Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “cyclic”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 271 records · Page 15

Cyclic Oxidation of FeCrAlY/Al2O3 Composites

Three-ply FeCrAlY/Al2O3 composites and FeCrAlY matrix-only samples were cyclically oxidized at 1000 C and 1100 C for up to 1000 1-hr cycles. Fiber ends were exposed at the ends of the composite samples. Following cyclic oxidation, cracks running parallel to and perpendicular to the fibers were observed on the large surface of the composite. In addition, there was evidence of increased scale damage and spallation around the exposed fiber ends, particularly around the middle ply fibers. This damage was more pronounced at the higher temperature. The exposed fiber ends showed cracking between fibers in the outer plies, occasionally with Fe and Cr-rich oxides growing out of the cracks. Large gaps developed at the fiber/matrix interface around many of the fibers, especially those in the outer plies. Oxygen penetrated many of these gaps resulting in significant oxide formation at the fiber/matrix interface far within the composite sample. Around several fibers, the matrix was also internally oxidized showing Al2O3 precipitates in a radial band around the fibers. The results show that these composites have poor cyclic oxidation resistance due to the CTE mismatch and inadequate fiber/matrix bond strength at temperatures of 1000 C and above.

Nesbitt, James A.↗

Modeling Step-Strain Relaxation and Cyclic Deformations of Elastomers

Data for step-strain relaxation and cyclic compressive deformations of highly viscous short elastomer cylinders are modeled using a large strain rubber viscoelastic constitutive theory with a rate-independent friction stress term added. In the tests, both small and large amplitude cyclic compressive strains, in the range of 1% to 10%, were superimposed on steady state compressed strains, in the range of 5% to 20%, for frequencies of 1 and 10 Hz. The elastomer cylinders were conditioned prior to each test to soften them. The constants in the viscoclastic-friction constitutive theory are determined by employing a nonlinear least-squares method to fit the analytical stresses for a Maxwell model, which includes friction, to measured relaxation stresses obtained from a 20% step-strain compression test. The simulation of the relaxation data with the nonlinear model is successful at compressive strains of 5%, 10%, 15%, and 20%. Simulations of hysteresis stresses for enforced cyclic compressive strains of 20% +/- 5% are made with the model calibrated by the relaxation data. The predicted hysteresis stresses are lower than the measured stresses.

Johnson, A.R.↗

Long-Term Cyclic Oxidation Behavior of Uncoated and Coated Re-108 and In-939 at 980 and 870 C

Very long-term cyclic oxidation behavior of Re108 and In939 with and without a protective coating was evaluated at 980 and 870 C, respectively. Re-108 and In-939 without a protective coating began to show a rapid weight loss at 3000 h due to scale spallation, indicating the need for an oxidation protective coating for longer than thousands of hours of oxidative life. NiAl-base coatings of a vapor phase aluminide (VPA), a pack aluminide (CODEP), and a slurry paint aluminide (SERMALOY J) were applied on Re-108 and In-939. The VPA and CODEP on Re-108 and all three coatings on In-939 showed excellent cyclic oxidation resistance out to 10,000 h. Coated alloys were annealed in an inert atmosphere to determine the loss of Al from the coating into the alloy substrate through diffusion. The Al loss from the coating through diffusion was twice as great as the Al loss through oxidation after 10,000 h of cyclic exposure. The oxidation life of VPA-coated Re-108 was estimated by calculating the amount of Al initially available for protective oxidation and the amount of Al lost through oxidation and diffusion.

Lee, K. N.↗

COSP for Windows: Strategies for Rapid Analyses of Cyclic Oxidation Behavior

COSP is a publicly available computer program that models the cyclic oxidation weight gain and spallation process. Inputs to the model include the selection of an oxidation growth law and a spalling geometry, plus oxide phase, growth rate, spall constant, and cycle duration parameters. Output includes weight change, the amounts of retained and spalled oxide, the total oxygen and metal consumed, and the terminal rates of weight loss and metal consumption. The present version is Windows based and can accordingly be operated conveniently while other applications remain open for importing experimental weight change data, storing model output data, or plotting model curves. Point-and-click operating features include multiple drop-down menus for input parameters, data importing, and quick, on-screen plots showing one selection of the six output parameters for up to 10 models. A run summary text lists various characteristic parameters that are helpful in describing cyclic behavior, such as the maximum weight change, the number of cycles to reach the maximum weight gain or zero weight change, the ratio of these, and the final rate of weight loss. The program includes save and print options as well as a help file. Families of model curves readily show the sensitivity to various input parameters. The cyclic behaviors of nickel aluminide (NiAl) and a complex superalloy are shown to be properly fitted by model curves. However, caution is always advised regarding the uniqueness claimed for any specific set of input parameters,

Smialek, James L.↗

Cyclic Failure Mechanisms of Thermal and Environmental Barrier Coating Systems Under Thermal Gradient Test Conditions

Plasma-sprayed ZrO2-8wt%Y2O3 and mullite+BSAS/Si multilayer thermal and environmental barrier coating (TBC-EBC) systems on SiC/SiC ceramic matrix composite (CMC) substrates were thermally cyclic tested under high thermal gradients using a laser high-heat-flux rig in conjunction with furnace exposure in water-vapor environments. Coating sintering and interface damage were assessed by monitoring the real-time thermal conductivity changes during the laser heat-flux tests and by examining the microstructural changes after exposure. Sintering kinetics of the coating systems were also independently characterized using a dilatometer. It was found that the coating failure involved both the time-temperature dependent sintering and the cycle frequency dependent cyclic fatigue processes. The water vapor environments not only facilitated the initial coating conductivity increases due to enhanced sintering and interface reaction, but also promoted later conductivity reductions due to the accelerated coating cracking and delamination. The failure mechanisms of the coating systems are also discussed based on the cyclic test results and are correlated to the sintering and thermal stress behavior under the thermal gradient test conditions.

Zhu, Dongming↗

Thermal Gradient Cyclic Behavior of a Thermal/Environmental Barrier Coating System on SiC/SiC Ceramic Matrix Composites

Thermal barrier and environmental barrier coatings (TBCs and EBCs) will play a crucial role in future advanced gas turbine engines because of their ability to significantly extend the temperature capability of the ceramic matrix composite (CMC) engine components in harsh combustion environments. In order to develop high performance, robust coating systems for effective thermal and environmental protection of the engine components, appropriate test approaches for evaluating the critical coating properties must be established. In this paper, a laser high-heat-flux, thermal gradient approach for testing the coatings will be described. Thermal cyclic behavior of plasma-sprayed coating systems, consisting of ZrO2-8wt%Y2O3 thermal barrier and NASA Enabling Propulsion Materials (EPM) Program developed mullite+BSAS/Si type environmental barrier coatings on SiC/SiC ceramic matrix composites, was investigated under thermal gradients using the laser heat-flux rig in conjunction with the furnace thermal cyclic tests in water-vapor environments. The coating sintering and interface damage were assessed by monitoring the real-time thermal conductivity changes during the laser heat-flux tests and by examining the microstructural changes after the tests. The coating failure mechanisms are discussed based on the cyclic test results and are correlated to the sintering, creep, and thermal stress behavior under simulated engine temperature and heat flux conditions.

Zhu, Dongming↗

Slow Crack Growth of Brittle Materials With Exponential Crack-Velocity Formulation: Constant Stress and Cyclic Stress Experiments - Part 3

The previously determined life prediction analysis based on an exponential crack-velocity formulation was examined using a variety of experimental data on advanced structural ceramics tested under constant stress and cyclic stress loading at ambient and elevated temperatures. The data fit to the relation between the time to failure and applied stress (or maximum applied stress in cyclic loading) was very reasonable for most of the materials studied. It was also found that life prediction for cyclic stress loading from data of constant stress loading in the exponential formulation was in good agreement with the experimental data, resulting in a similar degree of accuracy as compared with the power-law formulation. The major limitation in the exponential crack-velocity formulation, however, was that the inert strength of a material must be known a priori to evaluate the important slow-crack-growth (SCG) parameter n, a significant drawback as compared with the conventional power-law crack-velocity formulation.

Choi, Sung R.↗

A Deterministic Interfacial Cyclic Oxidation Spalling Model: Algebraic Approximation, Descriptive Parameters, and Normalized Universal Curve - Part 2

A cyclic oxidation interfacial spalling model has been developed in Part 1. The governing equations have been simplified here by substituting a new algebraic expression for the series (Good-Smialek approximation). This produced a direct relationship between cyclic oxidation weight change and model input parameters. It also allowed for the mathematical derivation of various descriptive parameters as a function of the inputs. It is shown that the maximum in weight change varies directly with the parabolic rate constant and cycle duration and inversely with the spall fraction, all to the 1/2 power. The number of cycles to reach maximum and zero weight change vary inversely with the spall fraction, and the ratio of these cycles is exactly 1:3 for most oxides. By suitably normalizing the weight change and cycle number, it is shown that all cyclic oxidation weight change model curves can be represented by one universal expression for a given oxide scale.

Smialek, James L.↗

Universal Behavior of a Cyclic Oxidation Model

A mathematical model has been generated to represent the iterative, discrete growth and spallation processes associated with cyclic oxidation. Parabolic growth kinetics (k(sub p)) over and a constant spall area (F(sub A)) were assumed, with spalling occurring interfacially at the thickest regions of the scale. Although most models require numerical techniques, the regularity and simplicity of this progression permitted an approximation by algebraic expressions. Normalization could now be performed to reflect all parametric effects, and a universal cyclic oxidation response was generated: W(sub u) = 1/2 {3J(sub u)(sup 1/2)+ J(sub u)(sup 3/2)} where W, is weight change normalized by the maximum and J(sub u) is the cycle number normalized by the number to reach maximum. Similarly, the total amount of metal consumed was represented by a single normalized curve. The factor [(S(sub c)-l)(raised dot)sqrt(F(sub A)k(sub p)DELTAt)] was identified as a general figure of merit, where S(sub c) is the mass ratio of oxide to oxygen and DELTAt is the cycle duration. A cyclic oxidation failure map was constructed, in normalized k(sub p)-F(sub A) space, as defined by the locus of points corresponding to a critical amount of metal consumption in a given time. All three constructions describe behavior for every value of growth rate, spall fraction, and cycle duration by means of single curves, but with two branches corresponding to the times before and after steady state is achieved.

Smialek, James L.↗

Calcium-independent activation of extracellular signal-regulated kinases 1 and 2 by cyclic strain

We have previously demonstrated that cyclic strain induces extracellular signal-regulated kinases 1 and 2 (ERK1/2) activation in endothelial cells (EC). The aim of this study was to investigate the effect of Ca2+ on the activation of ERK1/2. Bovine aortic EC were pretreated with a chelator of extracellular Ca2+, ethylaneglycol-bis(aminoethylether)-tetra-acetate (EGTA), a depleter of Ca2+ pools, 2,5-Di-(tert-butyl)-1,4-benzohydroquinone (BHQ), or a Ca2+ channel blocker, GdCl3, and subjected to an average 10 % strain at a rate of 60 cycles/min for 10 min. BHQ and GdCl3 did not inhibit the strain-induced ERK1/2 activation. Chelation of normal extracellular Ca2+ (1.8 mM) medium with EGTA (3 mM) acutely stimulated baseline phosphorylation and activation of ERK1/2, thereby obscuring any strain-induced activation of ERK1/2. However, in EC preincubated for 24 hours in Ca2+-free medium, elevated baseline phosphorylation was minimally activated by EGTA (200 microM) such that cyclic strain stimulated ERK1/2 in the presence or absence of BHQ. These results suggest a Ca2+ independence of the ERK1/2 signaling pathway by cyclic strain. Copyright 1998 Academic Press.

NASA Discipline Cell Biology↗

Cyclic Oxidation of High-Temperature Alloy Wires in Air

High-temperature alloy wires are proposed for use in seal applications for future re-useable space vehicles. These alloys offer the potential for improved wear resistance of the seals. The wires must withstand the high temperature environments the seals are subjected to as well as maintain their oxidation resistance during the heating and cooling cycles of vehicle re-entry. To model this, the wires were subjected to cyclic oxidation in stagnant air. of this layer formation is dependent on temperature. Slow growing oxides such as chromia and alumina are desirable. Once the oxide is formed it can prevent the metal from further reacting with its environment. Cyclic oxidation models the changes in temperature these wires will undergo in application. Cycling the temperature introduces thermal stresses which can cause the oxide layer to break off. Re-growth of the oxide layer consumes more metal and therefore reduces the properties and durability of the material. were used for cyclic oxidation testing. The baseline material, Haynes 188, has a Co base and is a chromia former while the other two alloys, Kanthal A1 and PM2000, both have a Fe base and are alumina formers. Haynes 188 and Kanthal A1 wires are 250 pm in diameter and PM2000 wires are 150 pm in diameter. The coiled wire has a total surface area of 3 to 5 sq cm. The wires were oxidized for 11 cycles at 1204 C, each cycle containing a 1 hour heating time and a minimum 20 minute cooling time. Weights were taken between cycles. After 11 cycles, one wire of each composition was removed for analysis. The other wire continued testing for 70 cycles. Post-test analysis includes X-Ray Diffraction (XRD), Scanning Electron Microscopy (SEM) and Energy Dispersive Spectroscopy (EDS) for phase identification and morphology.

Reigel, Marissa M.↗

Estrous Cyclicity in Mice During Simulated Weightlessness

Hindlimb unloading (HU) is a rodent model system used to simulate weightlessness experienced in space. However, some effects of this approach on rodent physiology are under-studied, specifically the effects on ovarian estrogen production which drives the estrous cycle. To resolve this deficiency, we conducted a ground-based validation study using the HU model, while monitoring estrous cycles in 16-weeks-old female C57BL6 mice. Animals were exposed to HU for 12 days following a 3 day HU cage acclimation period, and estrous cycling was analyzed in HU animals (n=22), normally loaded HU Cage Pair-Fed controls (CPF; n=22), and Vivarium controls fed ad libitum (VIV; n=10). Pair feeding was used to control for potential nutritional deficits on ovarian function. Vaginal cells were sampled daily in all mice via saline lavage. Cells were dried and stained with crystal violet, and the smears evaluated using established vaginal cytology techniques by two individuals blinded to the animal treatment group. Estrous cyclicity was disrupted in nearly all HU and CPF mice, while those maintained in VIV had an average normal cycle length of 4.8+/- 0.5 days, with all stages in the cycle visibly observed. CPF and HU animals arrested in the diestrous phase, which precedes the pre-ovulatory estrogen surge. Additionally, infection-like symptoms characterized by vaginal discharge and swelling arose in several HU animals, which we suspect was due to an inability of these mice to properly groom themselves, and/or due to the change in the gravity vector relative to the vaginal opening, which prevented drainage of the lavage solution. Pair-feeding resulted in similar weight gains of HU and CPF (1.5% vs 3.0%, respectively). The current results indicate that pair-feeding controlled weight gain and that the HU cage alone influenced estrous cyclicity. Thus, longer acclimation needs to be tested to determine if and when normal estrous cycling resumes in non-loaded mice in HU cages prior to HU testing. Future studies might also examine whether modifications to the vaginal lavage procedure might prevent the onset of the infection-like symptoms, and allow estrous cyclicity to be measured in this model system. Research supported by NNX15AB48G to JST.

Hindlimb Unloading↗

Estrous Cyclicity of Mice During Simulated Weightlessness

Hindlimb unloading (HU) is a rodent model system used to simulate weightlessness experienced in space. However, some effects of this approach on rodent physiology are under-studied, specifically the effects on ovarian estrogen production which drives the estrous cycle. To resolve this deficiency, we conducted a ground-based validation study using the HU model, while monitoring estrous cycles in 16-weeks-old female C57BL6 mice. Animals were exposed to HU for 12 days following a 3 day HU cage acclimation period, and estrous cycling was analyzed in HU animals (n22), normally loaded HU Cage Pair-Fed controls (CPF; n22), and Vivarium controls fed ad libitum (VIV; n10). Pair feeding was used to control for potential nutritional deficits on ovarian function. Vaginal cells were sampled daily in all mice via saline lavage. Cells were dried and stained with crystal violet, and the smears evaluated using established vaginal cytology techniques by two individuals blinded to the animal treatment group. Estrous cyclicity was disrupted in nearly all HU and CPF mice, while those maintained in VIV had an average normal cycle length of 4.8 0.5 days, with all stages in the cycle visibly observed. CPF and HU animals arrested in the diestrous phase, which precedes the pre-ovulatory estrogen surge. Additionally, infection-like symptoms characterized by vaginal discharge and swelling arose in several HU animals, which we suspect was due to an inability of these mice to properly groom themselves, andor due to the change in the gravity vector relative to the vaginal opening, which prevented drainage of the lavage solution. Pair-feeding resulted in similar weight gains of HU and CPF (1.5 vs 3.0, respectively). The current results indicate that pair-feeding controlled weight gain and that the HU cage alone influenced estrous cyclicity. Thus, longer acclimation needs to be tested to determine if and when normal estrous cycling resumes in non-loaded mice in HU cages prior to HU testing. Future studies might also examine whether modifications to the vaginal lavage procedure might prevent the onset of the infection-like symptoms, and allow estrous cyclicity to be measured in this model system.

fertilit↗

High-precision Method for Cyclic Loading of Small-Animal Vertebrae to Assess Bone Quality

One potentially important bone quality characteristic is the response of bone to cyclic (repetitive) mechanical loading. In small animals, such as in rats and mice, cyclic loading experiments are particularly challenging to perform in a precise manner due to the small size of the bones and difficult-to-eliminate machine compliance. Addressing this issue, we developed a precise method for ex vivo cyclic compressive loading of isolated mouse vertebral bodies. The method has three key characteristics: 3D-printed support jigs for machining plano-parallel surfaces of the tiny vertebrae; pivotable loading platens to ensure uniform contact and loading of specimen surfaces; and specimen-specific micro-CT-based finite element analysis to measure stiffness to prescribe force levels that produce the same specified level of strain for all test specimens. To demonstrate utility, we measured fatigue life for three groups (n = 5-6 per group) of L5 vertebrae of C57BL/6J male mice, comparing our new method against two methods commonly used in the literature. We found reduced scatter of the mechanical behavior for this new method compared to the literature methods. In particular, for a controlled level of strain, the standard deviation of the measured fatigue life was up to 5-fold lower for the new method (F-ratio = 4.9; p < 0.01). The improved precision for this new method for biomechanical testing of small-animal vertebrae may help elucidate aspects of bone quality.

Bone quality↗

Application Of Shakedown Analysis To Cyclic Creep Damage Limits

Shakedown analysis may be used to provide a conservative estimate of local rupture and hence cyclic creep damage for use in a creep-fatigue assessment. The shakedown analysis is based on an elastic-perfectly plastic material with a temperature-dependent pseudo yield stress defined to guarantee that a shakedown solution exists which does not exceed rupture stress and temperature for a defined life. The ratio of design life to the estimated maximum cyclic life is the shakedown creep damage. The methodology does not require stress classification and is also applicable to cycles over the full range of temperature above and below the creep regime. Full cyclic creep and damage analysis is the alternative when shakedown analysis appears to be excessively conservative.

Carter, Peter↗

THE ROLE OF MATERIAL MODELING ON STRAIN RANGE ESTIMATION FOR ELEVATED TEMPERATURE CYCLIC LIFE EVALUATION

High temperature nuclear reactors operating in the creep regime are designed to withstand numerous cyclic events. Current ASME code rules provide two basic paths for evaluating creep fatigue and ratcheting under these conditions; one based on full inelastic analysis intended to provide a representative stress and strain history and the other based on elastic material models with adjustments of varying complexity to account for inelastic stress and strain redistribution. More recent developments have used elastic-perfectly plastic analysis to bound the effects of cyclic service. However, these methods still rely on the separate evaluation of fatigue and creep damage utilizing a damage interaction diagram. There is a procedure under current development that uses creep-fatigue data from key feature test articles directly without the use of the damage interaction diagram. However, it requires a reasonable representation of the strain range in a structure as an input. This work develops a simplified procedure based on elastic perfectly-plasticity analysis that can be used to represent the strain range in a structure in the steady state under cyclic loading conditions.

Messner, Mark C.↗

Chemical-Biological Cyclic Process for Hexavalent Chromium Reduction to Trivalent Chromium in Aqueous Medium - 20224

Conventional treatment of chromium contamination focuses on immobilization of the highly toxic and water-soluble form Cr(VI), by reducing it to the relatively less toxic and less mobile trivalent form, Cr(III), using reducing compounds like ferrous sulfate or ferrous iron, Fe(II). The Cr(VI) also respond to biodegradation and subsequent reduction. During the reduction reaction, Fe(II) is oxidized to ferric, Fe(III), which, being at the highest oxidation state, has no ability to reduce Cr(VI), and therefore remediation process terminates. The good news is that metal-reducing bacteria, S. oneidensis MR-1, can regenerate Fe(II) from Fe(III) with the help of an organic electron donor in an appropriate bacterial media. Thus, in the Cr(VI) chemical remediation process, Fe(II) to Fe(III) conversion is reversed by the biological process, regenerating Fe(II) and the Cr(VI) chemical reduction process continues in a cyclic fashion. This study presents the results of regeneration of Fe(II) from fresh Fe(III) as well as from the reaction products of Cr(VI) and Fe(II). Both fresh Fe(III) and reaction product Fe(III) exhibited the same reduction behavior. Fe(II) production increased with the increase of initial concentration of Fe(III), resulting in 87.5% Fe(II) regeneration. The extent of Fe(III) reduction (Fe(II)t/Fe(III)0.hour) was 21 times higher than the extent of Cr(VI) reduction (Cr(VI)t/Cr(VI)0.hour) by S. oneidensis MR-1. In a cyclic process of sequential Cr(VI) addition, the amount of Fe(II) regeneration decreased with the increase in cycle number, a fixed quantity of starting S. oneidensis MR-1 could regenerate Fe(II) at least five times in a ten-hour period. More importantly, regenerated Fe(II) instantly reduced Cr(VI) to Cr(III). So, Fe(II) regeneration with metal-reducing bacteria has a good potential for application in groundwater and wastewater remediation in reducing Cr(VI) to Cr(III). As a comparison of chemical to biological transformation, chemical transformation of Cr(VI) by Fe(II) was almost 600 times greater than that of biological transformation. Therefore a chemical-biological cyclic process offers potential applications for remediation of groundwater and hexavalent chromium contaminated waste sites. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Extended Barton–Bandis model for rock joints under cyclic loading: Formulation and implicit algorithm

In this paper, the Barton–Bandis model for rock joints is extended to cyclic loading conditions, without any new material parameter. Also developed herein is an implicit solution algorithm for the extended Barton–Bandis model, which can also be used for the original Barton–Bandis model for which an implicit algorithm has been unavailable. To this end, we first cast the Barton–Bandis model into an incremental elasto-plastic framework, deriving an expression for the elastic shear stiffness being consistent with the original model formulation. We then extend the model formulation to cyclic loading conditions, incorporating the dependence of shear stress and dilation on the joint position and the shearing direction. The extension is achieved by introducing a few state-dependent variables which can be calculated with the existing material parameters. For robust and accurate utilization of the model, we also develop an implicit algorithm based on return mapping, which is unconditionally stable and guarantees the satisfaction of the strength criterion. We verify that the proposed model formulation and algorithm produce virtually the same results as the original Barton–Bandis model under monotonic shearing conditions. Here, we then validate the extended Barton–Bandis model against experimental data on natural rock joints under cycling loading conditions. The present work thus enables the Barton–Bandis model, which has been exceptionally popular in research and practice, to be applicable to a wider range of problems in rock mechanics and rock engineering.

58 GEOSCIENCES↗