Mechanical Properties and Microstructure Investigation of Lead Free Solder

While the electronics industry appears to be focusing on Sn-Ag-Cu as the alloy of choice for lead free electronics assembly, ,the exact composition varies by geographic region, supplier and user. Add to that dissolved copper and silver from the printed circuit board traces and surface finish, and there can be significant variation in the final solder joint composition. A systematic study of the mechanical and microstructural properties of Sn-Ag-Cu alloys with Ag varying from 2wt% to 4wt% and Cu varying from 0.5wt% to lSwt%, was undertaken in this research study. Different sample preparation techniques (water quenched, oil quenched and water quenched followed by reflow) were explored and the resulting microstructure compared to that of a typical reflowed lead free chip scale package (CSP) solder joint. Tensile properties (modulus, 0.2% yield strength and the ultimate tensile strength) and creep behavior of selected alloy compositions (Sn-4Ag-1 X u , Sn-4Ag-OSCu, Sn- 2Ag-1 X u , Sn-2Ag-OSCu, Sn-3.5Ag-O.SCu) were determined for three conditions: as- cast; aged for 100 hours at 125OC; and aged for 250 hours at 125OC. There was no significant difference in Young's Modulus as a function of alloy composition. After an initial decrease in modulus after 100 hours at 125"C, there was an insignificant change with further aging. The distribution of 0.2% strain yield stress and ultimate tensile strength as a function of alloy composition was more significant and decreased with aging time and temperature. The microstructures of these alloys were examined using light and scanning electron microscopy (LM and SEM) respectively and SEM based energy dispersive x-ray spectroscopy (EDS). Fracture surface and cross-section analysis were performed on the specimens after creep testing. The creep testing results and the effect of high temperature aging on mechanical properties is presented for the oil quenched samples. In general the microstructure of oil quenched specimen exhibited a eutectic region of Sn with moderately dispersed Ag3Sn intermetallic, surrounded by a dendritic Sn-rich phase. The SEM images of the fracture surface indicated the presence of a tough shear surface at the initial cavity break area and a break line in the middle of specimen along the failure direction. A hyperbolic-sine creep model was adopted and used to fit the creep experiment data. The effect on the mechanical properties by adding the quaternary element bismuth to the Sn-3.5Ag-0.8Cu alloy was measured and compared with the mechanical properties of the ternary alloys. The results of this research study provide necessary data for the modeling of solder joint reliability for a range of Sn-Ag-Cu compositions and a baseline for evaluating the effects of subsequent quaternary additions.

Wang, Qing↗

Design and development of a high-performance Ni-based superalloy WSU 150 for additive manufacturing

This work proposes a design and development strategy of a new nickel-based superalloy for additive manufacturing. A new Ni-based superalloy has been developed by the application of the combinatorial alloy development technique coupled with CALPHAD based solidification modeling by effectively suppressing the precipitation kinetics. The suppression of precipitation during processing paved a way for prevention of cracks during deposition. The new alloy "WSU 150" revealed excellent room temperature mechanical properties with a yield strength of 867 MPa, an ultimate tensile strength of 1188 MPa, and an elongation of 27.9% in the as-deposited condition. The mechanical properties of the heat-treated alloy were improved significantly to 1114 MPa yield strength, 1396 MPa ultimate tensile strength, and an elongation of 16.1%. Improvement in the mechanical properties is attributed to the additional precipitation and coarsening of γ' and carbides during heat-treatment. Microstructural investigation of the alloy revealed spherical γ' with a rippled size distribution from the center to the interdendritic region. The average size of the γ' particles in the as-deposited condition was found to be around 48 nm in the interdendritic region. Heat-treatment promoted the coarsening of γ' which is explained in the paper.

36 MATERIALS SCIENCE↗

CVD silicon carbide monofilament reinforced SrO-Al2O3-2SiO2 (SAS) glass-ceramic composites

Unidirectional CVD SiC fiber-reinforced SrO.Al2O3.2SiO2 (SAS) glass-ceramic matrix composites have been fabricated by hot pressing at various combinations of temperature, pressure and time. Both carbon-rich surface coated SCS-6 and uncoated SCS-0 fibers were used as reinforcements. Almost fully dense composites have been obtained. Monoclinic celsian, SrAl2Si2O8, was the only crystalline phase observed in the matrix from x-ray diffraction. During three point flexure testing of composites, a test span to thickness ratio of approximately 25 or greater was necessary to avoid sample delamination. Strong and tough SCS-6/SAS composites having a first matrix crack stress of approximately 300 MPa and an ultimate bend strength of approximately 825 MPa were fabricated. No chemical reaction between the SCS-6 fibers and the SAS matrix was observed after high temperature processing. The uncoated SCS-0 fiber-reinforced SAS composites showed only limited improvement in strength over SAS monolithic. The SCS-0/SAS composite having a fiber volume fraction of 0.24 and hot pressed at 1400 deg C exhibited a first matrix cracking stress of approximately 231 +/- 20 MPa and ultimate strength of 265 +/- 17 MPa. From fiber push-out tests, the fiber/matrix interfacial debonding strength (tau(sub debond)) and frictional sliding stress (tau(sub friction)) in the SCS-6/SAS system were evaluated to be approximately 6.7 +/- 2.3 MPa and 4.3 +/- 0.6 MPa, respectively, indicating a weak interface. However, for the SCS-0/SAS composite, much higher values of approximately 17.5 +/- 2.7 MPa for tau(sub debond) and 11.3 +/- 1.6 MPa for tau(sub friction) respectively, were observed; some of the fibers were so strongly bonded to the matrix that they could not be pushed out. Examination of fracture surfaces revealed limited short pull-out length of SCS-0 fibers. The applicability of various micromechanical models for predicting the values of first matrix cracking stress and ultimate strength of these composites were examined.

Bansal, Narottam P.↗

Effects of HCP/BCC element ratios on the room-temperature tensile properties of Ti-Zr-Hf-Nb-Ta refractory high-entropy alloys

Equiatomic and non-equiatomic Ti-Zr-Hf-Nb-Ta refractory high-entropy alloys (RHEAs) were arc melted, homogenized, cold rolled, and recrystallized to produce single-phase, body-centered cubic (BCC), microstructures with weak texture and equiaxed grains 76–199 μm in size. Here, the non-equiatomic alloys had either a 60:40 or 80:20 atomic ratio of hexagonal close-packed (HCP) elements (Ti + Zr + Hf) to BCC elements (Nb + Ta). Alloy compositions were measured after thermomechanical processing to determine the concentrations of the major (substitutional) and minor (interstitial) elements. We investigated how elastic constants and uniaxial tensile properties were affected by changes in the relative concentrations of the constituent elements at fixed HCP:BCC ratios. Yield strengths ranged from 801 to 922 MPa and ultimate tensile strengths from 815 to 933 MPa. Good agreement is obtained between the experimental yield strengths and those predicted by a strength theory based on edge dislocations indicating that the observed compositional effects are due to their effects on shear modulus and volume misfit. Fracture occurred by dimpled rupture with fracture strains of 19.4%–25.7%, but uniform strains were an order of magnitude lower at 1.1%–3.2%, calling into question the useable ductility (prior to necking) of RHEAs considered to be ductile based on their fracture strain. Contrary to predictions in the literature that HCP elements promote ductility, our present results show that increasing the HCP:BCC ratio decreases both the total strain and the uniform strain. Similar trends were not evident in the yield or ultimate strengths; rather, strengths were affected mainly by shear modulus and volume misfit.

BCC high-entropy alloys↗

Analyzing Mechanical integrity of Microwave resonant Cavity flowmeter

The microwave resonant cavity flow sensor has been proposed to address the difficulties of measuring high-temperature molten salt flow in reactor vessels. The flow sensor consists of a metallic cylindrical cavity coupled to a microwave waveguide. The cylindrical cavity has one of the flat surfaces thin enough to undergo microscopic deflection due to dynamic pressure of the exerted by the flowing fluid. Deflection of the membrane causes a shift in the microwave resonant frequency. Fluid velocity can be estimated from the calibration curve. The objective of this report is to investigate mechanical integrity of the flowmeter’s membrane. The membrane is a thin stainless-steel circular plate with a clamped edge, subjected to uniform load. By calculating the stress on the plate due to deflection and, comparing the stress to the material ultimate tensile strength and yield strength, it can be estimated if the plate will fail. If the maximum stress is greater than the yield strength, the plate will undergo plastic deformation, and the sensor will be disabled. A stress greater than the ultimate tensile strength will cause the plate to fracture. The stress on the plate was calculated with an analytic closed form solution model, and with COMSOL Structural Mechanics Module which does not involve any approximations. Stresses in both the analytic model and COMSOL numerical model were calculated for stainless steel 316 thin circular plates under room temperature conditions, where the fluid is water. The diameter of the circular plate is approximately one inch, and thickness is 10mil. Fluid flow velocity is in the range from 0.5m/s to 1m/s. The results from the two models are similar. Both the analytic model and COMSOL model showed that maximum stresses on the plate, which are at the radial boundary of the plate, are three orders of magnitude smaller than the yield strength and ultimate tensile strength. This indicates that the sensor is at a low risk of mechanical failure.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Characterization and repair of core gap manufacturing defects for wind turbine blades

Various wind turbine blade components, such as shear webs and skins, commonly use fiber-reinforced composite sandwich structures with a core material like balsa or foam. During manufacturing, core gap defects may result from the misalignment of adjacent foam or balsa core sheets in the blade mold. It is important to understand the influence that core gaps have on the structural integrity of wind turbine blades and how to mitigate their influence. This research characterized the effects of core gap defects at the manufacturing and mechanical levels for both epoxy and next-generation thermoplastic composites. Common repair methods were assessed and compared. Multiple defect sizes were compared using temperature data gathered with thermocouples embedded during manufacturing to core gap defect characteristics obtained using image-mapping techniques, optical microscopy, and mechanical characterization by long beam flexure. Results showed that peak exothermic temperatures during curing were closely related to core gap size. The long beam flexure tests determined that transverse core gaps under pure bending loads can have a substantial effect on the ultimate facesheet strength of both epoxy and thermoplastic composite sandwich structures (up to 25% strength reduction), although the size of the defect itself had less of an influence on the magnitude of the strength reduction. The supporting image-mapping techniques indicated that the distortion of the composite facesheets by the core gaps contributed to the premature failures. The repair methods used in this study did very little to improve the ultimate strength of the sandwich panels that previously had core gap defects. The repair of the thermoplastic panel resulted in a further loss in ultimate facesheet strength. This research demonstrated that there is a vital need for the development of a compatible thermoplastic polymer repair resin system and appropriate resin specific repair procedures for the next generation of recyclable thermoplastic wind blades.

17 WIND ENERGY↗

Long Term Displacement Data of Woven Fabric Webbings Under Constant Load for Inflatable Structures

Inflatable modules for space applications offer weight and launch volume savings relative to current metallic modules. Limited data exist on the creep behavior of the restraint layer of inflatable modules. Long-term displacement and strain data of two high strength woven fabric webbings, Kevlar and Vectran, under constant load is presented. The creep behavior of webbings is required by designers to help determine service life parameters of inflatable modules. Four groups of different webbings with different loads were defined for this study. Group 1 consisted of 4K Kevlar webbings loaded to 33% ultimate tensile strength and 6K Vectran webbings loaded to 27% ultimate tensile strength, group 2 consisted of 6K Kevlar webbings loaded to 40% and 43% ultimate tensile strength, and 6K Vectran webbings loaded to 50% ultimate tensile strength, group 3 consisted of 6K Kevlar webbings loaded to 52% ultimate tensile strength and 6K Vectran webbings loaded to 60% ultimate tensile strength, and group 4 consisted of 12.5K Kevlar webbings loaded to 22% ultimate tensile strength, and 12.5K Vectran webbings loaded to 22% ultimate tensile strength. The uniquely designed test facility, hardware, displacement measuring devices, and test data are presented. Test data indicate that immediately after loading all webbings stretch an inch or more, however as time increases displacement values significantly decrease to fall within a range of several hundredth of an inch over the remainder of test period. Webbings in group 1 exhibit near constant displacements and strains over a 17-month period. Data acquisition was suspended after the 17th month, however webbings continue to sustain load without any local webbing damage as of the 21st month of testing. Webbings in group 2 exhibit a combination of initial constant displacement and subsequent increases in displacement rates over a 16-month period. Webbings in group 3 exhibit steady increases in displacement rates leading to webbing failure over a 3-month period. Five of six webbings experienced local damage and subsequent failure in group 3. Data from group 4 indicates increasing webbing displacements over a 7-month period. All webbings in groups 1, 2, and 4 remain suspended without any local damage as of the writing of this paper. Variations in facility temperatures over test period seem to have had limited effect on long-term webbing displacement data.

Kenner, Winfred S.↗

Using post-processing heat treatments to elucidate precipitate strengthening of additively manufactured superalloy 718

The poor machinability and extensive work hardening of Ni-based superalloys makes additive manufacturing an attractive option for producing geometrically complex components with distinct microstructures. Although previous studies show recovery of high strength at room temperature, very few studies demonstrate successful properties at elevated temperatures required for industrial applications. Here, the objectives of this study are to present a post-build heat treatment for high strength across a wide temperature range, determine the strength contribution of nanoscale precipitating phases to the overall mechanical properties of superalloy 718, and from these, provide a comprehensive microstructure-property relationship for wrought and AM 718 to guide efforts to simulate the properties of AM components. Laser powder bed fusion–produced superalloy 718 was characterized at multiple length scales using scanning electron microscopy and transmission electron microscopy in the as-built condition and with multiple heat treatments designed to form combinations of γ', γ", and δ precipitates. Uniaxial tensile tests performed from room temperature to 600 °C on subsize specimens determined the yield strength, elastic modulus, ultimate tensile strength, fracture stress, and uniform elongation. Precipitates in this work proved to be weak barriers to dislocation motion through a dispersed barrier model, but they provided strength to the alloy through their consistent high density. The relative contribution to the yield strength from γ" remained consistent between 48% and 57% of the total strength up to 600 °C, the primary influence on the high temperature strength of superalloy 718. The strength factors for γ" and δ precipitates were found to trend inversely with tensile test temperature and may be attributable to the differences in precipitate coherency. A post-build heat treatment is recommended to maintain high strength at elevated temperatures. A quantitative microstructure-property relationship, dependent on precipitate size, density, and morphology, was derived and can estimate the yield strength across a wide temperature range applicable to the operational regimes for superalloy 718.

36 MATERIALS SCIENCE↗

Accurate and uncertainty-aware multi-task prediction of HEA properties using prior-guided deep Gaussian processes

Surrogate modeling techniques have become indispensable in accelerating the discovery and optimization of high-entropy alloys (HEAs), especially when integrating computational predictions with sparse experimental observations. This study systematically evaluates the training and testing performance of four prominent surrogate models—conventional Gaussian processes (cGP), Deep Gaussian processes (DGP), encoder-decoder neural networks for multi-output regression and eXtreme Gradient Boosting (XGBoost)—applied to a hybrid dataset of experimental and computational properties of the 8-component HEA system Al-Co-Cr-Cu-Fe-Mn-Ni-V. We specifically assess their capabilities in predicting correlated material properties, including yield strength, hardness, modulus, ultimate tensile strength, elongation, and average hardness under dynamic/quasi-static conditions, alongside auxiliary computational properties. The comparison highlights the strengths of hierarchical deep modeling approaches in handling heteroscedastic, heterotopic, and incomplete data commonly encountered in materials science. Our findings illustrate that combined surrogate models such as DGPs infused with machine-learned priors outperform other surrogates by effectively capturing inter-property correlations and by assimilating prior knowledge. This enhanced predictive accuracy positions the combined surrogate models as powerful tools for robust and data-efficient materials design.

36 MATERIALS SCIENCE↗

ATF Cladding Mechanical Properties Report: Capability Demonstration

This report documents mechanical testing capability demonstration activities performed in fiscal year (FY)2025 at Oak Ridge National Laboratory(ORNL)on chromium-coated (Cr-coated) and uncoated advanced zirconium alloy claddings irradiated in the High Flux Isotope Reactor (HFIR) to approximately 4 displacements per atom (dpa), corresponding to ~13GWd/t burnup. Specimens were prepared in axial tension (ATT) and ring tension (RTT) geometries, and passive silicon carbide(SiC)thermometry (TM) was employed to determine irradiation temperatures, which averaged 38–43 °C below the 330 °C design target. Mechanical testing at ambient temperature demonstrated the expected irradiation-induced hardening, with yield strength(YS)and ultimate tensile strength(UTS)values increasing substantially relative to unirradiated counterparts. However, this strengthening was accompanied by a reduction in ductility, as indicated by lower uniform and total elongations(UE and TE). Both coated and uncoated claddings exhibited similar mechanical response, though Cr-coated specimens showed surface cracking perpendicular to the loading direction, attributable to the hardness mismatch between the coating and substrate. Fracture in all cases remained ductile, and no coating spallation was observed following HFIR irradiation. Complementary efforts were directed toward the fabrication of test specimens from commercially irradiated cladding (rod 47I, ~31.1 GWd/t average burnup). Axial sectioning and computer numerical control(CNC)machining successfully produced ATT geometries suitable for benchmarking against HFIR-irradiated specimens. This capability enables direct comparison of cladding behavior between test reactor and commercial reactor environments, thereby supporting the validation of HFIR as a surrogate irradiation platform for accident tolerant fuel (ATF) development. Once HFIR irradiations are completed in FY26,the relevant comparison tests will be completed. Collectively, the FY 2025 PIE campaign has provided mechanical performance data for irradiated advanced claddings The demonstrated capabilities support the framework for mechanical testing and further evaluations in subsequent years. These efforts will represent an important contribution toward the licensing and deployment of Cr-coated zirconium alloy cladding as a near-term ATF solution.

36 MATERIALS SCIENCE↗

Comparison of AMZIRC and GRCop-84

The mechanical properties of two copper alloys with high thermal conductivity, GRCop-84 and AMZIRC, were compared. These are competing alloys in high temperature, high heat flux applications such as rocket nozzles. The GRCop-84 data presented was taken from previous work. The results of new tensile, creep, and compression tests on AMZIRC are presented. Tests were done on as-received hard drawn material, and on material that had been subjected to a heat treatment designed to simulate a brazing operation at 935 C. As-received AMZIRC was found to have excellent properties at temperatures below 550 C, with room temperature yield and ultimate tensile strengths of about 500 MPa, and ductile failures. By comparison, GRCop-84 s room temperature tensile yield and ultimate strengths are about 200 and 380 MPa respectively. However, the simulated brazing heat treatment substantially decreased the mechanical properties of AMZIRC; and the strength of as-received AMZIRC dropped precipitously as test temperatures exceeded 500 C. The properties of GRCop-84 were not significantly affected by the 935 C heat treatment. As a result, there appear to be advantages to GRCop- 84 over AMZIRC if use or processing temperatures of greater than 500 C are expected. Tensile creep tests were done at 500 and 650 C. At these temperatures, the creep properties of GRCop-84 were superior to AMZIRC s. At equivalent rupture life and stress, GRCop-84 was found to have a 150 C temperature advantage over AMZIRC; for equivalent rupture life and temperature GRCop-84 was two times stronger.

de Groh, Henry C. III↗

Sodium Exposure Tests of A709 Steel (FY2020 Progress Report)

Sodium exposure tests were conducted on the first commercial heat, H58776 of A709 steel. Six different processing and heat treatment conditions were investigated, including three processing conditions, namely, Argon-Oxygen-Decarburization (AOD), Electro-slag Remelting (ESR), and Electro-slag Remelting with subsequent homogenization (HOMO), and two heat treatment conditions, i.e. solution annealing at 1100°C (SA1100°C) or 1150°C (SA1150°C). Specimens of AOD-SA1100°C, AOD-SA1150°C, ESR-SA1100°C, ESR-SA1150°C, HOMO-SA1100°C, and HOMO-SA1150°C were tested in sodium at 650°C and for times up to 10,152 h. Specimens in the AOD-SA1100°C and AOD-SA1150°C conditions were also tested in sodium at 550 and 600°C. Parallel thermal aging experiments were carried out for comparison with sodium exposure tests to separate the thermal and sodium effects. It was found that A709 H58776 generally showed a weight loss after sodium exposures at 650°C except a few data points of the ESR-SA1100°C specimens. The corrosion rate showed large variations in the initial stage and decreased with increasing exposure time. Long-term exposure tests are needed to determine its steady-state corrosion rate. The AOD-SA1100°C and HOMO-SA1100°C specimens showed similar tensile responses after thermal or sodium exposures at 650°C. The yield stress increased, the ultimate tensile strength decreased, and the uniform and total elongations were reduced after thermal or sodium exposures. A longer exposure time had a minimal effect on the tensile strength but further reduced the tensile ductility. The sodium-exposed specimens had higher tensile strength than the thermally-aged specimens. In contrast, the ESR-SA1100°C specimens showed an increase in the yield stress and the ultimate tensile strength after thermal or sodium exposures at 650°C and ~10,000 h. The AOD-SA1150°C and ESR-SA1150°C specimens showed similar tensile behavior after thermal or sodium exposures at 650°C.Thermal or sodium exposures at 650°C increased the yield stress, decreased the ultimate tensile strength, and reduced uniform and total elongations. There were minimal differences in tensile properties between the sodium-exposed and thermally-aged specimens after an ~3000 h exposure. After an exposure for ~10,000 h the sodium-exposed specimens showed higher yield stress and ultimate tensile strength and lower uniform and total elongations than the thermally-aged specimens. For the HOMO-SA1150°C specimens, thermal or sodium exposures at 650°C significantly increased the yield stress but had a minimal effect on the ultimate tensile strength. Both uniform and total elongations were significantly reduced at an exposure time of ~3,000 h, and they were further reduced after an exposure of ~10,000 h. The sodium-exposed specimens had lower tensile ductility than the thermally-aged specimens. Before exposure, the stress-strain curves of the specimens in all six processing-heat treatment conditions showed serrations indicating the dynamic aging effect at 650°C. Thermal aging or sodium exposures at 650°C after ~10,000 h completely removed the serrations of the flow curves in A709 H58776, indicating strong precipitation during thermal or sodium exposures. Longer-term sodium exposure tests are needed to determine the steady-state corrosion rates in sodium for A709 H58776 and fully understand the influence of sodium exposures on its mechanical performance.

36 MATERIALS SCIENCE↗

Laser Powder Directed Energy Deposition of Steels for Nuclear Applications

This comprehensive investigation examines the structure–property relationships in two nuclear alloy systems—Alloy 709 (A709) austenitic stainless steel and Grade 92 (G-92) ferritic/martensitic (F/M) steel—manufactured via directed energy deposition (DED) for sodium-cooled fast reactor applications. This study establishes the fundamental mechanisms for controlling microstructures for optimizing the mechanical performance of additively manufactured nuclear materials through systematic heat treatment optimization and multiscale characterization. As-deposited A709 steel develops a complex multiscale strengthening architecture consisting of a fine cellular solidification structure with diameter of 2-3 µm within10–50 µm grains, elevated dislocation densities from rapid thermal cycling, and grain boundary precipitates that activate concurrent Hall–Petch, dislocation, and precipitation hardening mechanisms to achieve exceptional properties [yield strength (YS): 603 MPa, ultimate tensile strength (UTS): 844 MPa, Vickers hardness: 220 HV] that achieve a 44% superior strength compared to that of the wrought material. Heat treatments produce different results. Solution annealing (SA) dissolves the cellular structure and reduces the hardness to 190 HV. Precipitation treatment (PT) keeps the cellular structure but adds carbides, allowing the hardness to reach 205 HV. The best approach combines both treatments (SA+PT) and creates uniform precipitate distributions with M 23 C 6 carbides at the grain boundaries and MX carbonitrides in the matrix, achieving a hardness of 195 HV. However, directional differences persist, with a 12%–15% strength variation between orientations due to the inherited layered microstructural architecture that survives aggressive heat treatment. While tensile testing at 550°C demonstrates 40%–50% thermal softening with dynamic strain aging, DED A709 steel still maintains a 71% higher YS than that of the wrought material. Ion irradiation studies (100–400 dpa) of DED A709 steel reveal progressive radiation damage with increasing void density and radiation-induced segregation causing nickel enrichment and chromium depletion, which will ultimately compromise mechanical properties. As-deposited G-92 exhibits exceptional strength (UTS: 1650–1700 MPa, 430 HV) through a complex microstructure containing both ferrite and martensite phases, a high geometrically necessary dislocation (GND) density (17.04×10 14 /m 2 ), and fine carbides. Heat treatments create distinct changes. Normalizing produces fresh martensite with the highest hardness (460 HV) and an increased GND density (20.23×10 14 /m 2 ). Tempering develops dual precipitation systems and reduces the hardness to 290 HV. The optimal approach uses sequential normalizing plus tempering, achieving balanced properties with the lowest hardness (250 HV) and a reduced GND density (11.01×10 14 /m 2 ). A processing-dependent anisotropy is observed: horizontal specimens achieve superior ductile behavior, while vertical specimens exhibit brittle failure. A tempering heat treatment successfully mitigates this anisotropic behavior by transforming the hard martensitic as-deposited structure into tempered martensite enabling both horizontal and vertical specimens to exhibit similar stress–strain characteristics with visible necking behavior. Remarkably, testing at 550°C reveals a reversal in the anisotropy, where as-deposited specimens achieve near isotropy with superior thermal stability (a 15%–20% strength reduction), while tempered specimens develop an orientation dependence with a 25%–30% strength reduction. Both alloy systems demonstrate that DED processing creates specimens with a superior strength through refined microstructural features, though with distinct strengthening mechanisms—austenitic through cellular structures and precipitates versus F/M through phase transformations and precipitates. Heat treatment optimization requires alloy-specific approaches, with A709 benefiting from controlled precipitation while G-92 requires careful phase transformation control. The results show that DED manufacturing can produce nuclear materials with exceptional performance, but directional effects and temperature-dependent behavior must be carefully considered for reactor component design and qualification.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Effect of Strain Rate on Mechanical Properties of Wrought Sintered Tungsten at Temperatures above 2500 F

Specimens of wrought sintered commercially pure tungsten were made from 1/8-inch swaged rods. All the specimens were recrystallized at 4050 F for 1 hour prior to testing at temperatures from 2500 to 4000 F at various strain rates from 0.002 to 20 inches per inch per minute. Results showed that, at a constant temperature, increasing the strain rate increased the ultimate tensile strength significantly. The effects of both strain rate and temperature on the ultimate tensile strength of tungsten may be correlated by the linear parameter method of Manson and Haferd and may be used to predict the ultimate tensile strength at higher temperatures, 4500 and 5000 F. As previously reported, ductility, as measured by reduction of area in a tensile test, decreases with increasing temperature above about 3000 F. Increasing the strain rate at temperatures above 3000 F increases the ductility. Fractures are generally transgranular at the higher strain rates and intergranular at the lower strain rates.

Sikora, Paul F.↗

Matrix density effects on the mechanical properties of SiC/RBSN composites

The room temperature mechanical properties were measured for SiC fiber reinforced reaction-bonded silicon nitride composites (SiC/RBSN) of different densities. The composites consisted of approx. 30 vol percent uniaxially aligned 142 micron diameter SiC fibers (Textron SCS-6) in a reaction-bonded Si3N4 matrix. The composite density was varied by changing the consolidation pressure during RBSN processing and by hot isostatically pressing the SiC/RBSN composites. Results indicate that as the consolidation pressure was increased from 27 to 138 MPa, the average pore size of the nitrided composites decreased from 0.04 to 0.02 microns and the composite density increased from 2.07 to 2.45 gm/cc. Nonetheless, these improvements resulted in only small increases in the first matrix cracking stress, primary elastic modulus, and ultimate tensile strength values of the composites. In contrast, HIP consolidation of SiC/RBSN resulted in a fully dense material whose first matrix cracking stress and elastic modulus were approx. 15 and 50 percent higher, respectively, and ultimate tensile strength values were approx. 40 percent lower than those for unHIPed SiC/RBSN composites. The modulus behavior for all specimens can be explained by simple rule-of-mixture theory. Also, the loss in ultimate strength for the HIPed composites appears to be related to a degradation in fiber strength at the HIP temperature. However, the density effect on matrix fracture strength was much less than would be expected based on typical monolithic Si3N4 behavior, suggesting that composite theory is indeed operating. Possible practical implications of these observations are discussed.

Bhatt, Ramakrishna T.↗

Matrix density effects on the mechanical properties of SiC fiber-reinforced silicon nitride matrix properties

The room temperature mechanical properties were measured for SiC fiber reinforced reaction-bonded silicon nitride composites (SiC/RBSN) of different densities. The composites consisted of approx. 30 vol percent uniaxially aligned 142 micron diameter SiC fibers (Textron SCS-6) in a reaction-bonded Si3N4 matrix. The composite density was varied by changing the consolidation pressure during RBSN processing and by hot isostatically pressing the SiC/RBSN composites. Results indicate that as the consolidation pressure was increased from 27 to 138 MPa, the average pore size of the nitrided composites decreased from 0.04 to 0.02 microns and the composite density increased from 2.07 to 2.45 gm/cc. Nonetheless, these improvements resulted in only small increases in the first matrix cracking stress, primary elastic modulus, and ultimate tensile strength values of the composites. In contrast, HIP consolidation of SiC/RBSN resulted in a fully dense material whose first matrix cracking stress and elastic modulus were approx. 15 and 50 percent higher, respectively, and ultimate tensile strength values were approx. 40 percent lower than those for unHIPed SiC/RBSN composites. The modulus behavior for all specimens can be explained by simple rule-of-mixture theory. Also, the loss in ultimate strength for the HIPed composites appears to be related to a degradation in fiber strength at the HIP temperature. However, the density effect on matrix fracture strength was much less than would be expected based on typical monolithic Si3N4 behavior, suggesting that composite theory is indeed operating. Possible practical implications of these observations are discussed.

Bhatt, Ramakrishna T.↗

Shear assisted processing and extrusion of enhanced strength aluminum alloy tubing

Hollow extrusions are used in many industries to make strong, lightweight, and affordable structures. Shear Assisted Processing and Extrusion (ShAPE) enables the extrusion of many alloys, often with noteworthy properties. In this investigation, ShAPE was used to extrude 1 and 2 mm wall tubes of aluminum alloy 6063 measuring 12 mm in diameter at extrusion speeds up to 3.8 m/min. This speed is 10 and 15 times faster than has been reported for any alloy using ShAPE and friction stir back extrusion, respectively. Increasing the extrusion speed from 0.7 to 3.8 m/s resulted in using 68% less process energy at steady state. Microstructural analysis and tensile testing were performed on as-extruded tubes and tubes with a direct T5 heat treatment. Grain refinement from 65 µm to below 20 µm was observed. Growth of macroscale Mg 2 Si strengthening precipitates was not observed. ShAPE processing resulted in recrystallization, and extrusion speed was shown to influence final extrudate texture. Here, transmission electron microscopy analysis revealed that the as-extruded microstructure was free of nanoscale ß" strengthening precipitates. Nanoscale ß" was prominent in direct-aged (T5) ShAPE tubes, similar to a slightly over-aged conventional T6 microstructure. As-extruded tubes had ultimate tensile strengths on par with conventional T5 extrusions and approximately double the total elongation. Tubes that underwent a T5 heat treatment had yield and ultimate strengths averaging 198 and 234 MPa, respectively, with an average total elongation of 11%. The tensile test results are comparable to a conventional T6 heat treatment, but without the solutionization heat treatment step. Mechanical properties either remained flat or improved with increased extrusion speed, which suggests that ShAPE can be scaled up to an industrial process to create energy- and economically efficient high-strength extrusions.

36 MATERIALS SCIENCE↗

An evaluation of the interfacial bond properties between carbon phenolic and glass phenolic composites

The effects of moisture and surface finish on the mechanical and physical properties of the interfacial bond between the carbon/phenolic (C/P) and glass/phenolic (G/P) composite materials are presented. Four flat panel laminates were fabricated using the C/P and G/P materials. Of the four laminates, one panel was fabricated in which the C/P and G/P materials were cured simultaneously. It was identified as the cocure. The remaining laminates were processed with an initial simultaneous cure of the three C/P billets. Two surface finishes, one on each half, were applied to the top surface. Prior to the application and cure of the G/P material to the machined surface of the three C/P panels, each was subjected to the specific environmental conditioning. Types of conditioning included: (1) nominal fabrication environment, (2) a prescribed drying cycle, and (3) a total immersion in water at 160 F. Physical property tests were performed on specimens removed from the C/P materials of each laminate for determination of the specific gravity, residual volatiles and and resin content. Comparisons of results with shuttle solid rocket motor (SRM) nozzle material specifications verified that the materials used in fabricating the laminates met acceptance criteria and were representative of SRM nozzle materials. Mechanical property tests were performed at room temperature on specimens removed from the G/P, the C/P and the interface between the two materials for each laminate. The double-notched shear strength test was used to determine the ultimate interlaminar shear strength. Results indicate no appreciable difference in the C/P material of the four laminates with the exception of the cocure laminate, where 20 percent reduction in the strength was observed. The most significant effect and the ultimate strength was significantly reduced in the wet material. No appreciable variation was noted between the surface finishes in the wet laminate.

Jordan, Kelvin↗