffraction (SAED). The SAED patterns taken from the different positions on a single hexagonal Mg(OH){sub 2} nanoflake show different crystalline structures. The structure of the nanoflakes are polycrystalline and the probable formation mechanism of Mg(OH){sub 2} nanoflakes is discussed. Brunauer–Emmett–Teller (BET) analysis were performed to investigate the porous structure and surface area of the as-obtained nanoflakes.
In this work, neodymium (Nd) doped aluminum zinc oxide (Nd:AZO) films are prepared on glass substrates via simple spray nebulizer method for the first time. The different Nd doping concentrations were taken as 0%, 0.5%, 1% and 1.5 wt%, however, Al concentration was kept constant as 3 wt%. From X-ray diffraction (XRD) data, various structural properties like: crystallite size, microstrain, dislocation density, lattice constants and texture coefficient were investigated. XRD study confirmed that the Al and Nd were incorporated into ZnO. All the deposited films are of polycrystalline nature and hexagonal structure with (002) orientation. The topology studied by AFM showed that the film had low surface roughness and its values were slightly increased from 21 to 37 nm. Elemental mapping and EDAX studies confirmed the occurrence of Zn, O, Al and Nd in prepared Nd:AZO film. Transmission of deposited Nd:AZO film is around 92% in visible spectrum and estimated energy gap is ~ 3.31 eV. PL spectrum emitted one strong NBE emission at ~ 386 nm for all films, signify their better optical quality. Electrical parameters were studied by four probe measurement and low resistivity (ρ) i.e. ~ 4.12 × 10{sup −4} Ω cm and high carrier concentrations (n) i.e. ~ 3.96 × 10{sup 21} cm{sup −3} were observed for 1.5 wt% Nd:AZO films. The calculated value of ϕ is large as 14.33 × 10{sup −3} (Ω/sq){sup −1}, which are enough for an opto-electronic application.
Room temperature tensile strengths of as-received Hi-Nicalon fibers and those having BN/SiC, p-BN/SiC, and p-B(Si)N/SiC surface coatings, deposited by chemical vapor deposition, were measured using an average fiber diameter of 13.5 microns. The Weibull statistical parameters were determined for each fiber. The average tensile strength of uncoated Hi-Nicalon on was 3.19 +/- 0.73 GPa with a Weibull modulus of 5.41. Strength of fibers coated with BN/SiC did not change. However, coat with p-BN/SiC and p-B(Si)N/SiC surface layers showed strength loss of approx. 10 and 35 percent, respectively, compared with as-received fibers. The elemental compositions of the fibers and the coatings were analyzed using scanning Auger microprobe and energy dispersive x-ray spectroscopy. The BN coating was contaminated with a large concentration of carbon and some oxygen. In contrast, p-BN, p-B(Si)N, and SiC coatings did not show any contamination. Microstructural analyses of the fibers and the coatings were done by scanning electron microscopy (SEM), transmission electron microscopy (TEM), and selected area electron diffraction. Hi-Nicalon fiber consists of the P-SIC nanocrystals ranging in size from 1 to 30 nm embedded in an amorphous matrix. TEM analysis of the BN coating revealed four distinct layers with turbostatic structure. The p-BN layer was turbostratic and showed considerable preferred orientation. The p-B(Si)N was glassy and the silicon and boron were uniformly distributed. The silicon carbide coating was polycrystalline with a columnar structure along the growth direction. The p-B(Si)N/SiC coatings were more uniform, less defective and of better quality than the BN/SiC or the p-BN/SiC coatings.