Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CARBIDES”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 271 records · Page 15

Chemical interactions in the aluminum-carbon and aluminum-silicon carbide systems

XPS was used to investigate the influence of O2 and H2O on the formation of aluminum carbide at Al-C and Al-SiC interfaces. It was determined that dosing the interfaces with H2O catalyzed the formation of aluminum carbide in both systems. This result is consistent with the oxidation model of carbide formation (developed to understand the kinetics of aluminum carbide formation at graphite-aluminum interfaces). These results imply that the formation of aluminum carbide in graphite- and SiC-reinforced metal-matrix composites, which severely degrades the composite mechanical properties by degrading the fiber and interface strength is catalyzed.

Maruyama, Benji↗

Silicon carbide semiconductor technology for high temperature and radiation environments

Viewgraphs on silicon carbide semiconductor technology and its potential for enabling electronic devices to function in high temperature and high radiation environments are presented. Topics covered include silicon carbide; sublimation growth of 6H-SiC boules; SiC chemical vapor deposition reaction system; 6H silicon carbide p-n junction diode; silicon carbide MOSFET; and silicon carbide JFET radiation response.

Matus, Lawrence G.↗

Tensile and stress-rupture behavior of hafnium carbide dispersed molybdenum and tungsten base alloy wires

The tensile strain rate sensitivity and the stress-rupture strength of Mo-base and W-base alloy wires, 380 microns in diameter, were determined over the temperature range from 1200 K to 1600 K. Three molybdenum alloy wires; Mo + 1.1w/o hafnium carbide (MoHfC), Mo + 25w/o W + 1.1w/o hafnium carbide (MoHfC+25W) and Mo + 45w/o W + 1.1w/o hafnium carbide (MoHfC+45W), and a W + 0.4w/o hafnium carbide (WHfC) tungsten alloy wire were evaluated. The tensile strength of all wires studied was found to have a positive strain rate sensitivity. The strain rate dependency increased with increasing temperature and is associated with grain broadening of the initial fibrous structures. The hafnium carbide dispersed W-base and Mo-base alloys have superior tensile and stress-rupture properties than those without HfC. On a density compensated basis the MoHfC wires exhibit superior tensile and stress-rupture strengths to the WHfC wires up to approximately 1400 K. Addition of tungsten in the Mo-alloy wires was found to increase the long-term stress rupture strength at temperatures above 1400 K. Theoretical calculations indicate that the strength and ductility advantage of the HfC dispersed alloy wires is due to the resistance to recrystallization imparted by the dispersoid.

Yun, Hee Mann↗

Demonstration of Minimally Machined Honeycomb Silicon Carbide Mirrors

Honeycomb silicon carbide composite mirrors are made from a carbon fiber preform that is molded into a honeycomb shape using a rigid mold. The carbon fiber honeycomb is densified by using polymer infiltration pyrolysis, or through a reaction with liquid silicon. A chemical vapor deposit, or chemical vapor composite (CVC), process is used to deposit a polishable silicon or silicon carbide cladding on the honeycomb structure. Alternatively, the cladding may be replaced by a freestanding, replicated CVC SiC facesheet that is bonded to the honeycomb. The resulting carbon fiber-reinforced silicon carbide honeycomb structure is a ceramic matrix composite material with high stiffness and mechanical strength, high thermal conductivity, and low CTE (coefficient of thermal expansion). This innovation enables rapid, inexpensive manufacturing. The web thickness of the new material is less than 1 millimeter, and core geometries tailored. These parameters are based on precursor carbon-carbon honeycomb material made and patented by Ultracor. It is estimated at the time of this reporting that the HoneySiC(Trademark) will have a net production cost on the order of $38,000 per square meter. This includes an Ultracor raw material cost of about $97,000 per square meter, and a Trex silicon carbide deposition cost of $27,000 per square meter. Even at double this price, HoneySiC would beat NASA's goal of $100,000 per square meter. Cost savings are estimated to be 40 to 100 times that of current mirror technologies. The organic, rich prepreg material has a density of 56 kilograms per cubic meter. A charred carbon-carbon panel (volatile organics burnt off) has a density of 270 kilograms per cubic meter. Therefore, it is estimated that a HoneySiC panel would have a density of no more than 900 kilograms per cubic meter, which is about half that of beryllium and about onethird the density of bulk silicon carbide. It is also estimated that larger mirrors could be produced in a matter of weeks. Each cell is completely uniform, maintaining the shape of the inserted mandrel. Furthermore, the layup creates pressure that insures node bond strength. Each node is a composite laminate using only the inherent resin system to form the bond. This contrasts starkly with the other known method of producing composite honeycomb, in which individual corrugations are formed, cured, and then bonded together in a secondary process. By varying the size of the mandrels within the layup, varying degrees of density can be achieved. Typical sizes are 3/8 and 3/16 in. (approximately 10 and 5 millimeters). Cell sizes up to 1 in. (approximately 25 millimeters) have been manufactured. Similarly, the shape of the core can be altered for a flexible honeycomb structure.

Goodman, William↗

Carbide-based fuel assembly for thermal propulsion applications

Carbide-based fuel assembly includes outer structural member of ceramic matrix composite material (e.g., SiC—SiC composite), insulation layer of porous refractory ceramic material (e.g., zirconium carbide with open-cell foam structure or fibrous zirconium carbide), and interior structural member of refractory ceramic-graphite composite material (e.g., zirconium carbide-graphite or niobium carbide-graphite). Spacer structures between various layers provide a defined and controlled spacing relationship. A fuel element bundle positioned between support meshes includes a plurality of distributively arranged fuel elements or a solid, unitary fuel element with coolant channels, each having a fuel composition including high assay, low enriched uranium (HALEU). Fuel assemblies are distributively arranged in a moderator block and the upper end of the outer structural member is attached to a metallic inlet tube for hydrogen propellant and the lower end of the outer structural member is interfaced with a support plate, forming a nuclear thermal propulsion reactor.

Barringer, Eric A.↗

Silicon-carbide-on-insulator via photoelectrochemical etching

Silicon carbide on insulator is provided by bonding bulk silicon carbide to a substrate with an oxide-oxide fusion bond, followed by thinning the bulk silicon carbide as needed. A doping-selective etch for silicon carbide is used to improve thickness uniformity of the silicon carbide layer(s).

Lukin, Daniil M.↗

Syntheses, crystal structures and Si solubilities of new layered carbides Zr{sub 2}Al{sub 4}C{sub 5} and Zr{sub 3}Al{sub 4}C{sub 6}

Two types of new ternary carbides, Zr{sub 2}Al{sub 4}C{sub 5} and Zr{sub 3}Al{sub 4}C{sub 6}, have been synthesized and characterized by X-ray powder diffraction. The crystal structures were refined from laboratory X-ray powder diffraction data (CuK{alpha}{sub 1}) using the Rietveld method. These carbides form a homologous series with the general formula (ZrC){sub m}Al{sub 4}C{sub 3} (m=2 and 3). The crystal structures can be regarded as intergrowth structures where the Al{sub 4}C{sub 3}-type [Al{sub 4}C{sub 4}] layers are the same, while the NaCl-type [Zr{sub m}C{sub m+1}] layers increase in thickness with increasing m value. The new carbides are most probably the end members of continuous solid-solutions (ZrC){sub m}[Al{sub 4-x}Si{sub x}]C{sub 3} with 0{<=}x{<=}0.44. - Graphical abstract: Crystal structures of new layered carbides (ZrC){sub 2}Al{sub 4}C{sub 3} and (ZrC){sub 3}Al{sub 4}C{sub 3}.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Ni doping of semiconducting boron carbide

The wide band gap, temperature stability, high resistivity, and robustness of semiconducting boron carbide make it an attractive material for device applications. Undoped boron carbide is p type; Ni acts as a n-type dopant. Here we present the results of controlled doping of boron carbide with Ni on thin film samples grown using plasma enhanced chemical vapor deposition. The change in the dopant concentration within the thin film as a function of the dopant flow rate in the precursor gas mixture was confirmed by x-ray photoelectron spectroscopy measurements; with increasing dopant concentration, current-voltage (I-V) curves clearly establish the trend from p-type to n-type boron carbide.

36 MATERIALS SCIENCE↗

Surface Coating of Tungsten Carbide by Electric Exploding of Contact

Electric exploding of a tungsten carbide--cobalt material near-by high-speed steel surface forms on it a hardening coating. The essential structure properties of the formed coatings are determined by parameters of contact exploding electrode at the pulse current amplitude from above 106 A/cm2 and duration less than 10-4 s. The metallographic investigations of coating structures were done by microscope 'Neophot-24'. They have shown that the contact electric exploding caused the transfer of tungsten carbide and cobalt on the surface of high-speed steel. The breakdown of tungsten carbide--cobalt material took place during electrical exploding. The hardening layers of tungsten carbide and pure nanocrystalline tungsten have been formed upon the surface of high-speed steel as a result of electric exploding. Crystalline grains of tungsten have an almost spherical form and their characteristic size less than 400 nanometers. Micro hardness of the coating layers and high-speed steel structures was measured.

36 MATERIALS SCIENCE↗

Time-Dependent Stress Rupture Strength Degradation of Hi-Nicalon Fiber-Reinforced Silicon Carbide Composites at Intermediate Temperatures

The stress rupture strength of silicon carbide fiber-reinforced silicon carbide composites with a boron nitride fiber coating decreases with time within the intermediate temperature range of 700 to 950 degree Celsius. Various theories have been proposed to explain the cause of the time-dependent stress rupture strength. The objective of this paper is to investigate the relative significance of the various theories for the time-dependent strength of silicon carbide fiber-reinforced silicon carbide composites. This is achieved through the development of a numerically based progressive failure analysis routine and through the application of the routine to simulate the composite stress rupture tests. The progressive failure routine is a time-marching routine with an iterative loop between a probability of fiber survival equation and a force equilibrium equation within each time step. Failure of the composite is assumed to initiate near a matrix crack and the progression of fiber failures occurs by global load sharing. The probability of survival equation is derived from consideration of the strength of ceramic fibers with randomly occurring and slow growing flaws as well as the mechanical interaction between the fibers and matrix near a matrix crack. The force equilibrium equation follows from the global load sharing presumption. The results of progressive failure analyses of the composite tests suggest that the relationship between time and stress-rupture strength is attributed almost entirely to the slow flaw growth within the fibers. Although other mechanisms may be present, they appear to have only a minor influence on the observed time-dependent behavior.

Progressive Failure Analysis↗

Controlled synthesis of mesoporous carbon modified by tungsten carbides as an improved electrocatalyst support for the oxygen reduction reaction

Mesoporous carbon was modified with tungsten carbides by the carbothermal hydrogen reduction of a layer of chemisorbed 1:12 phosphotungstic anions (PW{sub 12}O{sub 40}{sup 3-}) on carbon surfaces. Depending on the temperature of carbothermal treatment, different tungsten species, i.e., W, W{sub 2}C, WC, were formed on the carbon matrix. No significant changes in both surface areas and mesostructures were observed during the formation of various tungsten species on carbon surfaces under high-temperature conditions. A uniform dispersion of Pt nanoparticles (1-6 nm) can be achieved via nanoconfinement on the surfaces of both mesoporouscarbon and tungsten carbide-modified mesoporous carbon. Pt nanoparticles supported on mesoporous carbons modified with tungsten carbide (Pt/WC-C) exhibit enhanced electrocatalytic activities relative to the control, in which mesoporous carbons without carbide modification were directly used as a support (Pt/C). In addition, both enhanced thermal stability and good electrochemical stability were observed for the Pt/WC-C electrocatalyst.

08 HYDROGEN↗

Thermal expansion of SiC at high pressure-temperature and implications for thermal convection in the deep interiors of carbide exoplanets

Recent astrophysical observations have shown that some stars have sufficiently high carbon-to-oxygen ratios and may host planets composed mainly of carbides instead of silicates and oxides. From the low thermal expansion of SiC at 1 bar, it can be inferred that the buoyancy force of thermal anomalies is much lower in the carbide planets than in the silicate planets. However, numerous studies have shown that high pressure in planetary interiors can fundamentally change the physical properties of materials. In this work we have measured the pressure-volume-temperature relations of two SiC polymorphs (3C and 6H) at pressures and temperatures up to 80 GPa and 1900 K and 65 GPa and 1920 K, respectively, in the laser-heated diamond anvil cell combined with synchrotron X-ray diffraction. We found no evidence of dissociations of these phases up to our maximum pressure condition, supporting the stability of SiC to 1900 km depth in Earth-size Si-rich carbide planets. Following the Mie-Grüneisen approach, we fit our data to the Birch-Murnaghan or the Vinet equations of state combined with the Debye approach. We found that the pressure-induced change in the thermal expansion parameter of SiC is much smaller than that of Mg silicate perovskite (bridgmanite). Our new measurements suggest that the thermal buoyancy force may be stronger in the deep interiors of Si-rich carbide exoplanets than in the “Earth-like” silicate planets.

58 GEOSCIENCES↗

Stability, Magnetism and Hardness of Iron Carbides from First-Principles Calculations

The stability, electronic structure, magnetism and hardness of iron carbides in eight different space groups were investigated by the first-principles calculations. The electron-ion interactions were modelled using the Vanderbilt ultra-soft pseudopotentials (USPP) and norm-conserving pseudopotentials (NCPP). Generalized gradient approximation (GGA) in the Perdew-Burke-Ernzerhof (PBE) formulation was used to describe the exchange-correlation energy. The calculated lattice parameters for USPP were in good agreement with experimental results. The formation enthalpy, cohesive energy and elastic constants revealed that with the exception of hex-Fe{sub 2}C, all Fe-C compounds were both thermodynamically and mechanically stable. Meanwhile, the iron carbides’ bulk and shear moduli were also calculated and compared. Furthermore, magnetic properties were studied and it was found that the average magnetic moment of Fe{sub 23}C{sub 6} (2.123 μ{sub B}) was the largest among these compounds, with a value close to that of pure α-Fe (2.24 μ{sub B}μ. As expected, hex-Fe{sub 2}C is a paramagnetic metal based on the obtained densities of states and partial densities of states. Furthermore, the magnetic behaviour of iron carbides with polymorphic transformation was almost identical. Finally, several semi-empirical methods were used for estimating the hardness of the iron carbides.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Precipitation Kinetics of M{sub 23}C{sub 6} Carbides in the Super304H Austenitic Heat-Resistant Steel

The precipitation kinetics of M{sub 23}C{sub 6} carbides in Super304H and TP304H steels were investigated using the selective-etching method, SEM backscattered electron images and Image-Pro-Plus 6.0 software. Precipitation–temperature–time (PTT) diagrams of M{sub 23}C{sub 6} carbides in the as-received Super304H (fine grains), coarsened Super304H (coarse grains) and TP304H (coarse grains) steels all show the typical C-shaped character with nose temperature range from 800 to 850 °C. Compared with the TP304H steel, the same trend is found of the PTT curve of M{sub 23}C{sub 6} carbides for both kinds of Super304H steels, but their start lines move to the right and finish lines to the left. The preferential formation of Nb(C,N) phase at grain boundaries in the Super304H steels inhibited the nucleation of M{sub 23}C{sub 6} carbides in the early stage of precipitation, causing the right shift of the start line of PTT curve. The main reason for the left shift of the finish line of the two Super304H steels was the quicker growing and coarsening rate of M{sub 23}C{sub 6} in the later precipitation stage due to their higher C content than in TP304H. For the difference in PPT curves between the two grain sizes of the Super304H steel, the lower diffusion rate of atoms in the coarse-grained Super304H steel may explain its righter finish line than the fine-grained counterpart, while the reason for its lefter start line is due to the higher solute segregation along coarse-grained boundaries.

36 MATERIALS SCIENCE↗

Formation of Lamellar Carbides in Alloy 617-HAZ and Their Role in the Impact Toughness of Alloy 617/9%Cr Dissimilar Welded Joint

The relationship between the microstructure and impact toughness, especially the formation of the lamellar carbides and its effect on the impact toughness of the heat-affected zone of Alloy 617 (Alloy 617-HAZ), was systematically investigated. Impact test was performed on Alloy 617/9%Cr dissimilar welded joints aged for different time at 620 °C. The results showed that the characteristic zones of the whole welded joint revealed decreased impact toughness with increasing the aging time. The impact energies in weld metal showed high stability despite the aging process, while the Alloy 617-HAZ for all testing specimens presented the lowest impact toughness with various aging time. Meanwhile, the mixed grains were found in the base metal (BM) and heat-affected zone of Alloy 617, together with the twins with different widths located in the interior of the large grains. The columnar and equiaxed grain zones appear alternately due to the multilayer and multi-pass welding technique. In particular, compared with Alloy 617-BM, coarsened and even lamellar carbides were observed in Alloy 617-HAZ. These special carbides can separate the grains and therefore result in the formation of intergranular fracture morphology in Alloy 617-HAZ. Besides, the microhardness distribution was tested with a proper load, and the results exhibited that the weld possessed the highest hardness for all specimens with various aging time. The higher microhardness in Alloy 617-HAZ compared with that in Alloy 617-BM was attributed to the high density of the dislocations, which could be detected by transmission electron microscope. As a result, the coarsened carbides aggregated in the grain boundaries to form the lamellar layer are deemed as the main factor to reduce the impact toughness in Alloy 617-HAZ.

36 MATERIALS SCIENCE↗

The Effect of Bainite Type on the Evolution of Carbide Constituent During an Accelerated Aging in Cr-Mo-V Steel

This paper aims to understand the effect of the type of bainite (i.e., the lower, the upper and the granular, developed by bainitic hardening at 550, 650 and 750 °C, respectively) on the evolution of carbide constituent due to a subsequent aging (at 700 °C for up to 500 h). The secondary carbides were identified by x-ray diffraction in the configurations of M{sub 3}C, M{sub 7}C{sub 3}, M{sub 23}C{sub 6}, M{sub 2}C, M{sub 6}C and MC (M=Fe, Cr, Mo, Mn and V), which varied with the time of aging. Despite that the three types of bainites shared similar constituent of carbides after the aging for 2-100 h, the constituent of the upper bainite (M{sub 7}C{sub 3} + M{sub 23}C{sub 6} + MC) was different from that of granular bainite and lower bainite (M{sub 7}C{sub 3} + M{sub 23}C{sub 6} + MC + M{sub 6}C) after the aging for 500 h. The concentration of the enrichment of alloying elements in ferrite matrix plays a dominant role in governing the precipitation of carbides in the aged steel.

36 MATERIALS SCIENCE↗

Role of Titanium, Carbon, Boron, and Zirconium in Carbide and Porosity Formation during Equiaxed Solidification of Nickel-Based Superalloys

This work analyses the effect of Ti in the MC carbide formation and also in the γ/γ´ eutectic promotion in two nickel-based alloys melted under vacuum conditions and solidified into ceramic molds. The role of boron, carbon and zirconium on the porosity level after solidification of both alloys was also investigated; since the alloys were vacuum melted, it is assumed that the observed porosity is due to micro-shrinkage. The chemical compositions for two alloys were: 20.2Cr-13.7Co-4.78Mo-1.19Al-0.69Ti-0.08C-2.34Fe for Alloy 1, and 20.5Cr-15.6Co5.03Mo-1.57Al-3.42Ti-0.15C-1.64Fe-0.076Zr-0.01%B for Alloy 2. Results showed a higher volume fraction of MC carbides and the γ/γ´ eutectic for the Alloy 2 with higher titanium content since this element is a carbide and γ/γ´ eutectic promoter. The porosity level in the Alloy 2, with higher amounts of carbon, boron and zirconium was considerably lower than that for the Alloy 1. These results are discussed in terms of different phenomena caused by the segregating effects of boron, carbon and zirconium towards the interdendritic regions and the formation of zirconium carbides that produce an expansion in volume when they are formed at the end of the solidification process.

36 MATERIALS SCIENCE↗

Increasing the catalytic stability by optimizing the formation of zeolite-supported Mo carbide species ex situ for methane dehydroaromatization

The synthesis of zeolite-supported Mo carbide species was investigated by testing different reduction/carburization conditions applied to a zeolite-supported Mo oxide catalyst, with the aim to find the optimized treatment conditions essential to form stable supported Mo carbide catalysts ex situ for application in methane dehydroaromatization reaction. Four types of treatment were performed and studied using temperature-programmed reduction and carburization profiles: (1) heating the catalyst in a reducing gas, H 2 , up to reaction temperature and switching to CH 4 ; (2) heating the catalyst in a reducing gas, H 2 , mixed with dilute CH 4 ; (3) heating the catalyst in CH 4 up to reaction temperature; and (4) heating the catalyst in an inert gas (commonly He) up to reaction temperature and then switching to CH 4 or to H 2 followed by CH 4 or to H 2 /CH 4 mixture. Each of these processes were stopped at intermediate points to analyze the phases that were present in order to identify the structural evolution of the supported Mo carbides that originate from the supported Mo oxides. Once the supported carbides were formed, they were quenched under the same gas mixture, and then they were each tested in methane dehydroaromatization via previous heating to reaction temperature in He flow. Despite all of them showing only presence of Mo 2 C species on HZSM-5, the catalytic properties were dramatically different. Catalysts treated in H 2 or CH 4 /H 2 showed remarkably higher stability. These catalysts reflected a higher Mo dispersion and thus exposure on the active surface.

36 MATERIALS SCIENCE↗