Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “weight loss”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 253 records · Page 14

Development of polyphenylquinoxaline graphite composites.

The potential of polyphenylquinoxaline (PPQ)/graphite composites to serve as structural material at 316 C (600 F) has been demonstrated using a block copolymer, BICo(1:3), PPQ derivative. Initially, 13 polyphenylquinoxalines were evaluated. From this work, four candidate polymers were selected for preliminary evaluation as matrices for HMS graphite fiber reinforced composites. The preliminary composite evaluation enabled selection of one of the four polymers for advanced composite preparation and testing. Using an experimentally established cure schedule for each of the four polymers, preliminary laminates of 50% resin volume content, prepared without postcure, were tested for flexure strength and modulus, interlaminar shear strength (short beam), tensile strength, and modulus of ambient temperature. The potential of PPQ/graphite laminates to serve as short term structural materials at temperatures up to 371 C (700 F) was demonstrated through weight loss experiments.

Shdo, J. G.↗

Additional thermal fatigue data on nickel and cobalt-base superalloys

The fluidized bed technique was used to measure the relative thermal fatigue resistance of 21 superalloys: B1900, B1900 DID, IN-100, MAR-M 200, Udimet 700 wrought and cast, NX-188, WAZ-20, TAZ-8A, M22, IN 713C, IN 738, IN 162, MAR-M 509, Rene 80, RBH, NASA VI A, TD-NiCr, MAR-M 302, WI-52, and X-40. IN-100, MAR-M 200, NX-188, WAZ-20 and TAZ-8A were also tested in the directionally solidified form. B1900, B1900 DID, IN-100, MAR-M200, Udimet 700, NX-188, WAZ-20 and TAZ-8A were tested with surface protection. Among the 36 variations of composition, solidification method, and surface protection the cycles to cracking differed by 2 to 3 orders of magnitude. Some alloys suffered serious weight losses and oxidation. Previous fluidized bed thermal fatigue data on some of these alloys were reported in N71-10027. Thermal fatigue data, oxidation, and dimensional changes are reported in N73-30507. Metallographic and hardness data are given in this report.

Howes, M. A. H.↗

Flame retardant polyphosphazenes

Six polyphosphazene compositions were prepared by reaction of three bis-tertiary phosphines with two phenyl-s-triazine derived diazides. All six polyphosphazenes produced were completely characterized, four of them were furthermore subjected to isothermal gravimetric analysis, smoke density measurements, flammability and oxidative thermal degradation testing. The results of the characterization studies indicate that only low molecular weight oligomers, possibly of a cyclic structure, were obtained in the polymerization reactions. Despite this, however, two of the materials showed no weight loss after 96 hr at 200 C, one did not autoignite at 500 C in air, and all four self extinguished when exposed to a flame as soon as contact between flame and resin was lost. The only toxic decomposition products to be concerned about were found to be hydrogen cyanide and benzene. Under the conditions employed it was proven, however, that the quantities of toxic products are greatly reduced if no ignition takes place, e.g., if thermal decomposition proceeds at a sufficiently low rate.

Paciorek, K. L.↗

Caloric balance during simulated and actual space flight

The in-flight caloric intakes of all Apollo astronauts are examined and shown to average about 25 kcal per kg per day. Measurement of weight changes following recovery indicates that about 0.15 kg of fat was lost per man per day in-flight for an average deficit of about 19 kcal per kg per day. Measurement of the caloric intake of astronauts under ground-based conditions and during hypobaric exposure indicated a caloric requirement which was not significantly different from the in-flight requirement adjusted for weight loss. Partial metabolic balance data and measurements of bone loss and body volume revealed that protein and mineral losses also occurred to an extent which would reduce the size of estimated in-flight caloric deficits.

Rambaut, P. C.↗

Modular liquid-cooled helmet liner for thermal comfort

A modular liquid-cooled helmet liner made of eight form-fitting neoprene patches was constructed. The liner was integrated into the sweatband of an Army SPH-4 helicopter aircrew helmet. This assembly was tested on four subjects seated in a hot (47 C), humid (40%) environment. Results indicate a marked reduction in the rate of increase of physiological body functions. Rectal temperature, weight loss, heart rate, and strain indices are all reduced to approximately 50% of uncooled levels. The cooling liner removed from 10% to 30% of total metabolic heat produced. This study also demonstrated the technical feasilibity of using a cooling liner in conjunction with a standard hard helmet. Potential applications of the cooling liner in thermally stressful environments are numerous, notably for helicopter and other aircrews.

Williams, B. A.↗

Development of high temperature resistant graphite fiber coupling agents

Surface treatments were investigated as potential coupling agents to improve the elevated temperature shear strength retention of polyimide/graphite and polyphenylquinoxaline/graphite composites. The potential coupling agents were evaluated by fiber strand tensile tests, fiber and composite weight losses at 533 and 588K, and by interlaminar shear strength retention at 533 and 588K. The two surface treatments selected for more extensive evaluation were a coating of Ventromer T-1, a complex organometallic reaction product of titanium tetrachloride and trimethyl borate, and a polyphenylquinoxaline (PPQ) sizing which was pyrolyzed in nitrogen to form a carbonaceous layer on the fiber. Pyrolyzed polyphenylquinoxaline is a satisfactory coupling agent for polyimide/Thornel 300 graphite fiber composites. During 1000 hours aging at 588K such composites lose a little over half their transverse tensile strength, and suffer a slight loss in flexural modulus. No degradation of flexural strength or interlaminar shear strength occured during 1000 hours aging at 588K. None of the coupling agents examined had a markedly beneficial effect with polyphenylquinoxaline composites.

Griffin, R. N.↗

Effects of multifunctional crosslinking agents on the thermomechanical properties of polyimide films

Three polyfunctional amines were synthesized. Polyimide films containing varying amounts of the amine crosslinking agents were prepared. Their thermomechanical properties were compared with those of control film samples prepared from difunctional amines. The effect of crosslink density on isothermal weight loss, polymer softening, and glass transition temperature is discussed.

Delvigs, P.↗

Effect of thermal cycling in a Mach 0.3 burner rig on properties and structure of directionally solidified gamma/gamma prime - delta eutectic

Tensile and stress rupture properties at 1040 C of a thermally cycled gamma/gamma prime - delta eutectic were essentially equivalent to the as-grown properties. Tensile strength and rupture life at 760 C appeared to decrease slightly by thermal cycling. Thermal cycling resulted in gamma prime coarsening and Widmanstatten delta precipitation in the gamma phase. An unidentified precipitate, presumably gamma prime, was observed within the delta phase. The eutectic alloy exhibited a high rate of oxidation-erosion weight loss during thermal cycling in the Mach 0.3 burner rig.

Gray, H. R.↗

Molecular fluxes from a spacecraft measured with quartz microbalances

A technique has been developed to obtain a characterization of the self-generated environment of a spacecraft and its variation with time, angular position, and distance. The density, pressure, outgassing flux, total weight loss, and other important parameters were obtained from data provided by two mass measuring crystal microbalances, mounted back to back, at a distance of 1 m from the spacecraft equivalent surface. The strongest source appeared to be caused by a material diffusion process which produced a directional density at 1 m distance of about 160 billion molecules per cu cm after 1 h in vacuum and decayed to 1.6 billion molecules per cu cm after 200 h. Self-contamination of the spacecraft was equivalent to that which occurs in a 300-km altitude orbit.

Scialdone, J. J.↗

Intumescent coating modeling

A thermal response mathematical model for an intumescent coating system is developed. The model predicts indepth temperature profiles of the solid as a function of the fundamental kinetic, mass, and heat-transfer properties of the original coating system. In the model, swelling is based on an empirical function of the paint's weight loss. The model is used to describe the effectiveness of the coating for thermal protection. Using the thermal response time at the backface of the material as a criterion, a sensitivity analysis is made with respect to variation in individual properties, such as total expansion, to provide a guide for designing improved intumescing agents. The sensitivity analysis shows that total expansion and rate of expansion, along with other material properties, are important parameters for providing thermal protection. Finally, backface temperature histories are predicted and compared to experimental data obtained from a representative fire environment. Predicted temperatures agree within a maximum error of plus or minus 20%.

Cagliostro, D. E.↗

Weightlessness - A case history

A review of the average bodily systems functioning aboard Skylab II after 20 days of weightlessness is presented. Condition of eyes, ears, nose and throat, gastrointestinal tract, vestibular organs, cardiovascular system, musculoskeletal system, sleep, general appearance, skin, abdomen, and extremities is summarized. The general health of the crewmen is good, although there are some slight anomalies, such as weight loss, dry skin, nasal speech, and paresthesia of the soles of the feet.

Kerwin, J. P.↗

Endocrine responses in long-duration manned space flight

Endocrine measurements to assess the physiological cost of the combined stresses of space flight are considered from two aspects. First, fluid and electrolyte balance are correlated with weight loss, changes in the excretion of aldosterone and vasopressin and fluid compartments. The second area involves estimation of the physiological cost of maintaining a given level of performance during space flight by analysis of urinary catecholamines and cortisol. Inter-individual variability is demonstrated for most experimental indices measured. The measured changes are consistent with the hypothesis that a relative increase in thoracic blood volume upon transition to the zero-gravity environment can be interpreted as a true volume expansion resulting in an osmotic diuresis.

Leach, C. S.↗

Sublimation behavior of silicon nitride /Si3N4/ coated silicon germanium /SiGe/ unicouples

For the Multi-Hundred Watt (MHW) Radioisotope Thermoelectric Generator (RTG), the silicon germanium unicouples are coated with silicon nitride to minimize degradation mechanisms which are directly attributable to material sublimation effects. A program is under way to determine the effective vapor suppression of this coating as a function of temperature and gas environment. The results of weight loss experiments, using Si3N4 coated hot shoes (SiMo), operating over a temperature range from 900 C to 1200 C, are analyzed and discussed. These experiments were conducted both in high vacuum and at different pressures of carbon monoxide (CO) to determine its effect on the coating. Although the results show a favorable vapor suppression at all operating temperatures, the pressure of the CO and the thickness of the coating have a decided effect on the useful lifetime of the coating.

Stapfer, G.↗

Effects of multifunctional crosslinking agents on the thermomechanical properties of polyimide films

The potential of high temperature resistant polymers such as polyimides (PI) and polyphenylquinoxalines (PPQ) as matrix resins in fiber-reinforced composites has not been fully realized to date. One of the problems associated with these resins is that they exhibit creep, or thermoplastic yielding under load at temperatures approaching 316 C (600 F). The purpose of this investigation was to further reduce thermoplastic behavior of polyimide resins by substituting a controlled amount of the diamine monomer with crosslinking agents having a higher amine functionality. The knowledge gained from a study of the thermomechanical properties of the crosslinked resins would then be used in the fabrication of fiber-reinforced polyimide composites. This report describes the synthesis and characterization of three new polyfunctional amines. Polyimide films containing varying amounts of the cross-linking agents were prepared, and their properties compared with those of control samples prepared with difunctional amines. The effect of crosslink density on isothermal weight loss, polymer softening, and glass transition temperatures is discussed.

Delvigs, P.↗

High gas velocity oxidation and hot corrosion testing of oxide dispersion-strengthened nickel-base alloys

Several oxide dispersion strengthened (ODS) nickel-base alloys were tested in high velocity gases for cyclic oxidation resistance at temperatures to 1200 C and times to 500 hours and for hot corrosion resistance at 900 C for 200 hours. Nickel-chromium-aluminum ODS alloys were found to have superior resistance to oxidation and hot corrosion when compared to bare and coated nickel-chromium ODS alloys. The best of the alloys tested had compositions of nickel - 15.5 to 16 weight percent chromium with aluminum weight percents between 4.5 and 5.0. All of the nickel-chromium-aluminum ODS materials experienced small weight losses (less than 16 mg/sq cm).

Deadmore, D. L.↗

Explosive and pyrotechnic aging demonstration

The survivability was experimentally verified of fine selected explosive and pyrotechnic propellant materials when subjected to sterilization, and prolonged exposure to space environments. This verification included thermal characterization, sterilization heat cycling, sublimation measurements, isothermal decomposition measurements, and accelerated aging at a preselected elevated temperature. Temperatures chosen for sublimation and isothermal decomposition measurements were those in which the decomposition processess occurring would be the same as those taking place in real-time aging. The elevated temperature selected (84 C) for accelerated aging was based upon the parameters calculated from the kinetic data obtained in the isothermal measurement tests and was such that one month of accelerated aging in the laboratory approximated one year of real-time aging at 66 C. Results indicate that HNS-IIA, pure PbN6, KDNBF, and Zr/KC10 are capable of withstanding sterilization. The accelerated aging tests indicated that unsterilized HNS-IIA and Zr/KC104 can withstand the 10 year, elevated temperature exposure, pure PbN6 and KDNBF exhibit small weight losses (less than 2 percent) and B/KC104 exhibits significant changes in its thermal characteristics. Accelerated aging tests after sterilization indicated that only HNS-IIA exhibited high stability.

Rouch, L. L., Jr.↗

Thermogravimetric study of reduction of oxides present in oxidized nickel-base alloy powders

Carbon, hydrogen, and hydrogen plus carbon reduction of three oxidized nickel-base alloy powders (a solid solution strengthened alloy both with and without the gamma prime formers aluminum and titanium and the solid solution strengthened alloy NiCrAlY) were evaluated by thermogravimetry. Hydrogen and hydrogen plus carbon were completely effective in reducing an alloy containing chromium, columbium, tantalum, molybdenum, and tungsten. However, with aluminum and titanium present the reduction was limited to a weight loss of about 81 percent. Carbon alone was not effective in reducing any of the alloys, and none of the reducing conditions were effective for use with NiCrAlY.

Herbell, T. P.↗

Development of polyphenylquinoxaline graphite composites

Six polyphenylquinoxalines (PPQ) containing pendant cyano (CN) groups were synthesized. The polymers were characterized in terms of inherent viscosity, glass transition temperature, softening temperature and weight loss due to aging in air at 316 C (600 F). The potential for crosslinking PPQs by trimerization of pendant CN groups was investigated. A polymer derived from 1 mole 3,3,4,4 -tetraaminobenzophenone, .2 mole p-bis(p -cyanophenoxyphenylglyoxalyl)benzene and .8 mole p-bis(phenylglyoxalyl)benzene was selected for more extensive characterization in HM-S graphite fiber-reinforced composites. Mechanical properties were determined using composites made from HM-S fiber and polymer and composites made from HM-S fiber, polymer and a potential CN group trimerization catalyst. Composite mechanical properties, inter-laminar shear strength and flexure properties, were determined over the temperature range of +21 C to 316 C.

Shdo, J. D.↗