At least 271 records · Page 15

Seismic Strengthening of Carpentry Joints in Traditional Timber Structures

The static and dynamic behavior of timber structures largely depends on their connections. In traditional timber construction, elements are usually connected with carpentry joints based on contact pressure and friction, often with only minor reinforcement generically intended to avoid disassembling. In current practice, interventions for the upgrading of carpentry joints are mainly based on empirical knowledge according to tradition. Often they produce a general strengthening of the connection, but are not specific for the case of seismic action. Strengthening on heuristic bases may be only partially effective or possibly disproportioned. The behavior of the carpentry joints most used in roof structures is examined. The birdsmouth joint, connecting rafters to the tie beam, has been studied first, characterizing its behavior numerically and experimentally in monotonic and cyclic conditions. Other forms of the rafter-to-tie connection, the double notch joint and the case of parallel rafters, are discussed. Some general criteria for the seismic strengthening of these joints are presented.

58 GEOSCIENCES↗

M3FT-16OR020202112 - Report on viability of hydrothermal corrosion resistant SiC/SiC Joint development

Hydrothermal corrosion of four types of the silicon carbide (SiC) to SiC plate joints were investigated under PWR and BWR relevant chemical conditions without irradiation. The joints were formed by metal diffusion bonding using molybdenum or titanium interlayer, reaction sintering using Ti-Si-C system, and SiC nanopowder sintering. Most of the formed joints withstood the corrosion tests for five weeks. The recession of the SiC substrates was limited. Based on the recession rate of the bonding layers, it was concluded that all the joints except for the molybdenum diffusion bond are promising under the reducing activity environments. The SiC nanopowder sintered joint was the most corrosion tolerant under the oxidizing activity environment among the four joints.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Out of Plane Stresses Using a Beam-Based Elastic Foundation Bonded Joint Model

Efficient, semi-analytical models of bonded joints are utilized for initial joint design and sizing due to their convenience and speed. Many of these models are based on beam and plate theories, which are most applicable when in-plane stresses/strains dominate. While this can be a sensible assumption for obtaining the deformations of the joint, out of plane (transverse) stresses are often of critical importance for failure in bonded joints composed of fiber reinforced composite materials. Since through-thickness strains are neglected in these semi-analytical theories, the present study shows a method to back-calculate the out of plane stresses based on stress balance equations, which use the in-plane stresses and displacements that have already been obtained. The method was implemented within the Joint Element Designer (JED) software, and verification and validation examples have been shown. As is typical for these types of models, corner stress singularities are not captured by the JED model, but the general trends of the stress and deformation fields agreed with a higher fidelity finite element model. As such, this method for obtaining out of plane stresses, when coupled with the JED code, is very useful for the complete stress analysis of bonded composite joints.

composites↗

Structural Analysis, Modeling, and Testing of Multi-nut Joint for TriTruss Structure

The Multi-nut joint, developed at NASA Langley Research Center (LaRC), was designed to assemble TriTruss modules for a doubly curved 65.6-feet telescope support structure. Axial and bending tests for a multi-nut joint in the TriTruss structure were conducted to characterize the structural performance of the multi-nut joint and to obtain the installation torque value of the attachment fastener. This paper describes the summary of the axial and bending tests of the multi-nut joint, along with the test results. The equivalent axial stiffness (EA) and equivalent bending stiffness (EI) of the multi-nut joint were characterized based on these test results and are presented in this report. Additionally, finite element models (FEMs) of the axial and bending test specimens were developed, and the predicted axial and bending responses of the multi-nut joint were compared with the test results. Test-analysis comparison results show that the predicted axial load-displacement response of the test specimen was within 5 percent of the test results, while the predicted load-bending response of the test specimen exhibited a consistent trend with the test data.

TriTruss↗

Structural Analysis, Modeling, and Testing of Multi-nut Joint for TriTruss Structure

The Multi-nut joint, developed at NASA Langley Research Center (LaRC), was designed to assemble TriTruss modules for a doubly curved 65.6-feet telescope support structure. Axial and bending tests for a multi-nut joint in the TriTruss structure were conducted to characterize the structural performance of the multi-nut joint and to obtain the installation torque value of the attachment fastener. This paper describes the summary of the axial and bending tests of the multi-nut joint, along with the test results. The equivalent axial stiffness (EA) and equivalent bending stiffness (EI) of the multi-nut joint were characterized based on these test results and are presented in this report. Additionally, finite element models (FEMs) of the axial and bending test specimens were developed, and the predicted axial and bending responses of the multi-nut joint were compared with the test results. Test-analysis comparison results show that the predicted axial load-displacement response of the test specimen was within 5 percent of the test results, while the predicted load-bending response of the test specimen exhibited a consistent trend with the test data.

Structural analysis↗

Microstructure and Mechanical Property Improvement in Laser-Welded TC4 Titanium Alloy and 301L Stainless Steel Joints Without Filler Metal

Pulsed laser welding of Ti alloy to stainless steel (SS) has been applied without filler metal. When the laser beam was focused on the Ti alloy–SS interface, large volumes of Ti-Fe intermetallics were formed in the joint. These Ti-Fe intermetallics were highly brittle, causing the joint to crack spontaneously after welding. The brittle coarse Ti-Fe intermetallics seriously deteriorates the joint strength of Ti alloy and SS; therefore, it is necessary to control the quantities and distributions of brittle Ti-Fe intermetallics in the joint. The amount of melted base materials was controlled by changing laser offset to control the melted proportion and thus control the quantity and distribution of brittle Ti-Fe intermetallics in weld. When laser beam was on the SS side, melting amount of Ti alloy in weld was decreased. When laser beam was on the Ti alloy side, melting amount of SS in weld was decreased. When the laser offset was 0.35 mm away from SS side, the sample realizes the effective connection between Ti alloy and SS. A compound layer was formed at the SS side with the main microstructure of β-Ti and TiFe{sub 2}. The joint fractured at the compound layer with the maximum tensile strength of 182 MPa. Microstructures and mechanical properties of joints were improved by changing laser offset.

36 MATERIALS SCIENCE↗

Creep Deformation and Rupture Behavior of P92 Steel Weld Joint Fabricated by NG-TIG Welding Process

The creep deformation and rupture behavior of P92 steel weld joint fabricated by narrow-gap TIG (NG-TIG) welding process have been investigated at 923 K over a stress range of 80-140 MPa. The prior-austenite grain size, M{sub 23}C{sub 6} precipitate size and hardness have been found to vary significantly in the weld joint. The reduction in hardness from weld metal to base metal with a trough at the outer edge of heat-affected zone (HAZ) has been observed. Coarsening of M{sub 23}C{sub 6} precipitate, recovery of martensite lath dislocation structure and formation of subgrain structure led to lower hardness in the intercritical HAZ. The creep rupture life of NG-TIG weld joint was lower than the base metal, the difference in creep rupture life between base metal and weld joint has been increased significantly with decrease in applied stress. The fracture location in the joint changed from base metal at high-stress regime to the fine grain (FG) HAZ (Type IV cracking) under lower stress level. Fracture in the FGHAZ evidenced the significant reduction in ductility, localized deformation and extensive localized cavitation. Extensive Laves phase formation with significant loss of solution strengthening contribution from tungsten and coarsening of M{sub 23}C{sub 6} precipitate with prolonged creep exposure led to reduction in hardness and more extensive cavitation in the FGHAZ resulting in premature Type IV failure of the weld joint. Weld strength reduction factor about 0.59 has been evaluated for 10{sup 5} h at 923 K.

36 MATERIALS SCIENCE↗

Effect of Welding Parameters on Junction Structure and Fracture Behavior of Friction-Stir-Welded Joints of 2024 Aluminum Alloys

In this paper, the effect of welding speed and tool rotation speed on the junction structure and fracture behavior of friction-stir-welded joints was investigated with use of 2024 aluminum alloys of 3.2 mm thick. Results show that the formation of junction structure is more affected by tool rotation speed than by welding speed due to the differences of heat input levels. When welding speed is at 100 mm/min and tool rotation speed is in the range of 400-600 r/min, the joint junction structure causes complete bonding with no welding defects. While under improper welding parameters, the junction structure causes the precipitate aggregation on the bonding line and the partial bonding with the appearance of both tunnel defects and kissing bond defects. Meanwhile, the results of tensile tests show that the tensile fracture of all FSW joints occur at the weld center. The failure mode of joints with defects-free junction structure characterized by shear fracture is ductile. While the failure mode of joints with defects-existent junction structure characterized by layered fracture surface is brittle. Furthermore, that heterogeneous microstructure, precipitate aggregation and welding defects converge inside the junction structure is the main factor affecting the tensile properties and fracture behavior of the friction-stir-welded joint.

36 MATERIALS SCIENCE↗

Flow Patterns, Microstructure and Mechanical Properties of AZ31/Al6061 Dissimilar Friction Stir-Welded Joints

Dissimilar joints between die-cast AZ31 and extruded Al6061-T6 were joined using friction stir welding technology at a constant transverse speed (50 mm/min) and rotation rate of 800 or 1000 rpm. The flow patterns, microstructure evolution and intermetallic compounds in dissimilar joints were studied by optical and scanning electron microscopy. The relationship between microstructure and tensile properties was analyzed. The microhardness distribution along the horizontal centerline in cross section was investigated. Local flow without obvious mixing existed between Mg and Al metals in the tool shoulder-affected zone. For the tool-pin-affected zone, two typical zones, namely, the “extrusion zone” and “flow zone” existed because of the different flow modes of the plastic metals. The phase analysis showed that intermetallic compounds, including Al{sub 12}Mg{sub 17} and Al{sub 3}Mg{sub 2} formed in banded structures. Phase analysis showed that a joint with welding parameters of 800 rpm and 50 mm/min (Joint-500) had good mechanical properties because of the more uniform microstructure distribution and fewer intermetallic compounds. Fracture analysis indicated some microvoids and lamellate intermetallic compounds in the fracture surface of the joint with welding parameters of 1000 rpm and 50 mm/min (Joint-1000), which deteriorated its tensile strength significantly.

36 MATERIALS SCIENCE↗

Development of Technology for Detachment of Calandria Tube Rolled Joint of Pressurised Heavy Water Reactors

Coolant channel assembly of PHWRs consisting mainly of pressure tube and calandria tube undergoes sag due to irradiation enhanced creep during its life time. Typical service life of the pressure tube is limited to about 15 full power years due to such ageing related degradation. On account of the degradation the pressure tube needs replacement more than twice during the licensed period of reactor operation. As the sag in the calandria tube is also excessive, it has to be replaced to facilitate installation of new and straight pressure tube during retubing and to avoid interference of sagged calandria tube with horizontal reactivity devices. The calandria tube and the tube sheet are joined by sandwich type rolled joints. For detaching the joint an improved technique has been developed that helps to detach the joint without affecting the groove geometry and integrity of the tube sheet. The system works on the principle of fast thermal cycle of heating and cooling of the insert and calandria tube in the rolled joint region while applying axial load to the calandria tube. Though rolled joint detachment by induction heating technique has been in use in CANDU reactors for removal of pressure tubes and calandria tubes, the present design incorporates a liquid nitrogen for faster cooling and simultaneous application of load with a gripping module for detachment and removal of calandria tube and the insert from the tube sheet of end shield in shorter time. This paper describes the methodology of rolled joint detachment, challenges involved in the design, features of the detachment system, findings of experimental trials and observations.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Effect of Ni content in Cu 1-x Ni x coating on microstructure evolution and mechanical properties of W/Mo joint via low-temperature diffusion bonding

The 93W and Mo1 refractory metals were bonded with different Cu 1- x Ni x coating interlayers of various Ni content using plasma-activated sintering at 700 °C. The effects of the Ni content in the Cu 1- x Ni x coating interlayer on the interfacial microstructure evolution and mechanical properties of the W/Mo joints were studied. The maximum average shear strength of the W/Mo joint was 316.5 MPa when the Ni content of the Cu 1- x Ni x coating interlayer was 25 %. When the Ni content of the Cu 1- x Ni x coating interlayer was below 50 %, the atomic diffusion at the W/Mo joint interface was adequate without the formation of intermetallic compounds, as demonstrated by the High Resolution Transmission Electron Microscope analyses of the joints. The presence of Ni in Cu 1- x Ni x promoted diffusion bonding at the interface, which contributed to the high mechanical properties of the W/Mo joint. With an increase in the Ni content of the Cu 1- x Ni x coating interlayer, the MoNi intermetallic compound (IMC) nucleated and grew at the Cu 1- x Ni x coating/Mo1 interface. When the Ni content of the Cu 1- x Ni x coating interlayer was above 50 %, the generation of a brittle MoNi IMC weakened the shear strength of the W/Mo joint dramatically.

36 MATERIALS SCIENCE↗

Hydrothermal corrosion of silicon carbide joints without radiation

In this paper, hydrothermal corrosion of four types of the silicon carbide (SiC) to SiC plate joints were investigated under pressurized water reactor and boiling water reactor relevant chemical conditions without irradiation. The joints were formed by metal diffusion bonding using molybdenum or titanium interlayer, reaction sintering using Ti—Si—C system, and SiC nanopowder sintering. Most of the joints withstood the corrosion tests for five weeks. The recession of the SiC substrates was limited. Based on the recession of the bonding layers, it was concluded that all the joints except for the molybdenum diffusion bond are promising under the reducing environments without radiation. Finally, the SiC nanopowder sintered joint was the most corrosion tolerant under the oxidizing environment among the four joints.

36 MATERIALS SCIENCE↗

A dual-phase microstructural approach to damage and fracture of Ti 3 SiC 2 /SiC joints

We investigate the microcracking mechanisms responsible for Ti 3 SiC 2 /SiC joint damage observed at the macroscopic scale after neutron irradiation experiments in detail. A dual-phase microstructural approach to damage and fracture of Ti 3 SiC 2 /SiC joints is developed that uses a finely discretized two-phase domain based on a digital image of an actual microstructure involving embedded Ti 3 SiC 2 and SiC phases. The behaviors of SiC and Ti 3 SiC 2 in the domain are described by the continuum damage mechanics (CDM) model reported in Nguyen et al., J. Nucl. Mater., 2017, 495:504–515. This CDM model describes microcracking damage in brittle ceramics caused by thermomechanical loading and irradiation-induced swelling. The dual-phase microstructural model is applied to predict the microcracking mechanisms occurring in a typical Ti 3 SiC 2 /SiC joint subjected to heating to 800 °C followed by irradiation-induced swelling at this temperature and cooling to room temperature after the applied swelling has reached the maximum swelling levels observed in the experiments for SiC and Ti 3 SiC 2 . The model predicts minor damage of the joint after heating but significant microcracking in the SiC phase and along the boundaries between SiC and Ti 3 SiC 2 as well as along the bonding joint during irradiation-induced swelling and cooling to room temperature. Our predictions qualitatively agree with the limited experimental observations of joint damage at this irradiation temperature.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Mechanical performance of neutron-irradiated dissimilar transition joints of aluminum alloy 6061-T6 and 304L stainless steel

Bimetallic transition joints using aluminum alloy 6061-T6 and stainless steel 304 L are useful in providing reliable stainless steel welds on nuclear components at temperatures below 200 °C, while maintaining the attractive radiation tolerance of the aluminum alloy. The mechanical performance of inertia welded Al6061-T6:304LSS transition joints was evaluated after neutron irradiation up to 3.45 dpa at 100 °C (maximum) in the High Flux Isotope Reactor to determine the viability of using these transition joints for nuclear and reactor applications. Neutron radiation produced moderate hardening (Δσ y ≈ MPa) with limited change in ductility. Tensile specimens were produced from multiple transition joints and no batch-to-batch variation was found. Finally, tensile responses were found to align with typical responses of wrought Al6061-T6, indicating that the behavior of the joints was dictated by the Al6061-T6 section of the joint.

36 MATERIALS SCIENCE↗

Characterization of bulk stainless steel joints developed through microwave hybrid heating

Processing of metallic materials through microwave heating is a challenging area of research. In the present work, joining of stainless steel-316 to stainless steel-316 in the bulk form has been carried out by placing stainless steel-316 powder at the interface and through targeted heating using microwave hybrid heating. The trials were carried out in a multimode microwave applicator at a frequency of 2.45 GHz and power 900 W. The developed joints were characterized using X-ray diffraction, field emission scanning electron microscopy equipped with energy dispersive X-ray spectroscope and measurement of Vicker's microhardness, porosity and tensile strength. The X-ray diffraction spectrum of the developed joint shows the presence of chromium carbide, iron carbide and iron silicide phases that eventually contribute to enhancement of the microhardness of the joint. The scanning electron microscope micrographs confirm classical metallurgical bonding between the substrate and the interface (molten powder) layer; the epitaxial growth rate was observed adjacent to the fusion zone. The average observed Vicker's microhardness in the joint zone on the grain boundary was significantly higher than that inside the grains due to the presence of various hard phases at the grain boundaries. Evaluation of the tensile strength of the joints showed an average ultimate tensile strength of 425.0 MPa with an average elongation of 9.44%. - Highlights: • Joining of stainless steel (SS-316) plates using microwave hybrid heating • Epitaxial growth rate observed adjacent to the fusion zone of welded joint • The ultimate tensile strength of the order of 425.0 MPa with 9.44% elongation.

36 MATERIALS SCIENCE↗

Temperature-dependent transformation from whisker- to nanoparticle-strengthened composite interface in the Al{sub 2}O{sub 3}/Ag-based alloy system and mechanical properties of the joints

Al{sub 4}B{sub 2}O{sub 9}-whisker-coated Al{sub 2}O{sub 3} ceramics were bonded by AgCu–4.5 wt.%Ti alloy in vacuum. The microstructure of the whisker-coated Al{sub 2}O{sub 3} joints was investigated by scanning electron microscopy, transmission electron microscopy and X-ray diffraction. A continuous (Cu,Al){sub 3}Ti{sub 3}O layer formed against the alloy at lower bonding temperatures, and a complex transition zone bordering the whiskers was observed, which consisted of Ag nanoparticles, titanium oxides, TiB{sub 2}, (Cu,Al){sub 3}Ti{sub 3}O nanoparticles and possible Ag{sub 3}Al. As the bonding temperature increased, the Al{sub 2}O{sub 3}/AgCuTi interface was found to transform from whisker- to nanoparticle-strengthened composite region. Bend test results revealed that both the whiskers grown on Al{sub 2}O{sub 3} and the dispersive nanoscale products in the alloy played positive roles in improving the joint properties. The maximum bend strength of the whisker-coated Al{sub 2}O{sub 3} joints was 313 MPa at the bonding temperature of 820 °C. - Highlights: • Al{sub 4}B{sub 2}O{sub 9}-whisker-coated Al{sub 2}O{sub 3} ceramics were bonded by AgCu–4.5 wt.%Ti alloy in vacuum. • Microstructures of whisker-coated Al{sub 2}O{sub 3} joints were investigated in detail. • Both whiskers and the dispersive nanoscale products can improve the joint properties. • The maximum bend strength of the whisker-coated Al{sub 2}O{sub 3} joints was 313 MPa.

36 MATERIALS SCIENCE↗

On the formation mechanism of solid-solution Cu-to-Cu joints in the Cu/Ni/Ga/Ni/Cu system

Highlights: • The mechanism of Cu/(Ni,Cu,Ga)/Cu solid-solution joint formation is elaborated. • Ga is the dominant diffusion species in the Cu/Ni/Ga/Ni/Cu bonding system. • Loose and columnar Ni{sub 3}Ga{sub 7} layer is formed by the (001)-textured Ni/Ga reactions. • Cu significantly accelerates the growth of Ni{sub 3}Ga{sub 7} layer by enhancing Ga diffusion. • Supersaturated Cu in Ni{sub 2}Ga{sub 3} phase promotes the formation of the final fcc phase. - Abstract: Copper (Cu)-to-Cu interconnection is crucial in electronic packaging for applications ranging from three-dimensional integrated circuits to die-attachment in wide band-gap devices. Solid-solution phases are innate with better ductility and electrical and thermal conductivity over intermetallic compounds, which are brittle, electrical resistant, and unstable; yet are commonly seen in electronic joints. The desired solid-solution Cu-to-Cu joints have recently been demonstrated using transient-liquid-phase bonding with gallium (Ga) as the filler material to bond Cu substrates with electroplated nickel (Ni) as under-bump-metallurgy. The Cu/Ni/Ga/Ni/Cu couples can fully transform into the Cu/face-centered cubic (fcc)-(Ni,Cu,Ga)/Cu solid-solution joints. However, why and how the solid-solution joints were formed remains unclear. Here we proposed the formation mechanism of the fcc-(Ni,Cu,Ga) solid-solution joints based on five sets of Cu-Ni-Ga couples, namely the Ni/Ga, Ni/Cu/Ga, Ni/Ni/Ga, (Cu,Ni)/Ga, and Cu/Ni/Ni{sub 3}Ga{sub 7}/Ni{sub 3}Ga{sub 7}/Ni/Cu reactions. The roles of each element in the Cu-Ga-Ni interactions as well as the reaction progressions are elaborated.

36 MATERIALS SCIENCE↗

An Experimental and Numerical Study of Plasma Treatment Effects on Adhesive Joints of Metals, CFRTPs, and Metal–CFRTP Combinations

This work investigates the effects of plasma surface treatment on both the local adherend–adhesive interfacial strength and the global lap shear strength (LSS) of adhesively-bonded joints composed of metals, CFRTPs, and metal-CFRTP combinations, using AA6061 and CFRPPA as representative examples. Experimental and computational results show that plasma treatment improved the ratio of CFRPPA–adhesive interfacial normal strength to adhesive tensile strength (sint,n/scri,t,adhesive) from 0.59–1.00 to 0.91–1.73, leading to an average 90% increase in LSS for CFRPPA-related joints. In contrast, the LSS and sint,n/scri,t,adhesive values of AA6061–AA6061 joints (>=2.27) remained nearly unchanged after plasma treatment. The enhanced joint bonding was further supported by post-failure surface morphologies from three-dimensional profilometry and simulations, showing a transition from dominant interfacial failure to mixed modes involving interfacial, cohesive, and slight fiber-peeling failures. The LSS evolution with respect to sint,n/scri,t,adhesive was numerically established until the saturation of the LSS of various joints, and the behavior of AA6061–CFRPPA T-joints with varying interfacial strengths was also modeled. This study highlights the importance of local interfacial bonding strength, rather than global LSS, for understanding and optimizing the mechanical performance of adhesively-bonded composite–metal and composite-composite structures via different surface modification strategies.

Qiao, Yao (ORCID:0000000265867604)↗