Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ASH”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 271 records · Page 15

Optimum concentration of fly ash nanoparticles to stabilize CO 2 foams for aquifer and soil remediation

Contamination caused by non-aqueous phase liquids (NAPLs) in aquifers and soil is an important challenge that requires effective remediation techniques. One potential approach is through the use of CO 2 foams to displace NAPLs from permeable media. CO 2 foams generated only by surfactants are not stable enough for the efficient removal of NAPLs contamination. This shortcoming may be alleviated via the use of nanoparticles (NPs)-surfactant mixtures as a stabilizing agent. This work focuses on the evaluation of the optimum concentration of fly ash nanoparticles for stabilizing CO 2 foam with the combined action of the surfactant. The performance of this foam is evaluated in remediating a contaminated 41 mm × 36 mm surrogate permeable medium in a microfluidic device. Mixtures of fly ash, a by-product of coal-burning power plants, and alpha-olefin sulfonate (AOS) and lauramidopropyl betaine (LAPB) surfactants are used to generate stable foams. The results show that a 1000 mg/L AOS-LAPB surfactant solution along with 1000 mg/L of fly ash NPs produces the best performance. Formation of deposits in the matrix is observed. These deposits, which are more prominent at higher NP concentrations, appear to adversely affect displacement, displacement efficiency and remediation of the medium. This study demonstrates that using fly ash nanoparticles and optimizing their concentration can effectively stabilize CO 2 foams and improve the displacement efficiency for aquifer and soil remediation.

54 ENVIRONMENTAL SCIENCES↗

Landfilled coal ash for carbon dioxide capture and its potential as a geopolymer binder for hazardous waste remediation

In this report, the legacy of global fossil fuel usage is not just the increase in global warming due to CO 2 production, but also the billions of tons of toxic coal ash disposed in landfills. This investigation evaluates the merits of using high-calcium landfilled coal fly ash of different disposal durations and granulated blast furnace (GBF) slag as primary raw materials for production of a new class of geopolymer binder. Processing of landfilled coal fly ash, GBF slag and supplementary raw materials into a geopolymer binder was accomplished by a simple, scalable milling process in the absence of heating under a carbon dioxide environment. The resultant geopolymer cement binders were tested for carbon dioxide uptake, compressive strength, and heavy metal stabilization. The geopolymer binder demonstrated a desired balance of carbon dioxide uptake, strength and safety. These results also indicate that the performance of the geopolymer binder depends on the landfill disposal age of the coal fly ash.

29 ENERGY PLANNING, POLICY, AND ECONOMY↗

Reassessing early-age strength development of high-volume fly ash concretes for precast buildings

Increasing beneficial use of fresh or landfilled fly ash as a replacement for Portland cement can be more challenging for the construction of precast buildings or similar applications requiring rapid strength development. Therefore, the framework presented in this paper aims to reassess high-volume fly ash concretes but in the context of facilitating more sustainable precast buildings. More specifically, the framework was used to characterize strength development of concrete mixes with a target minimum 24-hour compressive strength of 24.1 MPa (3500 psi), selected as an example strength development metric to demonstrate the framework, and comprised of 40% Class C, Class F, and landfilled (harvested) fly ash – as a high-volume replacement of Type III or Type IL cement. High-early strength was driven by optimized dosages of commercial grade gypsum and accelerating admixtures, in addition to optimal aggregate packing and mix proportioning strategies. Early-age mechanical properties including compressive strength, modulus of rupture, and modulus of elasticity were reevaluated within 24 hours of batching with respect to common precast production demands. Simple data analyses were then used to highlight cases where currently accepted design provisions for the aforementioned properties are either overly-conservative or unconservative with respect to test data. Furthermore, the framework and demonstration of example mixes presented herein aim to promote confidence for using larger fractions of fresh or landfilled fly ashes for precast buildings to further enhance environmental benefits without sacrificing pertinent early-age structural performance.

42 ENGINEERING↗

Characterization of MSWI bottom ashes towards utilization as glass raw material

The characterization of the bottom ashes produced by two Portuguese municipal solid waste incinerators (MSWI) was performed with the aim of assessing the feasibility of using this waste as raw material in the production of glass that can be further processed as glass-ceramics for application in construction. Density and particle size distribution measurements were carried out for physical characterization. Chemical characterization revealed that SiO{sub 2}, a network glass former oxide, was present in a relatively high content (52-58 wt%), indicating the suitability for this waste to be employed in the development of vitreous materials. CaO, Na{sub 2}O and K{sub 2}O, which act as fluxing agents, were present in various amounts (2-17 wt%) together with several other oxides normally present in ceramic and glass raw materials. Mineralogical characterization revealed that the main crystalline phases were quartz (SiO{sub 2}) and calcite (CaCO{sub 3}) and that minor amounts of different alkaline and alkaline-earth aluminosilicate phases were also present. Thermal characterization showed that the decomposition of the different compounds occurred up to 1100 deg. C and that total weight loss was <10 wt%. Heating both bottom ashes at 1400 deg. C for 2 h resulted in a melt with suitable viscosity to be poured into a mould, and homogeneous black-coloured glasses with a smooth shiny surface were obtained after cooling. The vitrified bottom ashes were totally amorphous as confirmed by X-ray diffraction. The results from the present experimental work indicate that the examined bottom ashes can be a potential material to melt and to obtain a glass that can be further processed as glass-ceramics to be applied in construction.

36 MATERIALS SCIENCE↗

Stabilization of heavy metals in MSWI fly ash using silica fume

Highlights: • The stabilization of heavy metals in MSWI fly ash was investigated. • The addition of silica fume effectively reduced the leaching of Pb and Cd. • The relation of solid phase transformation and leaching behavior of heavy metals was discussed. - Abstract: The objective of this work was to investigate the feasibility and effectiveness of silica fume on stabilizing heavy metals in municipal solid waste incineration (MSWI) fly ash. In addition to compressive strength measurements, hydrated pastes were characterized by X-ray diffraction (XRD), thermal-analyses (DTA/TG), and MAS NMR ({sup 27}Al and {sup 29}Si) techniques. It was found that silica fume additions could effectively reduce the leaching of toxic heavy metals. At the addition of 20% silica fume, leaching concentrations for Cu, Pb and Zn of the hydrated paste cured for 7 days decreased from 0.32 mg/L to 0.05 mg/L, 40.99 mg/L to 4.40 mg/L, and 6.96 mg/L to 0.21 mg/L compared with the MSWI fly ash. After curing for 135 days, Cd and Pb in the leachates were not detected, while Cu and Zn concentrations decreased to 0.02 mg/L and 0.03 mg/L. The speciation of Pb and Cd by the modified version of the European Community Bureau of Reference (BCR) extractions showed that these metals converted into more stable state in hydrated pastes of MSWI fly ash in the presence of silica fume. Although exchangeable and weak-acid soluble fractions of Cu and Zn increased with hydration time, silica fume addition of 10% can satisfy the requirement of detoxification for heavy metals investigated in terms of the identification standard of hazardous waste of China.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Accelerated carbonation using municipal solid waste incinerator bottom ash and cold-rolling wastewater: Performance evaluation and reaction kinetics

Highlights: • Carbonation was performed using CO{sub 2}, wastewater and bottom ash in a slurry reactor. • A maximum capture capacity of 102 g CO{sub 2} per kg BA was achieved at mild conditions. • A maximum carbonation conversion of MSWI-BA was predicted to be 95% by RSM. • The CO{sub 2} emission from Bali incinerator could be expected to reduce by 6480 ton/y. • The process energy consumption per ton CO{sub 2} captured was estimated to be 180 kW h. - Abstract: Accelerated carbonation of alkaline wastes including municipal solid waste incinerator bottom ash (MSWI-BA) and the cold-rolling wastewater (CRW) was investigated for carbon dioxide (CO{sub 2}) fixation under different operating conditions, i.e., reaction time, CO{sub 2} concentration, liquid-to-solid ratio, particle size, and CO{sub 2} flow rate. The MSWI-BA before and after carbonation process were analyzed by the thermogravimetry and differential scanning calorimetry, X-ray diffraction, and scanning electron microscopy equipped with energy dispersive X-ray spectroscopy. The MSWI-BA exhibits a high carbonation conversion of 90.7%, corresponding to a CO{sub 2} fixation capacity of 102 g per kg of ash. Meanwhile, the carbonation kinetics was evaluated by the shrinking core model. In addition, the effect of different operating parameters on carbonation conversion of MSWI-BA was statistically evaluated by response surface methodology (RSM) using experimental data to predict the maximum carbonation conversion. Furthermore, the amount of CO{sub 2} reduction and energy consumption for operating the proposed process in refuse incinerator were estimated. Capsule abstract: CO{sub 2} fixation process by alkaline wastes including bottom ash and cold-rolling wastewater was developed, which should be a viable method due to high conversion.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Multiple stirred-flow chamber assembly for simultaneous automatic fractionation of trace elements in fly ash samples using a multisyringe-based flow system

There is a current trend in automation of leaching tests for trace elements in solid matrixes by use of flow injection based column approaches. However, as a result of the downscaled dimensions of the analytical manifold and execution of a single extraction at a time, miniaturized flow-through column approaches have merely found applications for periodic investigations of trace element mobility in highly homogeneous environmental solids. A novel flow-based configuration capitalized on stirred-flow cell extraction is proposed in this work for simultaneous fractionation of trace elements in three solid wastes with no limitation of sample amount up to 1.0 g. A two-step sequential extraction scheme involving water and acetic acid (or acetic acid/acetate buffer) is utilized for accurate assessment of readily mobilizable fractions of trace elements in fly ash samples. The W automated extraction system features high tolerance to flow rates ({<=} 6 mL min{sup -1}) and, as opposed to operationally defined batchwise methods, the solid to liquid ratio is not a critical parameter for, determination of overall readily leachable trace elements provided that exhaustive extraction is ensured. Analytical performance of the dynamic extractor is evaluated for fractionation analysis of a real coal fly ash and BCR-176R fly ash certified reference material. No significant differences were found at the 0.05 significance level between summation of leached concentrations in each fraction plus residue and concentration values of BCR-176R, thus revealing the accuracy of the automated method. Overall extractable pools of trace metals in three samples are separated in less than 115 min, even for highly contaminated ashes, versus 18-24 h per fraction in equilibrium leaching tests. The multiple stirred-flow cell assembly is thus suitable for routine risk assessment studies of industrial solid byproduct.

01 COAL, LIGNITE, AND PEAT↗

Surface tension measurements of coal ash slags under reducing conditions at atmospheric pressure

The global demand for reduced CO{sub 2} emission from power plants can be answered by coal gasification techniques. To develop integrated gasification combined cycles that incorporate hot syngas cleaning facilities, detailed knowledge of the thermophysical properties of coal ashes is imperative. Currently, the surface tension of liquid coal ash slags in a reducing environment was studied by means of the sessile drop method. Three different algorithms were employed to analyze the acquired drop images. The slags under consideration were obtained from black and brown coals as well as from an experimental gasification reactor. Typically, a sharp surface tension decrease with temperature was found in the melting interval of the ashes. This was followed by a temperature range of smooth drop contours during which a slight rise of the surface tension could mostly be observed. Bubbles at the circumference of the drops started to appear when approaching the measurement temperature limit of 1550{sup o}C. With regard to the temperature regime of uncorrugated drop profiles, coal ash slags exhibited surface tension values between 400 and 700 mN/m. 32 refs., 9 figs., 1 tab.

01 COAL, LIGNITE, AND PEAT↗

Influence of different lignosulphonates on the properties of desulfurant sorbents prepared by hydration of Ca(OH){sub 2} and fly ash

The influence of different lignosulphonates used as additives on the physicochemical properties and desulfurization behavior Of Mixtures of Ca(OH){sub 2} and fly ash was investigated. Sorbents were prepared by the hydration of fly ash and Ca(OH){sub 2} at 3:1 or 5:3 fly ash /Ca(OH){sub 2} initial weight ratios for 7 or 15 h, at 90{sup o}C and atmospheric pressure. The lignosulphonates tested are trade named: Borrebond 55-L, Borrebond 55-S, Borresperse Cal-50, and Borresperse NaI-50. The properties characterized in the sorbents include Ca(OH){sub 2} conversion, BET surface area, and X-ray diffraction pattern. The sorbents were tested in a flue gas desulfurization reaction at low temperature. The effect of the additives on the desulfurant properties of the sorbents depends greatly on the amount of additive, with the type of lignosulphonate used being less relevant. A positive effect was found when the weight of the additive was 0.1 or 0.2% of the initial amount of solid raw materials. When additives are used in low amounts, a general low increase in the specific surface area of the sorbents is found; this structural property and the hydrophilic character of lignosulphonates present in the sorbents, that increase the retention of the water from the flue gas, can explain the higher amounts of SO{sub 2} retained per mol of calcium with these sorbents. When lignosulfonates are added at higher amounts to the slurry of fly ash and Ca(OH){sub 2}, their agglomerating properties prevail and the raw materials remain unreacted in the sorbents that exhibit low surface areas and are unable to capture SO{sub 2} on their surface.

01 COAL, LIGNITE, AND PEAT↗

Preparation of Functionally Graded Materials (FGMs) Using Coal Fly Ash and NiCr-Based Alloy Powder by Spark Plasma Sintering (SPS)

Functionally Graded Materials (FGMs) were prepared by spark plasma sintering (SPS) using coal fly ash and NiCr alloy powder. The coal fly ash was produced by the Misumi Coal Thermal Power Station (Chugoku Electric Power Co., Inc.), with 80 wt% nickel and 20 wt% chromium (Fukuda Metal Foil and Powder Co., Ltd.) used as source materials. The sintering temperature in the graphite die was 1000 deg. C. X-ray diffraction patterns of the sintered coal fly ash materials indicated that mullite (3Al{sub 2}O{sub 3}{center_dot}2SiO{sub 2}) and silica (SiO{sub 2}) phases were predominant. Direct joining of coal fly ash and NiCr causes fracture at the interface. This is due to the mismatch in the thermal expansion coefficients (CTE). A crack in the FGM was observed between the two layers with a CTE difference of over 4.86x10{sup -6} K{sup -1}, while a crack in the FGM was difficult to detect when the CTE difference was less than 2.77x10{sup -6} K{sup -1}.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Naturally Occurring Radionuclides of Ash Produced by Coal Combustion. The Case of the Kardia Mine in Northern Greece

West Macedonia Lignite Center (WMLC), located in Northwest Greece, releases into the atmosphere about 21,400 tons/year of fly ash through the stacks of four coal fired plants. The lignite ash contains naturally occurring radionuclides, which are deposited on the WMLC basin. This work investigates the natural radioactivity of twenty six ash samples, laboratory produced from combustion of lignite, which was sampled perpendicularly to the benches of the Kardia mine. The concentrations of radionuclides {sup 40}K, {sup 235}U, {sup 238}U, {sup 226}Ra, {sup 228}Ra and {sup 232}Th, were measured spectroscopically and found round one order of magnitude as high as those of lignite. Subsequently the Radionuclide Partitioning Coefficients of radionuclides were calculated and it was found that they are higher for {sup 232}Th, {sup 228}Ra and {sup 40}K, because the latter have closer affinity with the inorganic matrix of lignite. During combustion up to one third of the naturally occurring radioisotopes escape from the solid phase into the flue gases. With comparison to relative global data, the investigated ash has been found to have relatively high radioactivity, but the emissions of the WMLC radionuclides contribute only 0.03% to the mean annual absorbed dose.

01 COAL, LIGNITE, AND PEAT↗

Improving lithium-ion battery performances by adding fly ash from coal combustion on cathode film

A lithium battery is composed of anode, cathode and a separator. The performance of lithium battery is also influenced by the conductive material of cathode film. In this research, the use of fly ash from coal combustion as conductive enhancer for increasing the performances of lithium battery was investigated. Lithium iron phosphate (LiFePO{sub 4}) was used as the active material of cathode. The dry fly ash passed through 200 mesh screen, LiFePO{sub 4} and acethylene black (AB), polyvinylidene fluoride (PVDF) as a binder and N-methyl-2-pyrrolidone (NMP) as a solvent were mixed to form slurry. The slurry was then coated, dried and hot pressed to obtain the cathode film. The ratio of fly ash and AB were varied at the values of 1%, 2%, 3%, 4% and 5% while the other components were at constant. The anode film was casted with certain thickness and composition. The performance of battery lithium was examined by Eight Channel Battery Analyzer, the composition of the cathode film was examined by XRD (X-Ray Diffraction), and the structure and morphology of the anode film was analyzed by SEM (Scanning Electron Microscope). The composition, structure and morphology of cathode film was only different when fly ash added was 4% of AB or more. The addition of 2% of AB on cathode film gave the best performance of 81.712 mAh/g on charging and 79.412 mAh/g on discharging.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Fly ash based zeolitic pigments for application in anticorrosive paints

The purpose of this work is to evaluate the utilization of waste fly ash in anticorrosive paints. Zeolite NaY was synthesized from waste fly ash and subsequently modified by exchanging its nominal cation Na{sup +} with Mg{sup 2+} and Ca{sup 2+} ions. The metal ion exchanged zeolite was then used as anticorrosive zeolitic pigments in paints. The prepared zeolite NaY was characterized using X-Ray diffraction technique and Scanning electron microscopy. The size, shape and density of the prepared fly ash based pigments were determined by various techniques. The paints were prepared by using fly ash based zeolitic pigments in epoxy resin and the percentages of pigments used in paints were 2% and 5%. These paints were applied to the mild steel panels and the anticorrosive properties of the pigments were assessed by the electrochemical spectroscopy technique (EIS).

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Coal fly ash and phospho-gypsum mixture as an amendment to improve rice paddy soil fertility

Rice is a plant that requires high levels of silica (Si). As a silicate NOD source to rice, coal fly ash (hereafter, fly ash), which has an alkaline pH and high available silicate and boron (B) contents, was mixed with phosphor-gypsum (hereafter, gypsum, 50%, wt wt{sup -1}), a by-product from the production of phosphate fertilizer, to improve the fly ash limitation. Field experiments were carried out to evaluate the effect of the mixture on soil properties and rice (Oryza sativa) productivity in silt loam (SiL) and loamy sand (LS) soils to which 0 (FG 0), 20 (FG 20), 40 (FG 40), and 60 (FG 60) Mg ha{sup -1} were added. The mixture increased the amount of available silicate and exchangeable calcium (Ca) contents in the soils and the uptake of silicate by rice plant. The mixture did not result in accumulation of heavy metals in soil and an excessive uptake of heavy metals by the rice grain. The available boron content in soil increased with the mixture application levels up to 1.42 mg kg{sup -1} following the application of 60 Mg ha{sup -1} but did not show toxicity. The mixture increased significantly rice yield and showed the highest yields following the addition of 30-40 Mg ha{sup -1} in two soils. It is concluded that the fly ash and gypsum mixture could be a good source of inorganic soil amendments to restore the soil nutrient balance in rice paddy soil.

01 COAL, LIGNITE, AND PEAT↗

Chemical composition and some trace element contents in coals and coal ash from Tamnava-Zapadno Polje Coal Field, Serbia

The chemical compositions and trace element contents (Zn, Cu, Co, Cr, Ni, Pb, Cd, As, B, Hg, Sr, Se, Be, Ba, Mn, Th, V, U) in coal and coal ash samples from Tamnava-Zapadno Polje coal field in Serbia were studied. The coal from this field belongs to lignite. This high volatility coal has high moisture and low S contents, moderate ash yield, and high calorific value. The coal ash is abundant in alumosilicates. Many trace elements such as Ni > Cd > Cr > B > As > Cu > Co > Pb > V > Zn > Mn in the coal and Ni > Cr > As > B > Cu > Co = Pb > V > Zn > Mn in the coal ash are enriched in comparison with Clarke concentrations.

01 COAL, LIGNITE, AND PEAT↗

Utilize Cementitious High Carbon Fly Ash (CHCFA) to Stabilize Cold In-Place Recycled (CIR) Asphalt Pavement as Base Coarse

The purpose of this study was to evaluate the performance of cementitious high carbon fly ash (CHCFA) stabilized recycled asphalt pavement as a base course material in a real world setting. Three test road cells were built at MnROAD facility in Minnesota. These cells have the same asphalt surface layers, subbases, and subgrades, but three different base courses: conventional crushed aggregates, untreated recycled pavement materials (RPM), and CHCFA stabilized RPM materials. During and after the construction of the three cells, laboratory and field tests were carried out to characterize the material properties. The test results were used in the mechanistic-empirical pavement design guide (MEPDG) to predict the pavement performance. Based on the performance prediction, the life cycle analyses of cost, energy consumption, and greenhouse gasses were performed. The leaching impacts of these three types of base materials were compared. The laboratory and field tests showed that fly ash stabilized RPM had higher modulus than crushed aggregate and RPM did. Based on the MEPDG performance prediction, the service life of the Cell 79 containing fly ash stabilized RPM, is 23.5 years, which is about twice the service life (11 years) of the Cell 77 with RPM base, and about three times the service life (7.5 years) of the Cell 78 with crushed aggregate base. The life cycle analysis indicated that the usage of the fly ash stabilized RPM as the base of the flexible pavement can significantly reduce the life cycle cost, the energy consumption, the greenhouse gases emission. Concentrations of many trace elements, particularly those with relatively low water quality standards, diminish over time as water flows through the pavement profile. For many elements, concentrations below US water drinking water quality standards are attained at the bottom of the pavement profile within 2-4 pore volumes of flow.

42 ENGINEERING↗

High Yield, Economical and Environmentally Benign Production of Rare Earth Elements from Coal Ash [Abstract]

Fly ash stored in landfills and ponds across the United States is an attractive, abundant domestic resource for the cost-effective recovery of rare earth elements (REE) and other critical minerals (CM). Physical Sciences Inc. (PSI) and its team members, Winner Water Services (WWS) and University of Kentucky/Center for Applied Energy Research (UK/CAER) successfully executed a multiphase program that developed and demonstrated pilot plant operations for cost-effective and environmentally-friendly production of rare earth element oxide (REO) concentrates, and the critical minerals scandium and aluminum (in the forms of salts or oxide products). We constructed and operated a sub-scale (0.5 kg/day) micropilot facility to demonstrate the key physical and chemical processing operations, predict yields, and troubleshoot process bottlenecks. The project team then designed, constructed and operated two decoupled pilot plant operations: (1) an operational pilot plant for physical separation processes with a capacity of 0.4 metric tons per day (tpd) where we optimized processes to produce selected ash fractions as the feedstock for chemical processing as well as valuable byproducts such as cement substitute, cenospheres, magnetic ash and secondary fuel carbon, and (2) an operational pilot plant for chemical processing with a capacity of 0.5 tpd that developed optimized processes for the production of: (a) REO concentrates, (b) critical minerals recovery (Sc, Al), and (c) beneficiated ash as valuable byproduct suitable for cement applications.

01 COAL, LIGNITE, AND PEAT↗

Nondestructive X-ray Inspection of Thermal Damage, Soot and Ash Distributions in Diesel Particulate Filters

We describe novel results of ongoing research at 3DX-RAY Ltd and Oak Ridge National Laboratory using new, commercially available, nondestructive x-ray techniques to make engineering measurements of diesel particulate filters (DPF). Nondestructive x-ray imaging and data-analysis techniques were developed to detect and visualize the small density changes corresponding to the addition of substances such as soot and ash to DPF monoliths. The usefulness of this technique was explored through the analysis of field-aged samples, accelerated-aged samples, and the synthetic addition of ash and soot to clean DPF samples. We demonstrate the ability to visualize and measure flaws in substrates and quantify the distribution of ash and soot within the DPF. We also show that the technology is sensitive enough for evaluations of soot and ash distribution and thermal damage without removing the DPF from its metal casing.

33 ADVANCED PROPULSION SYSTEMS↗