Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “cladding”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 271 records · Page 15

Bounding Pressure and Flammability Evaluations for a Department of Energy Standard Canister Loaded with Aluminum-Clad Spent Fuel

This report presents bounding pressurization and flammability evaluations from the radiolytic gas generation expected during extended (>50 years) dry storage of aluminum-clad spent nuclear fuel (ASNF) elements in a sealed Department of Energy (DOE) Standard Canister. The primary questions involving extended ASNF dry storage center around the adequacy of dry storage conditioning processes (i.e., drying) and the behavior of residual hydrated aluminum oxides on the cladding—specifically, the radiolytic breakdown of chemically bound water in these corrosion products. The objectives of the presented work include providing a bounding assessment of the pressure with respect to the DOE Standard Canister’s structural integrity limits and identifying the potential for forming flammable or explosive gas mixtures (i.e., exceedance of the lower flammability limit of the molecular hydrogen [H2] and oxygen [O2] concentrations). The evaluation results confirm the findings of previous, more complex M&S work. That is, the structural integrity of the canister remains unchallenged by a wide margin. Nevertheless, it is important to recognize that the presented pressure calculations consider a full breakdown of the chemisorbed water, including a consequent release of all available H2. In reality, the breakdown of water in these systems will likely remain incomplete, due to competing chemical and radiolytic reactions, thereby attaining an equilibrium in the storage environment.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Pellet Cladding Interaction In-Reactor Ramp Testing in a World without the Halden Boiling Water Reactor

One of the most crucial performance areas for fuel rods in water cooled nuclear power plants is interaction between cladding tubes and fuel pellets. Experimental programs in test reactors have provided key data to help fuel developers and plant operators understand Pellet Cladding Interaction (PCI) phenomena and optimize their strategies for reliable fuel performance. Approximately 50 years of “ramp” testing programs, where the fission heating rate is deliberately manipulated in test rods, have been performed in a handful of test reactors to reveal and understand PCI behaviors such as iodine-assisted stress corrosion cracking. Unfortunately, the test reactors most engaged in this type of work have all been retired over the years up to the recent and unexpected closure of the Halden Boiling Water Reactor which effectively caused a hiatus in PCI ramp testing programs. The need for ramp testing is crucial at this time to enable refined PCI understanding as more plants consider implementing flexible operations, increased fuel rod burnup limits, and new fuel technologies with enhanced accident tolerance. This paper reviews some of the key PCI phenomena that must be addressed with in-pile testing and surveys past test reactor’s methods for achieving the needed conditions. A strategic approach is then presented using test reactors and complimentary facilities which are still available today. Near term data opportunities are put forth along with capability development strategies that will ensure future longevity in this field of research.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Bounding Pressure and Flammability Evaluations of Aluminum-Clad Spent Nuclear Fuel Department of Energy Standard Canisters

This paper presents bounding pressure and flammability evaluations for DOE Standard Canister loaded with DOE-managed aluminum-clad spent nuclear fuel (ASNF). The objective of these evaluations is to gain confidence in the safety and feasibility of possible loading configurations for extended (>50 years) periods of dry storage, with particular focus on the dry storage canister pressures and potential for formation of a flammable atmosphere. The primary concern about the extended dry storage of ASNF is radiolytic gas generation. The aluminum cladding of these materials tends to corrode, and these corrosion products—typically aluminum oxides, such as boehmite, bayerite, or gibbsite—could carry water. This makes ASNF dry storage canisters difficult to dry. The gamma radiation field in dry storage environments could cause a radiolytic breakdown of residual water, forming chemical species such as molecular hydrogen (H2). The release of these species could increase the canister pressure and lead to the generation of a flammable canister atmosphere. The bounding evaluations presented within this study surmise conservative, but credible, conditions and processes. This includes the assumption of a full breakdown of a large quantity of free, physisorbed, and chemisorbed water (bound in a trihydrate, i.e., Al2O3 • 3H2O, layer). The considered dry storage configurations include a ~3 m (10 ft) long, ~46 cm (18 in) diameter (10 x 18) DOE Standard Canister loaded with 32 Advanced Test Reactor (ATR) ASNF elements, and a ~3 m (10 ft) long, ~61 cm (24 in) (10 x 24) diameter DOE Standard Canister loaded with 40 ATR ASNF elements. While the results of this study indicate the possibility of atmospheric hydrogen concentrations above the lower flammability limit, insufficient concentrations of oxygen will prevent the formation of flammable atmospheres. The maximum credible pressures remain well within the structural limits of the DOE Standard Canister.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Silicon Carbide Composite Cladding Qualification

This report examines the process to qualify a new fuel-cladding type focusing on the data requirements and types of irradiation testing necessary to meet the regulatory burden and related guidance applicable to fuel qualification of accident-tolerant fuel. The report considers the use of accelerated fuel qualification techniques and lead-test specimen programs that may shorten the timeline for qualifying fuel for use in a nuclear reactor at the desired burnup. The assessment framework particularly emphasizes the identification of key fuel manufacturing parameters, the specification of a fuel performance envelope to inform testing requirements, the use of evaluation models in the fuel qualification process, and the assessment of the experimental data used to develop and validate the empirical models and empirical safety criteria.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Evaluation of the effects of neutron irradiation on first-generation corrosion mitigation coatings on SiC for accident-tolerant fuel cladding

In this work, high purity SiC and SiC/SiC composites coated with commercial TiN, Cr, CrN, or CrN/Cr multilayer coatings were irradiated in Ar or flowing PWR water in the Massachusetts Institute of Technology Nuclear Reactor Laboratory (MITR). Irradiation in Ar was performed in the core. In the water environment, identical samples were placed in one of three different locations: in-core, providing exposure to neutron damage and radiolysis-affected water; above-core, where samples were exposed to radiolysis-affected water but not neutron damage, or outside of the core, where samples were exposed to the coolant water without the effects of radiation. Radiation in Ar revealed significant cracking of all but the TiN coatings, attributed to differential swelling between the coating and substrate. Lattice swelling was not observed in any of the coatings, but 0.2% void swelling was observed in the Cr coating. All of the coatings failed during water exposures in the core. Likewise, CrN/Cr spalled in each condition. Cr was protective, except under radiation damage as a result of cracking, and TiN severely degraded in the core with no coating was found following exposure. A SiC/coating ATF cladding system is anticipated to perform adequately following improvements in coating ductility and purity.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Steam oxidation of chromium corrosion barrier coatings for sic-based accident tolerant fuel cladding

SiC-based materials are currently being considered for accident tolerant fuel (ATF) cladding, however, there are concerns regarding hydrothermal corrosion rates and hermeticity. These issues may be addressed with the utilization of a Cr corrosion barrier coating (CBC) but the interaction of Cr with SiC under loss of coolant accident (LOCA) conditions needs to be investigated. In the present work, Cr coatings were deposited onto chemically vapor deposited (CVD) SiC with either high power impulse magnetron sputtering (HiPIMS), cathodic arc (CA), or a combination of both. Annealing and steam thermogravimetric analysis (TGA) was used to study reaction product formation with and without oxidation. Additionally, after 1200 °C annealing, formation of a Cr x C y carbide layer at the ambient interface and a Cr x Si y C z silicide layer at the SiC interface was observed. After 1200 °C TGA exposure, similar carbide and silicide layers were observed but with a Cr 2 O 3 outer reaction layer and a Si and O rich interfacial layer forming between the carbide and silicide layers. Initial mass gain of the coatings during the 1200 °C TGA exposure was parabolic and were similar to reported rates of chromia formation. Mass gain behavior and observed transitions in chromia microstructure indicate that metallic Cr may be consumed within the first ~1 h at 1200 °C and that subsequent chromia formation occurs at the expense of the underlying Cr carbide layer. Overall, the results show no detrimental impact of Cr coatings on the steam oxidation resistance of SiC up to 4 h at 1200 °C.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Insight into the interfacial microstructure and chemistry of hot isostatically pressed AA6061-AA6061 bonds for U-10Mo fuel cladding application

Here, in the present study, hot isostatic pressing (HIP) bonding was carried out using AA6061-AA6061 plates for U-10Mo monolithic fuel cladding application. HIP was performed at 560°C with an applied isostatic pressure of 103 MPa for 90 min. Interfacial microstructure characterizations were performed using scanning electron microscopy (SEM) combined with electron backscatter diffraction (EBSD) to quantify precipitate fractions and study recrystallization, grain growth, and orientation relationships across the interface. EBSD results confirmed that no interfacial grain growth occurred during the HIP process. Transmission electron microscopy (TEM) was also employed to quantify composition and identify phases of various precipitates and an oxide layer that formed at the interface during HIP bonding. Microstructural analyses revealed the formation of a large fraction of Mg 2 Si precipitate and a ~50 nm thick Mg-oxide layer at the interface. Further TEM analysis confirmed that the oxide layer was not continuous, and Mg 2 Al 2 O 5 oxide particles with an average size of 18 nm were present in the oxide layer. Finite element modeling analysis was performed to study the stress distribution at the interface during HIP processing.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Length scale effects of micro- and meso-scale tensile tests of unirradiated and irradiated Zircaloy-4 cladding

Zircaloy-4 is an essential material for cladding structures within fission-based reactors. To explore the changes in properties measured on differing length scales, FIB-machined micro-scale tensile tests were performed on both irradiated and control groups of Zircaloy-4. This was correlated with tensile testing on femtosecond laser-machined meso-scale specimens. Pronounced size effects were found when varying specimen geometry. Increases in tensile geometry size were associated with a reduction in measured yield stress for both irradiated and unirradiated samples. Here, meso-scale testing found strength and strain values similar to that of bulk-scale testing.

36 MATERIALS SCIENCE↗

Multidimensional modeling of fuel-cladding friction in an LWR fuel rod

Solving finite element problems with friction often increases the level of difficulty to obtain properly converged solutions. This type of challenge becomes more salient when advanced, possibly multiscale, material models are employed to capture the thermomechanical behavior of fuel and cladding materials. Here the present work details our recent developments in a nuclear fuel performance finite element code for the systematic consideration of friction in nuclear reactor finite element simulations. We show the application of friction and its effects on the mechanics of light-water reactor rods accounting for various fuel constitutive modeling techniques, model dimensionalities, pellet assumed geometries, and power conditions. In particular, we focus on the fuel rod mechanical behavior as it relates to fuel constitutive models, sensitivity to the coefficient of friction, pellet states of stress, and rod elongation. We discuss the trade-offs between the various multidimensional modeling options and highlight the relevance of frictional effects in the prediction of the fuel rod deformation and interfacial stresses. To relate our modeling results with actual reactor operation, simulations including frictional effects are compared with fuel rod elongation experimental data and some challenges for carrying out a full validation of the axial mechanics are discussed.

42 ENGINEERING↗

Investigations on the Thermal-hydraulic Behavior of Accident Tolerant Fuel Cladding Materials

Since the 2011 Fukushima accident, significant research has been devoted to developing accident-tolerant fuel (ATF) cladding materials. These investigations have mostly focused on the ability to resist runaway steam oxidation and retain mechanical strength and structural integrity under thermal shocks. However, much remains unknown about the materials’ thermal-hydraulic behavior, particularly under light-water reactor (LWR) operating conditions. Two phenomena that determine safety margins in both normal and off-normal operating conditions - i.e., the critical heat flux (CHF) and Leidenfrost point (LFP) temperature - have not been investigated thoroughly for ATF materials. Surface properties, such as wettability and roughness, are known to influence pool and flow boiling CHF, as well as the LFP temperature. However, little is known about the surface wettability of ATF materials, particularly at LWR pressure and temperature. Little has been done on flow-boiling CHF and quenching heat transfer, especially for droplet quenching. Nonetheless, it is known that CHF in transient conditions, e.g., an exponentially escalating power transient, can be significantly different from that expected in steady-state operation. Very few studies have investigated transient CHF, either on ATF materials or under LWR pressure and temperature. The thorough understanding of transient CHF under prototypical reactor conditions will benefit not only the deployment of ATF but also the upcoming national efforts to study transient ATF behavior in the Transient Reactor Test Facility (TREAT) at Idaho National Laboratory. In summary, as a part of ATF development efforts, there is an urgent need to understand how and how much these materials may affect two-phase heat transfer phenomena in nuclear reactor conditions.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Engineering Scale Drying of Aluminum-Clad Spent Nuclear Fuel: Experiment Report

Engineering-scale tests were performed to evaluate the relative effectiveness of forced gas and vacuum-drying processes on aluminum-clad spent nuclear fuel (ASNF) in preparation for extended dry storage. Drying models were developed to improve confidence in the likely range of conditions at the start of dry storage and to understand the factors most significant to each process. Testing was performed at the Holtec International Forced Helium Dehydration training facility in Camden, New Jersey, by students from the University of South Carolina in collaboration with Idaho National Laboratory. A full-size Type 1a basket, with a full-diameter vessel configuration (based on the Department of Energy standardized canister design), was used in combination with a 10 assembly surrogate ASNF arrangement to provide a proxy for geometry. A resistance heater incorporated in one assembly simulated the influence of 100 W decay heat. This instrumented chamber allowed testing of the removal of bulk water, physisorbed water, and chemisorbed water over a range of operating parameters with either drying process. Thick oxide films were grown on aluminum test plates to mimic the ASNF surface chemistry. These one-use test plates were housed within select assemblies during drying. Post-test analysis of these plates gave a measure of the moisture removed during each test, which was compared to a control. Instrumentation provided detailed thermal, humidity, and gas or pressure data relevant to each test. Model simulations generally compared favorably to instrument data for the tests. While both processes were able to remove bulk water, removal of chemisorbed water was shown to depend heavily on local temperature. To the disadvantage of vacuum drying, operations approaching or exceeding 220°C achieved consistently more dehydroxylation.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Milestone 1.2.11: H 2 Production from Surrogate Non-Native Corrosion Plumes on Aluminum 6061-T6 Fuel Cladding Surrogates

Thick, localized, “non-native” corrosion plumes have been identified on Advanced Test Reactor fuel elements, raising concern on their impact on the radiolytic formation of molecular hydrogen gas (H 2 ) from aluminum-clad spent nuclear fuel (ASNF) under proposed extended (> 50 years) dry storage conditions. Here, we report our findings on H 2 generation from the gamma irradiation (up to 52 MGy) of surrogate “non-native” corrosion plume coupons: ambient-temperature-corroded (~350 days in water) aluminum alloy 6061 (AA6061) coupons in helium gas environments with ~0% added relative humidity. Additionally, we provide a comparison of proposed ASNF drying techniques— vacuum drying only, vacuum drying + 100 °C for 4 hr, and vacuum drying + 220 °C for 4 hr—on the yield of H 2 from these surrogate systems. The presented data indicates that similar amounts of H 2 (~2 × 10–3 µmol J–1) are formed from gamma irradiated AA6061 coupons corroded under different temperature regimes, i.e., ambient/350 days vs. 90 C/30 days. These findings validate current, complimentary modelling predictions based on high-temperature-corrosion irradiation data only. Further, the application of a heat treatment procedure (100 and 220 °C), in conjunction with vacuum drying, accelerated the rate at which a steady-state H 2 yield was attained, in comparison to vacuum only, due to the removal of H 2 precursors in the form of adsorbed waters. Interestingly, within the confidence limits of our measurements, negligible difference in total H 2 yield was found between the two investigated heat treatment procedures.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

Evaluation of Increased Peak Temperatures for Spent Fuel Cladding Performance during Dry Storage (Rev.1)

NUREG-2214, “Managing Aging Processes in Storage (MAPS) Report,” (2019) documents the technical basis for age-related degradation mechanisms on spent nuclear fuel assemblies during dry storage operations. The technical bases have been reviewed, and hoop cladding stress calculations were conducted using the Fuel Analysis under Steady-state and Transients (FAST) code at elevated normal condition temperatures of 425°C and 450°C, and at an off-normal and accident conditions temperature of 600°C. The NUREG-2214 conclusions are substantiated by the referenced literature. The calculations demonstrate that the aging mechanisms primarily driven by hoop stress such as hydride reorientation, delayed hydride cracking, thermal and athermal (low-temperature) creep, and localized mechanical overload are either not credible or do not compromise the fuel assembly’s performance for increased peak normal condition temperatures of 425°C or 450°C during the up to 60-year dry storage period. Other aging mechanisms considered are also not credible for compromising the fuel assembly’s performance during 60-year dry storage with a peak temperature of 400ºC as specified in ISG – 11 Rev. 3, and the same is indicated for the increased peak normal condition temperatures of 425°C or 450°C.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Thermal Modeling Aluminum-Clad Spent Fuel Dry Storage Configurations [Slides]

A presentation covering the work done by the C430 Department at Idaho National Lab on thermal concerns for extended dry storage of aluminum clad spent nuclear fuel (ASNF). Computational fluid dynamics software Star CCM+ was used to model hypothetical accident conditions applied to a dry storage configuration containing ASNF. The hypothetical accident conditions being examined were a fire in which the dry storage configuration is fully engulfed in flames and a situation in which the vent ports of the overpack are completely blocked.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Modeling Approach for the Aluminum-clad Dry Storage Pilot using HFIR Fuel

To confirm that the dry storage of aluminum-clad research reactor spent nuclear fuel (ASNF) will remain within the safety envelope after applied drying schemes and that the resulting evolution of the gas space composition, temperature, and pressure conditions are understood, a dry storage pilot project is being established. The pilot will incorporate an instrumented lid for discrete interval or for on-demand gas composition and temperature monitoring of two DOE Standard Canisters (DSCs) loaded with three High Flux Isotope Reactor (HFIR) inner cores per DSC. Each DSC would be subjected to a separate alternative candidate drying scheme. Canisters will undergo 1 to 5 years of monitoring, including internal temperature and gas sampling to track pressure and composition changes. This report outlines the approach for modeling the ASNF-in-canister behavior in terms of evolving gas space conditions for the ASNF dry storage pilot using HFIR fuel. The ASNF has an adherent surface oxyhydroxide layer comprised of boehmite/bayerite that generates hydrogen when subjected to irradiation. Three-dimensional multi-physics computational fluid dynamics simulations will be executed to compute the thermal field within the DSC and provide inputs to a chemical model employed to compute pressure buildup as hydrogen is generated in the system. Implemented in Cantera, the chemical model solves gas phase and aluminum oxyhydroxide surface-mediated radiolysis reactions. Gas phase reactions are sourced from Wittman and Hanson (2015), whereas surface-mediated reactions are incorporated by fitting experimental data using an optimization algorithm (Abboud, 2023). Water radiolysis reactions from Wren and Ball (2001) are adopted with modifications as described in Abboud (2023c). Understanding the effect of the hydrogen buildup over time is important for long-term storage safety considerations. Modeling results will include the canister pressure, temperature, and composition evolution from the initial helium backfill with the addition of radiolytically-evolved chemical species (e.g., hydrogen and oxygen). The specific HFIR cores for the pilot program have not yet been selected, and the overall design is still in development. The CFD-chemical model used for this work will be based on prior models with necessary updates to allow for improved accuracy and efficiency. The experimental data obtained from the HFIR demonstration will be used to improve and validate the computational models to predict the ASNF-in-canister behavior.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Multiscale Modeling of Silicon Carbide Cladding for Nuclear Applications: Thermal Performance Modeling

The complex multiscale and anisotropic nature of silicon carbide (SiC) ceramic matrix composite (CMC) makes it difficult to accurately model its performance in nuclear applications. The existing models for nuclear grade composite SiC do not account for the microstructural features and how these features can affect the thermal and structural behavior of the cladding and its anisotropic properties. In addition to the microstructural features, the properties of individual constituents of the composites and fiber tow architecture determine the bulk properties. Models for determining the relationship between the individual constituents’ properties and the bulk properties of SiC composites for nuclear applications are absent, although empirical relationships exist in the literature. Here, a hierarchical multiscale modeling approach was presented to address this challenge. This modular approach addressed this difficulty by dividing the various aspects of the composite material into separate models at different length scales, with the evaluated property from the lower-length-scale model serving as an input to the higher-length-scale model. The multiscale model considered the properties of various individual constituents of the composite material (fiber, matrix, and interphase), the porosity in the matrix, the fiber volume fraction, the composite architecture, the tow thickness, etc. By considering inhomogeneous and anisotropic contributions intrinsically, our bottom-up multiscale modeling strategy is naturally physics-informed, bridging constitutive law from micromechanics to meso-mechanics and structural mechanics. The effects that these various physical attributes and thermo-physical properties have on the composite’s bulk thermal properties were easily evaluated and demonstrated through the various analyses presented herein. Since silicon carbide fiber-reinforced SiC CMCs are also promising thermal–structural materials with a broad range of high-end technology applications beyond nuclear applications, we envision that the multiscale modeling method we present here may prove helpful in future efforts to develop and construct reinforced CMCs and other advanced composite nuclear materials, such as MAX phase materials, that can service under harsh environments of ultrahigh temperatures, oxidation, corrosion, and/or irradiation.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗