At least 271 records · Page 15

Controllable nitrogen doping in as deposited TiO{sub 2} film and its effect on post deposition annealing

In order to narrow the band gap of TiO{sub 2}, nitrogen doping by combining thermal atomic layer deposition (TALD) of TiO{sub 2} and plasma enhanced atomic layer deposition (PEALD) of TiN has been implemented. By altering the ratio between TALD TiO{sub 2} and PEALD TiN, the as synthesized TiO{sub x}N{sub y} films showed different band gaps (from 1.91 eV to 3.14 eV). In situ x-ray diffraction characterization showed that the crystallization behavior of these films changed after nitrogen doping. After annealing in helium, nitrogen doped TiO{sub 2} films crystallized into rutile phase while for the samples annealed in air a preferential growth of the anatase TiO{sub 2} along (001) orientation was observed. Photocatalytic tests of the degradation of stearic acid were done to evaluate the effect of N doping on the photocatalytic activity.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Properties of HfLaO MOS capacitor deposited on SOI with plasma enhanced atomic layer deposition

Amorphous HfLaO dielectric film was successfully deposited on a silicon-on-insulator (SOI) substrate by plasma enhanced atomic layer deposition with in situ plasma treatment. The HfLaO film retained its insulating characteristics and is thermally stable even after annealing at 800 °C. The film has a dielectric constant of 27.3 and leakage of only 0.03 mA/cm{sup 2} at a gate bias of |Vg − V{sub fb}| = 1 V. The capacitance equivalent oxide thickness is 0.7 nm. A new parallel electrode testing structure was applied to measure C–V and J–V characteristics for the SOI samples. This testing method for metal–oxide–semiconductor capacitors has potential uses for measuring other layered substrates.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Epitaxial niobium dioxide thin films by reactive-biased target ion beam deposition

Epitaxial NbO{sub 2} thin films were synthesized on Al{sub 2}O{sub 3} (0001) substrates via reactive bias target ion beam deposition. X-ray diffraction and Raman spectra were used to confirm the tetragonal phase of pure NbO{sub 2}. Through XPS, it was found that there was a ∼1.3 nm thick Nb{sub 2}O{sub 5} layer on the surface and the bulk of the thin film was NbO{sub 2}. The epitaxial relationship between the NbO{sub 2} film and the substrate was determined. Electrical transport measurement was measured up to 400 K, and the conduction mechanism was discussed.

36 MATERIALS SCIENCE↗

Optical emission diagnostics of plasmas in chemical vapor deposition of single-crystal diamond

A key aspect of single crystal diamond growth via microwave plasma chemical vapor deposition is in-process control of the local plasma–substrate environment, that is, plasma gas phase concentrations of activated species at the plasma boundary layer near the substrate surface. Emission spectra of the plasma relative to the diamond substrate inside the microwave plasma reactor chamber have been analyzed via optical emission spectroscopy. The spectra of radical species such as CH, C{sub 2}, and H (Balmer series) important for diamond growth were identified and analyzed. The emission intensities of these electronically excited species were found to be more dependent on operating pressure than on microwave power. Plasma gas temperatures were calculated from measurements of the C{sub 2} Swan band (d{sup 3}Π → a{sup 3}Π transition) system. The plasma gas temperature ranges from 2800 to 3400 K depending on the spatial location of the plasma ball, microwave power and operating pressure. Addition of Ar into CH{sub 4}+H{sub 2} plasma input gas mixture has little influence on the Hα, Hβ, and Hγ intensities and single-crystal diamond growth rates.

36 MATERIALS SCIENCE↗

A Structural and Ellipsometric Investigation of Thin Gallium Oxide Layers Deposited on Si by Means of Laser Deposition

The morphology of Ga{sub 2}O{sub 3} layers deposited on a silicon substrate by pulse laser deposition is studied using scanning electron microscopy in the thickness range of 30–200 nm. Using spectroscopic ellipsometry in the wavelength range from 250 to 900 nm, the thickness of layers and dispersion of their optical parameters (complex pseudodielectric function ε, refractive and absorptive indices) have been determined and the fraction of voids has been estimated in the scope of the Bruggeman effective medium approximation. In the spectrum of the imaginary part ε{sub 2}, there is observed an increase in values in the region of energy E = 4.8 eV corresponding to the direct interband transition in the Ga{sub 2}O{sub 3} structure. X-ray structure analysis showed the presence of peaks typical for the β-Ga{sub 2}O{sub 3} structure. The results of the investigations can be used for the formation of wide-bandgap gallium oxide layers in developing devices of power electronics and in creating optoelectronic devices for the UV range.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Silicidation of Niobium Deposited on Silicon by Physical Vapor Deposition

Niobium was deposited by physical vapor deposition (PVD) using e-beam evaporation on bare (100) silicon substrates and SiO2 surfaces. The formation of niobium silicide was investigated by annealing PVD Nb films in the temperatures range 400–1000°C. At all elevated annealing temperatures the resistivity of Nb silicide is substantially higher than that of Nb. The Nb silicidation as a function of temperature has been investigated and different NbXSiy compounds have been characterized. It has been observed that the annealing of the Nb film on Si is accompanied by a strong volume expansion of about 2.5 of the resulting reacted film. The films' structural properties were studied using X-Ray diffraction (XRD), energy dispersive X-ray spectroscopy (EDS), and atomic force microscopy (AFM), which was not previously presented in the context of the extant NbSi literature. The X-Ray diffraction characterization of the Nb on Si sample annealed at 1000°C, showed the presence of hexagonal Nb5Si3 phases, with a dominant peak at the (200) plane, and NbSi2 phases. Fractal dimension calculations indicate a distinct transition from Stranski-Krastanov to Volmer-Weber film growth for NbSi formation at the annealing temperature of 600°C and above.

36 MATERIALS SCIENCE↗

Controlled exposure of CuO thin films through corrosion-protecting, ALD-deposited TiO 2 overlayers

Ultra-thin film coatings are used to protect semiconductor photoelectrodes from the harsh chemical environments common to photoelectrochemical energy conversion. These layers add contact transfer resistance to the interface that can result in a reduction of photoelectrochemical energy conversion efficiency of the photoelectrode. Here, we describe the concept of a partial protection layer, which allows for direct chemical access to a small fraction of the semiconductor underlayer for further functionalization by an electrocatalyst. The rest of the interface remains protected by a stable, inert protection layer. CuO is used as a model system for this scheme. Atomic layer deposition (ALD)-prepared TiO 2 layers on CuO thin films prepared from electrodeposited Cu 2 O allow for the control of interfacial morphology to intentionally expose the CuO underlayer. The ALD-TiO 2 overlayer shrinks during crystallization, while Cu 2 O in the underlayer expands during oxidation. As a result, the TiO 2 protection layer cracks to expose the oxidized underlying CuO layer, which can be controlled by preceding thermal oxidation. Furthermore, this work demonstrates a potentially promising strategy for the parallel optimization of photoelectrochemical interfaces for chemical stability and high performance.

14 SOLAR ENERGY↗

Preliminary Deposition Modeling: For Determining the Deposition of Corrosive Contaminants on SNF Canisters

This report fulfills the M3 milestone M3SF-20PN010207045. During fiscal year (FY) 2019, Pacific Northwest National Laboratory (PNNL) worked to develop initial deposition and particle tracking models which could be used to better understand how corrosive contaminants deposit on the surfaces of spent nuclear fuel (SNF) canisters during dry storage. These models may be useful in understanding the likelihood of chloride induced stress corrosion cracking (CISCC) on SNF canisters

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Interfacial Effects of Tin Oxide Atomic Layer Deposition in Metal Halide Perovskite Photovoltaics

Metal halide perovskites offer a wide and tunable bandgap, making them promising candidates for top–cell absorbers in tandem photovoltaics. In this work, the authors aim to understand the atomic layer deposition (ALD) precursor–perovskite interactions of the tin oxide ALD system and the role of organic fullerenes at the perovskite–tin oxide interface while establishing a framework for developing alternative perovskite–compatible ALD processes in the future. It is shown, in the case of tin oxide ALD growth with tetrakis(dimethylamino)tin(IV) and water on FA 0.83 Cs 0.17 Pb(I 0.83 Br 0.17 ) 3 perovskite, that perovskite stability is most sensitive to metal–organic exposure at elevated temperatures with an onset near 110 °C, resulting in removal of the formamidinium cation. Transitioning from ALD to pulsed–chemical vapor deposition tin oxide growth can minimize the degradation effects. Investigation of fullerenes at the perovskite interface shows that thin fullerene layers offer minor improvements to perovskite stability under ALD conditions, but significant enhancement in carrier extraction. Fullerene materials are undesirable due to fabrication cost and poor mechanical stability. Compositional tuning of the perovskite material can improve the fullerene–free device performance. Furthermore, this method is demonstrated with a bromine–rich perovskite phase to enable an 8.2% efficient perovskite device with all–inorganic extraction layers.

36 MATERIALS SCIENCE↗

Obtaining a Low and Wide Atomic Layer Deposition Window (150-275 °C) for In 2 O 3 Films Using an In III Amidinate and H 2 O

Indium oxide is a major component of many technologically important thin films, most notably the transparent conductor indium tin oxide (ITO). Despite being pyrophoric, homoleptic indium(III) alkyls do not allow atomic layer deposition (ALD) of In 2 O 3 using water as a co-precursor at substrate temperatures below 200 °C. Several alternative indium sources have been developed, but none allows ALD at lower temperatures except in the presence of oxidants such as O 2 or O 3 , which are not compatible with some substrates or alloying processes. We have synthesized a new indium precursor, tris( N , N' -diisopropylformamidinato)indium(III), compound 1 , which allows ALD of pure, carbon-free In 2 O 3 films using H 2 O as the only co-reactant, on substrates in the temperature range 150–275 °C. In contrast, replacing just the H of the anionic i PrNC(H)N i Pr ligand with a methyl group (affording the known tris( N , N' -diisopropylacetamidinato)indium(III), compound 2 ) results in a considerably higher and narrower ALD window in the analogous reaction with H 2 O (225–300 °C). Kinetic studies demonstrate that a higher rate of surface reactions in both parts of the ALD cycle gives rise to this difference in the ALD windows.

charge transport↗

Rationalization of solidification mechanism of Nd–Fe–B magnets during laser directed-energy deposition [Rationalization of solidification mechanism of neodymium-iron-boron magnets obtained after laser directed-energy deposition process]

Here, near-net fabrication techniques are highly beneficial to minimize rare earth metal usage to fabricate dense fully functional magnets. In this study, feasibility of using the directed-energy deposition technique for fabrication of magnets is evaluated. The results show that despite the ability to fabricate highly reactive materials in the laser deposition process, the magnetic coercivity and remanence of the hard magnets is significantly reduced. X-ray powder diffraction in conjunction with electron microscopy showed that the material experienced a primary Nd 2 Fe 17 B x solidification. Consequently, the absence of the hard magnetic phase resulted in deterioration of the build properties.

36 MATERIALS SCIENCE↗

Enhanced Dry Reforming of Methane on Ni and Ni-Pt Catalysts Synthesized by Atomic Layer Deposition

Atomic layer deposition (ALD) was used to deposit Ni and Pt on alumina supports to form monometallic and bimetallic catalysts with initial particle sizes of 1–2.4 nm. The ALD catalysts were more active (per mass of metal) than catalysts prepared by incipient wetness (IW) for dry reforming of methane (DRM), and they did not form carbon whiskers during reaction due to their sufficiently small size. Catalysts modified by Pt ALD had higher rates of reaction per mass of metal and inhibited coking, whereas NiPt catalysts synthesized by IW still formed carbon whiskers. Temperature-programmed reduction of Ni catalysts modified by Pt ALD indicated the presence of bimetallic interaction. Density functional theory calculations suggested that under reaction conditions, the NiPt surfaces form Ni-terminated surfaces that are associated with higher DRM rates (due to their C and O adsorption energies, as well as the CO formation and CH4 dissociation energies).

Environmental Molecular Sciences Laboratory↗