Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Tensile Testing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 289 records · Page 16

A comparative study of hydrogen embrittlement of 20SiMn2CrNiMo, PSB1080 and PH13-8Mo high strength steels

The present study has attempted to evaluate the hydrogen embrittlement (HE) of commercial 20SiMn2CrNiMo, PSB1080 and PH13-8Mo high strength steels using slow strain rate tensile tests with smooth cylindrical tensile specimens. The results reveal that three steels exhibit the superior strength and plasticity in the absence of hydrogen. However, the mechanical properties are deteriorated after hydrogen charging and the resistance to HE is 20SiMn2CrNiMo steel, PH13-8Mo steel and PSB1080 steel, which is ranked in a decreasing order. Fine lath boundaries in 20SiMn2CrNiMo steel disperse hydrogen atoms, reduce local hydrogen accumulation and then result in the lowest HE. Coherent NiAl precipitates in PH13-8Mo steel and O-Mg-Al-Si-Ca type inclusions in PSB1080 steel are responsible for the high HE susceptibility due to the concurrent effect of the stress concentration and hydrogen-enhanced decohesion mechanism. It is thus suggested that the inclusions in steels should be eliminated and the efforts concerning to obtain low HE susceptibility in steels strengthened by the coherent precipitates should be conducted to guarantee the safe service of engineering components fabricated from high strength steels.

36 MATERIALS SCIENCE↗

Microstructural characterization of hydrogen induced cracking in TRIP-assisted steel by EBSD

The present work evaluates hydrogen induced cracking by performing an elaborate EBSD (Electron BackScatter Diffraction) study in a steel with transformation induced plasticity (TRIP-assisted steel). This type of steel exhibits a multiphase microstructure which undergoes a deformation induced phase transformation. Additionally, each microstructural constituent displays a different behavior in the presence of hydrogen. The aim of this study is to obtain a better understanding on the mechanisms governing hydrogen induced crack initiation and propagation in the hydrogen saturated multiphase structure. Tensile tests on notched samples combined with in-situ electrochemical hydrogen charging were conducted. The tests were interrupted at stresses just after reaching the tensile strength, i.e. before macroscopic failure of the material. This allowed to study hydrogen induced crack initiation and propagation by SEM (Scanning Electron Microscopy) and EBSD. A correlation was found between the presence of martensite, which is known to be very susceptible to hydrogen embrittlement, and the initiation of hydrogen induced cracks. Initiation seems to occur mostly by martensite decohesion. High strain regions surrounding the hydrogen induced crack tips indicate that further crack propagation may have occurred by the HELP (hydrogen-enhanced localized plasticity) mechanism. Small hydrogen induced cracks located nearby the notch are typically S-shaped and crack propagation was dominantly transgranularly. The second stage of crack propagation consists of stepwise cracking by coalescence of small hydrogen induced cracks. - Highlights: • Hydrogen induced cracking in TRIP-assisted steel is evaluated by EBSD. • Tensile tests were conducted on notched hydrogen saturated samples. • Crack initiation occurs by a H-Enhanced Interface DEcohesion (HEIDE) mechanism. • Crack propagation involves growth and coalescence of small cracks. • Propagation is governed by the characteristics of phases on the crack path.

36 MATERIALS SCIENCE↗

Creep degradation in oxide-dispersion-strengthened alloys

Oxide dispersion strengthened Ni-base alloys in wrought bar form are studied for creep degradation effects similar to those found in thin gage sheet. The bar products evaluated included ODS-Ni, ODS-NiCr, and three types of advanced ODS-NiCrAl alloys. Tensile test specimens were exposed to creep at various stress levels at 1365 K and then tensile tested at room temperature. Low residual tensile properties, change in fracture mode, the appearance of dispersoid-free bands, grain boundary cavitation, and internal oxidation in the microstructure were interpreted as creep degradation effects. This work showed that many ODS alloys are subject to creep damage. Degradation of tensile properties occurred after very small amounts of creep strain, ductility being the most sensitive property. All the ODS alloys which were creep damaged possessed a large grain size. Creep damage appears to have been due to diffusional creep which produced dispersoid-free bands around boundaries acting as vacancy sources. Low angle and possibly twin boundaries acted as vacancy sources.

Whittenberger, J. D.↗

Effect of prior creep at 1365 K on the room temperature tensile properties of several oxide dispersion strengthened alloys

An experimental study was conducted to determine whether oxide dispersion-strengthened (ODS) Ni-base alloys in wrought bar form are subject to creep degradation effects similar to those found in thin-gage sheet. The bar products evaluated included ODS-Ni, ODS-NiCr, and advanced ODS-NiCrAl types; the alloys included microstructures ranging from an essentially perfect single crystal to a structure consisting of very small elongated grains. Tensile test specimens were exposed to creep at various stress levels at 1365 K and then tensile tested at room temperature. Low residual tensile properties, change in fracture mode, appearance of dispersoid free bands, grain boundary cavitation, and/or internal oxidation are interpreted as creep degradation effects. The amount of degradation depends on creep strain, and degradation appears to be due to diffusional creep which produces dispersoid free bands around grain boundaries acting as vacancy sources.

Whittenberger, J. D.↗

Low temperature mechanical properties, fractographic and metallographic evaluation of several alloy steels

The mechanical properties are presented of alloy steels, 4130, 4140, 4340, 6150, and 8740. Test specimens were manufactured from approximately 1.00 inch (2.54 cm) diameter bar stock which had been heat treated to two different hardness levels. The following mechanical tests were performed at temperatures of 80 F (+26.7 C), 0 F (-17.8 C), -100 F (-73 C), and -200 F (-129 C): (1) tensile test (Ultimate, yield, modulus, elongation, and reduction of area), (2) notched tensile test, (3) charpy V-notched impact test (impact energy), and (4) double shear strength test (ultimate and yield). The test data indicate excellent tensile strength, notched/unnotched tensile ratios, ductility, impact, and shear properties at all test temperatures, except at -200 F (-129 C) where the impact strength of the higher strength group of alloy steels, 4130 (Rc-37) and 4140 (Rc-44) decreased to approximately 9 ft. lbs. (12 joules) and 6 ft. lbs. (8 joules), respectively. Chemical, metallographic, and fractographic analyses were also performed to evaluate microstructure, microhardness and the effect of decrease in temperature on the ductile to brittle failure transition.

Montano, J. W.↗

Instrumented impact and residual tensile strength testing of eight-ply carbon eopoxy specimens

Instrumented drop weight impact testing was utilized to examine a puncture-type impact on thin carbon-epoxy coupons. Four different material systems with various eight-ply lay-up configurations were tested. Specimens were placed over a 10.3-mm diameter hole and impacted with a smaller tup (4.2-mm diameter) than those used in previous studies. Force-time plots as well as data on absorbed energy and residual tensile strength were gathered and examined. It was found that a critical impact energy level existed for each material tested, at which point tensile strength began to rapidly decrease with increasing impact energy.

Nettles, A. T.↗

An Assessment of Variability in the Average Tensile Properties of a Melt-Infiltrated SiC/SiC Composite

Woven SiC/SiC Ceramic Matrix Composites (CMCs), manufactured by the slurry-cast, melt-infiltration process are under consideration as combustor liner materials in aircraft gas turbine engines. Tensile properties (elastic modulus, proportional limit strength, in-plane tensile strength and strain to failure) of the CMC, manufactured during two separate time periods (9/99 and 1/01) were determined at 816 and 1024 C by conducting tensile tests on specimens machined from the CMC plates. A total of 24 tensile tests were conducted for each temperature and CMC variant combination. In this study average tensile properties of the two cMC variants were statistically compared to evaluate significant differences, if any, within the CMC's properties.

Kalluri, Sreeramesh↗

Crystal plasticity modeling and analysis for the transition from intergranular to transgranular failure in nickel-based alloy Inconel 740H at elevated temperature

The precipitation-strengthened Nickel alloy Inconel® 740H® (IN740H) exhibits increased ductility at higher applied strain rates during quasi-static tensile tests at an elevated temperature of 760°C. The examination of fracture surfaces in this context reveals a noteworthy transition of underlying fracture mechanisms from transgranular to intergranular fracture as the applied strain rate decreases from 1×10 -3 / s to 0.83×10 -4 / s . To thoroughly understand the mechanical response of IN740H under these conditions, this study develops a crystal plasticity finite element (CPFE) model. Further, this model incorporates various deformation mechanisms including dislocation slips, climb, and grain boundary sliding, which are relevant to the test conditions. The model is calibrated using data from both tensile tests at different strain rates and creep tests across a broad stress range at 760°C, enabling the accurate determination of model parameters for each mechanism. Simulation results well captured the experimental observations of different failure modes. At higher strain rates, the model shows a dominance of dislocation slip leading to heterogeneous plastic deformation and formation of transgranular shear bands causing the failure, while at lower strain rates, an increased activity of grain boundary sliding causes grain boundaries crack leading to intergranular failure.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Cu/Nb nano-composite wires processed by severe plastic deformation for applications in high pulsed magnets: effects of the multi-scale microstructure on the mechanical properties

Copper-based high strength and high electrical conductivity nano-composite wires reinforced by Nb nano-tubes are prepared by severe plastic deformation, applied with an Accumulative Drawing and Bundling process (ADB), for the windings of high pulsed magnets. The ADB process leads to a multi-scale Cu matrix containing up to N = 85{sub 4} (52.2.10{sup 6}) continuous parallel Nb tubes with diameter down to few tens nano-meters. After heavy strain, the Nb nano-tubes exhibit a homogeneous microstructure with grain size below 100 nm. The Cu matrix presents a multi-scale microstructure with multi-modal grain size distribution from the micrometer to the nano-meter range. The use of complementary characterization techniques at the microscopic and macroscopic level (in-situ tensile tests in the TEM, nano-indentation, in-situ tensile tests under high energy synchrotron beam) shed light on the interest of the multi-scale nature of the microstructure to achieve extreme mechanical properties, therefore allowing for design guidelines to further improve these properties. (authors)

36 MATERIALS SCIENCE↗

Effects of sigma-phase formation on some mechanical properties of a wrought nickel-base superalloy (IN-100)

The effect of sigma phase formation on an extruded and forged nickel base superalloy with the composition of the casting alloy IN-100 was studied. By adding only aluminum and titanium to remelt stock, three compositions were produced which had varying propensities for sigma formation. These compositions were given a four step heat treatment and were stress-ruptured or tensile tested. The very sigma prone composition had a shorter rupture life than the sigma-free or moderately sigma prone compositions when tested at 843 and 885 C. Elongation in room temperature tensile tests was considerably lower for the very sigma prone composition than for the other two wrought compositions after prolonged exposure at 732 or 843 C.

Dreshfield, R. L.↗

Fundamental Study of Micro-Defects in Electropolished EB-Welded and Hydroformed SRF Accelerating Structures

In the area of niobium elecropolishing fundamentals, we focused on understanding the influence of the surface topology, and geometry (with effects from gravity included. The formation of a viscous film is essential for the electropolishing process to take place. The exact nature and composition of the film formed on niobium is still unknown because of its solubility in the electrolyte. Extensive pitting may take place at surface where a stable film cannot form. This has to be taken into consideration while determining the speed with which the SRF cavities are rotated while EP. Hydrodynamic aspects must be taken into consideration while optimizing the polishing parameters. There is improvement in surface finish with polishing time. There is a huge change in surface quality when the EP time is increased from 2 hours to 4 hours but not much change takes place when the time is further increased to 6 hours. So keeping the economic points in view, about 100 um defect layer removal may be sufficient to get the desired performance. In the area of Electropolishing of untreated and treated niobium with Weld Joints we studied untreated and treated Nb, especially for the heat affected areas next to welded bumps, electropolished for different durations. The electropolishing of the untreated Nb caused the formation of pits on the surface at about 15 min but they disappeared when the electropolishing duration was more than 15 min. Electropolishing for 120 min smoothened the surface of untreated Nb by levelling the surface, but the severe formation of pits on the whole surface was found after 240 min. The treatment of Nb significantly changed the Nb surface morphology which was covered by grains of different size that looked light or dark in the optical microscope. The treated Nb was susceptible to pitting during the entire electropolishing starting from 15 min and the dark grains had more susceptibility to pitting than the light grains. In addition, electropolishing for 240 min again resulted in severe pit formation. In the area of Bulge test and microstructure studies, we worked to create a useful constitutive relationship for the complex stress state that accompanies SRF cavity formation. To do so, bulge tests were performed on Cu and Nb tube samples that exhibited the greatest degrees of uniaxial elongation after HT. The data from the bulge tests and an accompanying set of tensile tests provided input to a finite-element model that recreated the bulge tests numerically. As expected the model based on the bulge test results fit the experimental data well at least at low stress levels safely below the bursting pressure. Not so for that based on the tensile results. The results of the study emphasize the importance of for bulge testing rather than tensile testing when deriving the constitutional relationships eventually needed for modelling the hydroforming of Nb SRF cavities.

43 PARTICLE ACCELERATORS↗

Correlation of Microstructure and Mechanical Properties of Metal Big Area Additive Manufacturing

Metal Big Area Additive Manufacturing (MBAAM) is a novel wire-arc additive manufacturing method that uses a correction-based approach developed at the Oak Ridge National Laboratory (ORNL). This approach is an integrated software method that minimizes the dynamic nature of welding and compensates for build height. The MBAAM process is used to fabricate simple geometry thin walled specimens, using a C-Mn steel weld wire, to investigate the scatter in mechanical properties and correlate them to the underlying microstructure. The uni-axial tensile tests show isotropic tensile and yield properties with respect to building directions, although some scatter in elongation is observed. Large scatter is observed in the Charpy Impact tests. The microstructure characterization reveals mostly homogenous ferrite grains with some pearlite, except for some changes in morphology and grain size at the interface between the build and the base plate. The measured properties and microstructure are compared with the toughness and strength values reported in the literature, and a hypothesis is developed to rationalize the differences. Overall, the MBAAM process creates stable, isotropic, and weld-like mechanical properties in the deposit, while achieving a precise geometry obtained through a real-time feedback sensing, closed loop control system.

36 MATERIALS SCIENCE↗

Notch effects on room temperature tensile and bend properties of Ni3Al and Ni3Al+B

The notched mechanical properties of Ni3Al and Ni3Al+B prepared by powder metallurgy techniques have been determined in both tension and bending at room temperature. Tensile tests performed using double-notched specimens containing relatively blunt notches produced intergranular fracture in both Ni3Al and Ni3Al+B, with evidence of fracture initiating in an intergranular manner ahead of the blunt notch in both cases. Estimates of notched fracture toughness from bend tests and of local grain boundary fracture stress from the notched tensile tests suggest an increase in these values with boron addition.

Khadkikar, P. S.↗

Composition-dependence of 316 austenitic stainless steel deformation and aging properties for high-temperature applications - 18696

The present article is part of a broader effort aimed at assessing the possibility of tailoring the plasticity of austenitic stainless steels for structural applications in nuclear reactors. Three annealed heats of 316 stainless steel with large differences in stacking fault energy, carbon content, and ferrite content were used to study deformation and aging behaviors. Deformation of samples was investigated at room temperature by conventional tensile testing and at 350 deg. C by in situ neutron diffraction tensile testing. Aging was studied after 15 h at 750 deg. C through X ray diffraction and nano-indentation. (authors)

36 MATERIALS SCIENCE↗

Water-assisted mechanical testing of polymeric thin-films

Thin films with a nanometer-scale thickness are of great interest to both scientific and industrial communities due to their numerous applications and unique behaviors different from the bulk. However, the understanding of thin-film mechanics is still greatly hampered due to their intrinsic fragility and the lack of commercially available experimental instruments. In this review, we first discuss the progression of thin-film mechanical testing methods based on the supporting substrate: film-on-solid substrate method, film-on-water tensile tests, and water-assisted free-standing tensile tests. By comparing past studies on a model polymer, polystyrene, the effect of different substrates and confinement effect on the thin-film mechanics is evaluated. These techniques have generated fruitful scientific knowledge in the field of organic semiconductors for the understanding of structure–mechanical property relationships. Here, we end this review by providing our perspective for their bright prospects in much broader applications and materials of interest.

42 ENGINEERING↗

Stiffness reductions during tensile fatigue testing of graphite/epoxy angle-ply laminates

The monitoring of modulus decay during fatigue testing as an indicator of damage accumulation and incipient failure has frequently been postulated. The present study was designed to generate tensile fatigue data under carefully controlled test conditions. A computerized data acquisition system was used to permit the measurement of dynamic modulus without interrupting the fatigue cycling. Two different 8-ply laminate configurations, viz, (+ or - 45)2s and (+ or - 67.5)2s, of a T300/5208 graphite/epoxy composite were tested. The (+ or 45)2s laminate did exhibit some modulus decay, although there was no well-defined correlation with applied stress level or number of cycles. The (+ or - 67.5)2s laminate did not exhibit any measurable modulus decay. Secondary effects observed included a slight recovery of the modulus decay after a test interruption, and a significant viscoelastic (creep) response of the (+ or - 45)2s laminate during fatigue testing.

Odom, E. M.↗

Mechanisms of Oxide Formation in the Self-Reacting Friction Stir Weld Process

The initial objective of this study was to evaluate the effect of an extended delay time between preweld cleaning and the completion of a self-reacting friction stir welding (SRFSW) process on the resulting quality of various thickness panels of AA2219-T87. The current NASA standard specifies no more than a 48 hour delay between preweld cleaning and actual welding. The concern is whether increasing the cleaning delay time results in development of the residual oxide defect (ROD) in SRFSW. This concern emanates from the possibility of increased time correlating with increased oxide layer thickness on the faying surfaces. Oxide content on the faying surfaces has been reported to correlate with the occurrence of the ROD which reduces mechanical properties. When the SRFSW process was first adopted by the NASA Marshall Space Flight Center (MSFC), unexpected low tensile values that resulted were attributed to oxides within the weld that appeared to follow the former faying surface contours. Mitigation of the ROD was achieved through a combination of modifications to the processing parameters, tool designs, and incorporation of a weld seam offset. Two operations are involved in preweld cleaning: the first is removal of oil and grease, and the second is removal of surface oxides. In arc welding, improper cleaning of the faying surfaces of aluminum welded joints can increase the sensitivity toward development of defects. As the aluminum is locally melted, these contaminants contribute toward the development of porosity, inclusions, entrapped oxides, and other discontinuities which can degrade the strength of the weld joint. For weldment of large structures, the weld joint is typically cleaned, fit-up, and tack welded prior to the final full penetration welding pass. Because of the stringent joint fit-up requirements for mismatch and peaking for launch vehicle structures, the joint fit-up can sometimes contribute to lengthy delays between cleaning and tack welding, especially for circumferential weld joints on large diameter components. When the conventional friction stir welding (CFSW) process was introduced at the NASA MSFC, there was no procedure for cleaning prior to the solid-state joining process. As the process expanded to include SRFSW, preparation of the faying, crown, and root surfaces were implemented to overcome the ROD. Although the solid-state process is not expected to reach temperatures high enough for dissociation of the native oxide layer, concern remained regarding the redeposition of the native oxide layer within the stir zone. NASA has previously established the allowable time at 48 hours between preweld cleaning and a SRFSW process. The effect of potential 2 contamination resulting from an extended delay to 188 hours was subsequently evaluated for SRFSWs using tensile testing and metallographic imaging. Tensile specimens were tested at room temperature (RT), and at cryogenic conditions of liquid nitrogen (LN2) and liquid hydrogen. No detrimental effect on weld quality, as determined by weld strength, was reported for cleaning delays of 48, 120, 168, 240 or 288 hours. While no trends were established in this study, which extended the delay from 48 to 188 hours, there were a few outliers in terms of ultimate tensile strength (UTS). According to M. Fisher's 2014 Boeing Company Memo no. EYBF-MAF-14-029, all outliers were above the minimum acceptance criteria, but out of family with respect to the average values. As the robustness and reliability of any process ultimately depends on the average values as well as the outliers, an understanding of the cause of these outliers will ultimately improve the process. This report examines those outliers and their possible causes.

Schneider, J. A.↗

Characteristics of laser welded wrought Mg-Al-Mn alloy

Magnesium alloys have gained increased attention in recent years as a structural metal because of their property merits, which necessitates the development of welding techniques qualified for applications in the aeronautic and automotive industries. Laser welding is known to be an excellent method for joining metals. In this paper, a 3 kW CO{sub 2} laser beam was used to weld the wrought Mg-Al-Mn alloy. The characteristics of the microstructure and the mechanical properties of the joints were analyzed by optical microscopy (OM), energy dispersive spectrometry (EDS), scanning electron microscopy (SEM), tensile testing and hardness testing. The experimental results show that the wrought Mg-Al-Mn alloy can be joined successfully using optimized welding conditions. The results of tensile testing show that the highest ultimate tensile strength (UTS) of the joints is up to 94% of that of the base metal. The base metal consists of a typical rolled structure, the narrow heat affected zone (HAZ) has no obvious grain coarsening, and the fusion zone consists of fine grains with a high density of {gamma}-Mg{sub 17}Al{sub 12} precipitates. The hardness test results indicate that the microhardness in the fusion zone is higher than that of the base metal. The elemental analysis reveals that the Mg content in the weld is lower than that of the base metal, but the Al content is slightly higher.

36 MATERIALS SCIENCE↗