Quantitative Tester And Reconditioner For Hand And Arm

Apparatus measures torques, forces, and motions of hand, wrist, forearm, elbow, and shoulder and aids in reconditioning muscles involved. Used to determine strengths and endurances of muscles, ranges of motion of joints, and reaction times. Provides quantitative data used to assess extent to which disuse, disease, or injury causes deterioration of muscles and of motor-coordination skills. Same apparatus serves as exercise machine to restore muscle performance by imposing electronically controlled, gradually increasing loads on muscles. Suitable for training and evaluating astronauts, field testing for workers' compensation claims, and physical therapy in hospitals. With aid of various attachments, system adapted to measure such special motions as pinching, rotation of wrist, and supination and pronation of the forearm. Attachments are gloves, wristlets, and sleeves.

Engle, Gary↗

Fittings and Other Structural Parts of Airplanes

The strength and reliability of airplanes depend greatly on the careful design and manufacture of fittings, couplings, and other highly stressed parts. The more important parts of the airplane must be occasionally tested for increased loads and in order to avoid the possibility of defects creeping in during subsequent production. Strength tests are discussed for fittings for wing spar joints, fittings for strut connections, internal bracing, control gear, and landing gear.

Eydam, P↗

Nondestructive Evaluation of Adhesively Bonded Joints

The final report consists of 5 published papers in referred journals and a technical letter to the technical monitor. These papers include the following: (1) Comparison of the effects of debonds and voids in adhesive; (2) On the peak shear stresses in adhesive joints with voids; (3) Nondestructive evaluation of adhesively bonded joints by acousto-ultrasonic technique and acoustic emission; (4) Multiaxial fatigue life evaluation of tubular adhesively bonded joints; (5) Theoretical and experimental evaluation of the bond strength under peeling loads. The letter outlines the progress of the research. Also included is preliminary information on the study of nondestructive evaluation of composite materials subjected to localized heat damage. The investigators studied the effects of localized heat on unidirectional fiber glass epoxy composite panels. Specimens of the fiber glass epoxy composites were subjected to 400 C heat for varying lengths of time. The specimens were subjected to nondestructive tests. The specimens were then pulled to their failure and acoustic emission of these specimens were measured. The analysis of the data was continuing as of the writing of the letter, and includes a finite element stress analysis of the problem.

Nayeb-Hashemi, Hamid↗

An overview of the issues: physiological effects of bed rest and restricted physical activity

Reduction of exercise capacity with confinement to bed rest is well recognized. Underlying physiological mechanisms include dramatic reductions in maximal stroke volume, cardiac output, and oxygen uptake. However, bed rest by itself does not appear to contribute to cardiac dysfunction. Increased muscle fatigue is associated with reduced muscle blood flow, red cell volume, capillarization and oxidative enzymes. Loss of muscle mass and bone density may be reflected by reduced muscle strength and higher risk for injury to bones and joints. The resultant deconditioning caused by bed rest can be independent of the primary disease and physically debilitating in patients who attempt to reambulate to normal active living and working. A challenge to clinicians and health care specialists has been the identification of appropriate and effective methods to restore physical capacity of patients during or after restricted physical activity associated with prolonged bed rest. The examination of physiological responses to bed rest deconditioning and exercise training in healthy subjects has provided significant information to develop effective rehabilitation treatments. The successful application of acute exercise to enhance orthostatic stability, daily endurance exercise to maintain aerobic capacity, or specific resistance exercises to maintain musculoskeletal integrity rather than the use of surgical, pharmacological, and other medical treatments for clinical conditions has been enhanced by investigation and understanding of underlying mechanisms that distinguish physical deconditioning from the disease. This symposium presents an overview of cardiovascular and musculoskeletal deconditioning associated with reduced physical work capacity following prolonged bed rest and exercise training regimens that have proven successful in ameliorating or reversing these adverse effects.

NASA Program Space Physiology and Countermeasures↗

Analytical and experimental investigation of aircraft metal structures reinforced with filamentary composites. Phase 2: Structural fatigue, thermal cycling, creep, and residual strength

Specimens representative of metal aircraft structural components reinforced with boron filamentary composites were manufactured and tested under cyclic loading, cyclic temperature, or continuously applied loading to evaluate some of the factors that affect structural integrity under cyclic conditions. Bonded, stepped joints were used throughout to provide composite-to-metal transition regions at load introduction points. Honeycomb panels with titanium or aluminum faces reinforced with unidirectional boron composite were fatigue tested at constant amplitude under completely reversed loading. Results indicated that the matrix material was the most fatigue-sensitive part of the design, with debonding initiating in the stepped joints. However, comparisons with equal weight all-metal specimens show a 10 to 50 times improved fatigue life. Fatigue crack propagation and residual strength were studied for several different stiffened panel concepts, and were found to vary considerably depending on the configuration. Composite-reinforced metal specimens were also subjected to creep and thermal cycling tests. Thermal cycling of stepped joint tensile specimens resulted in a ten percent decrease in residual strength after 4000 cycles.

Blichfeldt, B.↗

Microhardness Testing of Aluminum Alloy Welds

A weld is made when two pieces of metal are united or fused together using heat or pressure, and sometimes both. There are several different types of welds, each having their own unique properties and microstructure. Strength is a property normally used in deciding which kind of weld is suitable for a certain metal or joint. Depending on the weld process used and the heat required for that process, the weld and the heat-affected zone undergo microstructural changes resulting in stronger or weaker areas. The heat-affected zone (HAZ) is the region that has experienced enough heat to cause solid-state microstructural changes, but not enough to melt the material. This area is located between the parent material and the weld, with the grain structure growing as it progresses respectively. The optimal weld would have a short HAZ and a small fluctuation in strength from parent metal to weld. To determine the strength of the weld and decide whether it is suitable for the specific joint certain properties are looked at, among these are ultimate tensile strength, 0.2% offset yield strength and hardness. Ultimate tensile strength gives the maximum load the metal can stand while the offset yield strength gives the amount of stress the metal can take before it is 0.2% longer than it was originally. Both of these are good tests, but they both require breaking or deforming the sample in some way. Hardness testing, however, provides an objective evaluation of weld strengths, and also the difference or variation in strength across the weld and HAZ which is difficult to do with tensile testing. Hardness is the resistance to permanent or plastic deformation and can be taken at any desired point on the specimen. With hardness testing, it is possible to test from parent metal to weld and see the difference in strength as you progress from parent material to weld. Hardness around grain boundaries and flaws in the material will show how these affect the strength of the metal while still retaining the sample. This makes hardness testing a good test for identifying grain size and microstructure.

Bohanon, Catherine↗

Determining Exercise Strength Requirements for Astronaut Critical Mission Tasks: Reaching Under G-Load

The critical mission tasks assessments effort seeks to determine the physical performance requirements that astronauts must meet in order to safely and successfully accomplish lunar exploration missions. These assessments will determine astronaut preflight strength, fitness, and flexibility requirements, and the extent to which exercise and other countermeasures must prevent the physical deconditioning associated with prolonged weightlessness. The purpose is to determine the flexibility and strength that crewmembers must possess in order to reach Crew Exploration Vehicle controls during maneuvers that result in sustained acceleration levels ranging from 3.7G to 7.8G. An industry standard multibody dynamics application was used to create human models representing a 5th percentile female, a 50th percentile male, and a 95th percentile male. The additional mass of a space suit sleeve was added to the reaching arm to account for the influence of the suit mass on the reaching effort. The human model was merged with computer models of a pilot seat and control panel for the Crew Exploration Vehicle. Three dimensional paths were created that guided the human models hand from a starting position alongside its thigh to three control targets: a joystick, a keyboard, and an overhead switch panel. The reaching motion to each target was repeated under four vehicle acceleration conditions: nominal ascent (3.7G), two ascent aborts (5.5G and 7.8G) and lunar reentry (4.6G). Elbow and shoulder joint angular excursions were analyzed to assess range of motion requirements. Mean and peak elbow and shoulder joint torques were determined and converted to equivalent resistive exercise loads to assess strength requirements. Angular excursions for the 50th and 95th percentile male models remained within joint range of motion limits. For the 5th percentile female, both the elbow and the shoulder exceeded range of motion limits during the overhead reach. Elbow joint torques ranged from 10 N-m (nominal ascent) to 60 N-m (ascent abort). Shoulder joint torques ranged from 65 N-m (nominal ascent) to 280 N-m (ascent abort). Maximal equivalent exercise loads reached 30 lb in tricep extension, 9 lb in bicep curl, 110 lb in unilateral pullover and unilateral bench press for nominal conditions (lunar reentry), and 188 lb in unilateral pullover and unilateral bench press. The location of the pilot seat was found to be inadequately located to allow a 5th percentile female to reach the switches on the overhead panel. Elbow strength requirements were found to be well within population norms. Shoulder strength was found to be a limiting factor. Reaching under nominal ascent and lunar reentry conditions was found to require near maximal shoulder strength. Reaching under ascent abort conditions requires shoulder strength well beyond population norms. Pilot seats must adjust to accomodate a 5th percentile female. Exercise countermeasures must maintain maximal pullover and bench press strength to allow pilots to reach and operate controls during lunar reentry. Reaching will not be possible during ascent abort conditions. Flight controls should be built into armrests or flight control must be accomplished by autonomous systems during acceleration exceeding 4.6G.

Schaffner, Grant↗

Modeling Spacesuit-Human Interaction for Injury Risk Identification

Performing functional tasks while inside of the space suit introduces additional ergonomic challenges which can lead to musculoskeletal stresses and injuries in astronauts. Computational modeling of the suit-body interaction can be used alongside human-in-the-loop testing to understand and mitigate these risks and potentially improve the work performance. In this work, a static rigid-body model of the human body was integrated with the space suit and the process is described. This model enables prediction of the resulting joint torques and musculoskeletal loading from a simulated extravehicular activity (EVA) task. For representative EVA tasks, joint torque and body angles were used as parameters to predict the muscle strength required to achieve the task, as well as the percentage of the general and astronaut-like population that could achieve that strength demand. Population strength capability can be used as an indicator of the difficulty of a task and the level of injury risk for the given task types and crew anthropometry. The sensitivity of the model to inputs such as body joint location within the space suit and individual anthropometry will also be evaluated. Future work will use a database of3D human body scans and the movements of the body inside the suit during different EVA tasks to identify potential soft tissue contact points. The specific locations and magnitudes of contacts between the body and suit are expected to identify risk of repetitive tissue contact stresses. Overall, this model will provide a new tool to structurally identify the injury risks of EVA tasks and evaluate alternate strategies to reduce injury risk.

Garima Gupta↗

Design detail verification tests for a lightly loaded open-corrugation graphite-epoxy cylinder

Flat corrugated graphite-epoxy panels were tested in compression to verify selected design details of a ring-stiffened cylinder that was designed to support an axial compressive load of 157.6 kN/m without buckling. Three different sizes of subcomponent panels, with the same basic corrugation geometry, were tested: (1) 60.96-cm-long by 45.72-cm-wide panels to evaluate the local buckling strength of the shell wall design; (2) 91.44-cm-long by 45.72-cm-wide panels to evaluate a longitudinal joint and the load-introduction method; and (3) 254.0-cm-long by 91.44-cm-wide panels with four simulated-ring stiffeners to evaluate the ring-attachment method. The test results indicate that the modified shell-wall design, the longitudinal joint, the load-introduction method, and the stiffener-attachment method for the proposed cylinder have adequate strength to support the design load.

Davis, R. C.↗

Ultrasonic Nondestructive Characterization of Adhesive Bonds

Adhesives and adhesive joints are widely used in various industrial applications to reduce weight and costs, and to increase reliability. For example, advances in aerospace technology have been made possible, in part, through the use of lightweight materials and weight-saving structural designs. Joints, in particular, have been and continue to be areas in which weight can be trimmed from an airframe through the use of novel attachment techniques. In order to save weight over traditional riveted designs, to avoid the introduction of stress concentrations associated with rivet holes, and to take full advantage of advanced composite materials, engineers and designers have been specifying an ever-increasing number of adhesively bonded joints for use on airframes. Nondestructive characterization for quality control and remaining life prediction has been a key enabling technology for the effective use of adhesive joints. Conventional linear ultrasonic techniques generally can only detect flaws (delamination, cracks, voids, etc) in the joint assembly. However, more important to structural reliability is the bond strength. Although strength, in principle, cannot be measured nondestructively, a slight change in material nonlinearity may indicate the onset of failure. Furthermore, microstructural variations due to aging or under-curing may also cause changes in the third order elastic constants, which are related to the ultrasonic nonlinear parameter of the polymer adhesive. It is therefore reasonable to anticipate a correlation between changes in the ultrasonic nonlinear acoustic parameter and the remaining bond strength. It has been observed that higher harmonics of the fundamental frequency are generated when an ultrasonic wave passes through a nonlinear material. It seems that such nonlinearity can be effectively used to characterize bond strength. Several theories have been developed to model this nonlinear effect. Based on a microscopic description of the nonlinear interface binding force, a quantitative method was presented. Recently, a comparison between the experimental and simulated results based on a similar theoretical model was presented. A through-transmission setup for water immersion mode-converted shear waves was used to analyze the ultrasonic nonlinear parameter of an adhesive bond. In addition, ultrasonic guided waves have been used to analyze adhesive or diffusion bonded joints. In this paper, the ultrasonic nonlinear parameter is used to characterize the curing state of a polymer/aluminum adhesive joint. Ultrasonic through-transmission tests were conducted on samples cured under various conditions. The magnitude of the second order harmonic was measured and the corresponding ultrasonic nonlinear parameter was evaluated. A fairly good correlation between the curing condition and the nonlinear parameter is observed. The results show that the nonlinear parameter might be used as a good indicator of the cure state for adhesive joints.

Qu, Jianmin↗

Enhanced diffusion welding

Surfaces of unrecrystallized alloys are sanded and polished. This is followed by a two-step welding process by which the strength of the parent metal is retained at the weld joint. The first step forces the surfaces into intimate contact at a temperature where the metal still has good ductility. The second step causes diffusion, recrystallization, and grain growth across the original weld interface.

Holko, K. H.↗

Affordable, Robust Ceramic Joining Technology (ARCJoinT) Given 1999 R and D 100 Award

Advanced ceramics and fiber-reinforced ceramic matrix composites with high strength and toughness, good thermal conductivity, thermal shock resistance, and oxidation resistance are needed for high-temperature structural applications in advanced high-efficiency and high-performance engines, space propulsion components, and land-based systems. The engineering designs of these systems require the manufacturing of large parts with complex shapes, which are either quite expensive or impossible to fabricate. In many instances, it is more economical to build complex shapes by joining together simple geometrical shapes. Thus, joining has been recognized as an enabling technology for the successful utilization of advanced ceramics and fiber-reinforced composite components in high-temperature applications. However, such joints must retain their structural integrity at high temperatures and must have mechanical strength and environmental stability comparable to those of the bulk materials. In addition, the joining technique should be robust, practical, and reliable. ARCJoinT, which is based on the reaction-forming approach, is unique in terms of producing joints with tailorable microstructures. The formation of joints by this approach is attractive since the thermomechanical properties of the joint interlayer can be tailored to be very close to those of the base materials. In addition, high-temperature fixturing is not needed to hold the parts at the infiltration temperature. The joining process begins with the application of a carbonaceous mixture in the joint area, holding the items to be joined in a fixture, and curing at 110 to 120 C for 10 to 20 min. This step fastens the pieces together. Then, silicon or a silicon alloy in tape, paste, or slurry form is applied around the joint region and heated to 1250 to 1425 C (depending on the type of infiltrant) for 10 to 15 min. The molten silicon or silicon-refractory metal alloy reacts with carbon to form silicon carbide with controllable amounts of silicon and other phases as determined by the alloy composition. Joint thickness can be readily controlled through adjustments of the properties of the carbonaceous paste and the applied fixturing force. The photograph shows various shapes of silicon-carbide-based ceramics and fiberreinforced composites that have been joined using ARCJoinT. Thermomechanical and thermochemical characterization of joints is underway for a wide variety of silicon-carbidebased advanced ceramics and fiber-reinforced composites under the hostile environments that will be encountered in engine applications. ARCJoinT, which was developed by researchers at the NASA Glenn Research Center at Lewis Field, received R&D Magazine's prestigious R&D 100 Award in 1999.

Singh, Mrityunjay↗

Manufacture and performance of carbon/epoxy 3-D woven composites

This paper evaluates 3-D orthogonal woven carbon/epoxy composites. Preforms were manufactured on an automatic 3-D weaving machine developed at N.C. State University. Matrix infiltration was conducted at MBB Central Laboratories. Testing was carried out at both locations and the joint results will be reported. The properties investigated include: interlaminar shear strength, compression, compression after impact, bending, tensile and penetration resistance. The 3-D orthogonal woven composites were compared with laminated and other 3-D composites made with preforms having interlock structure. C-scans were used to examine the quality of infiltration and the damage area after impact. The performance of the composites made from the 3-D orthogonal preforms showed superior properties compared to the other composites. The penetration resistance test showed unexpectedly very good performance.

Brandt, J.↗

Integral Airframe Structures (IAS): Validated Feasibility Study of Integrally Stiffened Metallic Fuselage Panels for Reducing Manufacturing Costs

The Integral Airframe Structures (IAS) program investigated the feasibility of using "integrally stiffened" construction for commercial transport fuselage structure. The objective of the program was to demonstrate structural performance and weight equal to current "built-up" structure with lower manufacturing cost. Testing evaluated mechanical properties, structural details, joint performance, repair, static compression, and two-bay crack residual strength panels. Alloys evaluated included 7050-T7451 plate, 7050-T74511 extrusion, 6013-T6511x extrusion, and 7475-T7351 plate. Structural performance was evaluated with a large 7475-T7351 pressure test that included the arrest of a two-bay longitudinal crack, and a measure of residual strength for a two-bay crack centered on a broken frame. Analysis predictions for the two-bay longitudinal crack panel correlated well with the test results. Analysis activity conducted by the IAS team strongly indicates that current analysis tools predict integral structural behavior as accurately as built-up structure. The cost study results indicated that, compared to built-up fabrication methods, high-speed machining structure from aluminum plate would yield a recurring cost savings of 61%. Part count dropped from 78 individual parts on a baseline panel to just 7 parts for machined IAS structure.

Munroe, J.↗

Method for Estimating Thread Strength Reduction of Damaged Parent Holes with Inserts

During normal assembly and disassembly of bolted-joint components, thread damage and/or deformation may occur. If threads are overloaded, thread damage/deformation can also be anticipated. Typical inspection techniques (e.g. using GO-NO GO gages) may not provide adequate visibility of the extent of thread damage. More detailed inspection techniques have provided actual pitch-diameter profiles of damaged-hardware holes. A method to predict the reduction in thread shear-out capacity of damaged threaded holes has been developed. This method was based on testing and analytical modeling. Test samples were machined to simulate damaged holes in the hardware of interest. Test samples containing pristine parent-holes were also manufactured from the same bar-stock material to provide baseline results for comparison purposes. After the particular parent-hole thread profile was machined into each sample a helical insert was installed into the threaded hole. These samples were tested in a specially designed fixture to determine the maximum load required to shear out the parent threads. It was determined from the pristine-hole samples that, for the specific material tested, each individual thread could resist an average load of 3980 pounds. The shear-out loads of the holes having modified pitch diameters were compared to the ultimate loads of the specimens with pristine holes. An equivalent number of missing helical coil threads was then determined based on the ratio of shear-out loads for each thread configuration. These data were compared with the results from a finite element model (FEM). The model gave insights into the ability of the thread loads to redistribute for both pristine and simulated damage configurations. In this case, it was determined that the overall potential reduction in thread load-carrying capability in the hardware of interest was equal to having up to three fewer threads in the hole that bolt threads could engage. One- half of this potential reduction was due to local pitch-diameter variations and the other half was due to overall pitch-diameter enlargement beyond Class 2 fit. This result was important in that the thread shear capacity for this particular hardware design was the limiting structural capability. The details of the method development, including the supporting testing, data reduction and analytical model results comparison will be discussed hereafter.

Johnson, David L.↗

Mechanical Properties of Friction Stir Welds in A12195-T8

An extensive study of the mechanical properties of friction stir welded Al-Li 2195 has been conducted by Lockheed Martin Michoud Space Systems under contract to NASA. The study was part of a development program in which weld parameters were defined for using FSW to assemble large-scale aluminum cryogenic tanks. In excess of 300 feet of 0.320 in. gage plate material was welded and tested. The tests include room temperature and cryogenic temperature tensile tests and surface crack tension (SCT) tests, nondestructive evaluation, metallurgical studies, and photostress analysis. The results of the testing demonstrated improved mechanical properties with FSW as compared to typical fusion welding processes. Increases in ultimate tensile strength, cryogenic enhancement and elongation were observed with the tensile test results. Increased fracture toughness was observed with the SCT results. Nondestructive evaluations were conducted on all welded Joints. No volumetric defects were indicated. Surface indications on the root side of the welds did not significantly affect weld strength. The results of the nondestructive evaluations were confirmed via metallurgical studies. Photostress analysis revealed strain concentrations in multi-pass and heat-repaired FSW's. Details of the tests and results are presented.

Kinchen, David G.↗