Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “FRICTION STIR WELDING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 289 records · Page 16

Inspecting Friction Stir Welding using Electromagnetic Probes

A report describes the use of advanced electromagnetic probes to measure the dimensions, the spatial distribution of electrical conductivity, and related other properties of friction stir welds (FSWs) between parts made of the same or different aluminum alloy(s). The probes are of the type described in in another Tech Brief. To recapitulate: A probe of this type is essentially an eddy-current probe that includes a primary (driver) winding that meanders and multiple secondary (sensing) windings that meander along the primary winding. Electrical conductivity is commonly used as a measure of heat treatment and tempering of aluminum alloys, but prior to the development of these probes, the inadequate sensitivity and limited accuracy of electrical-conductivity probes precluded such use on FSWs between different aluminum alloys, and the resolution of those probes was inadequate for measurement of FSW dimensions with positions and metallurgical properties. In contrast, the present probes afford adequate accuracy and spatial resolution for the purposes of measuring the dimensions of FSW welds and correlating spatially varying electrical conductivities with metallurgical properties, including surface defects.

Kinchen, David G.↗

Impact of Backing Plate and Thermal Boundary Conditions for High-Speed Friction Stir Welding of 25-mm Thick Aluminum Alloy 7175-T79

Here this study demonstrates high-speed (150 mm/min) single pass friction stir butt joining of 25 mm thick aluminum alloy 7175-T79. To understand the impact of quenching and cooling rate on process responses, joint strength, and grain size distributions across the weld thickness, we performed a series of friction stir welding (FSW) trials in air and with a trailing water spray using steel and composite backing plates (BP). Welds made in air and trailing water spray exhibit significantly different hardness distributions across the nugget, heat affected zone (HAZ), and HAZ minimum hardness as evidenced by detailed microhardness mapping. The effect of trailing water spray (TWS) on joint efficiency overshadows the influence of BP composition due to the vastly different contribution to quenching. TWS also resulted in a multifaceted effect on FSW such as lowering processing temperature, increasing X and Z forces while lowering Y force, and narrow heat affecting zone. Finally, digital image correlation (DIC)-based fracture mode analysis and grain size measurements correlate with the hardness distribution.

42 ENGINEERING↗

A FEASIBILITY STUDY ON CRACK REPAIR IN AUSTENITIC STAINLESS STEEL DRY STORAGE CANISTERS USING ISOTHERMAL FRICTION STIR WELDING

In recent time, solid state crack repair techniques in spent nuclear fuel dry storage canisters (SNF-DSC) have garnered significant interest. Plates of austenitic stainless steels are usually arc welded to fabricate the cylindrical canisters which are prone to chloride-induced stress corrosion cracking. Friction stir welding (FSW) is considered to be a potential candidate for damage repair. In this work, electrical discharge machining was used to simulate cracks in 304L stainless steel plates of 12.7 mm thickness. Subsequently, isothermal FSW was carried out at two different temperatures (725 and 825°C) in order to repair the simulated crack. Microstructure-mechanical property correlations in FSWed plates were studied in detail. Significant grain refinement observed in the stir zone (SZ) was attributed to dynamic recrystallization occurring during FSW. A comparison of Vickers microhardness showed higher hardness and homogeneity in the 725°C SZ than its 825°C counterpart. The fraction of S3 boundary is found to be low in the SZ as compared to base metal (BM). Yield strength of the joints was found to be approximately 100 MPa higher than that of the BM accompanied by a drop in ductility by a factor of 2. Residual stress profile across 825°C weld was measured using x-ray diffraction.

Bhattacharyya, Madhumanti↗

Mechanical Properties and Wear Behavior of AA5182/WC Nanocomposite Fabricated by Friction Stir Welding at Different Tool Traverse Speeds

Grain growth inhibition at the heat-affected zone, improved weld strength and superior tribological properties of welds are desirable attributes of modern manufacturing. With the focused on these attributes, tungsten carbide (WC) nanoparticles were employed as reinforcements for the friction stir welding of 5-mm-thick AA5182 aluminum alloy by varying tool traverse speeds. The microstructure, microhardness, ultimate tensile strength, fracture and wear behavior of the resultant WC-reinforced welds were investigated, while unreinforced AA5182 welds were employed as controls for the study. The result shows that the addition of WC nanoparticles causes substantial grain refinement within the weld nugget. A decrease in traverse speed caused additional particle fragmentation, improved hardness value and enhanced weld strength in the reinforced welds. Improved wear rate and friction coefficient of welds were attained at a reduced traverse speed of 100 mm/min in the WC-reinforced welds. This improvement is attributed to the effects of reduced grain size/grain fragmentation and homogeneous dispersion of WC nanoparticles within the WC-reinforced weld nugget.

36 MATERIALS SCIENCE↗

Friction stir welding of thick 7175 aluminium alloy plates for deepwater riser applications

To substantially reduce the cost of extracting petroleum from ultra-deepwater sources, manufacturing risers from 7175 aluminium (Al) alloys rather than steels is being considered. Friction stir welding (FSW), a solid-phase joining technique, is widely applied to 7XXX Al alloys because its mechanical properties are retained within the nugget zone. And, the primary technical objective of the current study is the development of high-strength, corrosion-resistant weldments that connect 7175 Al riser flanges and pipes. However, as the welding thickness increases, the welding speed can be greatly impeded, which lowers the manufacturing efficiency and weakens the mechanical properties in the heat affected zone (next to the nugget). Therefore, obtaining high-performance thick plate 7175 Al alloy joints via FSW is challenging. To overcome this dilemma, the current work optimises the tool design and welding parameters for achieving high-performance joints between 25.4 mm thick 7175 Al alloy plates in butt joint configuration.

Wang, Tianhao↗

Friction-Stir Welding of Large Scale Cryogenic Fuel Tanks for Aerospace Applications

The Marshall Space Flight Center has established a facility for the joining of large-scale aluminum-lithium alloy 2195 cryogenic fuel tanks using the friction-stir welding process. Longitudinal welds, approximately five meters in length, were made possible by retrofitting an existing vertical fusion weld system, designed to fabricate tank barrel sections ranging from two to ten meters in diameter. The structural design requirements of the tooling, clamping and the spindle travel system will be described in this paper. Process controls and real-time data acquisition will also be described, and were critical elements contributing to successful weld operation.

Jones, Clyde S., III↗

Friction Stir Weld Modeling at MSFC: Kinematics

A "merry-go-round" computation model makes it easier to visualize how tracer experiments of varied sorts (chemical, shot, wire) are consistent with a "moving plug model" of flow around the friction stir welding pin-tool. The moving plug model comprises a twofold flow: 1. a primary rotation of a plug of metal with the tool, which moves metal around the tool by wiping it on and off the plug, and 2. a secondary, relatively slow circulation induced by the threads on the tool resembling a circular vortex ring around the tool.

Nunes, Arthur C., Jr.↗

Characterization of Residual Stress Effects on Fatigue Crack Growth of a Friction Stir Welded Aluminum Alloy

An on-line compliance-based method to account for residual stress effects in stress-intensity factor and fatigue crack growth property determinations has been evaluated. Residual stress intensity factor results determined from specimens containing friction stir weld induced residual stresses are presented, and the on-line method results were found to be in excellent agreement with residual stress-intensity factor data obtained using the cut compliance method. Variable stress-intensity factor tests were designed to demonstrate that a simple superposition model, summing the applied stress-intensity factor with the residual stress-intensity factor, can be used to determine the total crack-tip stress-intensity factor. Finite element, VCCT (virtual crack closure technique), and J-integral analysis methods have been used to characterize weld-induced residual stress using thermal expansion/contraction in the form of an equivalent delta T (change in local temperature during welding) to simulate the welding process. This equivalent delta T was established and applied to analyze different specimen configurations to predict residual stress distributions and associated residual stress-intensity factor values. The predictions were found to agree well with experimental results obtained using the crack- and cut-compliance methods.

Newman, John A.↗

Effect of Zinc Interlayer in Microstructure Evolution and Mechanical Properties in Dissimilar Friction Stir Welding of Aluminum to Titanium

The welding of aluminum (Al) and titanium (Ti) is difficult and challenging due to the differences in their chemical and physical properties, and the formation of brittle intermetallic phases. In the present experiment, a zinc (Zn) interlayer was used during friction stir welding of Al to Ti. The weld was characterized in detail to understand the mechanisms associated with microstructural evolution and improvement in mechanical properties of the weld. X-ray computed tomography results reveal three-dimensional distribution of particles and flakes of titanium in the weld nugget. It was also observed that Ti particles are inhomogeneously distributed in the weld and the distribution depends on their morphology. Such a distribution of Ti was informative in understanding material flow. In addition, the consolidation of Zn in the Al matrix reveals the nature of material flow in the weld nugget as well. The importance of the Zn interlayer and mechanism of phase formation was explored in this study. It was characterized that the mechanical mixing of Zn with Al and Ti alters phase evolution and restricts the formation of conventional Al{sub 3}Ti intermetallic phase. The presence of zinc homogenizes elemental distribution and inhibits the formation of brittle intermetallic phases, which leads to a substantial improvement in mechanical properties of the weld.

36 MATERIALS SCIENCE↗

Investigation of Abnormal Grain Growth in a Friction Stir Welded and Spin-Formed Al-Li Alloy 2195 Crew Module

In order to improve manufacturing efficiency and reduce structural mass and costs in the production of launch vehicle structures, NASA is pursuing a wide-range of innovative, near-net shape manufacturing technologies. A technology that combines friction stir welding (FSW) and spin-forming has been applied to manufacture a single-piece crew module using Aluminum-Lithium (AL-Li) Alloy 2195. Plate size limitations for Al-Li alloy 2195 require that two plates be FSW together to produce a spin-forming blank of sufficient size to form the crew module. Subsequent forming of the FSW results in abnormal grain growth (AGG) within the weld region upon solution heat treatment (SHT), which detrimentally impacts strength, ductility, and fracture toughness. The current study seeks to identify microstructural factors that contribute to the development of AGG. Electron backscatter diffraction (EBSD) was used to correlate driving forces for AGG, such as stored energy, texture, and grain size distributions, with the propensity for AGG. Additionally, developmental annealing treatments prior to SHT are examined to reduce or eliminate the occurrence of AGG by promoting continuous, or uniform, grain growth

Tayon, Wesley A.↗

Effect of niobium interlayer in dissimilar friction stir welding of aluminum to titanium

Highlights: • In the present study, FSW of Al to Ti with Nb interlayer has been characterized. • Fragmentation and distribution of Nb and Ti have been correlated with properties. • Ternary mixing and chemical reaction reduced the brittleness of the joint. • Al in the weld nugget showed a gradient in microstructural features. • The weld with Nb interlayer exhibited higher ductility. - Abstract: The most important issue associated with dissimilar welding is the formation of detrimental intermetallics and consequent reduction in mechanical properties of the weld. It was expected that addition of an interlayer would modify the pattern of the intermetallic formation. The present investigation deals with Friction Stir Welding of aluminum (Al) to titanium (Ti) in presence of niobium (Nb) interlayer. X-ray Computed Tomography results highlighted that fine particles of both Ti and Nb are homogeneously distributed. Large Ti particles are substantially fragmented whereas large Nb particles remain as flakes. Microstructural features of the nugget zone indicated a complex mixing of materials. Jointing had been perceived through elemental diffusion at the interfaces of Al/Ti and Ti/Nb. However, Nb restricted the reaction between Al and Ti, and acted as an efficient interlayer to retard the formation of brittle Al{sub 3}Ti intermetallic phase. Mechanisms of microstructural evolution in Al side of the weld have been identified as Dynamic Recovery, Dynamic Recrystallization and particle stimulated nucleation. Significant improvement in the tensile ductility had been observed due to the presence of finer particles. The presence of Nb in the weld nugget influences the microstructural evolution and tensile properties of the weld by reducing the formation of intermetallics.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Rapidly Cooled Friction Stir Welded Ti-6Al-4V Alloys

Two mm-thick Ti-6Al-4V alloy plates were friction stir butt welded under natural- and rapid-cooling conditions. The microstructures and mechanical properties of joints were investigated and compared. The rapid cooling via spraying cooling liquid nitrogen on the plate top surface was beneficial to obtaining a narrower cross section and finer and more uniform grains in the stir zone than those obtained by natural cooling. Joint tensile strength of 1021 MPa and elongation of 1.88% under the rapid-cooling condition respectively reached 102.7 and 150.4% of those under the natural-cooling condition, respectively. The uniform-and-compact equiaxed grains led to equiaxed dimples on the fracture surface, which demonstrated a ductile fracture of the welding joints.

36 MATERIALS SCIENCE↗

Friction Stir Welding of ODS and RAFM Steels

Advanced structural materials such as oxide dispersion strengthened steels and reduced-activation ferritic/martensitic steels are desired in fusion reactors as primary candidate materials for first wall and blanket structures, due to their excellent radiation and high-temperature creep resistance. However, their poor fusion weldability has been the major technical challenge limiting practical applications. For this reason, solid-state friction stir welding (FSW) has been considered for such applications. In this paper, the effect of FSW parameters on joining similar and dissimilar advanced structural steels was investigated. Scanning electron microscopy and electron backscatter diffraction methods were used to reveal the effects of FSW on grain size, micro-texture distribution, and phase stability. Hardness mapping was performed to evaluate mechanical properties. Finally, post weld heat treatment was also performed to tailor the microstructure in the welds in order to match the weld zone mechanical properties to the base material.

36 MATERIALS SCIENCE↗

Demonstration of friction stir Welding (FSW) Technology for packaging of used nuclear fuel - 15025

With uncertainty surrounding the disposal of US Used Nuclear Fuel (UNF), the nuclear industry is making an effort to identify an interim storage solution. One of the alternatives is to simply manage UNF on-site until a permanent repository can be established - extended storage. In an effort to provide a technical basis for extended storage, the Department of Energy (DOE) performed a gap analysis identifying several issues that need to be addressed. One of the issues relates to the performance of the UNF dry storage container (DSC). DSC container welds (fabricated using conventional fusion welding processes) are sensitive to Stress Corrosion Cracking (SCC), and their extended-term performance is questionable. Fluor, the Pacific Northwest National Laboratory (PNNL) and the Savannah River National Laboratory (SRNL) believe that Friction Stir Welding (FSW) technology may be able to address the DSC issue. The Fluor team collaborated on a project to demonstrate feasibility of FSW for DSC packaging (closure-welding). This paper reports on a 2-year project in which FSW process conditions were established (for DSC container materials and dimensions) and used in the preparation of mechanical and corrosion specimens for testing and evaluation. In addition to FSW test specimens, fusion welded specimens were prepared and tested in like manner for comparative purposes. The results show excellent mechanical properties (meeting construction code requirements) and significant improvement in corrosion performance - over the fusion welded specimens. It is believed these findings will be of significant value to efforts underway to provide a technical basis for DSC extended storage performance. FSW technology appears to be an acceptable alternative or candidate process, capable of addressing the SCC sensitivity issues associated with fusion-welded DSC fabrication welds. In addition, as an alternative to on-site, extended storage of UNF, the DOE has proposed the development and construction of a Consolidated Interim Storage Facility (CISF). UNF would be accepted from the many, local sites for consolidation at one or more CISFs until a permanent repository could be established. A recent CISF study indicates that UNF currently packaged into DSCs will likely be re-packaged into containers suitable for permanent storage. The study also indicates that re-packaging is best performed under water in a pool. FSW technology has several specific advantages for this application, 1) because it utilizes machine-tool equipment, a welding station can easily perform a cutting operation, and 2) FSW has been successfully demonstrated capable of joining container materials under water. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Simulated Service and Stress Corrosion Cracking Testing for Friction Stir Welded Spun Formed Domes

Simulated service testing (SST) development was required to help qualify a new 2195 aluminum lithium (Al-Li) alloy spin forming dome fabrication process for the National Aeronautics and Space Administration (NASA) Exploration Development Technology Program. The application for the technology is to produce high strength low weight tank components for NASA s next generation launch vehicles. Since plate material is not currently manufactured large enough to fabricate these domes, two plates are joined by means of friction stir welding. The plates are then pre-contour machined to near final thicknesses allowing for a thicker weld land and anticipating the level of stretch induced by the spin forming process. The welded plates are then placed in a spin forming tool and hot stretched using a trace method producing incremental contours. Finally the dome receives a room temperature contour stretch to final dimensions, heat treatment, quenching, and artificial aging to emulate a T-8 condition of temper. Stress corrosion cracking (SCC) tests were also performed by alternate immersion in a sodium chloride (NaCl) solution using the typical double beam assembly and with 4-point loaded specimens and use of bent-beam stress-corrosion test specimens under alternate immersion conditions. In addition, experiments were conducted to determine the threshold stress intensity factor for SCC (K(sub ISCC)) which to our knowledge has not been determined previously for Al-Li 2195 alloy. The successful simulated service and stress corrosion testing helped to provide confidence to continue to Ares 1 scale dome fabrication

Stewart, Thomas J.↗

Friction stir welding bobbin tool

A bobbin tool is disclosed that includes a top shoulder, a bottom shoulder, and an axial pin that extends between the top and bottom shoulders. The bottom shoulder has an annular shoulder end surface, a back surface opposite the annular shoulder end surface, and a side surface that joins the annular shoulder end surface and the back surface. One or more and radially-extending blades may be disposed on the side surface of the bottom shoulder and/or one or more axially-extending blades may be disposed on the back surface. The one or more blades provide the bobbin tool with an ability to friction stir weld a variable thickness workpiece assembly, axially plunged through the workpiece assembly along an axis of rotation of the bobbin tool, and/or be extracted through the workpiece assembly along an axis of rotation of the bobbin tool.

47 OTHER INSTRUMENTATION↗

Elucidation of microstructural evolution of beta-type titanium alloy joint during friction stir welding using liquid CO2 cooling

Highlights: • Microstructural evolution during FSW was elucidated along real material flow line. • Stirring and cooling stages of FSW can be investigated separately using CO{sub 2} cooling. • In stirring stage, discontinuous dynamic recrystallization predominantly occurred. • In cooling stage, static recovery and grain growth mainly occurred. - Abstract: Normal friction stir welding (FSW) and liquid CO{sub 2} cooling FSW were conducted on the β-type Ti-15V-3Cr-3Al-3Sn (Ti-15-3, mass%) alloy plates under a processing condition. Since liquid CO{sub 2} cooling with high cooling efficiency can freeze the microstructure formed during the high-temperature stirring stage of FSW, it is possible to separately elucidate the microstructural evolution of the Ti-15-3 alloy during the high-temperature stirring stage and the post-stirring cooling stage in FSW. The deformation temperature during the normal and the CO{sub 2} cooling FSW was similar in the top and the bottom of stir zone, which is considered to be owing to that the top and bottom are located adjacent to the heat sources, i.e., the shoulder and probe surfaces. In the high-temperature stirring stage of FSW, discontinuous dynamic recrystallization predominantly occurred, and a simple shear texture generated in an early stage of the material flow around the tool, then the microstructure started to evolve steadily after a steady-state dynamic recrystallization. In the post-stirring cooling stage of FSW, static recovery and grain growth were found to mainly occur within the stir zone.

36 MATERIALS SCIENCE↗

Effect of Pin Tool Shape on Metal Flow During Friction Stir Welding

It has been shown that metal moves behind the rotating Friction Stir Pin Tool in two separate currents or streams. One current, mostly on the advancing side, enters a zone of material that rotates with the pin tool for one or more revolutions and eventually is abandoned behind the pin tool in crescent-shaped pieces. The other current, largely on the retreating side of the pin tool is moved by a wiping process to the back of the pin tool and fills in between the pieces of the rotational zone that have been shed by the rotational zone. This process was studied by using a faying surface copper trace to clarify the metal flow. Welds were made with pin tools having various thread pitches. Decreasing the thread pitch causes the large scale top-to-bottorn flow to break up into multiple vortices along the pin and an unthreaded pin tool provides insufficient vertical motion for there to be a stable rotational zone and flow of material via the rotational zone is not possible leading to porosity on the advancing side of the weld.

McClure, J. C.↗