Room-temperature fabrication of garnet-type solid-electrolyte: Optimizing particle size for high ionic conductivity

Dense and uniform Li 6.25 Al 0.25 La 3 Zr 2 O 12 (Al-doped LLZO) solid-electrolyte film of ~24 µm thickness is successfully fabricated by room temperature aerosol deposition (AD) method. The process optimization study revealed that careful control of particle size and morphology is one of critical determinants in the development of a compact AD membrane. Notably, our method facilitated an impressive ionic conductivity of approximately 10 –5 S cm –1 , bypassing the necessity for post-annealing processes, a milestone in itself. However, it is hypothesized that the attained conductivity is somewhat restrained by factors such as smaller grain size and potential surface degradation due to moisture exposure during fabrication, indicating avenues for further research. Looking forward, detailed investigations into the film's microstructure and its impact on transport properties will be a focal point, alongside potential enhancements through post-annealing and particle coating strategies. Finally, this research hints at a promising trajectory for the development of high-efficiency solid-state battery technology.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of H + Exchange and Surface Impurities on Bulk and Interfacial Electrochemistry of Garnet Solid Electrolytes

Contact loss and current constriction pose significant challenges at the Li metal interface of solid-state batteries. For garnet-structured Li 7 La 3 Zr 2 O 12 (LLZO), these effects are amplified by Li + /H + exchange and surface contamination reactions, which lead to conductivity losses and poor Li wetting. In this study, we utilize a variety of surface treatment processes across 37 cells to selectively induce proton exchange and contamination reactions in LLZO. The resulting bulk and surface chemistry is systematically characterized and correlated to changes in electrochemical properties. Additionally, we combine impedance analysis and finite element method modeling to deconvolute sources of impedance contributions at the Li metal interface. Specifically, we show that constriction impedance at the Li metal interface arises not solely from voids, but also from ionically-resistive surface contaminants. Further, these findings emphasize the connection between ionic conductivity and constriction, demonstrating that micron-scale ionically-resistive components increase constriction even with identical contact geometries. Finally, we leverage our comprehensive dataset to highlight unstable overpotential growth as a failure mechanism, additionally showing that the phase of a cell’s impedance is a sensitive indicator for the onset of interfacial instability. Overall, this study clarifies the impacts of proton exchange and surface contamination on electrochemical properties at the Li|solid electrolyte interface and elucidates insights that are generalizable to other solid-state battery systems.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Strategic Melamine Coating on Lithium Metal for Li 3 N-Rich Solid Electrolyte Interphase and Improved Battery Cycling Stability

The practical applications of lithium (Li) metal batteries (LMBs) are limited by challenges such as dendrite formation and unstable solid electrolyte interphase (SEI), especially at higher C-rates. Here, this study introduces melamine-coated Li metal anodes (LMAs), forming a Li 3 N-rich SEI layer that improves ionic conductivity and mechanical stability. The optimized melamine-coated LMA demonstrated uniform coverage resulting in denser Li deposition, nearly doubled cycle life (~148 cycles at 0.5 C, 1C = 4.1 mA cm -2 ), compared to Bare-Li. These findings emphasize that coating materials-induced beneficial SEI components could lead to improvement of LMB performance.

Batteries↗

Standalone sulfide based lithium ion-conducting glass solid electrolyte and associated structures, cells and methods

A standalone lithium ion-conductive solid electrolyte including a freestanding inorganic vitreous sheet of sulfide-based lithium ion conducting glass is capable of high performance in a lithium metal battery by providing a high degree of lithium ion conductivity while being highly resistant to the initiation and/or propagation of lithium dendrites. Such an electrolyte is also itself manufacturable, and readily adaptable for battery cell and cell component manufacture, in a cost-effective, scalable manner.

Visco, Steven J.↗

Standalone sulfide based lithium ion-conducting glass solid electrolyte and associated structures, cells and methods

A standalone lithium ion-conductive solid electrolyte including a freestanding inorganic vitreous sheet of sulfide-based lithium ion conducting glass is capable of high performance in a lithium metal battery by providing a high degree of lithium ion conductivity while being highly resistant to the initiation and/or propagation of lithium dendrites. Such an electrolyte is also itself manufacturable, and readily adaptable for battery cell and cell component manufacture, in a cost-effective, scalable manner.

Visco, Steven J.↗

Tuning Solid Electrolyte Interphase Formation before Plating Onset in Anode-Free Sodium Batteries

Sodium (Na) batteries are of growing interest due to the higher earth abundance of sodium than lithium, as well as their promising theoretical energy density when metallic Na anodes are used. However, Na plating and stripping are heavily influenced by the physicochemical properties of the solid electrolyte interphase (SEI), which is directly influenced by the solvent and salt used for the electrolyte. While most studies focus on the SEI that forms on the surface of Na metal after plating, we expand this analysis by identifying a nanoscale “pre-plating” SEI that forms on the current collector (CC) prior to the onset of Na plating. Here, we systematically investigate an array of Na salt and glyme solvents in the electrolyte and determine the associated impacts on pre-plating SEI formation on aluminum CCs. By combining analytical electrochemistry approaches with a multimodal suite of spectroscopy techniques (X-ray, infrared, and Raman), supported by density functional theory calculations, we reveal a direct correlation between the Na + coordination environment and pre-plating SEI composition. We find that longer-chain glymes produce larger proportions of organic alkoxide products in the interphase, consistent with increased Na + −glyme interactions, while the fraction of salt-derived inorganic products (e.g., NaF) correlates with Na + −anion coordination. These insights highlight the critical influence of electrolyte composition particularly solvent identity and Na + coordination on the initial SEI formation in anode-free Na batteries.

anode-free batteries↗

On the dynamics of the fluoroethylene carbonate generated solid electrolyte interphase on silicon anodes during calendar life aging

Here, the widespread use of silicon (Si)-rich anodes in lithium-ion batteries (LIBs) is impeded by an unstable solid electrolyte interphase (SEI) incurring insufficient cell life. Fluoroethylene carbonate (FEC) additive in the electrolyte significantly improves cycle life. However, the gains on calendar life remain unclear; the SEI structure still undergoes detrimental alterations at rest. Thus, elucidating the SEI dynamics during calendar aging is critical to mitigating time-dependent capacity degradation. ATR-FTIR, XPS, and ToF-SIMS are used herein to investigate the SEI structure before and after calendar aging. Si cycled without FEC exhibits no notable SEI chemistry changes Pre- and Post-aging, leaving poor passivation as the main failure pathway. Conversely, the FEC-SEI starts as short oligomeric species from FEC/EC electroreduction prior to aging; after calendar aging, polymerized carbonates become consistently more prominent. Unexpectedly, the deposition of self-polymerized FEC species results from time exposure to the delithiated Si specifically as opposed to the lithiated surface. This unexpected finding is supported by another recent Si calendar-aging research, which albeit not investigating FEC, finds global failure of the SEI upon delithiation resulting in ∼247 fold more reactive surface compared to the lithiated.

Batteries↗

Impacts of vacancy-induced polarization and distortion on diffusion in Solid Electrolyte Li 3 OCl

We report that Lithium-rich oxychloride antiperovskites are promising solid electrolytes for enabling next-generation batteries. Here, we report a comprehensive study varying Li + concentrations in Li 3 OCl using ab initio molecular dynamics simulations. The simulations accurately capture the complex interactions between Li + vacancies (V$^'_{Li}$), the dominant mobile species in Li 3 OCl. The V$^'_{Li}$ polarize and distort the host lattice, inducing additional non-vacancy-mediated diffusion mechanisms and correlated diffusion events that reduce the activation energy barrier at concentrations as low as 1.5% V$^'_{Li}$. Our analyses of discretized diffusion events in both space and time illustrate the critical interplay between correlated dynamics, polarization and local distortion in promoting ionic conductivity in Li 3 OCl.

25 ENERGY STORAGE↗

The Study of the Binder Poly(acrylic acid) and Its Role in Concomitant Solid–Electrolyte Interphase Formation on Si Anodes

In this work we use neutron reflectometry to study how the polymeric binder, poly(acrylic acid) (PAA), affects the in situ formation and chemical composition of the solid–electrolyte interphase (SEI) formation on a silicon anode at various states of charge. The reflectivity is correlated with electrochemical quartz crystal microbalance to better understand the viscoelastic effects of the polymer during cycling. The use of model thin films allows for a well-controlled interface between the amorphous Si surface and the PAA layer. If the PAA perfectly coats the Si surface and standard processing conditions are used, the binder will prevent the lithiation of the anode. The PAA suppresses the growth of a new layer formed at early states of discharge (open circuit voltage to 0.8 V vs Li/Li+), protecting the surface of the anode. At 0.15 V, the SEI layer underneath the PAA changes in chemical composition as indicated by an increase in the scattering length density and thickness as the layer incorporates components from the electrolyte, most likely the salt. At lithiated and delithiated states, the SEI layer changes in chemical composition and grows in thickness with delithiation and shrinks during lithiation.

36 MATERIALS SCIENCE↗

Solvation Rule for Solid-Electrolyte Interphase Enabler in Lithium-Metal Batteries

Despite the exceptionally high energy density of lithium metal anodes, the practical application of lithium-metal batteries (LMBs) is still impeded by the instability of the interphase between the lithium metal and the electrolyte. To formulate a functional electrolyte system that can stabilize the lithium-metal anode, the solvation behavior of the solvent molecules must be understood because the electrochemical properties of a solvent can be heavily influenced by its solvation status. Here, we unambiguously demonstrated the solvation rule for the solid-electrolyte interphase (SEI) enabler in an electrolyte system. In this study, fluoroethylene carbonate was used as the SEI enabler due to its ability to form a robust SEI on the lithium metal surface, allowing relatively stable LMB cycling. The results revealed that the solvation number of fluoroethylene carbonate must be ≥ 1 to ensure the formation of a stable SEI in which the sacrificial reduction of the SEI enabler subsequently leads to the stable cycling of LMBs.

25 ENERGY STORAGE↗

Three-Man Solid Electrolyte Carbon Dioxide Electrolysis Breadboard

The development of the Three-Man (2.2 lb CO2/man-day) Solid Electrolyte CO2 Electrolysis Breadboard consisted of a Phase 1 and 2 effort. The Phase 1 effort constituted fabrication of three electrolysis cell types and performing parametric testing, off-design testing, and cell life testing. The Phase 2 consisted of the preliminary design, incorporation of palladium (Pd) tubes for hydrogen separation from the electrolyzer cathode feed gases, design support testing, final design, fabrication, and performance testing of the breadboard system. The results of performance tests demonstrated that CO2 electrolysis in an oxygen reclamation system for long duration space-based habitats is feasible. Closure of the oxygen system loop, therefore, can be achieved by CO2 electrolysis. In a two step process the metabolic CO2 and H2O vapor are electrolyzed into O2, H2, and CO. The CO can subsequently be disproportionated into carbon and CO2 in a carbon deposition reactor and the CO2 in turn be recycled and electrolyzed for total O2 recovery. The development effort demonstrated electrolyzer system can be designed and built to operate safely and reliably and the incorporation of Pd tubes for hydrogen diffusion can be integrated safely with predictable performance.

Isenberg, Arnold O.↗

Multi-modal characterization methods of solid-electrolyte interphase in silicon-graphite composite electrodes

Composite silicon-graphite (Si-Gr) anodes can improve battery energy density, due to Si's high gravimetric capacity, while mitigating mechanical degradation of the anode and solid-electrolyte interphase (SEI) caused by Si volumetric expansion. Optimizing these anodes is challenging, in part due to difficulty characterizing the SEI structure and composition. In this work, we present multi-modal characterization of the SEI on composite Si-Gr anodes to relate SEI chemical composition and structure to functional properties. Discrepancies in elemental concentrations from X-ray photoelectron spectroscopy, Auger electron spectroscopy, and energy-dispersive X-ray spectroscopy (EDS) are attributed to varying information depth and lateral resolution of the individual probes. However, by combining quantitative composition information with spatially resolved element mapping from scanning transmission electron microscopy, EDS, and electron energy loss spectroscopy, a holistic picture of the SEI emerges. We observe the bilayer SEI structure and a direct correlation between elemental Li and F, suggesting that most Li in the SEI exists as lithium fluoride (LiF). Further, LiF concentration is directly proportional to the maximum SEI resistivity, as determined by scanning spreading resistance microscopy. Lastly, there is an inverse relationship between lithium carbonate and LiF concentration in the SEI, providing insight into the detailed chemistry of SEI formation and evolution.

25 ENERGY STORAGE↗

Understanding Solid Electrolyte Interphase Nucleation and Growth on Lithium Metal Surfaces

Experiments and theory are needed to decode the exact structure and distribution of components of a passivation layer formed at the anode surface of Li metal batteries, known as the Solid Electrolyte Interphase (SEI). Due to the inherent dynamic behavior as well as the lithium reactivity, the SEI structure and its growth mechanisms are still unclear. This study uses molecular simulation and computational chemistry tools to investigate the initial nucleation and growth dynamics of LiOH and Li2O that provide us with thermodynamics and structural information about the nucleating clusters of each species. Following the most favorable pathways for the addition of each of the components to a given nascent SEI cluster reveals their preferential nucleation mechanisms and illustrates different degrees of crystallinity and electron density distribution that are useful to understand ionic transport through SEI blocks.

25 ENERGY STORAGE↗