Spall kinetics model description

Under high-rate loading in tension, metals can sustain much larger tensile stresses for sub-microsecond time periods than would be possible under quasi-static conditions. This type of failure, known as spall, is not adequately reproduced by hydrocodes with commonly used failure models. The Spall Kinetics Model treats spall by incorporating a time scale into the process of failure. Under sufficiently strong tensile states of stress, damage accumulates over this time scale, which can be thought of as an incubation time. The time scale depends on the previous loading history of the material, reflecting possible damage by a shock wave. The model acts by modifying the hydrostatic pressure that is predicted by any equation of state and is therefore simple to implement. Examples illustrate the ability of the model to reproduce the spall stress and resulting release waves in plate impact experiments on stainless steel.

36 MATERIALS SCIENCE↗

PLZT Film Capacitors for Power Electronics and Energy Storage Applications

Ceramic film capacitors with high dielectric constant and high breakdown strength hold special promise for applications demanding high power density. By means of chemical solution deposition, we deposited ≈2-μm-thick films of lanthanum-doped lead zirconate titanate (PLZT) on LaNiO3-buffered Ni (LNO/Ni) foils and platinized silicon (PtSi) substrates. The dielectric properties and energy storage performance of the resulting samples were determined under a high level of applied electric field. X-ray diffraction stress analysis revealed that PLZT on LNO/Ni bears a compressive stress of ≈370 MPa while PLZT on PtSi endures a tensile stress of ≈250 MPa. Compressive stress was found to lead to heightened polarization, improved tunability, increased irreversible domain wall motion, and enhanced breakdown strength for PLZT deposited on the LNO/Ni as compared with the PtSi substrate. We observed a tunability of ≈55 and ≈40 % at room temperature under 100 kV/cm applied field, remanent polarization of ≈23.5 and ≈7.4 µC/cm^2, coercive electric field of ≈25.6 and ≈21.1 kV/cm, and dielectric breakdown strength of ≈2.6 and ≈1.5 MV/cm for PLZT deposited on LNO/Ni foils and PtSi substrates, respectively. A high recoverable energy density of ≈85 J/cm^3 and energy conversion efficiency of ≈65 % were measured on the PLZT film grown on LNO/Ni.

ceramic film capacitor↗

Residual stress evaluation of components produced via direct metal laser sintering

Direct metal laser sintering is an additive manufacturing process which is capable of fabricating three-dimensional components using a laser energy source and metal powder particles. Despite the numerous benefits offered by this technology, the process maturity is low with respect to traditional subtractive manufacturing methods. Relationships between key processing parameters and final part properties are generally lacking and require further development. In this study, residual stresses were evaluated as a function of key process variables. The variables evaluated included laser scan strategy and build plate preheat temperature. Residual stresses were measured experimentally via neutron diffraction and computationally via finite element analysis. Good agreement was shown between the experimental and computational results. Results showed variations in the residual stress profile as a function of laser scan strategy. Compressive stresses were dominant along the build height (z) direction, and tensile stresses were dominant in the x and y directions. Build plate preheating was shown to be an effective method for alleviating residual stress due to the reduction in thermal gradient.

36 MATERIALS SCIENCE↗

In situ stress measurements during electrochemical cycling of lithium-rich cathodes

Layered lithium transition metal oxides (Li 1+x M 1-x O 2 , M= Ni, Mn, Co) are attractive cathode materials for lithium-ion batteries due to their high reversible capacity but suffer from structural changes and voltage fade. In this study, we use stress as a novel way to track irreversible changes in Li 1.2 Mn 0.55 Ni 0.125 Co 0.125 O 2 (LR-NMC) cathodes. A unique and unpredicted stress signature is observed during the first delithiation. Initially, a tensile stress is observed, consistent with volume contraction from lithium removal, however, the stress reverses and becomes compressive with continued charging beyond 4 V vs Li/Li + , indicating volume expansion; this phenomenon is present in the first cycle only. The origin of this irreversible stress during delithiation is likely oxygen loss and the resulting cation rearrangement. Here, Raman spectroscopy provides evidence of the layered-to-spinel phase transition after cycling in the LR-NMC films, as well as recovery of the original spectra upon re-annealing in an oxygen environment.

25 ENERGY STORAGE↗

Longitudinal shear behavior of several oxide dispersion strengthened alloys

Two commercial oxide dispersion strengthened (ODS) alloys, MA-753 and MA-754, and three experimental ODS alloys, MA-757E, MA-755E, and MA-6000E, were tested in shear at 760 C. Comparisons were made with other turbine blade and vane alloys. All of the ODS alloys exhibited less shear strength than directionally solidified Mar-M 200 = Hf or then conventionally cast B-1900. The strongest ODS alloy tested, MA-755E, was comparable in both shear and tensile strength to the lamellar directionally solidified eutectic alloy gamma/gamma prime - delta. Substantial improvements in shear resistance were found for all alloys tested when the geometry of the specimen was changed from one generating a transverse tensile stress in the shear area to one generating a transverse compressive stress. Finally, 760 C shear strength as a fraction of tensile strength was found to increase linearly with the log of the transverse tensile ductility.

Glasgow, T. K.↗

Longitudinal shear behavior of several oxide dispersion strengthened alloys

Two commercial oxide dispersion strengthened (ODS) alloys, MA-753 and MA-754, and three experimental ODS alloys, MA-757E, MA-755E, and MA-6000E, were tested in shear at 760 C. Comparisons were made with other turbine-blade and vane alloys. All of the ODS alloys exhibited less shear strength than directionally solidified Mar-M 200 + Hf or than conventionally cast B-1900. The strongest ODS alloy tested, MA-755E, was comparable in both shear and tensile strength to the lamellar directionally solidified eutectic alloy gamma/gamma-prime - delta. Substantial improvements in shear resistance were found for all alloys tested when the geometry of the specimen was changed from one generating a transverse tensile stress in the shear area to one generating a transverse compressive stress. Finally, 760-C shear strength as a fraction of tensile strength was found to increase linearly with the log of the transverse tensile ductility.

Glasgow, T. K.↗

Controlling stress corrosion cracking in mechanism components of ground support equipment

The selection of materials for mechanism components used in ground support equipment so that failures resulting from stress corrosion cracking will be prevented is described. A general criteria to be used in designing for resistance to stress corrosion cracking is also provided. Stress corrosion can be defined as combined action of sustained tensile stress and corrosion to cause premature failure of materials. Various aluminum, steels, nickel, titanium and copper alloys, and tempers and corrosive environment are evaluated for stress corrosion cracking.

Majid, W. A.↗

US NRC-Sponsored Research on Stress Corrosion Cracking Susceptibility of Dry Storage Canister Materials in Marine Environments - 13344

At a number of locations in the U.S., spent nuclear fuel (SNF) is maintained at independent spent fuel storage installations (ISFSIs). These ISFSIs, which include operating and decommissioned reactor sites, Department of Energy facilities in Idaho, and others, are licensed by the U.S. Nuclear Regulatory Commission (NRC) under Title 10 of the Code of Federal Regulations, Part 72. The SNF is stored in dry cask storage systems, which most commonly consist of a welded austenitic stainless steel canister within a larger concrete vault or overpack vented to the external atmosphere to allow airflow for cooling. Some ISFSIs are located in marine environments where there may be high concentrations of airborne chloride salts. If salts were to deposit on the canisters via the external vents, a chloride-rich brine could form by deliquescence. Austenitic stainless steels are susceptible to chloride-induced stress corrosion cracking (SCC), particularly in the presence of residual tensile stresses from welding or other fabrication processes. SCC could allow helium to leak out of a canister if the wall is breached or otherwise compromise its structural integrity. There is currently limited understanding of the conditions that will affect the SCC susceptibility of austenitic stainless steel exposed to marine salts. NRC previously conducted a scoping study of this phenomenon, reported in NUREG/CR-7030 in 2010. Given apparent conservatisms and limitations in this study, NRC has sponsored a follow-on research program to more systematically investigate various factors that may affect SCC including temperature, humidity, salt concentration, and stress level. The activities within this research program include: (1) measurement of relative humidity (RH) for deliquescence of sea salt, (2) SCC testing within the range of natural absolute humidity, (3) SCC testing at elevated temperatures, (4) SCC testing at high humidity conditions, and (5) SCC testing with various applied stresses. Results to date indicate that the deliquescence RH for sea salt is close to that of MgCl{sub 2} pure salt. SCC is observed between 35 and 80 deg. C when the ambient (RH) is close to or higher than this level, even for a low surface salt concentration. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Free-edge stress analysis of glass-epoxy laminates with matrix cracks

The effect of matrix cracks on the composite delamination and interlaminar stresses is investigated in (+15/90n/-15)s glass-epoxy laminates (with values of n equal to 0, 1, 2, or 3) subjected to monotonically increasing tension loads. Three-dimensional (3D) and quasi-3D (Q3D) finite-element analyses are used to model the free-edge stress states in the laminates with and without a matrix crack, respectively. The Q3D results show that in-plane transverse tensile stresses exist in the +15 deg plies near the free edges of all of the laminates used and that only the interlaminar shear stress is high at the +15/theta interface. The results of 3D analysis indicate that large tensile interlaminar normal as well as shear stresses develop at the intersection of the matrix crack and the free edge. This suggests that the interlaminar normal stress plays a significant role in the failure of these laminates.

Fish, John C.↗

Electronic Excitation‐Driven β‐Ga 2 O 3 Metastability Transformation and Self‐Organization Mechanism: β→κ/γ/δ Phases

Here, irradiation-driven multiphase self-organization presents emergent opportunities for the customization of nanoscale engineering properties, dynamically tuning strain-field distributions and interfacial electronic structures. Responding to intense electronic excitation-induced energy deposition, the dominant phase transformations, with varying Gibbs free energy $Δ,G^o_f$ are confirmed as β → κ → γ → δ that are located in specific microregions for Gallium (III) oxide (Ga 2 O 3 ), as follows: (i) Surface-localized interstitial accumulation under compressive stress triggers β → δ via semi-coherent interface formation. (ii) Tensile stress within latent tracks drives vacancy-mediated oxygen layer truncation (4/12 periodicity along ⟨0001⟩), stabilizing coherent 4H (ABCB) κ and 3C (ABC) β (ABC) interfaces through strain-compensated octahedral distortion. (iii) Screw dislocation-mediated lattice relaxation induces β → γ via cation disordering (Ga 3+ occupancy at β-interstitial sites), forming metastable spinel γ with mixed occupancy across 16d/8a Wyckoff sites. Irradiation-driven β-Ga 2 O 3 →κ/γ/δ transitions, as mechanistically revealed via inelastic thermal spike (i-TS) calculations and molecular dynamics simulations, induce defect-mediated nonlinear photoresponse, critical for optoelectronic engineering.

Han, Xinqing [Shandong Univ., Jinan (China)]↗

Lateral cracks during sliding indentation on various optical materials

A series of static and sliding indentation (ie, scratching) was performed and characterized on a wide range of optical workpiece materials [single crystals of Al 2 O 3 (sapphire), SiC, Y 3 Al 5 O 12 (YAG), CaF 2 , and LiB 3 O 5 (LBO); a SiO 2 –Al 2 O 3 –P 2 O 5 –Li 2 O glass ceramic (Zerodur); and glasses of SiO 2 :TiO 2 (ULE), SiO 2 (fused silica), and P 2 O 5 –Al 2 O 3 –K 2 O–BaO (Phosphate)] at various applied loads using various indenters (Vickers, 10 µm conical, and 200 µm conical). Despite having different load dependencies, the lateral crack depth formed during sliding indentation quantitatively scales with that formed during static indentation, explaining why static indentation has been historically effective in describing various grinding parameters. Depending on the indenter geometry, the amount of residual trench damage (plastic deformation and local fracturing) during sliding indentation was often enhanced by more than an order of magnitude compared with static indentation. A simple ploughing scratch model, which considers both tangential and normal stresses (where the tangential stress is amplified by relatively small tangential contact area), explains this enhancement and other observed trends. Accounting for the high correlation between residual trench depth and volumetric fracturing, the model is extended to estimate the amount of fracture damage as a function of the material properties of the workpiece, indenter geometry, and applied load. Such a model has utility in the design of optimized grinding processes, particularly the abrasive geometry. Finally, at higher loads (>1 N), lateral cracks were often observed to preferentially propagate in the forward scratching direction, as opposed to perpendicular to the scratch as typically observed. High-speed imaging of the scratch process confirms that these cracks propagate ahead of the sliding indenter during the scratching event. Finite element stress analysis suggests the ploughing frictional forces increase the mode I tensile stresses at the leading edge of the sliding indenter explaining the direction of crack propagation of such cracks.

36 MATERIALS SCIENCE↗

In Situ Stress Evolution in Li 1+x Mn 2 O 4 Thin Films during Electrochemical Cycling in Li-Ion Cells

Real time monitoring of stress evolution in electrodes during electrochemical cycling can help quantify the driving forces that dictate their mechanical degradation. In the present work, in-situ stress evolution in thin films of spinel Li 1+x Mn 2 O 4 (LMO) was measured by monitoring the change in the elastic substrate curvature during electrochemical cycling in a specially designed beaker cell in the 3.5–4.3 V (vs. Li/Li+) voltage range. The LMO thin films were prepared using a solution deposition technique and their structures and morphologies were characterized by X-ray diffraction (XRD), Raman spectroscopy and scanning electron microscopy (SEM). The stress evolution in the early part of the first delithiation cycle (<4.05 V) was consistent with the XRD data. However, stress evolution during later stages of the first delithiation cycle (>4.05 V) was not consistent with the XRD results, and showed irreversible behavior, suggesting irreversible changes in the electrode. Beyond the first delithiation cycle, the stress evolution was reversible, with a steady buildup of compressive and tensile stress during lithium insertion and extraction, respectively. Measurements on LMO films of varying thicknesses suggest that the first cycle irreversibility in stress response arises primarily from the electrode bulk.

25 ENERGY STORAGE↗

Thermal stress analysis of ceramic gas-path seal components for aircraft turbines

Stress and temperature distributions were evaluated numerically for a blade-tip seal system proposed for gas turbine applications. The seal consists of an abradable ceramic layer on metallic backing with intermediate layers between the ceramic layer and metal substrate. The most severe stresses in the seal, as far as failure is concerned, are tensile stresses at the top of the ceramic layer and shear and normal stresses at the layer interfaces. All these stresses reach their maximum values during the deceleration phase of a test engine cycle. A parametric study was carried out to evaluate the influence of various design parameters on these critical stress values. The influences of material properties and geometric parameters of the ceramic, intermediate, and backing layers were investigated. After the parametric study was completed, a seal system was designed which incorporated materials with beneficial elastic and thermal properties in each layer of the seal. An analysis of the proposed seal design shows an appreciable decrease in the magnitude of the maximum critical stresses over those obtained with earlier configurations.

Kennedy, F. E.↗

External stress-corrosion cracking of a 1.22-m-diameter type 316 stainless steel air valve

An investigation was conducted to determine the cause of the failure of a massive AISI Type 316 stainless steel valve which controlled combustion air to a jet engine test facility. Several through-the-wall cracks were present near welded joints in the valve skirt. The valve had been in outdoor service for 18 years. Samples were taken in the cracked regions for metallographic and chemical analyses. Insulating material and sources of water mist in the vicinity of the failed valve were analyzed for chlorides. A scanning electron microscope was used to determine whether foreign elements were present in a crack. On the basis of the information generated, the failure was characterized as external stress-corrosion cracking. The cracking resulted from a combination of residual tensile stress from welding and the presence of aqueous chlorides. Recommended countermeasures are included.

Moore, Thomas J.↗

NASA-UVA Light Aerospace Alloy and Structures Technology Program (LA2ST)

This report documents the progress achieved over the past 6 to 12 months on four graduate student projects conducted within the NASA-UVA Light Aerospace Alloy and Structures Technology Program. These studies were aimed specifically at light metallic alloy issues relevant to the High Speed Civil Transport. Research on Hydrogen-Enhanced Fracture of High-Strength Titanium Alloy Sheet refined successfully the high resolution R-curve method necessary to characterize initiation and growth fracture toughnesses. For solution treated and aged Low Cost Beta without hydrogen precharging, fracture is by ductile transgranular processes at 25 C, but standardized initiation toughnesses are somewhat low and crack extension is resolved at still lower K-levels. This fracture resistance is degraded substantially, by between 700 and 1000 wppm of dissolved hydrogen, and a fracture mode change is affected. The surface oxide on P-titanium alloys hinders hydrogen uptake and complicates the electrochemical introduction of low hydrogen concentrations that are critical to applications of these alloys. Ti-15-3 sheet was obtained for study during the next reporting period. Research on Mechanisms of deformation and Fracture in High-Strength Titanium Alloys is examining the microstructure and fatigue resistance of very thin sheet. Aging experiments on 0. 14 mm thick (0.0055 inch) foil show microstructural agility that may be used to enhance fatigue performance. Fatigue testing of Ti-15-3 sheet has begun. The effects of various thermo-mechanical processing regimens on mechanical properties will be examined and deformation modes identified. Research on the Effect of Texture and Precipitates on Mechanical Property Anisotropy of Al-Cu-Mg-X and Al-Cu alloys demonstrated that models predict a minor influence of stress-induced alignment of Phi, caused by the application of a tensile stress during aging, on the yield stress anisotropy of both modified AA2519 and a model Al-Cu binary alloy. This project is no longer included in the NASA-UVA LAST program. Research on the Creep Behavior and Microstructural stability of Al-Cu-Mg-Ag and Al-Cu-Li-Mg-Ag showed that the creep resistance of three candidate aluminum alloys (C415, C416 and ML377) was much superior compared to that of the current Concorde alloy, AA2618. Creep induced change in precipitates at grain boundaries was observed in the alloy which exhibits the highest creep strain of the three examined. The other two alloys developed no detectable microstructural changes at grain boundaries under the creep conditions tested.

Gangloff, Richard P.↗

Research on the Corrosion Behavior of X70 Pipeline Steel Under Coupling Effect of AC + DC and Stress

The coupling effect of stray AC (alternating current) + DC (direct current) and tensile stress-induced X70 pipeline corrosion is complicated with its mechanism uncovered. In this work, the corrosion behavior of X70 pipeline steel under three different corrosion (including an individual AC corrosion, mixed AC + 150 MPa tensile stress corrosion, coupling effect of AC + a 30 A/m{sup 2} DC interference and 150 MPa tensile stress corrosion) conditions in Dagang soil simulated solution was investigated by COMSOL Multiphysics software simulation, electrochemical tests, scanning electron microscope and other techniques. The results indicated that with the increase in AC density, the open-circuit potential of the X70 steel samples was negatively shifted and corrosion rate increased in three different corrosion conditions. The corrosion rates of X70 steel samples under individual AC interference were almost unchanged when 150.9 MPa tensile stress was applied. When applying 30 A/m{sup 2} DC interference, the corrosion rate of X70 steel increases significantly. Therefore, the factors affecting corrosion performance of X70 pipeline steel were DC > AC > stress. Under individual AC interference, uniform corrosion occurred on the X70 steel at an AC current density of less than 30 A/m{sup 2}, while the pitting corrosion occurred at an AC current density of greater than 100 A/m{sup 2}. The application of tensile stress and DC had a certain inhibitory effect on pitting corrosion.

36 MATERIALS SCIENCE↗

Stress In A Fiber During Curing Of Surrounding Matrix Resin

Experiments run to determine variation in tensile stress in single fiber during curing of matrix resin surrounding fiber. Study part of effort to understand physical mechanisms affecting residual stresses in matrix/fiber composites, with view toward optimizing curing cycles (in particular, optimizing temperature-vs.-time schedules of final cooldowns to ambient temperature) to minimize residual stresses. Results signify primary mechanisms affecting residual stress in fibers are thermal expansion and contraction and cure shrinkage of matrix material.

Bowles, Kenneth J.↗

Surface Modification of High-Carbon Steel Using Fiber Laser and Its Thermal, Microstructural and Tribological Analysis

In this study, surface modification of high-carbon steel was carried out using 2 kW fiber laser and thermal, microstructural and tribological characterizations were performed. The process parameters selected for laser surface treatment were laser power (600-1500 W) and scan speed (3000-4500 mm/min). Infrared pyrometer was used to record the surface temperature during the process. The metallographic analysis was carried out using an optical microscope to find the depth and width of the laser-treated zone. Scanning electron microscopy and energy-dispersive spectroscopy were performed to reveal the microstructure and compositional changes taking place in the laser-treated zone. It was observed that the dendritic growth took place from the top surface toward the center of the laser-treated zone. The amount of dendritic growth can be related to the maximum surface temperature generated during the process. XRD analysis indicated the formation of some intermetallic compounds and phase shifts taking place in the laser-treated zone. Residual stress analysis was performed to analyze the amount of stress accumulation in the laser-treated zone. When the temperature cycle was analyzed, it was found that the melting of the steel resulted in the formation of a surface under compressive stress while the non-melt hardened zone developed a surface under tensile stress. The maximum Vickers microhardness value achieved was about 958.8 HV{sub 0.5} for 1500 W power and 3000 mm/min scan speed. Scratch test was performed on the laser-treated track, and it was found that the hardened zone showed better tribological properties with respect to the parent material. Finally, it was observed that the surface roughness value increased with higher heat input probably due to high rate of oxide formation as well as due to the presence of martensite in the laser-treated zone.

36 MATERIALS SCIENCE↗