Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Stainless Steel”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 271 records · Page 15

Documentation of Stainless Steel Lithium Circuit Test Section Design

The Early Flight Fission-Test Facilities (EFF-TF) team was tasked by Naval Reactors Prime Contract Team (NRPCT) to design, fabricate, and test an actively pumped lithium (Li) flow circuit. This Li circuit takes advantage of work in progress at the EFF TF on a stainless steel sodium/potassium (NaK) circuit. The effort involved modifying the original stainless steel NaK circuit such that it could be operated with Li in place of NaK. This new design considered freeze/thaw issues and required the addition of an expansion tank and expansion/extrusion volumes in the circuit plumbing. Instrumentation has been specified for Li and circuit heaters have been placed throughout the design to ensure adequate operational temperatures and no uncontrolled freezing of the Li. All major components have been designed and fabricated prior to circuit redesign for Li and were not modified. Basic circuit components include: reactor segment, Li to gas heat exchanger, electromagnetic liquid metal pump, load/drain reservoir, expansion reservoir, instrumentation, and trace heaters. The reactor segment, based on a Los Alamos National Laboratory 100-kW design study with 120 fuel pins, is the only prototypic component in the circuit. However, due to earlier funding constraints, a 37-pin partial-array of the core, including the central three rings of fuel pins (pin and flow path dimensions are the same as those in the full design), was selected for fabrication and test. This Technical Publication summarizes the design and integration of the pumped liquid metal Li flow circuit as of May 1, 2005. This supplement contains drawings, analysis, and calculations

Godfroy, Thomas J.↗

Interpretation of Ion Irradiation and Neutron Irradiation Damage in Additively Manufactured 316 Stainless Steel using Multiscale Modeling

The accelerated adoption of nuclear energy necessitates advanced manufacturing technologies, such as additive manufacturing, to meet heightened supply chain requirements and support innovative reactor technologies. Due to the unique microstructural characteristics of additively manufactured materials under distinct solidification conditions, comprehensive evaluation of their performance in reactor environments is essential. The Advanced Materials and Manufacturing Technologies program under the Department of Energy's Office of Nuclear Energy focuses on understanding the irradiation performance and damage evolution of laser powder bed fusion 316 stainless steel, with an emphasis on integrating ion and neutron irradiation data to accelerate the development and qualification of materials for advanced nuclear reactor applications. While ion irradiation is a cost- and time-effective method, modeling and simulation are required to interpret the data for the broader range of irradiation conditions encountered in advanced reactors. In fiscal year 2025, integrated multiscale modeling and simulations were conducted to assess irradiation damage in additively manufactured 316 stainless steel. Key outcomes include predictions of chromium enrichment at grain boundaries, nickel enrichment at dislocation cell walls and void surfaces, and heterogeneous void evolution under ion and neutron irradiation conditions. Cluster dynamics simulations revealed the coarsening of voids at high irradiation temperatures and the suppression of void growth by high network dislocation density, while also demonstrating significant growth and coarsening of voids and self-interstitial atom loops at low dose rates. Machine learning-accelerated atomistic simulations highlighted the impact of the local environment and chromium concentration on vacancy diffusivity, providing key insights on the influence of composition on void swelling and radiation-induced segregation. Additionally, molecular dynamics simulations demonstrated the presence of defect production bias and a significant effect of carbon content on defect cluster behavior. These combined efforts aim to predict the performance of additively manufactured materials under various reactor conditions, supporting their qualification for nuclear reactor applications by interpreting ion irradiation data. This report underscores the potential of integrated multiscale modeling to analyze ion irradiation data in the effort to accelerate the qualification of additively manufactured materials for nuclear reactor components.

316 stainless steel↗

Detecting Thermally-Induced Spinodal Decomposition with Picosecond Ultrasonics in Cast Austenitic Stainless Steels

Destructive techniques to monitor nuclear reactor component health may not always be available during service, as they are time-consuming and often require pre-installed inspection coupons. Non-destructive evaluation (NDE) techniques can bridge this gap by rapidly identifying the state of mission-critical reactor components, via inference between NDE-measurable material properties and those of ultimate interest, such as ductility and toughness. Here, we demonstrate one such inference about the health of thermally aged cast austenitic stainless steels. Observations of surface acoustic wave peak (SAW) splitting correlate with spinodal decomposition-induced embrittlement as destructively measured by Charpy impact energy. Elastodynamic calculations and molecular dynamics simulations of the effects of spinodal decomposition on elastic moduli support that the new acoustic modes present are due to stiffening in the δ-ferrite domains. Finally, this discovery enables one to probe structure-property relationships in materials in a greatly accelerated manner, suggesting that similar inference methods can be used to determine material fitness-for-service, or to quickly uncover new structure-property relationships.

304-type stainless steel↗

Hydrogen embrittlement of additively manufactured austenitic stainless steel 316 L

Additive manufacturing (AM) is a promising means of production of austenitic stainless steel (SS) parts for hydrogen service. The hydrogen embrittlement resistance of SS 316 L parts manufactured by powder-bed-fed selective laser melting (SLM) and directed energy deposition (DED) was examined using slow strain rate tensile testing. The influence of the hierarchical AM microstructures on mechanical response, microstructural evolution, and void formation were analyzed using multiscale electron microscopy. Furthermore, the presence of hydrogen reduced ductility in as-built DED materials, but did not significantly influence the response in as-built SLM material or heat-treated materials. Microstructural features driving these different responses are discussed.

36 MATERIALS SCIENCE↗

Understanding a novel form of intergranular corrosion of stainless steel 316L exposed to molten LiCl-Li 2 O-Li

We report stainless steel 316 L exposed to LiCl-Li2O molten salt containing Li metal for 500 and 1000 h experiences deep intergranular attack and bulk void formation. This degradation is due to a synergistic corrosion mechanism, different than other forms of molten salt corrosion, where Cr and Mn oxides and carbides form along grain boundaries and are dissolved by Li metal. Synchrotron transmission X-ray microscopy 3D imaging is used to show corrosion morphology and Cr enrichment and depletion in a novel format that has not previously been used for bulk corrosion samples.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Shock compression of single-crystal austenitic FeCr18Ni12.5 stainless steel to 60 GPa

We measured the austenitic FeCr18Ni12.5 stainless steel Hugoniot as a function of crystallographic direction to approximately 60 GPa. We shock-compressed FeCr18Ni12.5 samples oriented along $\langle$100$\rangle$, $\langle$110$\rangle$, and $\langle$111$\rangle$ to mean stresses ranging 30.5–58.1 GPa via Ta plate impact in a large-bore powder gun and measured the free-surface velocities with laser interferometry. We unambiguously observed the largest post-shock free-surface velocity along $\langle$100$\rangle$ in each experiment, which consequently produced the lowest shock velocity along that orientation. However, the propagation of experimental uncertainties through the impedance matching scheme used to compute the shock velocity produced sufficient uncertainty overlap to preclude definitive conclusion of Hugoniot anisotropy.

36 MATERIALS SCIENCE↗

Caustic Neutralization and Precipitation of Acidic Dissolved Simulated Stainless Steel–Clad Plutonium and Plutonium/Uranium Nuclear Fuel

Simulated dissolved stainless steel (SS) clad Pu and Pu/U nuclear fuel in HNO 3 was neutralized to a free hydroxide (OH - ) concentration of 0.6 M. A thermal neutron poison, Gd, was added to the simulants at concentrations of either ~3 - 6 g/L or ~37 - 38 g/L. The supernate Pu concentration the day of neutralization ranged from 0.48 to 8.75 mg/L. The supernate Pu concentration of a simplified simulant neutralized to 0.6 M OH - above precipitated solids containing Pu was demonstrated to decrease over 18 days. A significant portion of precipitated Pu was found to be insoluble in 8 M HNO 3 at ambient temperature, but essentially quantitative Pu dissolution was achieved in 11.5 M HNO 3 /0.1 M KF at 100 °C. The difficulty in dissolving the Pu precipitate is believed to be due to the formation of refractory PuO 2 •xH 2 O during the neutralization process. Initial Gd concentrations of ~37 – 38 g/L were found to result in a greater Al precipitation when neutralized to 0.6 M OH - than initial Gd concentrations of ~3 – 6 g/L. Physical properties of the resultant slurries were measured and used to calculate limiting flowrates and slurry velocities by gravity only in transfer piping between the Savannah River Site’s H-Canyon Facility and the Concentration, Storage, and Transfer Facility (CSTF). These results were compared to calculated deposition velocities to predict if solids would settle during the transfer. The Newtonian model was found to be reasonable for each diluted slurry evaluated. Deposition velocities of Pu containing slurries are lower than nuclear fuel slurries primarily composed of U due to the high density of Pu solids. In conclusion, dilution of slurries reduces the margin between the slurry and deposition velocities due to the reduction in viscosity because higher viscous forces on the particles promote maintained suspension.

Actinide Neutralization↗

Stainless-steel elbows formed by spin forging

Large seamless austenitic stainless steel elbows are fabricated by spin forging /rotary shear forming/. A specially designed spin forging tool for mounting on a hydrospin machine has been built for this purpose.

Source record↗

Stabilizing stainless steel components for cryogenic service

Warpage and creep in stainless steel valve components are decreased by a procedure in which components are machined to a semifinish and then cold soaked in a bath of cryogenic liquid. After the treatment they are returned to ambient temperature and machine finished to the final drawing dimensions.

Holden, C. F.↗

Forming "dynamic" membranes on stainless steel

"Dynamic" zirconium polyacrylic membrane is formed directly on stainless steel substrate without excessive corrosion of steel. Membrane is potentially useful in removal of contaminated chemicals from solution through reversed osmosis. Application includes use in filtration and desalination equipment, and in textile industry for separation of dyes from aqueous solvents.

Brandon, C. A.↗

Method of forming dynamic membrane on stainless steel support

A suitable member formed from sintered, powdered, stainless steel is contacted with a nitrate solution of a soluble alkali metal nitrate and a metal such as zirconium in a pH range and for a time sufficient to effect the formation of a membrane of zirconium oxide preferably including an organic polymeric material such as polyacrylic acid.

Gaddis, Joseph L.↗

Observations of Atmospheric Corrosion Testing on Heated Austenitic Stainless Steel Surfaces: Exploring the Role of Inert Dust Particulates and Seawater

Relevant atmospheric corrosion laboratory testing environments were developed to explore the influence of inert dust and seawater on the corrosion susceptibility of stainless steel in spent nuclear fuel dry storage conditions. Measurements from dust collected on in-service dry storage canisters were applied to develop exposure conditions. Three atmospheric exposure conditions, two static and one cyclic, were examined with three different surface coverages: co-deposited large dust and seawater, co-deposited small dust and seawater, and solely seawater. Stainless steel coupons representative of spent nuclear fuel dry storage canister material were subjected to the various corrosion environments, with the results from exposures up to 1 year presented here. Post exposure, corrosion damage was analyzed using optical microscopy, scanning electron microscopy, and energy dispersive X-ray spectroscopy. Initial observations are presented herein, and potential implications with respect to the influence of inert dust particles on corrosion susceptibility are summarized. In general, the co-deposition of dust and salt resulted in larger pits and exhibited mixed modes of corrosion that were not observed in the no-dust conditions (i.e., crevicing, filiform, and pits within pits). The presence of the inert dust may influence brine spreading and/or act as crevice formers, leading to enhanced corrosion. This study highlights the significance of incorporating dust particulate(s) beyond the deliquescent chemistries to fully evaluate atmospheric corrosion severity.

Sea salt↗

A FEASIBILITY STUDY ON CRACK REPAIR IN AUSTENITIC STAINLESS STEEL DRY STORAGE CANISTERS USING ISOTHERMAL FRICTION STIR WELDING

In recent time, solid state crack repair techniques in spent nuclear fuel dry storage canisters (SNF-DSC) have garnered significant interest. Plates of austenitic stainless steels are usually arc welded to fabricate the cylindrical canisters which are prone to chloride-induced stress corrosion cracking. Friction stir welding (FSW) is considered to be a potential candidate for damage repair. In this work, electrical discharge machining was used to simulate cracks in 304L stainless steel plates of 12.7 mm thickness. Subsequently, isothermal FSW was carried out at two different temperatures (725 and 825°C) in order to repair the simulated crack. Microstructure-mechanical property correlations in FSWed plates were studied in detail. Significant grain refinement observed in the stir zone (SZ) was attributed to dynamic recrystallization occurring during FSW. A comparison of Vickers microhardness showed higher hardness and homogeneity in the 725°C SZ than its 825°C counterpart. The fraction of S3 boundary is found to be low in the SZ as compared to base metal (BM). Yield strength of the joints was found to be approximately 100 MPa higher than that of the BM accompanied by a drop in ductility by a factor of 2. Residual stress profile across 825°C weld was measured using x-ray diffraction.

Bhattacharyya, Madhumanti↗