Elevated temperature contact creep and friction of nickel-based superalloys using machine learning assisted finite element analysis

Nickel-based superalloys with superior thermochemical, mechanical, and tribological properties are highly utilized for critical components in several high temperature applications such as gas turbines and nuclear reactors. Inconel 617, in particular, is considered as one of the main candidate superalloys for tribo-components in very-high-temperature gas-cooled nuclear reactors. Recent findings indicate that this alloy grows unique surface oxide especially in a high-temperature helium environment with distinctive wear, friction, and contact properties. Here, this study investigates the high temperature contact area evolution and frictional behavior of Inconel 617 using finite element simulation and provides predictive models for the contact and friction performance at different normal loads, dwell times, and temperatures. High temperature helium-aged Inconel 617 top surface properties (up to 600 °C) are utilized along with a single asperity-based deformable elastic-plastic contact model under combined normal and tangential loading. Machine learning is used to assist the finite element results and to predict friction coefficient as well as contact area evolution. While a small difference is observed in the instantaneous friction coefficient (no dwell time) for all temperatures, friction coefficient increases considerably with dwell time. This shows that the effect of contact creep for longer dwell times significantly dominants the effect of high temperature variation in basic mechanical parameters such as modulus and yield strength. It is found that increasing temperature and dwell times lead to the friction coefficient increase, yet the dominance of dwell time effects decreases at higher temperatures and loads. While the analysis is presented for Inconel 617, the methodology is easy to be generalized and can be applied to other HT alloys.

36 MATERIALS SCIENCE↗

Reanalysis of Cost and Moist Air Oxidation Performance for CF8C-Plus and Other Alloys for AUSC Applications

This report provides an economic analysis of CF8C-Plus and other candidate materials for Advanced Ultra Supercritical (AUSC) applications, including 347HFG, HR6W, Sanicro 25, Super 304H, Grade 92, SAVE12AD, Inconel 617, and Inconel 740H. An assessment of their moist air oxidation performance is also included. When compared with the aforementioned alloys, CF8C-Plus shows a favorable balance between cost, creep strength and moist air oxidation resistance in the temperature range of 600-700°C. Furthermore, its castability makes it additionally attractive from a manufacturing perspective. Materials with higher Ni content, such as HR6W, Sanicro 25, Inconel 617, and Inconel 740H, have better creep strength but the improved performance comes with increased cost. Stainless steel 347HFG exhibits inferior creep strength and lower moist air oxidation resistance, but at a greater cost, compared with CF8C-Plus. Super 304H, another stainless steel, has similar creep strength and cost compared to CF8CPlus at 700°C, but may not have as good moist air oxidation resistance. Grade 92 has lower creep strength and unfavorable economy compared with CF8C-Plus. SAVE12AD also has lower creep strength than CF8C-Plus, but has lower cost to use at 600°C. Both Grade 92 and SAVE12AD are also limited to the maximum use temperature of 649°C per ASME code case requirements.

36 MATERIALS SCIENCE↗

Gear Test Assembly - Experimental Testing and Analysis of Gears and Bearings - FY2026

The Gear Test Assembly (GTA) is an experimental test apparatus built and installed in the Mechanisms and Engineering Test Loop (METL) at Argonne National Laboratory (ANL). While designed to accommodate a variety of components intended for use in advanced compact in-vessel transfer machine, the focus of GTA been the testing of large radial spur gears. The performance of the components used in GTA motivates the choices made in the design, components, and material choices for the forthcoming METL test articles; the Gripper Test Assembly (GrTA), and the Bearing Test Assembly (BTA). To date, GTA has completed nine experimental testing campaigns and achieved over 21 million revolutions under prototypic sodium fast reactor loads and operating conditions. This report provides an overview and results for the two most recent experiments Campaign #8 and Campaign #9. `Campaign #8 was the first campaign to make use of a set of nickel alloy radial spur gears, made from Hastelloy C-22HS, and combined with heat-treated tapered roller bearings. The bearings and torque profile used allowed Campaign #8 to be directly compared with Campaign #1 where Inconel 718 gears were used instead. Campaign #8 attained 1,058,880 shaft revolutions within 23% of the 1,314,855 revolutions achieved in Campaign #1. These results demonstrate that the heat-treated tapered roller bearings show consistent increased lifetimes, approximately three times longer than for non heat-treated taper rollers, and that the particular material of the gear does not play a substantial role in performance. Similar to Campaign #7 where bearing failure resulted in fragmentation and transport of bearing material into the gear teeth led to tooth damage in the Inconel gears, a similar process led to the damage of the Hastelloy gears. Subsequent NDE analysis showed that the damage was only limited to the tooth surface and does not extend into the gear interiors. Based on the NDE reports, the Hastelloy gears can be reconditioned and put back into service for future campaigns as was done for the Inconel gears. Reconditioned Inconel 718 gears damaged in Campaign #7 were returned to service in Campaign #9 and paired with non heat-treated tapered roller bearings. In Campaign #9 a novel set of operating conditions were implemented whereby the gears and bearings were cycled between hot, submerged refueling conditions where fuel handling operations occurred and cold, dry, and inert conditions where the sodium was drained and the vessel was allowed to cool simulating long, ex-vessel storage of the fuel handling machine. A total of eight of these operating cycles were achieved before a bearing failure occurred after the accumulation of 475,692 shaft revolutions were achieved. During Campaign #9, one of the drive motors was damaged and over the course of a 240 day standby period, the entire GTA drive system was upgraded from a 480VAC system to a 240VAC system that provided the opportunity to consolidate wall-space in the METL facility and provide more space for additional test articles being installed in the coming year. The over 475,000 shaft revolutions achieved in Campaign #9 eclipses the previous record for lifetime of non heat-treated tapered roller bearings held by Campaign #3 of 392,000 shaft revolutions. Further analysis and future campaigns hope to shed light on the cause of this approximately 17% increase in lifetime.

42 ENGINEERING↗

Tungsten wire-reinforced superalloys for 1093 C (2000 F) turbine blade applications

Various combinations of fiber and matrix materials were fabricated and evaluated for the purpose of selecting a specific combination that exhibited the best overall properties for a turbine blade application. A total of seven matrix alloys, including Hastelloy X, Nimonic 80A, Inconel 600, Inconel 625, IN-102, FeCrA1Y, were investigated reinforced with either 218CS tungsten, or W-Hf-C fibers. Based on preliminary screening studies, FeCrA1Y, Inconel 600 and Inconel 625 matrix composites systems were selected for extended thermal cycle tests and for property evaluations which included stress rupture, impact, and oxidation resistance. Of those investigated, the FeCrA1Y matrix composite system exhibited the best overall properties required for a turbine blade application. The W-Hf-C/FeCrA1Y system was selected for further property evaluation. Tensile strength values of up to 724 MPa (105,000 psi) were obtained for this material at 982 C and 607 MPa at 1093 C.

Friedman, G. I.↗

Post-test examination of a pool boiler receiver

A subscale pool boiler test apparatus to evaluate boiling stability developed a leak after being operated with boiling NaK for 791.4 hr at temperatures from 700 to 750 C. The boiler was constructed using Inconel 625 with a type 304L stainless steel wick for the boiler and type 316 stainless steel for the condenser. The boiler assembly was metallurgically evaluated to determine the cause of the leak and to assess the effects of the NaK on the materials. It was found that the leak was caused by insufficient (about 30 pct.) joint penetration in a butt joint. There was no general corrosion of the construction materials, but the room temperature ductility of the Inconel 625 was only about 6.5 pct. A crack in the heat affected zone of the Inconel 625 near the Inconel 625 to type 316 stainless steel butt joint was probably caused by excessive heat input. The crack was observed to have a zone depleted of iron at the crack surface and porosity below that zone. The mechanism of the iron depletion was not conclusively determined.

Dreshfield, Robert L.↗

Cryogenic Brush Seal Test Results

Brush seals are compliant, contact seals that have long-life, low-leakage characteristics desirable for use in rocket engine turbopumps. 50.8-mm (2.0 inch) diameter brush seals with a nominal initial radial interference of 0.127-mm (0.005 inch) were tested in liquid nitrogen at shaft speeds up to 35,000 rpm and differential pressure loads up to 1.21 MPa (175 psi) per brush. The measured leakage rate of a single brush was 2-3 times less than that measured for a 12-tooth, 0.127-mm (0.005 inch) radial clearance labyrinth seal used as a baseline. Stage effects were studied and it was found that two brush seals with a large separation distance leaked less than two brushes tightly packed together. The maximum measured groove depth on the Inconel 718 rotor was 25.4 (mu)m (0.001 inch) after 4.31 hours of shaft rotation. The Haynes-25 bristles wore approximately 25.4-76.2 (mu)m (0.001-0.003 inch) under the same conditions. Three seal runner coatings, chromium carbide, Teflon impregnated chromium, and zirconium oxide, were tested in liquid hydrogen at 35,000 and 65,000 rpm with separate 50.8 mm diameter brush seals made of Haynes-25 bristles and having a nominal initial radial interference of 129 rpm. Two bare Inconel-718 rotors were also tested as a baseline. The test results revealed significant differences between the wear characteristics of the uncoated and coated seal runners. At both speeds the brush seal with the bare Inconel-718 seal runner exhibited significant bristle wear with excessive material transferring to the runner surface. In contrast, the coated seal runners inhibited the transfer and deposit of bristle material. The chromium carbide coating showed only small quantities of bristle material transferring to its surface. The Teflon impregnated chromium coating also inhibited material transfer and provided some lubrication. This coating, however, is self-sacrificing. The Teflon remained present on the low speed runner, but it was completely removed from the high speed brush seal, which was tested considerably longer. The tests of the Teflon coating revealed the importance of using a lubricating and low friction coating for brush seals to reduce bristle and seal runner wear. The zirconium oxide coating exhibited the greatest amount of coating wear, while the brushes incurred only slight wear. Further testing of ceramics is recommended before making a final judgement on the viability of ceramic coatings for brush seals because of the contrast between the results reported by Carlile and the results presented herein. Strictly based on the results presented hereinabove, the chromium carbide and Teflon impregnated chromium coatings were considered preferable to the uncoated Inconel-718 and zirconium oxide coatings because of their good wear resistance and characteristics to inhibit bristle material wear and transfer to the seal runner.

Proctor, Margaret P.↗

Improved Seals for High Temperature Airframe Applications

Current thermal barrier seals, such as those used on the Space Shuttle, are insufficient to fully meet the demands of future hypersonic vehicles and reentry spacecraft. Previous investigations have demonstrated limited usage temperatures, as evidenced by a decreased ability to maintain sealing effectiveness at high temperatures (i.e., inadequate resiliency). In order to improve resiliency at elevated temperatures, Rene 41 (Allvac) was substituted for Inconel X-750 (Special Metals Corp.) as the spring tube material in the existing seal design. A seal construction incorporating the Rene 41 spring tube was fabricated and tested against the baseline Inconel X-750 spring tube seal. Although resiliency improvements were not as dramatic as in previous tests with the spring tubes alone, seals incorporating the Rene 41 spring tube exhibited an average 20 percent resiliency enhancement up to 1750 F when compared to seals containing the Inconel spring tube. In addition, the seals with the Rene 41 spring tubes showed less reduction in resiliency as temperatures increased above 1200 F. Results also indicated the Saffil (Saffil Ltd.) insulation in the core of the seal contributed more to resiliency than previously thought. Leakage data did not demonstrate an improvement with the seal containing the Rene 41 spring tube. However, based upon resiliency results, one could reasonably expect the Rene 41 version of the seal to track gap openings over a wider range. Therefore it would exhibit lower leakage than the Inconel X-750 version as the seal gap opens during a typical mission.

DeMange, Jeffrey J.↗

Determining the Effects of Neutron Irradiation on the Structural Integrity of Additively Manufactured Heat Exchangers for Very Small Modular Reactor Applications, DOE Final Report (Project # 19-16980)

Auburn University (AU) teamed with the University of Missouri Research Reactor (MURR) and Kansas State University (KSU) to determine how to best use laser-powder bed fusion (L-PBF) additive manufacturing (AM) methods for generating radiation resistant nickel-based superalloys, Inconel alloy 625 and 718, for special purpose reactor (SPR) or very small modular reactor (vSMR) heat-exchangers (HeXs). Compact, conformal, and durable HeXs that are tolerant of extreme environments are needed for supporting the technical maturity of next-generation, portable compact reactors. AM is an enabler for realizing this new wave of HeXs – providing a means to make customizable hot and cold stream architectures with novel flow path geometries (e.g., tortuous channels with non-uniform, asymmetric cross-sections) and reduced layer-to-layer contact resistance (i.e., no separate bonding procedure required). AM further enables a more time/cost efficient means for fabricating SPRs by reducing the number of suppliers required for HeX assembly and allowing for on-site HeX fabrication. The project aim has been to better understand how neutron irradiation affects the microstructure and properties of additively manufactured nickel-based superalloys, to accelerate their safe, reliable use in the modular reactor industry. The major objective was to qualify/quantify the microstructure and microhardness of nickel-based superalloys (including Inconel 718 and 625) additively manufactured via the L-PBF process in the neutron-dosed (irradiated) and non-irradiated states over a course of 3 years. Effects of build orientation during L-PBF and post-AM heat treatments on neutron resistance, microstructure and mechanical properties were also investigated. Neutron damage mechanisms via hardening were characterized. This project combined subject-matter experts in AM, mechanical/microstructure metallic part characterization, and neutron irradiation, as well as unique assets and capabilities at AU and MURR at MU, to ensure project results translated to effectively addressing known gaps in nuclear science and engineering. Parts were fabricated using L-PBF systems readily available at AU. Specimens were then irradiated using MURR facilities; a manipulator equipped hot cell was also used to measure material hardness after dosing. MURR, a 10 MW, light-water nuclear reactor, is the largest, highest powered, highest-flux university owned research reactor in the U.S. The major findings in this project provide evidence that AM can serve as an alternative way to build structural components for future advanced small modular reactors using advanced materials like Inconel 625 (IN625) or Inconel 718 (IN718). After full spectrum neutron irradiation, vertically as-built AM IN625 samples were observed to display better resistance towards radiation-induced-hardening defects relative to traditionally machined metals. A Vickers microhardness tester, using settings of 1 kgf and dwell time of 15 seconds per indentation, was used to measure hardness in this study. The as-built, vertically printed samples experienced 1.2% of radiation hardening vs. 5.25% radiation hardening observed in wrought IN625. Another set of IN625 and IN718 samples were exposed to fast neutron irradiation. It was observed that IN718 showed more resistance towards radiation hardening compared to IN625 samples indicating IN718 had a better performance. Results showed that the IN718 samples experienced less change (-2.5 to 3.24 %) in microhardness. On the other hand, IN625 samples underwent more (0.9 to 7.21%) change in microhardness after fast neutron irradiation. AM IN625 samples were irradiated using an ion (proton) beam in cyclotron. The mechanical properties of AM samples post irradiation were compared with wrought samples. The irradiated region on the samples were tested using nano-hardness indention. It was observed that the beam current and time used in this study generated an annealing effect and thus reduced the hardness of the samples. The sum of the project results provide precious insight into how one may minimize radiation hardening in AM materials while maintaining material property constraints. Results should assist engineers in selecting an appropriate heat treatment for AM nickel-based superalloys for increased radiation resistance. Results should increase confidence levels for adopting AM for building nuclear reactor components which perform the same or better than conventionally manufactured components. Fast neutron irradiation testing provided an accelerated means of obtaining radiation effects without making materials radioactive and difficult to handle.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Ignition of Metals in Heated Supersonic Particle Impact with Inert Particulate

The conventional understanding of particle impact ignition characteristic elements relies on the following principles: 1) flammable particulate (except in the case of titanium and aluminum target materials); 2) gas velocity greater than 100 ft/s; 3) Impact point ranging from 45° to perpendicular to the path of the particle [1]; 4) flammable target material. To test assumptions about particulate flammability being necessary for particle impact ignition of less reactive target materials, such as Inconel 718, testing was performed with inert particulate. Supersonic particle impact testing was conducted with heated gas and 1500-µm sapphire particulate on various target materials: 304 stainless steel, wrought and selective laser melted Inconel 718, and Monel 400. Posttest characterization of impact craters was performed on each type of metallic target sample, including surface characterization performed by light optical microscopy and scanning electron microscopy with energy dispersive spectroscopy. Full consumption of the stainless steel and wrought Inconel 718 targets were noted to occur with sequential impacts. The results of testing will be discussed in detail, as well as recommendations for updating the understanding of the particle impact ignition mechanism.

Particle Impact↗

Elucidating the corrosion mechanism of commercial Ni-based Superalloys in UCl3 containing-chloride Molten Salt Systems

Molten salt reactors (MSRs) have gained renewed interest, providing several advantages over their predecessors, including the capability to consume spent fuels, enhancing the environmental sustainability of the uranium fuel cycle. For example, molten chloride fast reactors (MCFRs) can reach criticality with molten chloride spent fuel containing high concentrations of impurities, such as actinide products like uranium chloride (UCl3). However, the redox potential of chloride molten salt fuels may change in the presence of these impurities, dictating their corrosivity and in turn the corrosion performance of structural components, such as those constructed from nickel (Ni)-based alloys. The purpose of this investigation is to assess the extent of corrosion of Ni-based alloy, Inconel 617, when exposed to UCl3-LiCl-KCl eutectic salt. Inconel 617 one of only six structural materials that are fully qualified by the American Society for Mechanical Engineers (ASME) Boiler and Pressure Vessel Code for high-temperature nuclear reactor components, making it a technologically mature material to consider for constructing MCFRs. Inconel 617 specimens were submerged in a static LiCl-KCl-UCl3 eutectic salt mixture heated at 700 C for 1000 h under an inert atmosphere. Upon completion, the extent of corrosion was analyzed through a multi-modal characterization approach spanning the engineering to nanoscale, employing computed tomography, focused-ion beam, and transmission electron microscopy techniques. Results from this investigation will enhance our understanding of property-to-performance relationships of candidate structural materials for MSRs with respect to corrosion resistance and interactions between the salt and alloy interface.

36 MATERIALS SCIENCE↗

Nanotwinned alloys under high pressure

Nanotwinned alloys are of interest due to their high strength and ductility, but twin boundaries may not be stable under shear. Computational studies indicate that high hydrostatic pressure may suppress detwinning mechanisms. Here, in this study, we investigate the microstructural changes of nanotwinned-nanocrystalline copper-nickel and Inconel 725 alloys under quasi-hydrostatic pressures up to 50 gigapascals (GPa). The alloys are compressed in a diamond anvil cell. In-situ x-ray diffraction (XRD) and ex-situ transmission electron microscopy (TEM) were employed to monitor microstructural changes. Twin boundary deformation and grain growth occur at 11.4 GPa quasi-hydrostatic pressure in the copper-nickel alloy. Molecular dynamics (MD) simulations reveal that hydrostatic pressure causes elevated local shear stress at grain boundaries, which leads to atomic rearrangements. A superposition of hydrostatic and deviatoric pressures lead to partial dislocation mediated twin boundary migration. In contrast, the Inconel 725 alloy showed stable twin and grain boundaries up to a quasi-hydrostatic pressure of 12.7 GPa. Texture, high solid solution strengthening, and low stacking fault energy are hypothesized to the enhanced microstructural stability in Inconel 725.

36 MATERIALS SCIENCE↗

Radiation Effects Related to Repaired BWR Core Shrouds

The material properties of the core shroud and supporting tie rod components are important factors for Boiling Water Reactor (BWR) life extension considerations. Given the variability of nickel and boron content found in 304 stainless steel shroud plates, and XM-19 and Inconel X-750 tie rod materials, this paper combines the latest spectral information in the vicinity of the core shroud to calculate hydrogen and helium gas production limits as well as atomic displacement damage spanning 80 full-power years (FPY) using the SPECTER code. Results indicate that, whereas boron has little effect on the atomic displacement damage, helium production from boron can be important and must be included in weldability assessments. Since the boron concentration is uncertain, helium generation is calculated assuming a composition range based on specifications and reported measurements. The results show that helium production caused by transmutations in the 304 SS shroud material are dominated by the concentration of boron and will have a significant impact on weldability after only a few years of service. For tie rods, the susceptibility to irradiation-assisted stress corrosion cracking (IASCC) has been assessed by determining helium production in Inconel X-750 IASCC specimens irradiated in the Advanced Test Reactor (ATR) reactor and correlating with the helium produced in a BWR. As a tie rod material in a high thermal neutron flux environment, Inconel X-750 is more likely to be IASCC sensitive during service in a BWR due to helium than the XM-19 stainless steel alloy because of a greater nickel content and boron concentration. Weldability of the core shroud plate material, IASCC of the tie rod materials, and the gamma photon contribution to radiation damage are discussed.

radiation damage in materials, BWR↗

Formulation and testing of a high-tin borosilicate nuclear waste glass for in-can melting

Here, borosilicate waste glasses were successfully developed to immobilize two high-level waste raffinate streams via an in-can melter process with an Inconel 601 canister at 1050 °C. Measured viscosity and crystallinity thermal profiles were within the targeted processing constraints for the in-can melter process. Measured chemical durability of the glass by ASTM C1285–21 (Method A), ranged from normalized loss of boron, NL(B) = 1.44 – 2.65 g•m -2 , and NL(B) decreased with increased waste loading, accompanied by increased SnO 2 crystallinity. Measured corrosion of the in-can melter canister by a glass melt showed that Inconel 601 performed well at 1100 °C for up to 500 hr. Resistance polarization measurements versus time revealed that Inconel 601 corrosion rates in (and by) glass melts decreased from an initial rate of 63 mm•y -1 down to 10.2 mm•y -1 after 137 h with increased duration, which was attributed to formation of an oxide passivation layer (mainly Cr 2 O 3 ) at the alloy-glass interface.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Experimental investigations of Critical Heat Flux re-occurrence on post-CHF surfaces

Under the extreme environments of light water reactors, the cladding materials demonstrate evolutionary transformations in terms of material compositions, surface morphologies, and thermal-physical properties. This study investigates how the temperature overshooting of Critical Heat Flux (CHF) affects the re-occurrence of CHF on the post-CHF surfaces. Experimental results reveal that the CHF difference between as-received and post-CHF surfaces can be significant, which depends on materials. CHF is enhanced on post-CHF Stainless Steel (SS 316) specimens while it deteriorates on post-CHF Inconel-600 specimens. In comparison with the as-received surfaces, the post-CHF surface of SS 316 is more hydrophobic, while Inconel 600 is more hydrophilic. The scanning electron microscope micrographs of post-CHF surfaces show that surface morphologies that are structured by oxide crystals are formed on SS 316 samples but not on Inconel 600 samples. The physical rationale behind the CHF difference could be boiling heat transfer conjugated with thermal-physical proprieties of investigated surface materials and surface morphologies features. In conclusion, the results imply that it is indispensable to bookkeep the evolutionary changes of cladding surface materials, especially for cladding candidates of Accident Tolerant Fuel since operation histories can leave footprints on cladding surfaces, thus resulting in CHF re-occurrence differences.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Integrated modeling of cracking during deep penetration laser welding of nickel alloys

During deep penetration laser welding of nickel alloys, interactions between composition and processing conditions can lead to the formation of defects. Inconel 740H, for example, has demonstrated a susceptibility to horizontal fusion zone cracking at locations between 70% and 80% of the weld depth during laser welding at powers above 5 kW. Coupling three-dimensional heat transfer, fluid flow, and stress modeling tools allowed that both the strain rate and stress normal to the solidification direction to be calculated. In the Inconel 740H welds, cracks formed at locations where the strain rate and stress simultaneously reached critical levels. No cracking was observed in the Inconel 690 welds, since the strain rate and stress did not simultaneously reach these critical levels.

36 MATERIALS SCIENCE↗

Best Practices for Shielding Analyses of Activated Metals and Spent Resins from Reactor Operation

This report investigated best practices for performing shielding evaluations of Type B waste packages, as defined in 10 CFR Part 71 regulations on packaging and transportation of radioactive material, or packages for which the contents are not defined before loading and may include a broad range of nuclides, geometries, and non-fuel materials. The following non-fuel waste streams were analyzed: Activated metals from decommissioned commercial power reactors, including Type 304 stainless steel, reactor vessel steel, and Inconel, Control blades from boiling water reactors, Neutron-activated corrosion products on surfaces of activated metals, and Spent resins from power plant operations. Measured elemental compositions, including major constituents and impurities, for steel and Inconel samples from commercial power reactors were used in activation calculations to determine radionuclide inventories in activated metals. For a simplified cask model, 60 Co contribution to the total external package dose rate at 30 days after shutdown varied from approximately 60% to 95%, depending on the activated metal, initial cobalt impurity concentration in the metal, and the thickness of the overpack gamma shield. Its maximum contribution to the total external package dose rate of approximately 100% was reached within the time interval of 2 to 5 years after shutdown and was maintained for up to 45 to 60 years after shutdown, depending on material, initial cobalt impurity concentration, and shield thickness. Thereafter, the 60 Co contribution to external package dose rate decreased with increasing decay time. Cobalt-60 is primarily produced by neutron reactions with the cobalt impurity in steel and Inconel. Other important radionuclides in activated metals contributing to package external dose rate are radionuclides with relatively short decay times, including 51 Cr, 59 Fe, 58 Co, and 54 Mn. These radionuclides may be represented as an equivalent 60 Co activity/source because 60 Co gamma ray emissions are bounding in terms of source strength and energy to other important radionuclides identified in the analyzed activated metals. Approaches for modeling the neutron-activated corrosion products that may be attached to activated reactor components were analyzed in this report. It was demonstrated that a surface source is more conservative than a uniform volumetric source for the treatment of neutron-activated corrosion products with respect to external package dose rates. An analysis of the maximum radionuclide loadings reported on spent resins identified the radionuclides 137 Cs, 60 Co, 134 Cs, 65 Zn, and 58 Co as the primary contributors to external package dose rate. For a resin cooled for 3.08 years, the external package dose rate was entirely produced by the reported 137 Cs and 60 Co inventory. The neutron sources from actinides found on spent resins or activated metals produced negligible dose rates and may be ignored in dose rate analyses. Effects of idealized waste material, source geometry, and spatial material/source distributions on external package dose rates were determined based on dose rate results for a simplified cask model under normal conditions of transport. Type 304 stainless steel, zirconium, and aluminum with adjusted mass densities based on a maximum content weight were analyzed for material modeling effects on external package dose rate. These materials produced identical external package dose rates within the statistical uncertainties of the dose rate estimates. Among four different source geometry configurations with homogeneous material of different mass densities, uniform volumetric source distribution, and the same source strength, the geometry configuration with lowest mass density (i.e., minimum self-shielding effect among the four cases) was most conservative. Spatial source distributions that better represent localized peak 60 Co activity values were more conservative than a uniform volumetric source distribution, assuming the same weight and total source strength per package. The increase in external dose rate caused by localized source peaks can be as much as the ratio between source peak activity density to average activity density, depending on the location of the activated metal with peak activity density. Therefore, the shielding analysis may be simplified if localized peak activities and the average activity per package can be measured/determined and documented at the time of cask loading. For simplicity, external package dose rates may be determined based on average source activity and a uniform volumetric source distribution. The dose rate results from that calculation model multiplied by the ratio of peak activity density to average activity density will produce maximum dose rate values for conservative estimates.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Application of Refractory High-Entropy Alloys for Higher-Reliability and Higher-Efficiency Brayton Cycles and Advanced Nuclear Reactors

An exceptional set of newly-discovered advanced superalloys known as refractory high-entropy alloys (RHEAs) can provide near-term solutions for wear, erosion, corrosion, high-temperature strength, creep, and radiation issues associated with supercritical carbon dioxide (sCO2) Brayton Cycles and advanced nuclear reactors. In particular, these superalloys can significantly extend their durability, reliability, and thermal efficiency, thereby making them more cost-competitive, safer, and reliable. For this project, it was endeavored to manufacture and test certain RHEAs, to solve technical issues impacting the Brayton Cycle and advanced nuclear reactors. This was achieved by leveraging Sandia’s patents, technical advances, and previous experience working with RHEAs. Herein, three RHEA manufacturing methods were applied: laser engineered net shaping, spark plasma sintering, and spray coating. Two promising RHEAs were selected, HfNbTaZr and MoNbTaVW. To demonstrate their performance, erosion, structural, radiation, and hightemperature experiments were conducted on the RHEAs, stainless steel (SS) 316 L, SS 1020, and Inconel 718 test coupons, as well as bench-top components. The experimental data is presented, analyzed, and confirms the superior performance of the HfNbTaZr and MoNbTaVW RHEAs vs. SS 316 L, SS 1020, and Inconel 718. In addition, to gain more insights for larger-scale RHEA applications, the erosion and structural capabilities for the two RHEAs were simulated and compared with the experimental data. The experimental data confirm the superior performance of the HfNbTaZr and MoNbTaVW RHEAs vs. SS and Inconel. Most importantly, the erosion and the coating material experimental data show that erosion in sCO2 Brayton Cycles can be eliminated completely if RHEAs are used. The experimental suite and validations confirm that HfNbTaZr is suitable for harsh environments that do not include nuclear radiation, while MoNbTaVW is suitable for harsh environments that include radiation.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Conjugate Heat Transfer Analysis in Pressurized Helium Gas Cooling Channels

Los Alamos National Laboratory (LANL) is working with NorthStar Medical Radioisotopes (NMR) on their efforts to produce Mo-99 from the irradiation of Mo-100 targets. The NMR target consists of an Inconel window that allows the electron beam to penetrate and irradiate a stack of Mo-100 disks. The irradiation process generates large amounts of heat and is cooled using pressurized helium gas flowing at 400 g/s. LANL provides both numerical analysis support and experimental support. Computational fluid dynamics (CFD) and conjugate heat transfer (CHT) analysis are performed on the NMR target to analyze the helium flow and volumetric heating through the NMR system. In this iteration of numerical analysis, we update the Mo-100 disk thickness to 0.74 mm and the gap between the Inconel window and the first disk to 0.69 mm. Estimates of the heat flux from the electron beams from Monte Carlo N-Particle code (MCNP) analysis were combined with CFD to perform the CHT analysis. The pressure drop through the targets, force applied on the first disk, beam window and target disk temperatures are some of the quantities estimated using the simulations. The pressure drop through the target was estimated as 0.198 MPa, while the force due to venturi effects across the first disk was estimated to be 100 N. The results show maximum window temperatures over 600 °C and peak disk temperatures over 1600 °C. Past work has shown that beyond 650-700 °C, the Inconel window becomes susceptible to yield and rupture. The increased temperature in these results reduces the margin of error possible on beam spot size. The disk temperatures showed a sinusoidal distribution with the 6 th – 8 th disk from each window exhibiting highest disk temperatures. The peak temperature of the stainless steel housing was close to 316 °C and that of the laminations and spacers was approximately 582 °C.