Strain to failure measurements of Cr coatings with different processing
Differently processed Cr coatings on Zircaloy cladding were assessed for coating strain to failure. This report includes i) quantification of Cr coating strain to failure for several coating variants, ii) incorporation of high throughput analysis developed utilizing artificial intelligence, and iii) develop a hoop direction coating strain to failure testing approach for high temperatures that doesn’t require digital image correlation strain measurements. Room temperature strain to failure measurements indicated that heat treatment had an impact on strain to failure of the coating, with increasing heat treatment temperature increasing the average strain to failure of the Cr coating.