Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Spinel”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 271 records · Page 15

Amphibole and hercynite spinel in Shergotty and Zagami Magmatic water, depth of crystallization, and metasomatism

Amphibole and spinel occur in the Shergotty and Zagami meteorites only in magmatic inclusions in pigeonite. The trapped magma is essentially identical to the parental magmas for Shergotty and Zagami. The amphibole is a kaersutite with minimal halogen content; by inference, it must have been hydrous. If so, the Shergotty and Zagami melts contained at least 0.2 wt pct H2O and were probably H2O-undersaturated. Pressures in excess of 1 kilobar seem necessary for the formation of amphibole. Spinel replaces magnetite in the inclusions, and olivine replaces magnetite elsewhere in the meteorites. To stabilize spinel, the melt in the inclusions must have become enriched in Al during fractionation, possibly because the small volume of the inclusions made nucleation of plagioclase unlikely. Pervasive replacement of magnetite through reduction reactions suggests that Shergotty and Zagami interacted with hydrogen-rich fluids during their cooling.

Treiman, A. H.↗

A refractory inclusion in the Kaba CV3 chondrite - Some implications for the origin of spinel-rich objects in chondrites

The first detailed petrographic and mineralogical study of a Ca, Al-rich inclusion (CAI) from the Kaba CV3 chondrite is reported. This 'fine-grained' CAI contains abundant small, rounded, rimmed, spinel-rich objects which have important features in common with the spinel-rich objects in other carbonaceous and ordinary chondrites. These nodules are interpreted as fractionated distillation residues of primitive dust. However, the available data do not unambiguously rule out a condensation origin for at least some of these objects. Finally, the preservation of distinct diopside-hedenbergite rims on the spinel-rich bodies and the small grain size of many minerals in the CAI matrix material both suggest that the CAI accreted cool and had a relatively cool thermal history in the Kaba parent body.

Fegley, B., Jr.↗

The distribution of chromium among orthopyroxene, spinel and silicate liquid at atmospheric pressure

The Cr distributions for a synthetic silicate melt equilibrated with bronzitic orthopyroxene and chromite spinel between 1334 and 1151 C over a range of oxygen fugacities between the nickel-nickel oxide and iron-wuestite buffers are studied. The occurrence, chemical composition, and structure of the orthopyroxene-silicate melt and the spinel-silicate melt are described. It is observed that the Cr content between bronzite and the melt increases with falling temperature along a given oxygen buffer and decreases with falling oxygen fugacity at a given temperature; however, the Cr content of the melt in equilibrium with spinel decreases with falling temperature and increases with lower oxygen fugacity.

Barnes, S. J.↗

A unique, (almost) unaltered spinel-rich fine-grained inclusion in Kainsaz

A unique, spinel-rich, extremely porous fine-grained inclusion in the Kainsaz (CO3) meteorite is reported. This inclusion is the least altered fine-grained inclusion yet discovered, having escaped almost entirely the secondary alterations experienced by Allende fine-grained inclusions. The inclusion is comprised of loosely packed 5-30 microns spinel grains mantled by thin layers of melilite, anorthite, and diopsidic pyroxene. The inclusion, which has over 30 vol pct void space, is one of the most spinel-rich, most porous fine-grained inclusions seen to date. The mineralogy of the inclusion matches that which has been predicted for a precursor of the altered mineral assemblages of Allende fine-grained inclusions, though a lack of interstitial material in the Kainsaz inclusion reduces the likelihood of a direct genetic relationship between the two (Allende fine-grained inclusions contain abundant interstitial material). Its mineralogical composition confirms that the precursors of other, more altered, fine-grained inclusions were assemblages of refractory minerals exclusively.

Holmberg, B. B.↗

S-asteroids 387 Aquitania and 980 Anacostia - Possible fragments of the breakup of a spinel-bearing parent body with CO3/CV3 affinities

Asteroids 387 Aquitania and 980 Anacostia are anomalous members of the S-class. Their reflectance spectra exhibit a strong broad absorption feature longwards of 1.5 micron and no significant feature near 1 micron. Their spectra indicate the presence of spinel, an aluminum-magnesium oxide mineral commonly present in inclusions in CV3 and CO3 meteorites. Spinel probably makes up only a small percentage of the surface assemblages of these asteroids, but its spectral effect may be enhanced by its presence in fine-grained white inclusions in immature asteroid regoliths. It is speculated that Aquitania and Anacostia represent material formed in the same nebular zone as the CV3 and CO3 chondrites but either: (A) at an earlier time in the nebula when such inclusions might have been a relatively larger fraction of the nebular grain population; or (B) in local regions where nebular processes (e.g., settling to the midplane) had concentrated such inclusions. The close similarity of two orbital elements (a, i) suggests that Aquitania and Anacostia may be members of a partially dispersed asteroid family produced by the early disruption of a spinel-bearing parent body.

Burbine, Thomas H.↗

Identification of Presolar Spinel Grains from a Murray Residue by Multi-Detection Raster Imaging

Grain size separate CG from the Murray CM2 carbonaceous chondrite contains mostly spinel grains of average diameter 0.5 m. Zinner et al. found that approximately 1% of these spinel grains are of presolar origin as determined by their large O isotopic anomalies. These O isotopic measurements were made with the NanoSIMS on individual grains that were well separated from one another on a gold foil. The grains were selected for analysis from secondary electron and secondary O-16(-) images. The primary beam was then successively deflected onto these single grains for O isotopic analysis. While single grain analysis on dispersed samples is effective for finding relatively abundant anomalous grains, ion imaging in a raster mode on tightly packed grains might be more efficient for locating few anomalous grains among predominantly isotopically normal grains. In fact, this was the analysis mode used by Messenger et al. to discover presolar silicates in interplanetary dust particles. In an exploratory effort that is also geared toward establishing the optimum isotopic imaging technique in the search for presolar silicate grains in primitive meteorites, we measured O isotopic ratios in spinel grains from the Murray CG separate by raster imaging of areas with more or less tightly packed grains.

Nguyen, A.↗

Comparative Planetary Mineralogy: Valence State Partitioning of Cr, Fe, Ti, and V Among Crystallographic Sites in Olivine, Pyroxene, and Spinel from Planetary Basalts

We have considered the valence-state partitioning of Cr, Fe, Ti, and V over crystallographic sites in olivine, pyroxene, and spinel from planetary basalts. The sites that accommodate these cations are the M2 site (6-8 coordinated) and M1 site (6 coordinated) in pyroxene, the M2 site (6-8 coordinated) and M1 site (6 coordinated) in olivine, and the tetrahedral and octahedral sites in spinel. The samples we studied are basalts from Earth, Moon, and Mars, which have fO2 conditions that range from IW-2 (Moon) to IW+6 (Earth) with Mars somewhere between at IW to IW+2. In this range of fO2 the significant elemental valences are (from low to high fO2) Ti4+, V3+, Fe2+, Cr2+, Cr3+, V3+, V4+, and Fe3+. V2+ and Ti3+ play a minor role in the phases considered for the Moon, and are probably in very low concentrations. V5+ plays a minor role in these phases in terrestrial basalts because it is probably in lower abundance than V4+ and it has an ionic radii that is so small (0.054 nm, 6- coordinated,[1]) that it is almost at the lower limit for octahedral coordination. The role of Cr2+ in the Moon is significant, as Sutton et al. [2] found that lunar olivine contains mostly Cr2+ while coexisting pyroxene contains mostly Cr3+. Hanson one vacancy only accommodates one V4+. Thus more vacancies are required in V4+ substitutions into olivine. In the Moon V3+ is much more abundant than V4+ [7, 8]. Thus in lunar chromite V3+ follows Cr3+, whereas in Earth V4+ (which is much greater in abundance than V3+) follows Ti4+ (eg in ulv spinel). We could go on in this vein for some time but space limitations do not permit us to do so.

Papike, J. J.↗

An Integrated, Layered-Spinel Composite Cathode for Energy Storage Applications

At low operating temperatures, commercially available electrode materials for lithium-ion batteries do not fully meet the energy and power requirements for NASA fs exploration activities. The composite cathode under development is projected to provide the required energy and power densities at low temperatures and its usage will considerably reduce the overall volume and weight of the battery pack. The newly developed composite electrode material can provide superior electrochemical performance relative to a commercially available lithium cobalt system. One advantage of using a composite cathode is its higher energy density, which can lead to smaller and lighter battery packs. In the current program, different series of layered-spinel composite materials with at least two different systems in an integrated structure were synthesized, and the volumetric and gravimetric energy densities were evaluated. In an integrated network of a composite electrode, the effect of the combined structures is to enhance the capacity and power capabilities of the material to levels greater than what is possible in current state-of-the-art cathode systems. The main objective of the current program is to implement a novel cathode material that meets NASA fs low temperature energy density requirements. An important feature of the composite cathode is that it has at least two components (e.g., layered and spinel) that are structurally integrated. The layered material by itself is electrochemically inactive; however, upon structural integration with a spinel material, the layered material can be electrochemically activated, thereby delivering a large amount of energy with stable cycling. A key aspect of the innovation has been the development of a scalable process to produce submicronand micron-scale particles of these composite materials. An additional advantage of using such a composite electrode material is its low irreversible loss (.5%), which is primarily due to the unique activation of the composite. High columbic efficiency (greater than 99%) upon cycling may indicate the formation of a stable SEI (solid-electrolyte interface) layer, which can contribute to long cycle life. The innovation in the current program, when further developed, will enable the system to maintain high energy and power densities at low temperatures, improve efficiency, and further stabilize and enhance the safety of the cell.

Hagh, Nader↗

Complex Intergrowths of Non-Stoichiometric Defect-Structured Hibonite and Al-Rich Spinel in an Allende Ca-Al-Rich Inclusion

Hibonite is a primary ultra-refractory mineral occurring in many Ca-Al-rich inclusions (CAIs) and is predicted to condense as the second major phase from a cooling gas of solar composition. Our previous microstructural studies of hibonite in carbonaceous chondrites revealed its unique microstructures consisting of numerous defects that contain Mg-enriched, wider spinel blocks in stoichiometric hibonite. Han, J. et al. [2 items] demonstrated experimentally that defect-structured hibonites can grow easily in the presence of minor Mg and are kinetically more stable than equilibrium assemblages predicted by thermodynamic calculations. However, a thermo-dynamic vs. structural stability of defect-structured hibonite relative to other early-condensed Al-rich phases such as corundum, grossite, and spinel remains poorly constrained. Here, we present the results of atomic resolution TEM (Transmission Electron Microscopy) imaging of hibonite in a compact Type A CAI in the Allende CV3 chondrite in order to better understand the crystal structure and chemistry of defect-structured hibonite and its associated Al-rich phases, especially non-stoichiometric, Al-rich spinel, in the context of the formation of first refractory solids in the early solar nebula.

Han, J.↗

Preliminary Characterization of Spinel Troctolite Clast Identified in Apollo Next Generation Sample Analysis (ANGSA) Core 73002

The lunar magnesian (Mg-) suite is a diverse lithological group composed of Mg-rich mafic minerals. The Mg-suite consists primarily of troctolites, norites, gabbronorites, and spinel troctolites. These rocks exhibit contradictory geochemical traits, with mafic minerals bearing high Mg# (molar 100×Mg/[Mg+Fe]) indicating primitive parental magmas, but also plagioclase saturation and enrichments in incompatible trace elements (i.e., KREEP) indicate more evolved parental magmas. A variety of models have been invoked to explain the occurrence and petrogenesis of the Mg-suite. Here, we report on a new spinel troctolite clast found in Apollo Next Generation Sample Analysis (ANGSA) program core 73002. Sample 73002 was acquired at Station 3 during Apollo 17 as the upper part of a double-drive tube with sample 73001. During processing, the spinel troctolite clast (0.066 g) was found at the 4.0–4.5 cm depth interval.

A. C. Stadermann↗

Method of microbially producing metal gallate spinel nano-objects, and compositions produced thereby

A method of forming a metal gallate spinel structure that includes mixing a divalent metal-containing salt and a gallium-containing salt in solution with fermentative or thermophilic bacteria. In the process, the bacteria nucleate metal gallate spinel nano-objects from the divalent metal-containing salt and the gallium-containing salt without requiring reduction of a metal in the solution. The metal gallate spinel structures, as well as light-emitting structures in which they are incorporated, are also described.

36 MATERIALS SCIENCE↗

Layered-spinel electrodes for lithium batteries

An electrode for a lithium-ion cell comprising a ‘layered-spinel’ composite oxide material is disclosed. The ‘layered-spinel’ can be a material of formula xLiMO2.(1−x)LiyM′zO4, wherein 0 < x < 1; LiMO2 is a lithium metal oxide having a layered structure in which M comprises one or more transition metals and optionally lithium, and has a combined average oxidation state of +3; and LiyM′zO4 is a lithium metal oxide having a spinel structure, 1≤y≤1.33, 1.66≤z≤2, and M′ comprises one or more transition metals, and has a combined average metal oxidation state in the range of about +3.5 to about +4.

25 ENERGY STORAGE↗

Reduced-temperature sintering of spinel-type coatings and layers with metallic alloy powder precursors

A method of forming a spinel coating on a substrate is disclosed including the steps of coating at least a portion of the substrate with a precursor including an alloy powder, and sintering the precursor at a temperature of less than 1000 degrees Celsius to form the spinel coating. The alloy powder used for the precursor can include particles having a particle size of less than 10 micrometers. The method can be utilized to form spinel coatings as contact surfaces between electrodes and interconnects of solid oxide fuel cell (SOFC) stacks.

Zhu, Jiahong↗

High-temperature thermochemical energy storage materials using doped magnesium-transition metal spinel oxides

High-temperature thermochemical energy storage materials using doped magnesium-transition metal spinel oxides are provided. —transition metal spinel oxides, such as magnesium manganese oxide (MgMn) 3 O 4 , are promising candidates for high-temperature thermochemical energy storage applications. However, the use of these materials has been constrained by the limited extent of their endothermic reaction. Embodiments described herein provide for doping magnesium-transition metal spinel oxides to produce a material of low material costs and with high energy densities, creating an avenue for plausibly sized modules with high energy storing capacities.

Muhich, Christopher↗

DEVELOPMENT OF NOVEL SPINEL REFRACTORIES FOR USE IN COAL GASIFICATION ENVIRONMENTS

Work has been performed by Oak Ridge National Laboratory (ORNL), in collaboration with industrial refractory manufacturer (Minteq International, Inc.), academic research partner (Missouri University of Science and Technology) and end users to employ novel refractory systems and techniques to reduce energy consumption of refractory lined vessels found in industries such as aluminum, chemical, glass, and pulp and paper. The objective of the project was to address the need for new innovative refractory compositions by developing a family of novel MgO-Al 2O3 spinel structured unshaped refractory compositions (castables, gunnables, shotcretes, etc) utilizing new aggregate materials, bond systems, protective coatings, and phase formation techniques. As part of the four-year project funded by the U.S. Department of Energy (DOE), materials have been developed specifically for coal gasification environments. Additionally, work has been performed to develop and apply low cost coatings using a colloidal approach for protection against corrosion attack of the refractory brick and to develop a light-weight back-up refractory system to help offset the high thermal conductivity inherent in spinel materials. This paper discusses the development of these materials, along with preliminary results achieved toward the reduction of chemical reactions and mechanical degradation by the service environment.

01 COAL, LIGNITE, AND PEAT↗

Antiferromagnetic Inverse Spinel Oxide LiCoVO 4 with Spin-Polarized Channels for Water Oxidation

Exploring highly efficient catalysts for the oxygen evolution reaction (OER) is essential for water electrolysis. Cost-effective transition-metal oxides with reasonable activity are raising attention. Recently, OER reactants' and products' differing spin configurations have been thought to cause slow reaction kinetics. Catalysts with magnetically polarized channels could selectively remove electrons with opposite magnetic moment and conserve overall spin during OER, enhancing triplet state oxygen molecule evolution. Herein, antiferromagnetic inverse spinel oxide LiCoVO 4 is found to contain d 7 Co 2+ ions that can be stabilized under active octahedral sites, possessing high spin states S = 3/2 (t 2g 5 e g 2 ). With high spin configuration, each Co 2+ ion has an ideal magnetic moment of 3 µ B , allowing the edge-shared Co 2+ octahedra in spinel to be magnetically polarized. Density functional theory simulation results show that the layered antiferromagnetic LiCoVO 4 studied contains magnetically polarized channels. The average magnetic moment (µ ave ) per transition-metal atom in the spin conduction channel is around 2.66 µ B . Such channels are able to enhance the selective removal of spin-oriented electrons from the reactants during the OER, which facilitates the accumulation of appropriate magnetic moments for triplet oxygen molecule evolution. Finally, the LiCoVO 4 reported has been identified as an oxide catalyst with excellent OER activity.

36 MATERIALS SCIENCE↗

Toward Stable, High‐Energy, Partially Disordered Mn‐Rich Spinel Cathodes by Revealing and Mitigating Surface Degradation

Mn-rich cathodes balance performance and sustainability but suffer from limited cyclability due to Mn dissolution and cathode-to-anode crosstalk. The Jahn-Teller (J-T) effect of Mn 3+ is often linked to the above phenomena, such as in spinel LiMn 2 O 4 . However, in typical voltage ranges, significant Mn 3+ only appears near the end of discharge, highlighting the need to reassess its role in driving Mn dissolution, structural degradation, and battery performance. Here, the spinel cathode's degree of disorder is tailored to expand the Mn redox range, enabling segmentation into J-T active and less active voltage ranges. Cycling at segmented voltage windows reveals surface degradation mechanisms with and without the major J-T effect. Despite a stronger J-T effect below 3.6 V vs. Li/Li + , Mn dissolution is less significant than above 3.6 V. Expanding the cycling window to 2.0–4.3 V causes severe degradation as the J-T active range induces a tetragonal phase and Mn 2+ -rich surface, driving Mn dissolution and consuming Li-ion inventory in full cells. Reducing electrolyte acidity minimizes Mn 3+ disproportionation, enabling a stable dopant-free Mn-only cathode with a 250 mAh g −1 specific capacity. These findings demonstrate that full cells using Mn-rich cathodes have the potential to avoid the notorious crosstalk problem through electrolyte engineering.

25 ENERGY STORAGE↗