Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “FRICTION STIR WELDING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 271 records · Page 15

Evaluating the Potential for Remote In-Process Monitoring of Tool Wear in Friction Stir Welding of Stainless Steel

A wear characterization study was performed to determine the useful lifetime of Polycrystalline Cubic Boron Nitride tooling for the friction stir welding (FSW) of stainless steel samples in support of a nuclear repair welding research and development program. In-situ and ex-situ laser profilometry were utilized as primary methods of monitoring tool geometry degradation, and volumetric defects were detected through both non-destructive and destructive techniques, as repeated welds of a standard sample configuration were produced. The spectral content of weld forces were examined to search for indications of evolving material flow conditions, caused by significant tool wear, that would result in the formation of defects, and an artificial neural network was trained and evaluated as a means of automatically detecting these conditions. Here, the resulting performance constituted a successful demonstration of in-process monitoring of tool wear and weld quality in FSW of a high melting temperature, high hardness material.

36 MATERIALS SCIENCE↗

Effects of Annealing Process on the Formability of Friction Stir Welded Al-Li Alloy 2195 Plates

Large rocket cryogenic tank domes have typically been fabricated using Al-Cu based alloys like Al-Cu alloy 2219. The use of aluminum-lithium based alloys for rocket fuel tank domes can reduce weight because aluminum-lithium alloys have lower density and higher strength than Al-Cu alloy 2219. However, Al-Li alloys have rarely been used to fabricate rocket fuel tank domes because of the inherent low formability characteristic that make them susceptible to cracking during the forming operations. The ability to form metal by stretch forming or spin forming without excessive thinning or necking depends on the strain hardening exponent "n". The stain hardening exponent is a measure of how rapidly a metal becomes stronger and harder. A high strain hardening exponent is beneficial to a material's ability to uniformly distribute the imposed strain. Marshall Space Flight Center has developed a novel annealing process that can achieve a work hardening exponent on the order of 0.27 to 0.29, which is approximately 50% higher than what is typically obtained for Al-Li alloys using the conventional method. The strain hardening exponent of the Al-Li alloy plates or blanks heat treated using the conventional method is typically on the order of 0.17 to 0.19. The effects of this novel annealing process on the formability of friction stir welded Al-Li alloy blanks are being studied at Marshall Space Flight Center. The formability ratings will be generated using the strain hardening exponent, strain rate sensitivity and forming range. The effects of forming temperature on the formability will also be studied. The objective of this work is to study the deformation behavior of the friction stir welded Al-Li alloy 2195 blank and determine the formability enhancement by the new annealing process.

Chen, Po-Shou↗

A new smoothed particle hydrodynamics non-Newtonian model for friction stir welding: Process modeling and simulation of microstructure evolution in a magnesium alloy

We present a new smoothed particle hydrodynamics (SPH) model for friction stir welding (FSW). FSW has broad commercial application in the marine, aerospace, rail, and automotive industries. However, development of the FSW process for each new application has remained largely empirical. Few established numerical modeling techniques have been developed that can explain and predict important features of the process physics involved in FSW. This is particularly true in the areas of material flow and mixing mechanisms. In this paper, we present a novel modeling approach to simulate FSW that may have significant advantages over current finite element or finite difference based methods. Unlike traditional grid-based methods, Lagrangian particle methods such as SPH can simulate the dynamics of interfaces, large material deformations, and the material’s strain and temperature history without employing complex tracking schemes. Three-dimensional simulations of FSW on AZ31 Mg alloy are performed. The temperature history and distribution, grain size, microhardness as well as the texture evolution are presented. Numerical results are found to be in good agreement with experimental observations.

Pan, Wenxiao↗

Phased Array Ultrasound: Initial Development of PAUT Inspection of Self-Reacting Friction Stir Welds

This slide presentation reviews the development of Phased Array Ultrasound (PAUT) as a non-destructive examination method for Self Reacting Friction Stir Welds (SR-FSW). PAUT is the only NDE method which has been shown to detect detrimental levels of Residual Oxide Defect (ROD), which can result in significant decrease in weld strength. The presentation reviews the PAUT process, and shows the results in comparison with x-ray radiography.

Rairigh, Ryan↗

Optimization of Tensile and Corrosion Properties of Dissimilar Friction Stir Welded AA2024-7075 Joints

In this work, we performed some joining experiments of dissimilar aluminum alloys AA2024-T351 and AA7075-T651 using friction stir welding (FSW) technique with different process parameters (rotational speed, welding speed and plunge depth). Response surface methodology based on a central composite rotatable design was used to establish the mathematical models predicting the tensile properties and corrosion rate of dissimilar FSW joints with some high confidence level. Analysis of variance method was employed to verify the developed models. Besides, the influences of FSW process parameters on tensile and corrosion properties of joints were analyzed. In order to obtain a desirable combination property of the dissimilar FSW joints, the optimum process parameters after experimental verification were proposed as: rotational speed 1495 rev/min, welding speed 187 mm/min and plunge depth 0.03 mm. This verification illustrated that the developed models are appropriate for the modeling and optimization of process.

36 MATERIALS SCIENCE↗

Autogeneous Friction Stir Weld Lack-of-Penetration Defect Detection and Sizing Using Directional Conductivity Measurements with MWM Eddy Current Sensor

Al 2195-T8 plate specimens containing Friction Stir Welds (FSW), provided by Lockheed Martin, were inspected using directional conductivity measurements with the MWM sensor. Sensitivity to lack-of-penetration (LOP) defect size has been demonstrated. The feature used to determine defect size was the normalized longitudinal component of the MWM conductivity measurements. This directional conductivity component was insensitive to the presence of a discrete crack. This permitted correlation of MWM conductivity measurements with the LOP defect size as changes in conductivity were apparently associated with metallurgical features within the first 0.020 in. of the LOP defect zone. Transverse directional conductivity measurements also provided an indication of the presence of discrete cracks. Continued efforts are focussed on inspection of a larger set of welded panels and further refinement of LOP characterization tools.

Goldfine, Neil↗

Microstructure of Friction Stir Welded AlSi9Mg Cast with 5083 and 2017A Wrought Aluminum Alloys

Wrought aluminum alloys 5083 and 2017A were each joined with cast aluminum alloy AlSi9Mg through friction stir welding in butt weld configurations. For each material system, the wrought and cast alloy positions, i.e., the advancing side or the retreating side, were exchanged between welding trials. The produced weldments were free from cracks and discontinuities. For each alloy configuration, a well-defined nugget comprised of alternating bands of the welded alloys characterized the microstructure. The degree of mixing, however, strongly depended on which wrought alloy was present and on its position during processing. In all cases, the cast AlSi9Mg alloy dominated the weld center regardless of its position during welding. Electron backscattered diffraction analysis showed that the grain size in both alloys (bands) constituting the nugget was similar and that the majority of grain boundaries exhibited a high angle character (20°-60°). Regardless of the alloy, however, all grains were elongated along the direction of the material plastic flow during welding. A numerical simulation of the joining process visualized the material flow patterns and temperature distribution and helped to rationalize the microstructural observations. The hardness profiles across the weld reflected the microstructure formed during welding and correlated well with the temperature changes predicted by the numerical model. Tensile specimens consistently fractured in the cast alloy near the weld nugget.

36 MATERIALS SCIENCE↗

The Role of Friction Stir Welding on the Microstructure and Mechanical Properties of AZ31B-H24 Mg alloy

In this study, an attempt was made to join AZ31B magnesium alloy by friction stir welding (FSW) process. A single tool with cylindrical screw threaded pin was used to investigate the effect of welding parameters on microstructure and mechanical properties of stir zone (SZ). Several welds were made at different rotational ({omega}) and traverse ({upsilon}) speeds, while the {omega}/{upsilon} ratios were kept constant. The optical and scanning electron microscopy were used to study the variation of microstructure across the welds. Moreover, micro-hardness and tensile tests were carried out to evaluate the mechanical properties of joints. It was found that {omega} plays more significant role on the resulted grain structure than {upsilon}, and at a constant {omega}/{upsilon} ratio, decreasing rotational speed decreased the size of grains, and hence, improved the hardness value and the tensile strength of the SZ.

36 MATERIALS SCIENCE↗

Adaptive relay autotuning under static and non-static disturbances with application to friction stir welding

When a traditional relay feedback test is biased, asymmetry is induced, erroneous system identification occurs, and the test may stop oscillating. Adaptive methods which restore symmetry to the relay test are developed, and additional methods are presented to detect and recover from a non-oscillation condition. This is demonstrated both in simulation and in a process with significant transients and disturbances - friction stir welding (FSW). In testing, it is shown that the adaptive method is able to restore symmetry even in the presence of severe and changing disturbances, including after the weld plunge where temperature gradients change rapidly. Finally, these improvements enable system identification of systems such as FSW in a more robust and accurate manner.

42 ENGINEERING↗

Microstructure evolution in the conventional single side and bobbin tool friction stir welding of thick rolled 7085-T7452 aluminum alloy

Highlights: • Comparison of microstructure evolution via EBSD of SS-FSW and BB-FSW was investigated. • Friction heat, strain rate and degree of recrystallization affected grain size. • Discontinuously dynamic recrystallization occurred in the weld nugget zone. • The degree of recrystallization was mainly controlled by the strain rate. - Abstract: The microstructure evolution during the conventional single side friction stir welding (SS-FSW) and the bobbin tool FSW (BB-FSW) of 7085-T7452 alloy thick plate was extensively studied by using the state-of-the-art materials characterization techniques. The Electron backscattering diffraction results reveal that a significant grain refinement and a larger percentage of high angle grain boundaries (HAGBs) exist in the weld nugget zone (WNZ) and the thermal-mechanical affected zone (TMAZ) compared with the base material. Meanwhile, more obviously inhomogeneous refined grains and HAGBs in WNZ along the thickness direction and a larger percentage of low angle grain boundaries (LAGBs) were observed in SS-FSW joint than that in BB-FSW joint. The change of the average grain size is the result of friction heat and strain rate of plastic deformation combined with a certain degree of recrystallization. Moreover, the recrystallization is mainly controlled by the strain rate during the FSW process. The presence of Cube and Cube ND after welding shows that the discontinuously dynamic recrystallization (DDRX) is a major factor in the final microstructural response. The research and findings help the understanding of the mechanism of microstructure homogenization and further optimizing the welding process for application.

36 MATERIALS SCIENCE↗

Texture and precipitation behavior of friction stir welded Inconel 825 alloy

The microstructure, texture pattern, and precipitation behavior of friction stir butt welded Inconel 825 alloy are highlighted here. The microstructure of bright regions and black-banded regions in the stir zone (SZ) is characterized by SEM, EBSD, and TEM with EDS. EBSD analysis justifies that the SZ exhibits a dynamic recrystallized structure. Grain boundary mapping corroborates the insignificant difference in the low- and high-angle grain boundaries fraction between the SZ, the thermo-mechanically affected zone, and the base metal. TEM analysis confirms the formation of nano twins and dispersion of nano-size precipitations in the grains, and at the grain boundaries as well. Grain refinement and nano-size precipitation formation in the SZ significantly enhanced both microhardness and tensile strength.

Das, Hrishikesh↗

Friction stir welding and self-ion irradiation effects on microstructure and mechanical properties changes within oxide dispersion strengthened steel $\mathrm{MA956}$

We report the joining process for oxide dispersion strengthened (ODS) alloys remains a key challenge facing the nuclear community. The microstructure and mechanical properties were characterized in the base material and friction stir welded ODS MA956 irradiated with 5 MeV Fe 2+ ions from 400 to 500°C up to 25 dpa. Nanoindentation was performed to assess changes in hardness and yield stress, and the dispersed barrier hardening (DBH) model was applied to described results. A combination of scanning transmission electron microscopy (STEM) and atom probe tomography (APT) were used to assess evolution of the microstructure including dispersoids, network dislocations and dislocation loops, nanoclusters, and solid solution concentrations. Overall, softening was observed as a result of increased dose, which was exacerbated at 500°C. The formation and coarsening of new dispersoids was noted while nanoclusters tended to dissolve in the base material, and were not observed in the stir zone. Solute nanocluster evolution was identified as a primary driver of the changes in mechanical properties.

36 MATERIALS SCIENCE↗

Friction Stir Welding for Aluminum Metal Matrix Composites (MMC's) (Center Director's Discretionary Fund, Project No. 98-09)

This technical memorandum describes an investigation of using friction stir welding (FSW) process for joining a variety of aluminum metal matrix composites (MMC's) reinforced with discontinuous silicon-carbide (SiC) particulate and functional gradient materials. Preliminary results show that FSW is feasible to weld aluminum MMC to MMC or to aluminum-lithium 2195 if the SiC reinforcement is <25 percent by volume fraction. However, a softening in the heat-affected zone was observed and is known to be one of the major limiting factors for joint strength. The pin tool's material is made from a low-cost steel tool H-13 material, and the pin tool's wear was excessive such that the pin tool length has to be manually adjusted for every 5 ft of weldment. Initially, boron-carbide coating was developed for pin tools, but it did not show a significant improvement in wear resistance. Basically, FSW is applicable mainly for butt joining of flat plates. Therefore, FSW of cylindrical articles such as a flange to a duct with practical diameters ranging from 2-5 in. must be fully demonstrated and compared with other proven MMC joining techniques for cylindrical articles.

Lee, J. A.↗

Comparison of the Effects of Tool Geometry for Friction Stir Welding Thin Sheet Aluminum Alloys for Aerospace Applications

In this presentation, the results of a recent study on the effect of pin tool design for friction stir welding thin sheets (0.040") of aluminum alloys 2024 and 7075 are provided. The objective of this study was to investigate and document the effect of tool shoulder and pin diameter, as well as the presence of pin flutes, on the resultant microstructure and mechanical properties at both room temperature and cryogenic temperature. Specifically, the comparison between three tools will include: FSW process load analysis (tool forces required to fabricate the welds), Static Mechanical Properties (ultimate tensile strength, yield strength, and elongation), and Process window documenting the range of parameters that can be used with the three pin tools investigated. All samples were naturally aged for a period greater than 10 days. Prior research has shown 7075 may require post weld heat treatment. Therefore, an additional pair of room temperature and cryogenic temperature samples was post-weld aged to the 7075-T7 condition prior to mechanical testing.

Merry, Josh↗

Effect of Preheating and Water Cooling on the Performance of Friction-Stir-Welded Aviation-Grade Aluminum Alloy Joints

This paper examined the effect of preheating and water cooling on the thermal, mechanical, metallurgical, and texture properties of friction-stir-welded AA6082. Joints are fabricated under different preheating (FSW-P) and water cooling (FSW-C) conditions. The experimental outcomes indicate that the preheating and water cooling enhance the mechanical properties of the joint. The maximum tensile strength of 295 MPa is obtained for FSW-P1. It is also observed that preheating has more impact on microhardness. Microstructural analysis using optical microscope and electron backscatter diffraction analysis indicated that FSW produced fine equiaxed grains in the nugget zone due to dynamic recrystallization. Texture analysis shows that finer grain grains are obtained under preheating and water cooling conditions. The minimum grain size of 5.3 µm is obtained under FSW-P1. X-ray diffraction analysis shows that Mg{sub 2}Si phase in nugget zone that is an indication of dissolution and formation of strengthening precipitates. Fracture analysis indicates that preheating also improves the ductility of the joint.

36 MATERIALS SCIENCE↗

Friction Stir Welded Aluminum-Lithium (Al-Li) 2050 Blanks for Spin Forming

Spin forming is a metalworking process used to produce axially-symmetric parts by the application of lateral pressure from a forming tool to a circular blank mounted on a revolving, heated mandrel. This process enables production of cones, domes, or caps that can incorporate features such as flat bulkheads. Friction stir welded (FSW) Al-Li 2195 blanks have been spin formed for single-piece, launch vehicle domes up to 5 m in diameter. Al-Li 2050 plate has the advantage of availability up to 165 mm thick,whereas 2195 plate is traditionally only available up to 57 mm thick. Increased plate thickness enables greater design flexibility for machining of taller structural elements, such as stiffeners. However, 2050 is only available in plate widths up to ~3.9 m. This study demonstrated the capability of making custom 2050 blanks for spin forming large (>7.8 m in diameter), single-piece, light-weight flight articles (e.g., lunar habitats and landers) by FSW two (or more) plates together. Spin forming of welded 2050 blanks has not been attempted before this investigation. The objective was to evaluate the mechanical properties of 2050 parent material and FSW regions after spin forming and subsequent T6 heat treatment. A 3 m diameter x 38 mm thick 2050 blank was fabricated from two 1.5 m wide pieces by FSW and subsequently spin formed into a cone article. Additionally, three 1.2 m diameter x 8.1 mm thick 2050 blanks were produced by FSW and spin formed into subscale cone articles with varying strain input. Mechanical properties are reported for spin formed 2050-T6 parent material and FSW regions on the articles. Abnormal grain growth (AGG) in the FSW during heat treatment was expected based on prior experience with 2195. Implementation of an AGG suppression strategy during heat treatment reduced AGG in the FSW regions and improved ductility.

Spin forming↗

On the Effect of Quenching on Postweld Heat Treatment of Friction-Stir-Welded Aluminum 7075 Alloy

This work focuses on the effect of postweld heat treatment (PWHT) on the mechanical properties and microstructural evolution of aluminum 7075 alloy processed via friction stir welding (FSW). FSW is known to be capable of grain refinement in the nugget zone (NZ). Two different quench media (water and air) were employed for PWHT. Regardless of the quench media, the PWHT led to the occurrence of grain growth in the NZ of the FSWed aluminum 7075 alloy. Abnormal grain growth occurred in the water quenched specimen. It is shown that ductility and strength of FSWed aluminum 7075 alloy are strongly dependent on the quenching rate. Changes in the mechanical properties and microstructure reveal that only at lower cooling rate this alloy is prone to the formation of precipitate-free zones (PFZs) in the vicinity of grain boundaries. Eventually, the PFZs deteriorate mechanical properties of this alloy.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Characterization of Friction-Stir-Welded 316L Austenitic Stainless Steels

Fusion welding of austenitic stainless steels (ASSs) causes undesirable metallographic changes. An attempt has been made to join 3-mm-thick 316L ASS plates using friction stir welding and correlate the microstructural evolution and the mechanical properties under various welding conditions. Tungsten alloy (W-Re) tool was employed for welding. Successful joints were obtained within a range of traverse speeds (45-85 mm/min) used in this work. Various zones were observed across the joint line. The stir zone exhibited considerable grain refinement and traces of delta ferrite phase. EBSD images showed a decreasing grain size with increased traverse speed. XRD patterns and TEM images confirmed the existence of delta ferrite. The mechanical properties of the joints including microhardness, tensile strength, impact toughness and bending were further reported.

36 MATERIALS SCIENCE↗