At least 289 records · Page 16

Microstructural Characterization of the U-9.1Mo Fuel/AA6061 Cladding Interface in Friction-Bonded Monolithic Fuel Plates Irradiated in the RERTR-6 Experiment

Low-enrichment (U-235 < 20%) U-Mo monolithic fuel is being developed for use in research and test reactors. The earliest design for this fuel that was investigated via reactor testing was comprised of a nominally U-10Mo fuel foil encased in AA6061 (Al-6061) cladding. For a fuel design to be deemed adequate for final use in a reactor, it must maintain dimensional stability and retain fission products throughout irradiation, which means that there must be good integrity at the fuel foil/cladding interface. To investigate the nature of the fuel/cladding interface for this fuel type after irradiation, fuel plates that were tested in INL's Advanced Test Reactor (ATR) were subsequently characterized using optical metallography, scanning electron microscopy, and transmission electron microscopy. Results of this characterization showed that the fuel/cladding interaction layers present at the U-Mo fuel/AA6061 cladding interface after fabrication became amorphous during irradiation. Up to two main interaction layers, based on composition, could be found at the fuel/cladding interface, depending on location. After irradiation, an Al-rich layer contained very few fission gas bubbles, but did exhibit Xe enrichment near the AA6061 cladding interface. Another layer, which contained more Si, had more observable fission gas bubbles. Adjacent to the AA6061 cladding were Mg-rich precipitates, which was in close proximity to the region where Xe is observed to be enriched. In samples produced using a focused ion beam at the interaction zone/AA6061 cladding interface were possible indications of porosity/debonding, which suggested that the interface in this location is relatively weak.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Effects of Irradiation on the Microstructure of U-7Mo Dispersion Fuel with Al-2Si Matrix

The Reduced Enrichment for Research and Test Reactor program is developing low-enriched uranium U-Mo dispersion fuels for application in research and test reactors around the world. As part of this development, fuel plates have been irradiated in the Advanced Test Reactor and then characterized using optical metallography (OM) and scanning electron microscopy (SEM) to determine the as-irradiated microstructure. To demonstrate the irradiation performance of U-7Mo dispersion fuel plates with 2 wt% Si added to the matrix, fuel plates were tested to medium burnups at intermediate fission rates as part of the RERTR-6 experiment. Further testing was performed to higher fission rates as part of the RERTR-7A experiment, and very aggressive testing (high temperature, high fission density, high fission rate) was performed in the RERTR-9A, RERTR-9B and AFIP-1 experiments. As-irradiated microstructures were compared to those observed after fabrication to determine the effects of irradiation on the microstructure. Based on comparison of the microstructural characterization results for each irradiated sample, some general conclusions can be drawn about how the microstructure evolves during irradiation: there is growth of the fuel/matrix interaction layer (FMI), which was present in the samples to some degree after fabrication, during irradiation; Si diffuses from the FMI layer to deeper depths in the U-7Mo particles as the irradiation conditions are made more aggressive; lowering of the Si content in the FMI layer results in an increase in the size of the fission gas bubbles; as the FMI layer grows during irradiation more Si diffuses from the matrix to the FMI layer/matrix interface, and interlinking of fission gas bubbles in the fuel plate microstructure that may indicate breakaway swelling is not observed.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Calibration and validation of NRC fuel performance models

FRAPCON and FRAPTRAN are the steady-state and transient fuel performance codes, respectively, that are used by the U.S. Nuclear Regulatory Commission (NRC) in performing confirmatory calculations of licensee fuel performance codes and safety analysis methods during the review and approval of these codes and methods for light-water reactors. The NRC also uses these codes to perform calculations to direct regulatory research and to assist in the development of new regulations and regulatory guides. FRAPCON and FRAPTRAN are well-validated fuel performance codes that are kept in a constant state of maintenance. FRAPCON and FRAPTRAN have an extensive database of separate effects data used to validate individual material property and fuel performance models and an integral effects database used to assess the overall code prediction within the full range of fuel operations. The key code predictions that are of regulatory interest as they relate to various specified acceptable design limits are: fuel and cladding temperature, rod internal pressure, cladding hoop strain, cladding corrosion and hydriding, and fission gas release. To assess the ability of the code to accurately predict these values, the integral assessment database consists of measurements of fuel centerline temperature, fission gas release, void volume, cladding corrosion, and cladding hoop strain. This paper will discuss the activities that are performed to ensure that FRAPCON and FRAPTRAN represent the state of the industry and will describe the separate effect and integral effect databases that are used to validate the models and are continually being expanded to ensure validation over the full range of fuel operations.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Multiscale modeling for high burnup structure formation and associated pulverization

This report summarizes the lower length scale modeling work performed in the fiscal year 2023 under the Nuclear Energy Advanced Modeling and Simulation (NEAMS) program to capture the microstrutural evolution and associated pulverization criteria in the high burnup regions. This year, the resolution mechanisms within the cluster dynamics code has been updated and it influence on the bubble growth in HBS regions at the mesoscale is studied. To improve the accuracy of phase-field models of fission gas bubble growth, a new Helmholtz free energy for high-density Xe gas is derived from a virial equation of state. Two previously used strategies for representing net vacancy production in phase-field models of fission gas bubble growth are compared with each other and with analytical models of bubble growth. The vacancy source only model is found to be more convenient to parameterize realistically compared with the vacancy source+sink model. Furthermore, the phase-field-fracture simulation have been performed using MD- informed failure stress values and realistic HBS structure obtained from the phase-field simulations. We also present the uncertainty bands on prediction of the critical stress to account for the effect of the lower length scale variabilities on the failure criteria at the mesoscale. It is observed that pulverization may occur in partially restructured regions with restructuring fraction as low as 17%. In light of this, an update to the BISON’s pulverization criteria is recommended.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Uranium vacancy mobility at the sigma Σ5 symmetric tilt grain boundary in UO 2

An important consequence of the fissioning process occurring during burnup is the formation of fission products. These fission products alter the thermo-mechanical properties of the fuel. They also lead to macroscopic changes in the fuel structure, including the formation of bubbles that are connected to swelling of the fuel. Subsequent release of fission gases increase the pressure in the plenum and can cause changes in the properties of the fuel pin itself. It is thus imperative to understand how fission products, and fission gases in particular, behave within the fuel in order to predict the performance of the fuel under operating conditions. Fission gas redistribution within the fuel is governed by mass transport and the presence of sinks such as impurities, dislocations, and grain boundaries. Thus, to understand how the distribution of fission gases evolves in the fuel, we must understand the underlying transport mechanisms, tied to the concentrations and mobilities of defects within the material, and how these gases interact with microstructural features that might act as sinks. Both of these issues have been addressed in previous work under NEAMS. However, once a fission product has reached a sink, such as a grain boundary, its mobility may be different there than in the grain interior and predicting how, for example, bubbles nucleate within grain boundaries necessitates an understanding of how fission gases diffuse within boundaries. That is the goal of the present work. In this report, we describe atomic level simulations of uranium vacancy diffusion in the pressence of a Σ5 symmetric tilt boundary in urania (UO 2 ). This boundary was chosen as it is the simplest of the boundaries we considered in previous work on segregation and serves as a starting point for understanding defect mobility at boundaries. We use a combination of molecular statics calculations and kinetic Monte Carlo (kMC) to determine how the mobility of uranium vacancies is altered at this particular grain boundary. Given that the diffusion of fission gases such as Xe are tied to the mobility of uranium vacancies, these results given insight into how fission gas mobility differs at grain boundaries compared to bulk urania.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Calibration and Validation of NRC Fuel Performance Models

Pacific Northwest National Laboratory maintains steady-state and transient fuel performance codes for the U.S Nuclear Regulatory Commission (NRC). The NRC uses these codes in performing confirmatory calculations of licensee fuel performance codes and safety analysis methods during the review and approval of these codes and methods. The NRC also uses these codes to perform calculations to direct regulatory research and to assist in the development of new regulations and regulatory guides. Because of the safety-related uses for these codes, it is critically important that the codes are capable of accurately modeling modern fuel and operations and that the models and code predictions are well validated using data collected from conditions relevant to in-reactor conditions. FRAPCON and FRAPTRAN have an extensive database of separate effects data used to validate individual material property and fuel performance models and an integral effects database used to assess the overall code prediction within the full range of fuel operations. The key code predictions that are of regulatory interest as they relate to various specified acceptable design limits are; fuel and cladding temperature, rod internal pressure, cladding hoop strain, cladding corrosion and hydriding, and fission gas release. To assess the ability of the code to accurately predict these values, the integral assessment database consists of measurements of fuel centerline temperature, fission gas release, void volume, cladding corrosion, and cladding hoop strain. This paper will discuss the activities that are performed to ensure that FRAPCON and FRAPTRAN represent the state of the industry and will describe the separate effect and integral effect databases that are used to validate the models and are continually being expanded to ensure validation over the full range of fuel operations.

Geelhood, Kenneth J.↗

Multi-scale simulation of high burnup UO2 nuclear fuel during loss-of-coolant accident conditions

To improve the economics of commercial nuclear energy generation, U.S. utilities are currently seeking licensing approval to operate UO2 fuel to higher burnups. One significant safety issue that must be addressed to obtain approval is the potential for fine fragmentation/pulverization of the fuel during a loss-of-coolant accident (LOCA). It has been hypothesized that pulverization is caused by the rapid increase of pressure in fission gas bubbles in the high burnup region of the fuel during a LOCA. To better understand this phenomenon, a novel phase-field model of the fission gas bubble microstructure in UO2 has been developed and implemented in Idaho National Laboratory (INL)'s Marmot application for phase-field simulation of nuclear materials. Simulations of the bubble response to steady-state and transient conditions were conducted, and the results were used to inform a mechanistic model of pulverization in BISON, INL’s fuel performance simulation code.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Sister Rod Destructive Examinations (FY2021) Appendix C: Rod Internal Pressure, Void Volume, and Gas Transmission Tests

As a part of the DOE NE High Burnup Spent Fuel Data Project, Oak Ridge National Laboratory (ORNL) is performing destructive examinations (DEs) of high burnup (HBU) (>45 GWD/MTU) spent nuclear fuel (SNF) rods from the North Anna Nuclear Power Station operated by Dominion Energy. The SNF rods, called the sister rods or sibling rods, are all HBU and include four different kinds of fuel rod cladding: standard Zircaloy-4 (Zirc-4), low-tin (LT) Zirc-4, ZIRLO, and M5. This Appendix C documents the status of the ORNL Phase 1 DE activities [C-2, C-3] related to rod internal pressure and void volume measurement techniques, fission gas stack flow measurements applied to selected sister rods, and fission gas release calculations in Phase 1 of the sister rod test program.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Mechanical modeling of porous oxide fuel pellet A Test Problem

A poro-elasto-plastic material model has been developed to capture the response of oxide fuels inside the nuclear reactors under operating conditions. Behavior of the oxide fuel and variation in void volume fraction under mechanical loading as predicted by the developed model has been reported in this article. The significant effect of void volume fraction on the overall stress distribution of the fuel pellet has also been described. An important oxide fuel issue that can have significant impact on the fuel performance is the mechanical response of oxide fuel pellet and clad system. Specifically, modeling the thermo-mechanical response of the fuel pellet in terms of its thermal expansion, mechanical deformation, swelling due to void formation and evolution, and the eventual contact of the fuel with the clad is of significant interest in understanding the fuel-clad mechanical interaction (FCMI). These phenomena are nonlinear and coupled since reduction in the fuel-clad gap affects thermal conductivity of the gap, which in turn affects temperature distribution within the fuel and the material properties of the fuel. Consequently, in order to accurately capture fuel-clad gap closure, we need to account for fuel swelling due to generation, retention, and evolution of fission gas in addition to the usual thermal expansion and mechanical deformation. Both fuel chemistry and microstructure also have a significant effect on the nucleation and growth of fission gas bubbles. Fuel-clad gap closure leading to eventual contact of the fuel with the clad introduces significant stresses in the clad, which makes thermo-mechanical response of the clad even more relevant. The overall aim of this test problem is to incorporate the above features in order to accurately capture fuel-clad mechanical interaction. Because of the complex nature of the problem, a series of test problems with increasing multi-physics coupling features, modeling accuracy, and complexity are defined with the objective of accurate simulation of fuel-clad mechanical interaction subjected to a wide-range of thermomechanical stimuli.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Thick Films acoustic sensors devoted to MTR environment measurements. Thick Films acoustic sensors devoted to Material Testing Reactor environment measurements

The development of advanced instrumentation for in-pile experiments in Material Testing Reactor constitutes a main goal for the improvement of the nuclear fuel behavior knowledge. An acoustic method for fission gas release detection was tested with success during a first experiment called REMORA 3 in 2010 and 2011, and the results were used to differentiate helium and fission gas release kinetics under transient operating conditions. This experiment was lead at OSIRIS reactor (CEA Saclay, France). The maximal temperature on the sensor during the irradiation was about 150 deg. C. In this paper we present a thick film transducer produce by screen printing process. The screen printing of piezoelectric offers a wide range of possible applications for the development of acoustic sensors and piezoelectric structure for measurements in high temperature environment. We firstly produced a Lead Zirconate Titanate (PZT) based paste composed of Pz27 powder from Ferroperm, CF7575 glass, and organic solvent ESL 400. Likewise a Bismuth Titanate based paste synthesized in our laboratory was produced. With these inks we produced thick film up to 130 μm by screen printing process. Material properties characterizations of these thick-film resonators are essential for device design and applications. The piezoelectric coefficients d33 and pyro-electric P(T) coefficient are investigated. The highest P(T) and d33 are respectively 80 μC.m{sup -2}.K{sup -1} and 130 μC.N{sup -1} for the PZT transducer -which validates the fabrication process-. In view of the development of this transducer oriented for high temperature and irradiation environment, we investigated the electrical properties of the transducers for different ranges of frequencies and temperature - from 20 Hz up to 40 MHz between 30 and 400 deg. C. We highlight the evolution of the impedance response and piezoelectric parameters of screen printed piezoelectric structures on alumina. Shortly an irradiation will be realized in order to investigate their reliability towards neutron fluence. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Rate Theory Modeling and Simulations of Silicide Fuel at LWR Conditions

Uranium silicide (U 3 Si 2 ) fuel has higher thermal conductivity and higher uranium density, making it a promising candidate for the accident-tolerant fuel (ATF) used in light water reactors (LWRs). However, previous studies on the fuel performance of U 3 Si 2 , including both experimental and computational approaches, have been focusing on the irradiation conditions in research reactors, which usually involve low operation temperatures and high fuel burnups. Thus, it is important to examine the fuel performance of U 3 Si 2 at typical LWR conditions so as to evaluate the feasibility of replacing conventional uranium dioxide fuel with this silicide fuel material. As in-reactor irradiation experiments involve significant time and financial cost, it is appropriate to utilize modeling tools to estimate the behavior of U 3 Si 2 in LWRs based on all those available research reactor experimental references and state-of-the-art density functional theory (DFT) calculation capabilities at the early development stage. Hence, in this report, a comprehensive investigation of the fission gas swelling behavior of U 3 Si 2 at LWR conditions is introduced. The modeling efforts mentioned in this report was based on the rate theory (RT) model of fission gas bubble evolution that has been successfully applied for a variety of fuel materials at devious reactor conditions. Both existing experimental data and DFT-calculated results were used for the optimization of the parameters adopted by the RT model. Meanwhile, the fuel-cladding interaction was captured by the coupling of the RT model with simplified mechanical correlations. Therefore, the swelling behavior of U 3 Si 2 fuel and its consequent interaction with cladding in LWRs was predicted by the rate theory modeling, providing valuable information for the development of U 3 Si 2 fuel as an accident-tolerant alternative for uranium dioxide.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Radiation-induced grain subdivision and bubble formation in U 3 Si 2 at LWR temperature

Here, U 3 Si 2 , an advanced fuel form proposed for light water reactors (LWR), has excellent thermal conductivity and a higher fissile element density. However, limited understanding of the radiation performance and fission gas behavior of U 3 Si 2 is available at LWR conditions. This study explores the irradiation behavior of U 3 Si 2 by 300 KeV Xe + ion beam bombardment combining with in-situ transmission electron microscopy (TEM) observation. The crystal structure of U 3 Si 2 is stable against radiation-induced amorphization at 350 °C even up to a very high dose of 64 displacements per atom (dpa). Grain subdivision of U 3 Si 2 occurs at a relatively low dose of 0.8 dpa and continues to above 48 dpa, leading to the formation of high-density nanoparticles. Nano-sized Xe gas bubbles prevail at a dose of 24 dpa, and Xe bubble coalescence was identified with an increase of irradiation dose. The volumetric swelling resulting from Xe gas bubble formation and coalescence was estimated with respect to radiation dose, and a 2.2% volumetric swelling was observed for U 3 Si 2 irradiated at 64 dpa considering fission gas only. Due to extremely high susceptibility to oxidation, the nano-sized U 3 Si 2 grains upon radiationinduced grain subdivision were oxidized to nanocrystalline UO 2 in a high vacuum chamber for TEM observation, eventually leading to the formation of UO 2 nanocrystallites up to 80 dpa.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Design Report on the MiniFuel Instrumented Test Apparatus for Understanding Radiation Effects

Most nuclear fuels irradiations at Oak Ridge National Laboratory (ORNL) over the past decade have been conducted using MiniFuel—a static capsule design employing subscale fuel specimens to collect separate-effects irradiated fuel performance data. Irradiation conditions for MiniFuel experiments are predicted pre-test using reactor physics, and thermal models are verified post-irradiation via SiC dilatometry and various spectrometry methods. Relevant fuel performance parameters are also observed post-irradiation in a hot cell, thereby providing a single data point for each parameter representing the cumulative effects of the irradiation conditions. Substantially more data can be harvested from a single test and within a shorter duration by instrumenting irradiation vehicles and measuring desired quantities in situ. This report presents the design and analysis of the MiniFuel INstrumented Irradiation Test Apparatus for Understanding Radiation Effects (MINITAURE)—an instrumented test rig based on the separate-effects MiniFuel concept that aims to capture fission gas release (FGR) and thermal conductivity degradation of fuel specimens during irradiation in the High Flux Isotope Reactor (HFIR). MINITAURE will be integrated with the Materials Irradiation Facility (MIF) located in the HFIR building outside the reactor containment. The MIF will act as the instrumentation and control center for the experiment, enabling real-time feedback from in situ sensors and control of irradiation temperatures via a gas delivery system. Two unique capsule designs were developed to capture each phenomenon: the thermal conductivity capsule, which uses a thermopile method to estimate fuel specimen thermal conductivity, and the fission gas release capsule, which will have continuous flowing gas communication to high-purity germanium detectors that are housed in the MIF for monitoring FGR. This report details the reactor physics and heat transfer modeling activities that were used to inform the experiment design and predict capsule performance. It also describes out-of-pile activities conducted to stand up this new capability and verify the measurement techniques. Modeling efforts to date have demonstrated the feasibility of the in situ measurement techniques and supported the development of the MINITAURE assembly configuration. Out-of-pile testing of the thermal conductivity measurement shows promise in capturing relative changes in thermal conductivity. However, significant errors exist in the measured absolute value, posing a need for further refinement.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Formation of superlattice structure in irradiated materials: a phase field study

The formation and self-organization of fission gas bubbles under irradiation is a unique phenomenon, which affects the swelling behavior and mechanical stability of nuclear materials. We develop a phase field model to investigate the formation mechanism of fission gas bubbles, and associated material properties under different irradiation condition. The thermodynamic and kinetic origin of superlattice formation is systematically analyzed. In particular, the symmetry of the superlattice is dictated by the anisotropic diffusion of interstitial atoms, while the lattice parameter is determined by the instability of vacancy and gas concentration waves. The spatial distribution of gas bubbles strongly depends on the nucleation, growth and coarsening process, which leads to the formation of self-organized superlattice. This study provides a new insight into designing target experiments to tailor desired microstructure under irradiation.

36 MATERIALS SCIENCE↗

Sister Rod Destructive Examinations (FY23) Appendix C: Rod Internal Pressure, Void Volume, and Gas Transmission Tests

As a part of the DOE NE High Burnup Spent Fuel Data Project, Oak Ridge National Laboratory (ORNL) is performing destructive examinations (DEs) of high burnup (HBU) (>45 GWD/MTU) spent nuclear fuel (SNF) rods from the North Anna Nuclear Power Station operated by Dominion Energy. The SNF rods, called the sister rods or sibling rods, are all HBU and include four different kinds of fuel rod cladding: standard Zircaloy-4 (Zirc-4), low-tin (LT) Zirc-4, ZIRLO, and M5. The DEs are being conducted to obtain a baseline of the HBU rod’s condition before dry storage and are focused on understanding overall SNF rod strength and durability. Both fuel rods and empty cladding will be tested to derive material properties. Although the data generated can be used for multiple purposes, one primary goal for obtaining the postirradiation examination data and the associated measured mechanical properties is to support SNF dry storage licensing and relicensing activities by (1) addressing identified knowledge gaps and (2) enhancing the technical basis for post-storage transportation, handling, and consolidation activities. This appendix documents the status of the ORNL Phase 1 DE activities related to rod internal pressure and void volume measurement techniques, fission gas stack flow measurements applied to selected sister rods, and fission gas release calculations in Phase 1 of the sister rod test program.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Sister Rod Destructive Examinations (FY22) Appendix C: Rod Internal Pressure, Void Volume, and Gas Transmission Tests

As a part of the DOE NE High Burnup Spent Fuel Data Project, Oak Ridge National Laboratory (ORNL) is performing destructive examinations (DEs) of high burnup (HBU) (>45 GWD/MTU) spent nuclear fuel (SNF) rods from the North Anna Nuclear Power Station operated by Dominion Energy [C-1]. The SNF rods, called the sister rods or sibling rods, are all HBU and include four different kinds of fuel rod cladding: standard Zircaloy-4 (Zirc-4), low-tin (LT) Zirc-4, ZIRLO, and M5. The DEs are being conducted to obtain a baseline of the HBU rod’s condition before dry storage and are focused on understanding overall SNF rod strength and durability. Both fuel rods and empty cladding will be tested to derive material properties. Although the data generated can be used for multiple purposes, one primary goal for obtaining the postirradiation examination data and the associated measured mechanical properties is to support SNF dry storage licensing and relicensing activities by (1) addressing identified knowledge gaps and (2) enhancing the technical basis for post-storage transportation, handling, and consolidation activities. This appendix documents the status of the ORNL Phase 1 DE activities [C-2, C-3] related to rod internal pressure and void volume measurement techniques, fission gas stack flow measurements applied to selected sister rods, and fission gas release calculations in Phase 1 of the sister rod test program.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

An evaluation of the nuclear fuel performance code BISON

BISON is a modern finite-element based nuclear fuel performance code that has been under development at the Idaho National Laboratory (USA) since 2009. The code is applicable to both steady and transient fuel behavior and is used to analyze either 2D axisymmetric or 3D geometries. BISON has been applied to a variety of fuel forms including LWR fuel rods, TRISO-coated fuel particles, and metallic fuel in both rod and plate geometries. Code validation is currently in progress, principally by comparison to instrumented LWR fuel rods and other well known fuel performance codes. Results from several assessment cases are reported, with emphasis on fuel centerline temperatures at various stages of fuel life, fission gas release, and clad deformation during pellet clad mechanical interaction (PCMI). BISON comparisons to fuel centerline temperature measurements are very good at beginning of life and reasonable at high burnup. Although limited to date, fission gas release comparisons are very good. Comparisons of rod diameter following significant power ramping are also good and demonstrate BISON's unique ability to model discrete pellet behavior and accurately predict clad ridging from PCMI. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Examination of T-111 clad uranium nitride fuel pins irradiated up to 13,000 hours at a clad temperature of 990 C

The examination of 27 fuel pins irradiated for up to 13,000 hours at 990 C is described. The fuel pin clad was a tantalum alloy with uranium nitride as the nuclear fuel. Two nominal fuel pin diameters were tested with a maximum burnup of 2.34 atom percent. Twenty-two fuel pins were tested for fission gas leaks; thirteen pins leaked. Clad ductility tests indicated clad embrittlement. The embrittlement is attributed to hydrogen from an n,p reaction in the fuel. Fuel swelling was burnup dependent, and the amount of fission gas release was low, generally less than 0.5 percent. No incompatibilities between fuel, liner, and clad were in evidence.

Slaby, J. G.↗