Investigation into Interfacial Mixing Behavior of Blown Powder Deposited Inconel 625-Copper Alloy Bimetallic for Improvement of Bimetallic Joint Strength

Use of laser blown powder, directed energy deposition (DED) provides a method for fabrication of bimetallic functional materials for high heat flux applications. However, this relatively new process currently has a low technology readiness level (TRL). Key to increasing the TRL is a better understanding of the factors that control mixing of the bi-metallic materials at the interface. The resulting interfaces in specimens obtained from three vendors were characterized using optical and electron microscopy with electron dispersion spectroscopy in addition to mechanical testing. Based on the range of process parameters and resulting interfaces, a model is being developed to predict interfacial mixing for development of specifications for improved and repeatable microstructures.

Additive Manufacturing↗

Window Cooling Studies and Disk Vibration Testing on a Subset of Mo-100 Disks

Production of metastable Technetium-99 (Tc-99m), a radioactive tracer that emits gamma rays, is vital to the medical imaging community. Tc-99m is extracted from the decay of Molybdenum-99 (Mo-99) which has a half-life of about 2-3 days. The work presented in this report is part of the NNSA’s mission to produce Mo-99 commercially, within the US, without the use of highly enriched uranium (HEU) in support of nonproliferation and global security. Los Alamos National Laboratory (LANL) is working with NorthStar Medical Radioisotopes (NMR) on their efforts to produce Mo-99 through the irradiation of Mo-100 targets using an electron beam. The NMR target comprises a stack of approximately 60-70 Mo-100 disks with diameter 24 mm and thickness 0.74 mm held in stainless steel laminations, each separated using 0.25 mm thick stainless-steel spacers. The symmetric target stack is housed in an Inconel vessel with two Inconel windows on either side. Two electron accelerators are used to produce 40 MeV, 3.16 µA electron beams each that penetrate the Inconel windows and irradiate the Mo-100 disks. Approximately 90% of the total 250 kW beam power is deposited in the NMR target during the irradiation process, with a smaller percentage adding up to 2.2 kW of heat deposited on the Inconel window. During irradiation, pressurized helium gas flows through thin gaps between the disks cooling the beam window, target disks, disk laminations and spacers. Both NMR and LANL have found during cold testing of the target system (no heat deposition) that the Mo 100 disks undergo significant mass loss and disk breakage due to vibrations induced by the flowing helium gas. The mass loss is not only undesirable due to monetary loss from reduced final quantities of Mo-99, but also due to the hazards associated with radioactive material trapped in the cooling lines and particle filters. The effect of flow rate and target geometry on the flow induced vibrations need to be quantified, and recommendations provided to minimize this mass loss. LANL has previously also tested NMR’s Inconel beam window by heating the window, while flowing pressurized helium, using the average heat deposited on the window. However, the NMR beam is pulsed with a duty cycle of 12.5%, which introduces oscillation in temperature around the nominal 600 °C steady state value with each pulse. Available fatigue curves for Inconel are few, established for room temperature, and they are based on mechanical strain cycles not thermally induced strain as in the NMR target. The effect of pulsed beam heating on the Inconel window therefore needs to be quantified. This report details the experiments conducted to assess the factors that lead to mass loss in the NMR target disks as well as to understand the effect of a pulsed beam on NMR’s Inconel window. This work describes LANL’s experimental characterization of the flow induced vibrations and disk mass loss in a reduced scale set-up containing 5 to 10 Mo-100 disks. We use high speed imaging, displacement measurements and microphone measurements combined with signal processing to estimate the vibration frequency of each disk. The effect of disk thickness, target fit and duration of testing on the mass loss is described. We find that in the current configuration of NMR targets, the vibrations and mass loss on the first disk are minimized, while those in the adjacent disks are highest. The microphone and high-speed image data show that increased flow rates and increased duration of testing increases vibration frequency and mass loss. The mass loss is due to both disk rotation and back and forth motion. There are visible wear marks on the disks with the highest mass loss. We also note that the current NMR window gap reduces flow induced vibrations compared to the previous smaller gaps. Improved target holders significantly reduce disk mass loss to almost negligible quantities. This work finds that the larger window to first disk gap and improved target holder geometry should allow NMR to successfully conduct irradiations with minimal mass loss. The window tests were conducted to understand the effect of a pulsed beam on both the window longevity and to estimate the window temperature and displacement during pulsing. The experiments presented here were performed at significantly low power, due to the limitations of the induction heating system. The window temperature rose to approximately 73 °C with a significantly reduced power of 45 W without beam pulsing. With a 5 Hz pulse rate, 12.5% duty cycle, the window temperature remained constant at 26 °C. These experiments will be repeated with improved coil geometry and reported in upcoming journal papers.

42 ENGINEERING↗

Effect of magnesium oxide content on oxidation behavior of some superalloy-base cermets

The effect of increasing magnesium oxide (MgO) content on the cyclic oxidation resistance of hot-pressed cermets of MgO in NiCrAlY, MgO in Hoskins-875, MgO in Inconel-702, and MgO in Hastelloy-X was investigated. The cermets with magnesium oxide levels of 5, 10, 20, and 40 vol percent were examined. The cyclic oxidation behavior of these cermets at 1100 and 1200 C in still air was determined by a thermogravimetric method supplemented by X-ray diffraction analysis and light and electron microscopy. In all instances, MgO prevented grain growth in the metallic phase. No evidence of oxidation along interphase boundaries was detected. Cermets of MgO in NiCrAlY and MgO in Hoskins-875 were superior to cermets of MgO in Inconel-702 and MgO in Hastelloy-X. Their oxidation resistance was degraded only when the MgO content was 40 vol percent. The oxidation behavior of MgO-in-Inconel-702 powder cermets containing 5- and 10-vol percent MgO was approximately similar to that of pure Inconel-702 compacts. The 20- and 40-vol percent MgO content reduced the oxidation resistance of MgO-in-Inconel-702 powder cermets relative to that of pure Inconel-702.

Zaplatynsky, I.↗

Friction and Wear Characteristics of Candidate Foil Bearing Materials from 25 C to 800 C

The friction and wear behavior of unlubricated metal/metal sliding couples was investigated to screen potential candidates for high temperature foil bearings. The tribo-tests were run in an induction-heated high temperature pin-on-disk tribometer in an air atmosphere at a load of 4.9 N and at a sliding velocity of 1 m/s. The friction and wear properties of several nickel based alloys (Rene'41, Inconel X-750, Inconel 713C), iron based alloys (MA956 and Inconel 909) and a ceramic (Al2O3) were tested at 25, 500, and 800 C. In general, at elevated temperatures the alloys oxidized and formed a tenacious and lubricous oxide surface film or layer. At 800 C, Inconel X-750 versus Rene'41 had the lowest friction coefficient (0.27) and at 500 C, Inconel X-750 versus Inconel 909 the lowest pin wear (2.84 x 10(exp -6)cu mm/N-m). Gouging and severe wear of the softer material occurred whenever a significant difference in hardness existed between the pin and disk specimens.

DellaCorte, C.↗

Microstructure, hardness and cavitation erosion resistance of different cold spray coatings on stainless steel 316 for hydropower applications

There is an urgent need for repair of hydropower components that have undergone damage due to cavitation. Conventional repair methods involve melting of materials and can deteriorate material properties and cause distortion. This study investigated the relevant properties of different materials using solid phase processing—cold spray technology. Stainless steel (SS) 316, Inconel 625 and CrC-NiCr materials were cold spray deposited onto base metal SS 316, respectively. Cold spray achieved dense uniform deposits with low level porosity, and intimate contact between the deposit and the base metal was observed. Severe plastic deformation imparted during the cold spray process resulted in significant grain size refinement, nanostructured regions were observed in the deposits across the interfacial area. Cold sprayed deposits exhibited elevated hardness in contrast to that of the base metal SS 316. The cavitation erosion resistance of the deposits was evaluated with a cavitation erosion jet adhering to ASTM G134. Both SS 316 and Inconel 625 achieved better cavitation erosion resistance when compared to that of the SS 316 base metal, with the former exhibiting close to a 4 times improvement.

Jiang, Xiujuan↗

Report on Properties and Microstructure of 3D Printed Inc-718

The report presents the microstructure and mechanical properties of 3D printed Inconel 718 to assess its potential use as a structural material for the Transformation Challenge Reactor (TCR). The structural components near the outlet of the core will experience significant neutron fluxes and outlet coolant temperatures from the hot standby temperature of 300°C to nearly 550°C at the center of the part. These components must support the core in appropriate loading conditions and require structural analysis at relevant temperatures. Strong spatial and chemical heterogeneity was found in as-built (ASB) Inconel 718. Three heat treatments were designed and conducted to simplify the microstructure and determine how each precipitating phase contributed to the overall strength. Baseline mechanical properties were measured from uniaxial tensile tests on subsize SS-J2 specimens at room temperature and at elevated temperatures of 300, 450, and 600°C. Microstructure electron microscopy was performed on ASB Inconel 718 and heat treated to correlate the observed mechanical properties with nanoscale features. Homogenization of the microstructure led to a highly ductile Inconel with lower strength compared with wrought Inconel 718. The tensile properties of additively manufactured 718 using a standard ASTMrecommended heat treatment were consistent with literature and with the ASTM for the properties of this alloy. A higher fraction of the δ phase led to shorter uniform elongation without altering other engineering properties.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Advanced fabrication techniques for cooled engine structures

An improved design for regeneratively cooled engine structures was identified. This design uses photochemically machined (PCM) coolant passages. It permits the braze joint to be placed in a relatively cool area, remote from the critical hot face sheet. The geometry of the passages at the face sheet also minimizes stress concentration and, therefore, enhances the low cycle fatigue performance. The two most promising alloys identified for this application are Inconel 617 and Nickel 201. Inconel 617 was selected because it has excellent creep rupture properties, while Nickel 201 was selected because of its predicted good performance under low cycle fatigue loading. The fabrication of the PCM coolant passages in both Inconel 617 and Nickel 201 was successfully developed. During fabrication of Inconel 617, undesirable characteristics were observed in the braze joints. A development program to resolve this condition was undertaken and led to definition of an isothermal solidification process for joining Inconel 617 panels. This process produced joints which approach parent metal strength and homogeneity.

Buchmann, O. A.↗