Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Thermal damage”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 271 records · Page 15

Investigation of desorption of hydrogen gas from polymer matrix using thermal desorption analysis and finite element modeling

Polymer materials are used widely as sealing materials and liners in hydrogen storage and transportation infrastructure. During operating conditions, polymers are exposed to high pressure hydrogen gas periodically. When in contact, the hydrogen gas diffuses through the polymer material with ease due to its smaller sized molecules compared to the polymer molecules. In the event of rapid decompression of outside hydrogen gas, the hydrogen molecules within the polymer diffuse out. This process is known as the desorption of polymer and can cause blisters or cracking causing permanent damage to the polymer. Here, we used a combined experimental and modeling approach to investigate the desorption of the hydrogen gas in the polymer. Thermal desorption analysis (TDA) experiments were performed on the polymer sample exposed to the high-pressure hydrogen gas to measure the diffusion coefficient and equilibrium hydrogen concentration. Experiments also provided the quantity of hydrogen within the polymer during the desorption process which followed Fick’s law. However, for higher pressurization values, some anomaly was observed in the quantity of hydrogen remaining in the polymer sample. A continuum mechanics based coupled diffusion–deformation-damage model was deployed to simulate the gas desorption process in the material using the finite element method to understand its effect on the material. It was found that the anomaly in TDA results were due to the blister formation on the polymer surface which resulted in longer hydrogen retention. Simulations also showed that blister formation can be affected by multiple parameters such as the addition of filler particles, and pre-existing cavity size.

36 MATERIALS SCIENCE↗

Lattice response to ambient self-irradiation of δ-phase 239 Pu-Ga alloys exposed to cryogenic temperatures

Self-irradiation in plutonium is a continuous process that introduces radiation damage ranging from point defects to nanoscale radiation damage as well as decay daughter product impurities that require to be accommodated by the host material. These changes are affecting the structure and properties of the material by lattice swelling, mechanical strengthening, and other alterations. X-ray diffraction and dilatometry studies have shown that the room temperature self-irradiation of δ-phase Pu-Ga alloys (2 and 7 at%Ga) results in swelling of the lattice that saturates after 0.1–0.2 displacement per atom (dpa) of accumulated lattice damage. Here, for a better understanding of these self- irradiation processes, defect accumulation and damage evolution, this time-of-flight neutron diffraction study investigates the impact of ambient self-irradiation effects on the structural evolution of δ-phase 239 Pu-Ga alloys exposed to cryogenic temperatures (<120 K), associated with a varied history of storage time and thermal treatments. Two key behaviors were observed in the lattice evolution after exposure to cryogenic temperatures with respect to room-temperature accumulated self-irradiation damage. Samples with no self- irradiation damage accumulation under ambient conditions showed swelling of the lattice at the end of the measurement, while samples that accumulated significant self-irradiation damage under ambient conditions showed only a partial recovery of the lattice parameter value upon completion of the measurements (cooling followed by heating back to room temperature). Possible causes of the behavior are proposed, and their associated effects are discussed.

36 MATERIALS SCIENCE↗

DECOVALEX-2023: Task E Final Report

This is the Task E final report for DECOVALEX-2023. Task E is focused on understanding thermal, two-phase hydrological, and mechanical (TH2M) processes, especially related to predicting brine migration in the excavation damaged zone around a heated excavation in salt. Salt is attractive as a disposal medium for radioactive waste because it is self-healing and is essentially impermeable and essentially non-porous in the far field (away from excavations). Investigation of the short-term (days to years) near-field (centimeters to tens of meters) behavior of salt is important for radioactive waste disposal because this early period strongly controls the amount of brine in a salt repository. Brine leads to corrosion of waste forms and waste packages, and possible dissolution of radionuclides with brine transport being a potential transport vector to the accessible environment. The main test case used in Task E is the ongoing Brine Availability Test in Salt (BATS) heater test located underground at the Waste Isolation Pilot Plant (WIPP) near Carlsbad, New Mexico, USA. The Task was divided into a series of Steps. Step 0 was an introduction to processes in salt, that included matching historical unheated brine inflow data from boreholes at WIPP and matching temperature observations during BATS heater test 1a. Step 1 included validation of models against a thermo-poroelastic analytical solution relevant to heated boreholes in salt, and two-phase flow around an excavation in salt. Step 2 required all the individual components covered in steps 0 and 1 to come together to match observed brine inflow behavior during the BATS 1a heater test. There were a range of approaches from the teams, from mechanistic to prescriptive. Given the uncertainties in the problem, some teams used one- or two-dimensional models of the processes, while other teams included more geometrical complexity in three-dimensional models. The key learning points from Task E have been: • Heat conduction through salt typically requires non-linear thermal conductivity (as a function of temperature), but most models do a good job matching observations, given appropriate adjustments to the applied power and some thermocouple locations. • Thermal pressurization requires coupled thermal-hydrological-mechanical (THM) responses that consider the thermal expansion of the fluid and solid phases. • Initialization of two-phase flow models around a borehole or excavation in salt are more realistically represented as “wetting up”, rather than “drying down” (i.e., the initial state after excavation is mostly dry, rather than mostly wet). • The BATS 1a heater test includes a significant release of brine after the end of heating, which requires a large increase in permeability to recreate. Task E has been a great learning experience for all the teams involved, and feedback from the modeling teams has led to changes in the design of follow-on BATS experiments, which are now ongoing underground at WIPP. There was a balance throughout the task between freedom to model phenomena how each team saw fit, and prescriptiveness in problem design to bring the modeling teams closer together to allow attribution of smaller differences between models to different modeling choices. The modeling approaches seem to go through two phases: an early phase of discovery or testing, and a later phase of refinement and improvement. In future modeling efforts, different field data could be used (e.g., BATS 2) and more time should be included in the processes for teams to make multiple model refinement or even significant changes to their conceptual model or setup, based on lessons learned from the modeling exercise.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Mechanistic modeling of copper corrosions in data center environments

Air-side economizers are increasingly used to take advantage of “free-cooling” in data centers with the intent of reducing the carbon footprint of buildings. However, they can introduce outdoor pollutants to indoor environment of data centers and cause corrosion damage to the information technology equipment. Here, to evaluate the reliability of information technology equipment under various thermal and air-pollution conditions, a mechanistic model based on multi-ion transport and chemical reactions was developed. The model was used to predict Cu corrosion caused by Cl2-containing pollutant mixtures. It also accounted for the effects of temperature (25 °C and 28 °C), relative humidity (50%, 75%, and 95%), and synergism. It also identified higher air temperature as a corrosion barrier and higher relative humidity as a corrosion accelerator, which agreed well with the experimental results. The average root mean square error of the prediction was 13.7 Å. The model can be used to evaluate the thermal guideline for data centers design and operation when Cl2 is present based on pre-established acceptable risk of corrosion in data centers’ environment.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Interaction of Concentrated (68%) Aqueous Nitric Acid Solutions with Cheesecloth: A TGA-DSC-MS Study

The exposure of cotton cheesecloth to concentrated aqueous solutions of nitric acid reduced the onset of combustion by 30-40°C (from ~350°C to ~310°C) relative to that of both unexposed cheesecloth and cheesecloth that was rinsed immediately following exposure to the same solution. Cheesecloth exposed to concentrated (68%) nitric acid underwent three exothermic pre-combustion reactions which onset at 125-135°C, 160- 170°C and 200-210°C. These reactions give off mostly water vapor, with lesser amounts of NO and carbon dioxide. Exposure to concentrated nitric acid damages the cellulose polymers, oxidizing them, reducing them in length, and increasing their reactivity in response to thermal stress. Cheesecloth which was rinsed after exposure behaved similarly to unexposed cheesecloth, indicating that NC was not formed on exposure to the concentrated aqueous nitric acid solution. The addition of a 239Pu – 241Am spike in an aqueous nitric – hydrofluoric solution to the cheesecloth reduced the onset temperature of the first exothermic reaction to 126°C and lowered the onset temperature of combustion from ~310°C to ~275°C. When dried on to cellulose substrates in the presence of excess nitrate, metal ions may act as oxidizers, or may catalyze the oxidation of the carbonaceous material, lowering ignition temperatures. No evidence for the formation of nitrocellulose following the exposure of cheesecloth to nitric acid was observed during this study

36 MATERIALS SCIENCE↗

Accelerated Aging of PV Cables - The Development of Methods Towards Combined-Accelerated Stress Testing

PV cables allow the collection and distribution of electricity from modules to the energy grid. Durable cabling allows continuous operation of PV installations. Cables with a life less than that of the modules must be replaced - reducing electricity generation and adding to the system operating expense. We have examined the durability of a variety of representative cable samples using artificial UV weathering (IEC TS 62788-7-2) and combined accelerated stress testing (C-AST). Jackets in this study include PV-rated (polyolefin), building wire (PVC/PA), and multi-conductor (rubber, as in PV trackers), with some examples of black and red cables. Characterizations at read points include appearance (camera and optical microscope), surface roughness (linear profilometry), instrumented indentation, surface morphology (SEM), chemical composition (EDS), thermal decomposition (TGA), phase transition (DSC), crystalline structure (WAXS), and polymer chemical structure (FTIR). Complimentary examinations confirm damage to the external and interior layer(s) of less durable samples, including changes in morphology (e.g., cracking), chemistry (e.g., oxidation), structure, and mechanical performance (e.g., through-thickness modulus and hardness). The results may be generally compared to other examples from the field (PV installations) or after accelerated testing (IEC 61215). The methods in this study are presently being applied in a follow-on C-AST study, incorporating both dynamic and kinematic fixtures.

balance of systems↗

Understanding spectral dependance of laser-induced damage precursors in dielectric materials (Full report_23-ERD-006)

The performance of high-energy laser systems is constrained by laser-induced damage in dielectric coatings, particularly those containing hafnium oxide (HfO 2 ). While thresholds at fundamental Nd harmonics are well studied, the spectral dependence of damage initiation—especially under dual-wavelength irradiation—remains poorly characterized. This project provides the first systematic investigation of wavelength-dependent laser damage in hafnia coatings, focusing on nanoscale precursors such as craze lines, nanobubbles, stoichiometric variations, nodules, and controlled crystallization. Coatings were fabricated via ion beam sputtering and electron-beam deposition and characterized using spectrophotometry, ellipsometry, AFM, GI-XRD, RBS, PCI absorption, and fs/ns laser damage testing. Results show that craze lines, benign under infrared light, strongly initiate damage under UV due to wavelength-selective field intensification. Substituting xenon for argon suppresses nanobubbles and improves UV thresholds by up to 32%. Oxygen modulation reveals that fully oxidized films maximize UV resistance, though at the cost of porosity and stress in multilayers. HfO 2 –SiO 2 composites resist crystallization and defects while achieving ppm-level absorption and elevated thresholds, whereas full crystallization of HfO 2 enhances LIDT by reducing defects and improving thermal transport. Collectively, these findings link photon energy, defect states, and bandgap collapse, providing a predictive framework for wavelength-dependent laser damage. The outcomes directly inform the design of durable, multi-wavelength coatings for facilities such as NIF, MEC, HAPLS, and DPAL, advancing the readiness of next-generation optics.

36 MATERIALS SCIENCE↗

Development and testing of a solar flux heating freeze recovery system for molten salt parabolic troughs

A major obstacle preventing commercialization of molten salt parabolic trough plants is freeze protection and recovery of the solar field. One of the most common nitrate salt compositions under consideration allows for solar field outlet temperatures up to 565°C and begins solidifying above 240°C. Using molten salt directly in the solar field can significantly reduce thermal energy storage costs and the higher temperature compared to oil heat transfer fluids can power a more efficient power cycle, but the very high freezing point is cause for concern. This work builds on a previous modeling effort investigating different methods for melting Solar Salt frozen in the solar field, which suggested the viability of a novel solar heating method to lower costs of the freeze protection system. In this work higher fidelity models are developed to better investigate the melting process with a more detailed 3D geometry which includes the insulated bellows. The thermal-fluid model of the melting process is updated to include temperature dependent density and data for solid phase properties. In addition, a finite element model is developed to resolve thermal stresses at the point with highest thermal gradients. Results with the new model confirm the viability of using controllable solar flux heating to thaw salt frozen in the solar field without damaging the receiver; however, the presence of non-illuminated sections significantly slows down the melting process. Solar heating simulations with pauses off-sun of 120 and 60 s require 18.5 and 11.9 h to melt salt from a night-time temperature of 10°C with 1000 W m2 DNI, which results in maximum thermal stresses of 48.2 and 53.5 MPa, respectively. Adding 150 W m−1 to the solar heating simulation with a 60 s pause off-sun decreases both the melt time and thermal stresses due to the more uniform heating, suggesting a combined heating method may be the best option.

14 SOLAR ENERGY↗

Smaller and faster: a review of conventional and nanocalorimetry techniques for determining thermophysical properties of nuclear materials

Thermal analysis of nuclear materials is critical for the advancement of nuclear technology. The heat effects associated with heat capacity, phase transformation, and radiation damage can be measured with conventional calorimeters. However, conventional calorimetric techniques are often restricted in terms of heating rate and sample mass, especially when studying the limited amounts of materials subject to extreme conditions. In this review, we summarize conventional calorimetric studies of critical thermophysical and thermochemical properties of pure actinide metals (U, Np, Am, Pu), fast reactor metallic fuel alloy systems (U–Zr, U–Pu–Zr, Pu–U, Pu–Zr), and actinide oxides that are primary constituents or transmutation products in light water reactor fuel rods (U–O, Np–O, Am–O, Pu–O, Pu–U–O). Adiabatic and drop calorimetry have been the primary techniques used for these studies, however the development of fast scanning calorimetry using micro-electro-mechanical-based systems allows determination of thermodynamic properties from smaller sample masses. We report recent investigations that leverage the fast heating rates of nanocalorimetry by itself or combined with other characterization techniques. Furthermore, we then discuss opportunities for nanocalorimetry to provide solutions to some of the technical challenges inherent in thermal analysis of nuclear materials, namely a reduction in sample activity, emulating heating transients, investigation of phase evolution in irradiated samples, and characterization of radiation damage evolution. Nanocalorimetry has the potential to significantly advance the understanding of thermophysical properties in nuclear materials and thus accelerate the development of nuclear technology.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Effects of cyclic plasma heating on surface damage of micro-porous tungsten

The operating temperature window of solid tungsten (W) is dictated by its Ductile to Brittle Transition Temperature (DBTT) and re-crystallization temperature; roughly between 300-1300 °C. The brittleness of W at lower temperatures is exasperated when it undergoes recrystallization. We investigate here the thermal shock resistance of micro-porous W as a meta-material fabricated in a 3D open-cell network structure. We present experimental results for the effects of cyclic high-enthalpy arc-jet plasma on surface damage in three testing categories. Observed damage includes surface ablation of asperities, melting and solidification of W-fuzz on samples that have been exposed to a prior helium plasma, and micro-cracks at ligament triple junctions. Scanning electron microscope (SEM) observations show more micro-cracking on 54% and 23% foams compared to the 43% ones. In all tested samples, thermal expansion/contraction displacements were accommodated by ligament rotation and a network of micro-cracks. Furthermore, no large through-thickness crack were observed.

36 MATERIALS SCIENCE↗

Numerical investigation of thermomechanical response of multiscale porous Ultra-High Temperature Ceramics

Recent advances in Ultra-High Temperature Ceramics (UHTC) manufacturing have permitted the development of multiscale porous UHTC microstructures. Within the target application of hypersonic vehicles, dense UHTCs are suitable for thermal protection on leading edges, whereas porous UHTCs may find a role in providing thermally insulated interfaces for temperature-sensitive interior components. Designing vehicles incorporating porous UHTCs requires a characterization of their thermomechanical properties across the full range of expected operating temperatures spanning –20 °C–2500 °C. This research represents a preliminary study in performing this characterization. Several numerical experiments are performed using a coupled thermomechanical implementation of the Material Point Method to determine the temperature dependence of effective material properties both with and without damage. Furthermore, complex time-dependent boundary conditions derived from known hypersonic flight profiles are simulated in order to probe the various couplings between deformation, damage and heat transfer. It is shown that the model reveals the importance of micro-buckling in determining effective material stiffness and thermal conductivity.

36 MATERIALS SCIENCE↗

Impact of high-temperature annealing on hafnia-silica composite coatings deposited via ion beam sputtering for high-peak power 1064 nm lasers

The maximum power handling fluence of high-peak and average power laser systems is often limited by the laser damage of the coatings on optical components. Furthermore, these multilayer dielectric coatings are limited in their maximum power handling due to laser-damage-prone defects in the lower optical bandgap, higher optical index material. Some of these defects can be mitigated by thermal annealing to high temperatures, which can greatly reduce the linear absorbative precursors. Typically, hafnia and silica are the materials of choice for high-peak and average power laser systems in the ultraviolet through infrared spectral range; however, hafnia crystalizes readily when annealed at high temperatures. In this study, we prepare composite HfO 2 -SiO 2 coatings by co-sputtering hafnia and silica in an ion beam sputtering system and compare them to pure hafnia-based coatings. We demonstrate that crystallinity in hafnia can be completely suppressed when it is mixed with silica, such as the composite coatings in this study. High reflectors were fabricated and annealed, demonstrating that the multilayer dielectric stacks can survive high-temperature annealing and exhibit an excellent linear absorption of 0.2 +/- 1 ppm at 1064 nm. Short- and long-pulse laser damage was explored, demonstrating the complex relationship between linear absorption and the non-linear absorption which drives pulsed laser damage. These results provide an excellent route to the creation of very low linear absorption optical coatings, which also utilize low scattering materials that are best suited for high-peak and average power applications.

Harthcock, Colin [Lawrence Livermore National Labo↗

Experimental Testing of Particle Erosion and Attrition in CSP Systems

In CSP systems using solid particles for heat transfer, erosion from the falling particles can damage the system components upon impact, and from sliding against the component walls. Furthermore, the resulting attrition of particles can change the thermal performance due to alterations in particle morphology. The research on these issues has been limited to industrial applications, and don’t necessarily coincide with the operating conditions in CSP systems. In this work, we investigated the durability of the particles selected as the heat transfer media, as well as special substrate materials that are of interest as lining materials to the particle storage tanks and hoppers. Three different erosion phenomena were studied: impact, abrasion, and attrition erosion. The low-temperature experiments revealed negligible losses from attrition and abrasion erosion. Although the substrates indicated visible surface damage from impact erosion, the actual material mass loss was small even after a throughput of 500kg of particles 63 days of 1MW CSP plant operation assuming 14 hours per day of operation. Erosion is typically classified as impact, abrasion, or attrition erosion. For example, the CSP systems utilizing solid particles as heat transfer media will likely experience impact erosion on the receiver hopper and heat exchanger walls as the solid particles fall from the reservoir. Additionally, there will be sliding erosion along the receiver walls as particles move through the hopper, and lastly, there will also be attrition erosion as the particles rub against each other. The extent of erosion depends on many factors including but not limited to particle shape and size, material hardness/brittleness and ductility, and particle impact speed and angle. Mechanistic erosion equations that are available in the literature are mostly derived from data pertaining to specific experiments and therefore can’t be applied to all applications without suitable adjustments. Survey of the literature relating to particle-based receivers revealed that the most prevalent approach has been to choose low velocities to limit erosion, but to our knowledge, little effort has been put in to fully characterize erosion at the expected operating conditions. A relatively recent work investigated the erosion of wire mesh proposed for use in a particle receiver, where the results actually showed an increase in mass as oxidation occurred on the mesh surface but the work did not investigate the particle attrition rate, and the erosion rate of a solid substrate. The end goal of this work is to develop a comprehensive particle and substrate durability model that will allow a comprehensive understanding of particle-based CSP operating conditions on component durability.

14 SOLAR ENERGY↗

Experimental Safe Extremum Seeking for Accelerators

Here, we demonstrate the recent designs of safe extremum seeking (Safe ES) on the 1-km-long charged particle accelerator at the Los Alamos Neutron Science Center (LANSCE). Safe ES is a modification of extremum seeking (ES) which, in addition to minimizing an analytically unknown cost, also employs a safety filter based on an analytically unknown control barrier function (CBF) safety metric. Tuning is necessitated by accelerators being large complex systems, with many drifting parameters due to thermal effects and degradation. At the same time, safe operation (the maintenance of state constraints) is crucial, as damage brings astronomical costs, both financially and in operation downtime. Our measured (but analytically unknown) safety metric is the beam current. We perform multivariable Safe ES on three accelerator applications, in which we adapt 4, 6, and 3 magnet strength parameters, respectively. Two of the three applications are for validated simulation models of beamlines at LANSCE: the first for the proton radiography (pRad) beamline of 800-MeV protons for spot size tuning; the second on a high-performance code, HPSim, for tuning the low-energy beam transport (LEBT) region that contains a beam of 750-keV protons. The third is an experimental tuning of the steering magnets in the LEBT at LANSCE.

43 PARTICLE ACCELERATORS↗

Influence of Oxygen Flow and Stoichiometry on Optical Properties and Damage Resistance of Hafnium Oxide Thin Films

Hafnium oxide (HfO 2 ) is predominantly used as a high-index material in multi-layer dielectric coatings for high-peak- and high-average-power lasers, but laser damage often initiates within the HfO 2 layers despite their wide bandgap. Oxygen deficiency during deposition can introduce vacancy-related sub-bandgap states and absorptive defects, lowering damage resistance. This study investigates how oxygen flow during HfO 2 deposition with ion beam sputtering (IBS) affects its stoichiometry, defect formation, and nanosecond laser-induced damage threshold (LIDT) and whether single-layer trends predict multilayer performance. Single layers were deposited at varying oxygen flows, characterized for optical and structural properties, and tested for the LIDT at 1064 nm and 355 nm. Increasing oxygen flow drove the layer toward near-stoichiometric HfO 2 , reduced the refractive index, and altered the density of surface pinhole-like features. The single-layer LIDT at 355 nm increased with oxygen, whereas the 1064 nm LIDT was comparatively less sensitive to oxygen flow, consistent with the wavelength-dependent roles of absorptive precursors and microstructural defects. In contrast, a HfO 2 -based high-reflector (HR) showed a higher LIDT at lower oxygen flow, indicating that the family of damage precursors changes between single layers and multilayers; in stacks, structural properties such as stress, gas entrapment and thermal dissipation may outweigh the isolated absorptive defects found in single layers. These results demonstrate that the optimal oxygen flow condition depends on both LIDT wavelength and film architecture. We identified, for single layers, a 15–35 sccm window for maximizing the 1064 nm LIDT and a high-flow optimum (45 sccm) for the 355 nm LIDT and, for 355 nm HR stacks, a distinct lower-flow regime (~10 sccm).

Optics and optical instruments↗

Spark Channel Dynamics of Electrostatic Discharges

When two differently-charged objects are brought in close proximity to each other, the resulting high electric fields can cause electron avalanche breakdown of the air gap separating the objects, a process known as electrostatic discharge (ESD). If enough initial charge is stored on the objects, the electrical breakdown can proceed to ionize the air to such a degree that a highly conductive filament of plasma forms in the gap, known as a spark channel. The spark electrically bridges the air gap, resulting in a rapid pulse of current that neutralizes the charge difference. The current pulse produces significant heating of the gas in the spark, resulting in dissociation, ionization, thermal radiation, and hydrodynamic expansion. ESD presents a hazard to electrically-sensitive devices, with consequences such as economic losses (e.g. damaged electronics) or unsafe response (e.g. unintended ignition of flammable gas mixtures, initiation of detonators, etc.). For this thesis, the ESD spark is taken to occur between two conducting electrodes, with the spark channel being axisymmetric in a cylindrical coordinate system centered on the channel. An RLC-type circuit is used for the discharge model of the ESD event. The spark is treated as a time-dependent resistance that is in series with a capacitance, an inductance, and (optionally) a load resistance representing a “victim” component under threat from the ESD event. The primary motivation of this work is to use a numerical hydrodynamic model to understand the energy dissipation and transport processes in the spark. The model consists of the compressible Euler equations of mass, momentum, and energy conservation together with an Eddington/P1 approximation for thermal radiation transport. To close the hydrodynamic system, an equation of state (EOS) was fitted from tabular data for air that accounts for the dissociation and ionization of air species. The hydrodynamic equations are solved using a conservative Lagrangian finite volume method. These partial differential equations are coupled to the circuit equations by calculation of the spark resistance via numerical integration of the electrical conductivity of the channel. Computational results are compared against experimental measurements of discharge current and radial density of the spark channel.

42 ENGINEERING↗

Plasma Electrolytic Oxidation (PEO) Coatings as Superior Thermal Barriers for Engine Pistons. Final Report

Thermal barrier coatings (TBCs) have received considerable interest in internal combustion engines, as a means to increase overall efficiency. However, despite some promising results for coatings with adequate thermal properties, durability has remained a barrier to commercialization, which has damped interest from automotive manufacturers. The PEO-based TBC developed by IBC Materials has exceptional durability, and thermal properties comparable or superior to state of the art. In this Phase I effort, IBC has demonstrated this durability by coating pistons from a current production engine (Kohler KD440) and conducting thermal shock testing on several coated pistons. Following successful thermal shock testing, a piston was run in this engine for an extended period(>120h) and showed no evidence of damage to the piston coating or engine bore. The PEO-based TBC also increased heat rejection from the combustion chamber, resulting in significantly increased exhaust temperature. Operation of the engine with PEO-based TBCs was also found to delay the onset of fuel ignition, possibly due to reduced heat retention by the piston. After slightly modifying the engine operation to counteract this effect, a modest improvement (+0.8%) to overall efficiency was achieved. With additional tuning of coating parameters and combustion timing, it is very likely that additional gains can be realized. This result also points to the possibility of future designs which require less capacity from the cooling system (e.g. a radiator), which draws energy and adds mass and complexity to an overall powertrain.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

D retention and depth profile behavior for single crystal tungsten with high temperature neutron irradiation

Single crystalline W (tungsten) samples irradiated at 633, 963 and 1073 K by neutrons to a damage level of 0.1 dpa were exposed to a high-flux D (deuterium) plasma at 673, 873 and 973 K, respectively, in TPE (Tritium Plasma Experiment) at INL (Idaho National Laboratory). Deuterium desorption was analyzed by TDS (Thermal Desorption Spectroscopy), and D depth profiles were determined by NRA (Nuclear Reaction Analysis) at SNL (Sandia National Laboratories). HIDT (Hydrogen Isotope Diffusion and Trapping) simulation code was applied to evaluate D behavior for neutron-damaged W at higher temperature. The D retention at depths up to 3 f.tm for the neutron-damaged sample at 673 K was two orders of magnitude larger than that for undamaged tungsten, and its D desorption spectrum had a single broad stage at around 900 K. As the neutron irradiation/plasma exposure temperature increased, D retention was largely reduced, and the desorption temperature was increased to higher temperatures above 1100 K. The D depth profiles by NRA also showed D migration toward bulk by higher temperature irradiation, compared to undamaged W. The HIDT simulation indicated that the major binding energy of D was changed from 1.43 eV to 2.07 eV at higher neutron irradiation and plasma exposure temperatures, suggesting that some vacancies and small vacancy clusters would aggregate to form larger voids, or depopulation of weak traps at high D plasma exposure temperatures. It can be said that more stable trapping sites played dominant roles in the D retention at higher neutron irradiation and plasma exposure temperature. The binding energy by HIDT simulation was almost consistent with the reported value by TMAP, but the consideration of not only total D retention measured by TDS but also D depth profile by NRA led to the more accurate D behavior in neutron-damaged W.

36 MATERIALS SCIENCE↗